Recent Trends of Friction Stir Welding of Titanium (타이타늄 소재 마찰교반용접 기술 동향)

  • Chun, Chang-Keun;Kim, Sung-Wook;Kim, Heung-Joo;Chang, Woong-Seong;Noh, Joong-Suk
    • Journal of Welding and Joining
    • /
    • v.31 no.2
    • /
    • pp.16-20
    • /
    • 2013
  • Titanium and its alloys have been widely using in the various field of industry application due to high corrosion resistant properties and mechanical properties. Titanium is highly reactive in the high temperature state and the formation of titanium oxide and porosities in the nuggets of fusion welding will results in the degradation of the mechanical properties. For this reason the studies of friction stir welding for titanium have been investigated recently. The FSW zones of titanium were classified by the weld nugget (WN), the linear transition boundary (TB) and the heat affected zone (HAZ). The WN along with titanium parent was characterized by the presence of twins and dislocations. The average grain size and hardness of WN has been changed according to heat input. The grain refinement resulted from the FSW increased the hardness in the stir zone. Sound dissimilar joints between SUS 304 and CP-Ti were achieved using an advancing speed of 50 mm/min and rotation speeds in the range of 700-1100 rpm. Aluminum 1060 and titanium alloy Ti-6Al-4V plates were lap joined by friction stir welding, hence the ultimate tensile shear strength of joint reached 100% of Al 1060. Mg alloy and Ti were successfully butt joined by inserting a probe into the Mg alloy plate with slightly offsetting. But Ti-Al intermetallic compound layers formed at the interface of these joints.

A Experiment Study of Torch Distance on Automated Tandem GMA Welding System (탄뎀 가스메탈아크 용접의 토치 극간거리에 관한 실험적 연구)

  • Lee, Ji-Hye;Kim, Ill-Soo;Jung, Seong-Myeong;Lee, Jong-Pyo;Kim, Young-Su;Park, Min-Ho
    • Journal of Welding and Joining
    • /
    • v.30 no.6
    • /
    • pp.49-55
    • /
    • 2012
  • The tandem welding process is one of the most efficient welding processes widely used in material joining technique such as manufacturing of strong and durable structures. It facilitates high rate of joint filling with little increase in the overall rate of heat input due to the simultaneous deposition from two electrode wires. The two electrodes in tandem welding process helps in high-efficiency and high productive of welding process. In this study a automated tandem welding system is developed to determine the correlation between cathode and anode and compared with current ratio of the two electrode torch. Three different inter-electrode distances were chosen, 25mm, 35mm and 45mm to perform the experiment with three different current ratio. From the experiment results, the current ratio between two torch has a large impact on width, height and depth of penetration. In addition, a stable bead geometry is obtained when inter-electrode distance is 35mm.

Effects of GTAW Pulse Condition on Penetration, Discoloration and Bending Property for Titanium Tube (GTAW 펄스 용접 조건에 따른 타이타늄 정밀관의 용입, 변색 및 굽힘특성)

  • Min, Seonghwan;An, Sungyong;Park, Jitae;Park, Youngdo;Kang, Namhyun
    • Journal of Welding and Joining
    • /
    • v.32 no.6
    • /
    • pp.47-55
    • /
    • 2014
  • The purpose of the study is to produce a mechanically improved weld and minimum variation of color through comparing unpulsed and pulsed GTAW (Gas Tungsten Arc Welding) for pure titanium (CP grade7) tube. Pulsed GTAW using 60 A peak current and 20 A background current (1:9) achieved the wider window of welding conditions having part and full penetration without burn-through than the case of unpulsed GTAW. Moreover, the pulsed welding reduced a discoloration on the back bead of the weld and the size of microstructures (basket weave and serrated ${\alpha}$). That is because the pulsed welding has it's a low heat input and severe weld flow induced from electric current variation. Furthermore, the pulsed welding improved the bending property of the welded Ti tube. The enhanced bending property for the pulsed GTAW was due to the insignificant discoloration on the weld surface with maintaining the metal polish.

A study on the stress and strain during welding of plate-to-pipe joint (평판-관 구조물 용접시 발생하는 응력 및 변형율에 관한 연구)

  • 나석주;김형완
    • Journal of Welding and Joining
    • /
    • v.4 no.2
    • /
    • pp.30-39
    • /
    • 1986
  • In manufacturing of pipe walls for boiler units, distortion can result in pipe-web-pipe joints from the nonuniform expansion and contraction of the weld metal and the adjacent base metal during heating and cooling cycle of the welding process. In this study, the stresses and strains during longitudinal welding of the plate-to-pipe joint were investigated. Using the method of successive elastic solution, longitudinal stresses and strains during and after welding were calculated from the information of temperature distributions obtained by Rosenthal's equations. In order to confirm the validity of the numerical results, the temperature and residual stress distributions were measured and compared with the calculated results. In spite of some assumptions, the one-dimensional analytical results of residual stresses were in fairly good agreement with the experimental ones. The residual stresses due to welding of plate-to-pipe joints are tensile near the weld line and compressive in the base metal as in the welding of plates. the amount and distribution of residual stresses were deeply dependent on the heat input ratio of the plate and pipe.

