• 제목/요약/키워드: Wear resistance properties

검색결과 646건 처리시간 0.021초

Alumina/graphite 복합체의 마찰마모 특성 (Tribological Properties of Alumina/Graphite Composites)

  • 백용혁;정종인;박용갑;김주영
    • 한국세라믹학회지
    • /
    • 제34권4호
    • /
    • pp.380-386
    • /
    • 1997
  • The tribological properties of ceramics are very important in the application to engineering ceramic parts such as seal rings, pump parts, thread guides, and so on. In this study, the effects of graphite addition on the mechanical and tribological properties of alumina/graphite composites were investigated. The composites were prepared by the adding of graphite powder to the mixture of Al2O3, talc and calcium carbonate. Bending strength, water absorption, friction coefficient, the amount of worn out material at a certain time, and maximum surface roughness(Rmax) of the prepared composites were measured. Crystalline phases and microstructure were examined with XRD and SEM. The melt of Al2O3-CaO-MgO-SiO2 system was shown over 10 vol% graphite composition. As the amount of the graphite is increased, needle like crystals of mullite were formed and grown. We obtained the good properties of friction coefficients and wear resistance at the powder composition containing 15 vol% of graphite.

  • PDF

탄소섬유강화 질화규소 세라믹스의 마찰마모 특성 (Sliding Wear Properties of Carbon Fiber Reinforced $Si_3N_4$ Ceramics)

  • 박이현;윤한기;김부안;박원조
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2004년도 학술대회지
    • /
    • pp.347-351
    • /
    • 2004
  • [ $Si_3N_4$ ] composites have been extensively studied for engineering ceramics, because it has excellent room and high temperature strength, wear resistance properties, good resistance to oxidation, and good thermal and chemical stability. In the present work, carbon short fiber reinforced $Si_3N_4$ ceramics were fabricated by hot press method in $N_2$ atmosphere at $1800^{\circ}C$ using $Al_2O_3\;and\;Y_2O_3$ as sintering additives. Content of carbon short fiber was $0\%,\;0.1\%\;and\;0.3\%$. The composites were evaluated in terms of density, flexural strength and elastic modulus through the 3-point bending test at room temperature. Also, The wear behavior was determined by the pin on disk wear tester using silicon nitride ball. Experimental density and flexural strength decreased with increasing content of carbon fiber. But specific modulus increased with increasing content of carbon fiber. In addition, friction coefficient and specific wear loss decreased with increasing content of carbon short fiber by reason of interfacial defects between matrix and fiber.

  • PDF

플라즈마 질화처리한 GCD40의 기계적성질 및 내식성에 관한 연구 (A Study on the Mechanical Properties and Corrosion Resistance of GCD40 by Plasma Nitriding)

  • 김무길;정병호;김상수
    • 동력기계공학회지
    • /
    • 제6권1호
    • /
    • pp.74-81
    • /
    • 2002
  • The characteristics of corrosion resistance for the surface of ductile cast iron(GCD40) by plasma nitriding process have been studied in terms of electrochemical polarization behaviors including corrosion potential($E_{corr}$), anodic polarization trends, polarization resistance($R_p$), and also have been studied microstructures, hardness and specific wear of nitrided layer Nitrided layer showed an enhanced hardness values in all the plasma nitriding condition investigated. In the result of wear test, specific wear of nitrided specimens were much decreased than that of non-treated specimens. In the results of XRD, ${\gamma}'phase\;and\;{\varepsilon}$ phase were detected in nitrided surface. And it was found that ${\varepsilon}$ phase was decreased and ${\gamma}'phase$ was increased respectively, as the nitriding time became longer. In the test of corrosion resistance, natural potentials in all the nitrided specimens were towards noble directions than in the case of non-treated specimens. The measurement of electrode potentials revealed that corrosion resistivity of plasma nitrided specimens were higher than in the case of the non-treated specimens.

