Reflectance and Microhardness Characteristics of Sulfide Minerals from the Sambong Copper Mine (삼봉동광산산(三峰銅鑛山産) 유화광물(硫化鑛物)의 반사도(反射度)와 미경도(微硬度) 특성(特性))

  • Chi, Se Jung
    • Economic and Environmental Geology
    • /
    • v.17 no.2
    • /
    • pp.115-139
    • /
    • 1984
  • The Cu-Pb-Zn-Ag hydrothermal vein-type deposits which comprise the Sambong mine occur within calc-alkaline volcanics of the Cretaceous Gyeongsang Basin. The ore mineralization took place through three distinct stages of quartz (I and II stages) and calcite veins (III stage) which fill the pre-existing fault breccia zones. These stages were separated in time by tectonic fracturing and brecciation events. The reflection variations of one mineral depending on mineralization sequence are considered to be resulted from variation in its chemical composition due to different physico-chemical conditions in the hydrothermal system. The reflection power of sphalerite increases with the content of Fe substituted for Zn. Reflectances of the sphalerite grain are lower on (111) than on (100) surface. The spectral profiles depend on the internal reflection color. Sphalerite, showing green, yellow and reddish brown internal reflection, have the highest reflection power at $544m{\mu}$ (green), $593m{\mu}$ (yellow) and $615m{\mu}$ (red) wavelength, respectively. Chalcopyrite is recognized as biaxial negative from the reflectivity data of randomly oriented grains measured at the most sensitivity at $544m{\mu}$. The microindentation hardness against the Fe content (wt. %) for the sphalerite increases to 8.05% Fe and then decreases toward 9.5% Fe content. Vickers hardness of the sphalerite is considerably higher on surface of (100) than on (111). The relationship between Vickers hardness and crystal orientation of the galena was determined to be $VHN_{(111)}$ > $VHN_{(210)}$ > $VHN_{(100)}$. The softer sulfides have the wider variation of the diagonal length in the indentation. Diagonal length in the indentation is pyrite

  • PDF

A Study on Dimethacryloyloxy Alkane Derivatives Having an Anti-wear Performance as Lubricating Oil Additives (윤활유첨가제로써 마모억제 성능을 갖는 Dimethacryloyloxy Alkane 유도체에 관한 연구)

  • Han, Hye-Rim;Cho, Jung-Eun;Sim, Dae-Seon;Kang, Chung-Ho;Kim, Young-Wun;Jeong, Noh-Hee;Kang, Ho-Cheol
    • Applied Chemistry for Engineering
    • /
    • v.27 no.6
    • /
    • pp.583-589
    • /
    • 2016
  • Lubricant additives including zinc dialkyldithiophosphate (ZDDP) containing metal have been widely used due to the advantage of very low cost, but they can generate impurities such as ash. In this work, ZDDP containing metals was partially replaced with bis[3-(dialkyloxyphosphorothionyl) thio-2-methylpropanyloxy] butane (BAP4s) which was synthesized conveniently and effectively from alkanediol without any metal components. Also, the wear resistance property of synthesized BAP4s were studied. Wear scar diameter (WSD) values of BAP4s with butyl, octyl, decyl, dodecyl or tetradecyl groups were also measured by four-ball test. As the length of the alkyl group increased from 4 to 8, the WSD value of BAP4s decreased rapidly from 0.59 to 0.45 mm, but from 8 to 14, the value increased very slowly from 0.45 to 0.50 mm. Thus, among all BAP4s, B8P4 having BAP4 with the octyl group, showed the lowest WSD value. Furthermore, the WSD values were measured in a lubricant base oil mixed with a 0.50 percent concentration (w/w) of either BAP4 or ZDDP. The former was 0.55 mm, and the latter was 0.45 mm. The thermal stability and tribofilm formation peroperty were also measured by thermogravimetric analyzer (TGA) and energy-dispersive X-rays spectroscopy (EDS), respectively.