  • PDF

Effects of Reduction Groove Angle on Strength Characteristics of FCAW Weldment (FCAW 용접부 개선각 축소에 따른 강도특성)

  • Lee, Sang-Chul;Jo, Sung Woo;Yang, Jong Soo;Choi, Kyu Won;Seo, Jung Kwan
    • Journal of the Society of Naval Architects of Korea
    • /
    • v.53 no.6
    • /
    • pp.473-481
    • /
    • 2016
  • Thick plate is currently widely used in shipbuilding due to the increasing of size of ships. However, its use has increased welding groove angles and volume. The welder's technique must be good enough to improve productivity while preventing defects. Generally, the groove angle can be reduced to less than a flux-cored arc welding (FCAW) machine setting of $35{\pm}5^{\circ}$, requiring fewer welding passes while maintaining high productivity and reduced heat input. Therefore, welding technique can be prevented by improved mechanical properties and welding deformation. Welding defects such as lack of fusion (LF), lack of penetration (LP) and hot cracking should be considered when reducing the groove angle for related applications. In this study, a welding groove angle of $25{\pm}5^{\circ}$ is verified as suitable for FCAW design and fabrication. The experimental results confirm the effects on the strength characteristics of FCAW weldment when reducing groove angle to improve the productivity of shipbuilding industries.

Resistance, electron- and laser-beam welding of zirconium alloys for nuclear applications: A review

  • Slobodyan, Mikhail
    • Nuclear Engineering and Technology
    • /
    • v.53 no.4
    • /
    • pp.1049-1078
    • /
    • 2021
  • The review summarizes the published data on the widely applied electron-beam, laser-beam, as well as resistance upset, projection, and spot welding of zirconium alloys for nuclear applications. It provides the results of their analysis to identify common patterns in this area. Great attention has been paid to the quality requirements, the edge preparation, up-to-date equipment, process parameters, as well as post-weld treatment and processing. Also, quality control and weld repair methods have been mentioned. Finally, conclusions have been drawn about a significant gap between the capabilities of advanced welding equipment to control the microstructure and, accordingly, the properties of welded joints of the zirconium alloys and existing algorithms that enable to realize them in the nuclear industry. Considering the ever-increasing demands on the high-burnup accident tolerant nuclear fuel assemblies, great efforts should be focused on the improving the welding procedures by implementing predefined heat input cycles. However, a lot of research is required, since the number of possible combinations of the zirconium alloys, designs and dimensions of the joints dramatically exceeds the quantity of published results on the effect of the welding parameters on the properties of the welds.

ENHANCING TIG WELD PERFORMANCE THROUGH FLUX APPLICATION ATIG AND FBTIG PROCESSES

  • Marya, S.
    • Proceedings of the KWS Conference
    • /
    • 2002.10a
    • /
    • pp.70-75
    • /
    • 2002
  • The penetration potential of TIG welding in one single run is limited, though the process itself generates high quality welds with good weld cosmetics. This is one of the main reasons, which has contributed to its development in high duty applications such as those encountered in aeronautical, aerospace, nuclear & power plant applications. For these applications, stainless steels, titanium k nickel based alloys are most often used. As these materials remain very sensible to weld heat input k atmospheric pollution, stringent processing conditions are imposed. For example welding of titanium alloys requires argon shielding of weld zone and for 5 mm thick plates multi-pass runs & filler additions are required. This multi-run operation not only raises the welding cost, but also increases defect risks. In recent years, extensive interest has been raised by the possibility to increase weld penetrations through flux applications & the process is designated ATIG-activated TIG, or FBTIG-flux bounded TIG. The improved welding performance of such flux assisted TIG is related to arc constriction and surface tension effects on weld pool. The research work by authors has lead to the formulation of welding fluxes for stainless steels k titanium alloys with TIG Process. These fluxes are now commercialized & some applications in industry have already been carried out. FBTIG for aluminum has been proposed with silica application for AC mode TIG welding. The paper highlights the fundamentals of flux role in TIG welding and illustrates some industrial applications.