  • PDF

열소성변형공정을 시행한 회주철제 실린더 라이너의 재료물성에 관한 연구 (A Study on the Material Properties of Grey Cast Iron for Cylinder Liner Treated by Thermo Plastic Deformation Process)

  • 김태형;김종호
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제29권6호
    • /
    • pp.671-677
    • /
    • 2005
  • In internal combustion engines the usual material for the cylinder liner is because of its good wear resistance Apparently this wear resistance arises from the at iron to form a hard glazed surface when under sliding friction. When the cylinder liner wear limits, it shall be replace with new one according to the classification soci manufacturer's standards. However, adoption of alternative repairing method such a metalizing, thermo plastic deformation process became inevitable taking enormous cost renewal into consideration. In this paper. the material properties of cylinder liner of grey discussed on the basis of the results of experimental work of the thermo plastic deformation the worn out cylinder liner made of grey cast iron.

Sliding Wear of Alumina-silicon Carbide Nanocomposites

  • Kim, Seung-Ho;Lee, Soo-Wohn;Kim, Yun-Ho;Riu, Doh-Hyung;Tohru Sekino;Koichi Niihara
    • 한국세라믹학회지
    • /
    • 제38권12호
    • /
    • pp.1080-1084
    • /
    • 2001
  • Alumina-based nanocomposites have improved mechanical properties such as hardness, fracture toughness and fracture strength compared to monolithic ceramics. In this study, alumina with 5 vol% of nanosized SiC was sintered by a hot pressing technique at 1600$\^{C}$, 30 MPa for 1h in an argon gas atmosphere. Microstructures and mechanical properties in alumina-SiC nanocomposite were investigated. Moreover, tribological properties in air and water were compared each other. Relationships of wear properties with mechanical properties such as hardness, strength, and fracture toughness as well as microstructure were studied. Based on experimental results it was found that nanosized SiC retarded grain growth of matrix alumina. Mechanical properties such as hardness, fracture toughness and strength were improved by the addition of nanosized SiC in alumina. Improved mechanical properties resulted in increased sliding wear resistance. Tribological behavior of nanocomposites in water seemed to be governed by abrasive wear.

  • PDF

비대칭 펄스 DC 반응성 스퍼터링 법에 의한 CNx 박막의 기계적 특성에 관한 연구 (A Study on the Mechanical Properties of CNx Thin Films Deposited by Asymmetric Bipolar Pulsed D.C. Sputtering)

  • 김준호;김대욱;차병철;김선광;이병석;전신희;김대일;유용주
    • 열처리공학회지
    • /
    • 제22권5호
    • /
    • pp.290-297
    • /
    • 2009
  • In case of using Asymmetric Bipolar Pulsed DC (ABPD) power generator, thin film is efficiently deposited as ions are getting higher energy by suppressing target poisoning and electric arc. In this article, the mechanical properties of CNx thin films deposited on the STS 316L were compared with DC and ABPD power generators. The CNx thin films deposited with ABPD clearly improved wear resistance by higher ratio of sp3CN as compared with DC. Nb interlayer affected to increase the value of 10N of adhesion between CNx thin films and substrate. But, CNx thin films deposited with ABPD couldn't endure to wear load and decreased wear resistance as the films were too thinner than substrate. Nevertheless the higher substrate bias energy applied to perform the dense films, it wasn't shown benefits about the wear properties from DC sputtering. But, in case of using ABPD sputtering, the wear resistance was largely improved without changing morphology despite of thin films.

SiC입자강화 알루미늄기 복합재료의 마모특성 (Wear Characteristics of Al/SiCp Composites)

  • 김석원;박진성;대성주작
    • 한국주조공학회지
    • /
    • 제22권4호
    • /
    • pp.184-191
    • /
    • 2002
  • This study aims to investigate on the effects of alloying elements and heat treatment on the microstructures, wear and heat resistance of Al-Si-Cu-Mg-(Ni)/SiCp prepared by the duplex process developed in previous study, which consists of squeeze infiltration (1st process) and squeeze casting (2nd process). The hardness of composite increased with decrease in SiCp size and Ni addition in both the heat exposured composite and the as-cast one. And the heat and wear resisting properties was improved by the SiCp reinforcement and the Ni addition. The wear amount of Al/SiCp composite decreased with decreasing in the size of silicon carbide particle.