모재/중간층/박막의 H/E ratio 구배에 따른 Cr계 경질 박막의 기계적 특성에 관한 연구

  • Kim, Hoe-Geun;Song, Myeon-Gyu;Lee, Sang-Yul
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2018.06a
    • /
    • pp.135-135
    • /
    • 2018
  • 천이금속 질화물 코팅은 우수한 기계적 특성들로 인해 공구 코팅으로 많이 사용 되어왔다. 그 중에서도 특히 Cr계 경질 코팅은 높은 경도와 낮은 표면조도, 우수한 마찰특성 등 뛰어난 기계적 특성을 나타내므로 공구 코팅으로의 적용 가능성이 크다. 그러나 최근 공구산업의 발전으로 인해 공구가 더욱 가혹한 환경에서 사용됨에 따라, 공구의 수명을 향상시키고 보호하기 위해 코팅의 높은 밀착력이 요구되고 있으며, 모재와 코팅 사이에 중간층을 합성함으로써 공구의 밀착력을 향상시키는 연구가 활발히 진행되고 있다. 이전 연구에서 모재/중간층/코팅간의 경도와 탄성계수 비율(H/E ratio)의 구배가 코팅의 밀착력에 큰 영향을 미치는 것으로 확인되었다. 그러므로, WC 모재와 Cr계 코팅의 중간값의 H/E ratio를 갖는 중간층의 합성을 통해 코팅의 밀착력을 향상시킬 수 있을 것으로 판단된다. 본 연구에서는, 코팅의 밀착력을 향상시키기 위해 다양한 중간층을 증착한 CrZrN, CrAlN 코팅을 비대칭 마그네트론 스퍼터링 장비를 이용하여 합성하였다. 모재로는 디스크 형상의 WC-6wt.%Co 시편을 사용하였고 Cr, Zr, Si, Al single 타겟을 이용하여 Cr, CrN, CrZrN, CrZrSiN 등의 중간층이 증착된 코팅을 합성했다. 코팅의 합금상, 경도 및 탄성계수, 미세조직 및 조성, 표면 조도을 확인하기 위해 X-ray diffractometer (XRD), Fischer scope, field-emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectroscopy (EDS), atomic force microscopy를 사용하였고, 코팅의 밀착 특성을 분석하기 위해 scratch tester와 optical microscopy (OM)를 이용하였다. 코팅의 내열성을 확인하기 위해 코팅을 furnace에 넣어 공기중에서 500, 600, 700, 800, 900, $1,000^{\circ}C$로 30분 동안 annealing 한 후에 nano-indentation을 사용하여 경도를 측정하였다. CrZrN 및 CrAlN 코팅을 나노 인덴테이션으로 분석한 결과, 모든 코팅의 경도(33.4-35.8 GPa)와 탄성계수(384.1-391.4 GPa)는 중간층의 종류에 상관없이 비슷한 값을 보인 것으로 확인됐다. 그러나, 코팅의 마찰계수는 중간층의 종류에 따라 다른 값을 보였다. CrZrN 코팅의 경우 CrN 합금상 중간층을 갖을 때 가장 낮은 값을 보였으며, CrAlN 코팅의 경우 CrN/CrZrSiN 중간층을 증착하였을때 마찰계수는 0.34로 CrZrN 중간층을 증착하였을 때(0.41)에 비해 낮은 값을 보였다. 또한, 코팅의 마모율 및 마모폭도 비슷한 경향을 보인 것으로 보아, CrN/CrZrSiN 중간층을 합성한 CrAlN 코팅의 내마모성이 상대적으로 우수한 것으로 판단된다. 코팅의 밀착력의 경우도 마찰계수와 비슷한 경향을 보였다. 이것은 중간층의 H/E ratio가 코팅의 내마모성에 미치는 영향에 의한 결과로 사료된다. H/E ratio는 파단시의 최대 탄성 변형율로써, 모재/중간층/코팅의 H/E ratio 구배에 따라 코팅 내의 응력의 완화 정도가 변하게 된다. WC 모재 (H/E=0.040)와 CrAlN 코팅(H/E=0.089) 사이에서 CrN, CrZrSiN 중간층의 H/E ratio는 각각 0.076, 0.083으로 모재/중간층/코팅의 H/E ratio 구배가 점차 증가함을 확인 할 수 있었고, 일정 응력이 지속적으로 가해지면서 진행되는 마모시험중에 CrN과 CrZrSiN 중간층이 WC와 CrAlN 코팅 사이에서 코팅 내부의 응력구배를 완화시키는 역할을 함으로써 CrAlN 코팅의 내마모성이 향상된 것으로 판단된다. 모든 코팅을 열처리 후 경도 분석 결과, CrN/CrZrSiN 중간층을 증착한 CrAlN 코팅은 $1,000^{\circ}C$까지 약 28GPa의 높은 경도를 유지한 것으로 확인 되었고, 이는 CrZrSiN 중간층 내에 존재하는 SiNx 비정질상의 우수한 내산화성에 의한 결과로 판단된다.