  • PDF

The behavior of boron segregation according to heat input in the weld CGHAZ of low alloyed steel (용접 입열량에 따른 저합금강 용접부 CGHAZ의 보론 편석거동 분석)

  • Kim, Sang-Hoon;Lee, Jong-Ho;Lee, Kyung-Sub;Hwang, Byoung-Chul;Lee, Chang-Gil;Lee, Chang-Hee
    • Proceedings of the KWS Conference
    • /
    • 2009.11a
    • /
    • pp.60-60
    • /
    • 2009
  • 본 연구는 보론이 첨가된 저합금강 용접 열영향부에서의 보론 편석 거동 연구를 위해 보론이 10ppm 첨가된 저합금강을 이용하여 다양한 용접 입열량 및 외부 응력에 따른 용접부 CGHAZ의 보론 편석거동을 분석하였다. 이를 위해 Gleeble 시스템을 이용하여 다양한 입열량에 따른 CGHAZ를 열 및 열-응력 사이클을 통하여 재현하였다. 재현된 시편의 미세조직은 OM을 통하여 분석하고, 보론의 편석거동을 SIMS와 PTA 분석법을 통하여 분석하였다. 그 결과 입열량에 따른 보론의 편석 거동은 최초 입열량이 증가함에 따라 보론의 편석이 증가하다가 다시 감소하였는데 이는 비평형 편석 후 고온에서 유지시간이 길어짐에 따라 back diffusion 발생에 따른 영향으로 판단된다. 또한 외부 응력에 의한 보론 편석 거동 분석 결과, 용접 열 사이클 중 작용하는 외부 응력에 의해 결정립계 편석 감소하였는데 이는 외부 응력에 의한 오스테나이트 결정립 크기 감소에 따른 결정립계 증가의 영향으로 판단된다.

  • PDF

Effect of the Groove Shape of Ultra Thick Box-Column with Center Segregation under High Heat Input for Corner Welding (중심 편석층이 있는 극후판 박스-칼럼의 대입열 코너이음 용접시 그루브 형상의 영향)

  • 최원규;이종봉;권영두;구남서
    • Journal of Ocean Engineering and Technology
    • /
    • v.16 no.2
    • /
    • pp.72-79
    • /
    • 2002
  • In this study, time-dependent distributions of temperature and stresses, in the box-column welded from ultra thick plates with center segregation, has been analyzed by the commercial finite element package SYSWELD+, for several types and angles of groove. The major points of investigation are the optimum type and angle of groove that minimize weld stress specially at the center segregation, as well as temperature distribution, residual stresses and changes in the mechanical properties. The results can be summarized as follows; 1) Generally the thermal cycle at the root of groove exhibits relatively rapid cooling pattern, however, most of the other part weldment have a slow cooling pattern in all groove types. 2) Most of the micro-structures of weldment are composed of ferrite and pearlite, meanwhile we could find martensite and bainite locally a the root of the groove. 3) Optimum groove type for high heat input welding of box-column corner is a double groove type, and the optimum angle for the groove is 30~$45^{\circ}$ that minimize deformation and weld stress at the center segregation.

Optimization for Underwater Welding of Marine Steel Plates (선박용 강판의 수중 용접 최적화에 관한 연구)

  • 오세규
    • Journal of the Korean Society of Fisheries and Ocean Technology
    • /
    • v.20 no.1
    • /
    • pp.49-59
    • /
    • 1984
  • Optimizing investigation of characteristics of underwater welding by a gravity type arc welding process was experimentally carried out by using six types of domestic coated welding electrodes for welding of domestic marine structural steel plates (KR Grade A-1, SWS41A, SWS41B,) in order to develop the underwater welding techniques in practical use. Main results obtained are summarized as follows: 1. The absorption speed of the coating of domestic coated lime titania type welding-electrode became constant at about 60 minutes in water and it was about 0.18%/min during initial 8 minutes of absorption time. 2. Thus, the immediate welding electrode could be used in underwater welding for such a short time in comparison with the joint strength of in-atmosphere-and on-water-welding by dry-, wet-or immediate-welding-electrode. 3. By bead appearance and X-ray inspection, ilmenite, limetitania and high titanium oxide types of electrodes were found better for underwater-welding of 10 mm KR Grade A-1 steel plates, while proper welding angle, current and electrode diameter were 6$0^{\circ}C$, above 160A and 4mm respectively under 28cm/min of welding speed. 4. The weld metal tensile strength or proof stress of underwater-welded-joints has a quadratic relationship with the heat input, and the optimal heat input zone is about 13 to 15KJ/cm for 10mm SWS41A steel plates, resulting from consideration upon both joint efficiency of above-100% and recovery of impact strength and strain. Meanwhile, the optimal heat input zone resulting from tension-tension fatigue limit above the base metal's of SWS41A plates is 16 to 19KJ/cm. Reliability of all the empirical equations reveals 95% confidence level. 6. The microstructure of the underwater welds of SES41A welded in such a zone has no weld defects such as hydrogen brittleness with supreme high hardness, since the HAZ-bond boundary area adjacent to both surface and base metal has only Hv400 max with the microstructure of fine martensite, bainite, pearlite and small amount of ferrite.