분말고속도공구강의 마찰마모특성에 미치는 Co의 영향 (The Effects of Cobait on Wear and Friction Characteristics of PM-HSS)

  • 이한영;백금주;김용진;배종수;홍성현
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1998년도 제27회 춘계학술대회
    • /
    • pp.108-114
    • /
    • 1998
  • The mechanical characteristics of the high speed steel by powder metallurgy process(PM-HSS) has been reported to improve with several alloying constituents, such as high carbon, vanadium and cobalt. In this paper, sliding wear test has been conducted using a pin-on-disc machine for three PM-HSS which contains 0%, 5% and 12% cobalt respectively, in order to evaluate the effect of cobalt on wear properties of PM-HSS. The results of this study showed that the wear resistance of PM-HSS has been increased by the addition of cobalt on the range of experimental friction velocities. When compared with the effect of addition of cobalt, the wear resistance of PM-HSS with 5% cobalt has been found to be superior to that of PM-HSS with 12% cobalt.

  • PDF

탄화규소의 R-curve, 침식 및 마모 특성 (R-curve, erosion and wear of silicon carbide ceramics)

  • 채준혁;조성재;김석삼
    • 한국윤활학회:학술대회논문집
    • /
    • 한국윤활학회 1998년도 제27회 춘계학술대회
    • /
    • pp.139-145
    • /
    • 1998
  • This paper addresses the R-curve properties, wear resistance, and erosion resistance of the two silicon carbide ceramics with different microstructures, i.e. , fine grained SiC and in situ-toughened SiC(IST SIC). Fine grained SiC exhibits a relatively flat R-curve behavior whereas the IST SiC exhibits a increasing R-curve behavior. The increasing R-curve behavior in IST SiC is attributed to relatively weak grain boundaries. The rate of material removal during wear tests and erosion tests was higher for IST SiC than that for fine grained SiC. This is attributed to the weaker grain boundaries in IST SiC than that in fine grained SiC. It is implied that fracture toughness in short crack regime should be taken into consideration in the interpretation of the microscopical material removal process. We show that the higher the strength of grain boundaries is, the higher wear and erosion resistances are.

  • PDF

In vitro evaluation of a removable partial denture framework using multi-directionally forged titanium

  • Suzuki, Ginga;Shimizu, Satoshi;Torii, Mana;Tokue, Ai;Ying, Guo;Yoshinari, Masao;Hoshi, Noriyuki;Kimoto, Katsuhiko;Miura, Hiromi;Hayakawa, Tohru;Ohkubo, Chikahiro
    • The Journal of Advanced Prosthodontics
    • /
    • 제12권6호
    • /
    • pp.369-375
    • /
    • 2020
  • PURPOSE. This study evaluated the availability of multi-directionally forged (MDF) titanium (Ti) as a component of removable partial dentures (RPDs). MDF-Ti remarkably improved the mechanical properties of RPDs due to its ultrafine-grained structure. MATERIALS AND METHODS. The wear resistance, plaque adhesion, and machinability of MDF-Ti were tested. As controls, commercially pure (CP) titanium was used for wear, plaque adhesion, and machinability tests. For wear resistance, the volume losses of the titanium teeth before and after wear tests were evaluated. Plaque adhesion was evaluated by the assay of Streptococcus mutans. In the machinability test, samples were cut and ground by a steel fissure bur and carborundum (SiC) point. An unpaired t-test was employed for the analysis of the significant differences between MDF-Ti and the control in the results for each test. RESULTS. Wear resistance and plaque adherence of MDF-Ti similar to those of CP-Ti (P>.05) were indicated. MDF-Ti exhibited significantly larger volume loss than CP-Ti in all conditions except 100/30,000 g/rpm in machinability tests (P<.05). CONCLUSION. Although the wear resistance and plaque adherence of MDF-Ti were comparable to those of controls, MDF-Ti showed better machinability than did CP-Ti. MDF-Ti could be used as a framework material for RPDs.