  • PDF

Anti-corrosion properties for cross section of Mg films on galvalume steel coated by PVD process (PVD법에 의해 Mg 코팅된 갈바륨 도금강판의 단면부 내식특성)

  • Park, Jae-Hyeok;Kim, Sun-Ho;Park, Gi-Dong;Jeong, Jae-In;Yang, Ji-Hun;Lee, Gyeong-Hwang;Lee, Myeong-Hun
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2018.06a
    • /
    • pp.65-65
    • /
    • 2018
  • 갈바륨 도금강판은 알루미늄의 우수한 차폐 특성과 내열성, 열 반사성을 가지며 아연의 희생방식 특성을 겸비하여 동일 부착량의 용융 아연도금 및 알루미늄 도금강판에 비해 우수한 내식성을 나타낸다고 알려져 있다. 또한 이것은 표면이 미려하고 경제성이 높아 건자재 용도로 현재까지도 세계적으로 널리 이용되고 있다. 여기서 지칭하는 바륨 도금강판(galvalume steel)은 아연과 알루미늄 도금강판의 장점을 접목하기 위해 55 Al-43.4 Zn-1.6 Si (wt.%)로 구성되어 개발된 3원계 성분의 합금도금강판이다. 한편, 최근에는 강재의 내식성을 향상시키기 위한 다양한 연구 결과에 의해 Zn-Al-Mg의 3원계 합금도금강판도 개발되어 사용되고 있다. 이것은 기존의 아연도금 강판 보다 10배 정도의 우수한 내식성을 나타내는 것으로 보고되고 있다. 특히, 이것은 도금된 평판부의 내식성은 물론 절단된 도금 단면부의 내식성도 매우 우수하다고 알려져 있다. 그러나 상기한 갈바륨 도금강판의 경우에는 도금된 표면부에 비해 단면부의 내식성이 상대적으로 취약한 것으로 알려져 있다. 따라서 본 연구에서는 갈바륨 도금강판의 내식성을 종합적으로 향상시키기 위하여 이 갈바륨 도금강판 상에 PVD 스퍼터링법에 의해 Mg 코팅막의 제작을 시도하였다. 여기서 Mg 코팅막은 후처리 된 갈바륨 도금강판 상에 Ar 공정압력 2 및 20 mTorr 조건 중 1.5 및 $3{\mu}m$ 두께로 제작하였다. 또한 제작한 코팅막에 대해서는 모폴로지 관찰(SEM) 및 결정구조 분석(XRD)을 하였고, 분극측정, 염수분무 시험(SST) 및 복합부식 시험(CCT)에 의해 표면 및 단면부의 내식성평가를 수행하였다. 또한 여기서는 염수분무 및 복합부식 시험 후의 시험편도 채취 하여 표면 및 단면부위에 대한 원소조성 분석(EPMA)과 결정구조 분석(XRD)을 실시하였다. 이상의 실험 결과에 의하면, 본 실험에서 제작한 Mg 코팅막은 그 두께가 두꺼울수록 표면 Mg 결정립의 크기가 증가하였고, 그 부식속도가 증가하는 경향을 나타내었다. 또한 여기서는 공정압력이 높은 조건에서 제작한 막일수록 Mg(002)면 피크 강도가 감소하고 Mg(101)면 피크의 배향성이 증가하였다. 그때 그 막의 내식성은 향상되는 경향을 나타내었다. 그리고 종합적으로 염수분무 및 복합부식 시험 결과에 의하면 Mg이 코팅된 갈바륨 도금강판은 기존 갈바륨 도금강판 보다 내식성이 현저히 향상되었다. 특히, 단면부 내식성의 경우에는 기존 대비 5배 이상 향상되는 경향을 나타내었다. 여기서 단면부 내식특성 분석을 위한 EPMA 원소조성 분석 결과에 의거하면, 부식 초기에는 마그네슘의 부식생성물에 의해 단면부가 치밀하게 보호되고 있음을 확인할 수 있었다. 그 이후에는 부식이 지속적으로 진행됨에 따라 갈바륨 도금층에서 용출된 알루미늄 및 아연 성분이 마그네슘과 함께 치밀한 부식생성물을 형성하여 단면부를 차폐함에 따라 단면부의 내식성이 크게 향상된 것으로 생각된다. 이러한 부식생성물의 결정구조 분석 결과에 따르면, 염수분무와 복합부식 시험에서는 공통적으로 MgO, $Mg(OH)_2$ 이외에도 Simonkolleite상 등이 형성되었다. 또한 건-습 반복 부식시험인 복합부식시험 후에는 $Mg_5(CO_3)_4(OH)_24H_2O$(Hydromagnesite)상 등이 형성됨을 확인할 수 있었다. 즉, 본 실험에서 후처리된 갈바륨 도금강판 상에 제작한 마그네슘 코팅막의 경우에는 상기와 같은 다양한 부식반응에 의해 표면 및 단면부에 형성된 Mg계 부식생성물과 $Zn_5(OH)_8Cl_2H_2O$(Simonkolleite)상에 의해서 표면은 물론 단면부 내식성이 크게 향상된 것으로 사료된다.

  • PDF

Boulangerite from the Janggun Mine, Republic of Korea; Contributions to the Knowledge of Ore-Forming Minerals in the Janggun Lead-Zinc-Silver Ores (2) (한국·장군광산산 보울란저라이트에 대하여; 장군 연·아연·은 구성광물의 지식에 대한 기여 (2))

  • Lee, Hyun Koo;Imai, Naoya
    • Economic and Environmental Geology
    • /
    • v.26 no.2
    • /
    • pp.129-134
    • /
    • 1993
  • At the Janggun mine, boulangerite usually occurs as needles or irregularly-shaped grains, up to $500{{\mu}m}$ in longer dimensions, closely associated with galena, minerals of a tetrahedrite-freibergite series and bournonite in the peripheries of South A and B orebodies and the zone of manganoan carbonates surrounding them. In some places, especially at the top of South B orebody, it occures as "feather ore" consisting of its fine needles or "hairs" in small drusy cavities together with fine-grained euhedral galena, pyrite, manganoan carbonates, quartz, etc. In reflected light, it is bluish grey in colour exhibiting moderate bireflectance and is strongly anisotropic without any internal reflections. Reflectance in air is $R_{max}=43.2$, $R_{min}=35.7$ percent at wavelength of 580 nm, and VHN: $146-173\;kg/mm^2$ at a 50 g-load. The chemical composition on the average from 23 complete spot analyses by electron microprobe is, Pb 56.1, Sb 25.1, S 18.5, Total 99.6 (all in weight percent); the corresponding chemical formula calculated on the basis of S=11 is; $Pb_{5.16}Sb_{3.93}S_{11.0}$ which fulfils approximately the ideal formula $Pb_5Sb_4S_{11}$. The strongest reflections on the X-ray diffraction pattern are; $3.73\;{\AA}\;(10)$, $3.22\;{\AA}\;(5)$, $3.03\;{\AA}\;(4)$ and $2.82\;{\AA}\;(5)$ and the pattern is in harmonic with space group $C^5_{2h}-P2_1/a$. From the textural evidence of the microscopic observations, the mineral is considered to have been formed at the latest stage of hydrothermal lead-zinc-silver mineralization.

  • PDF

Studies on the Application of Cattle Slurry in Grassland III. Grazing preference as affected by application time of cattle slurry on pasture (혼파초지에서 액상구비 시용에 관한 연구 III. 방목이용 초지에서 액상구비 시용시기에 따른 가축기호성 비교)

  • Kim, Jae-Kyu;Seo, Sung
    • Journal of The Korean Society of Grassland and Forage Science
    • /
    • v.13 no.1
    • /
    • pp.43-48
    • /
    • 1993
  • This experiment was carried out to determine the effects of application time of cattle slurry on grazing pasture on the grass growth, dry matter yield, nutritive value, animal preference, and efficiency of pasture utilization. Four different application times of slurry(right now after grazing, 5th day, 10th day, and 15th day after grazing), and a no-slurry(control) plot were designed, 1991∼1992. Annual application amount of slurry was 40 ㎥/ha, and slurry was applicated in spring(2 times), summer and autumn. Total NPK fertilizer applicated were same as 280, 200 and 240 kg/ha in all treatment, respectively. The pasture was grazed with growing beef cattle(initial body wt.; ca. 250 kg) at every 30∼35 cm of plant height. The grass height, dry matter yield, crude protein yield, and other nutritive value were not different among treatments. However, the animal preference and efficiency of pasture utilization showed significant difference by application time of slurry. The highest grazing preference (1: the worst∼9: the best). and utilization efficiency (0∼100%) were observed by application time of right now after grazing (7.8, 76%), which was same to control(7.8, 77%), and followed by 5th day after grazing(7.3, 74%) and l0th day after grazing(6.9, 71%). But the preference and pasture utilization were greatly decreased at application time of cattle slurry of 15th day alter grazing(5.5, 60%). From the above results, the optimum application time of cattle slurry on grazing pasture to enhance animal preference, and efficiency of pasture utilization was within 5 days after grazing (less than 13.6 cm of plant height), and within 10 days after grazing (less than 18.5 cm of plant height) at least.

  • PDF

Effects of Solvent Extraction by Immersion on the Quality and Storage Stability of Rice (용매침지(溶媒浸漬)에 의한 탈지(脫脂)처리가 쌀의 품질(品質) 및 저장성(貯臧性)에 미치는 영향)

  • Cheigh, Hong-Sik;Kwon, Tai-Wan
    • Korean Journal of Food Science and Technology
    • /
    • v.4 no.4
    • /
    • pp.271-275
    • /
    • 1972
  • Effects of solvent extraction by immersion on the quality and storage stability of Korean rice were studied. Proportions of lipid extracted from whole grain of rice by immersing into two volumes(v/wt) of hexane and ethanol for 72 hours at room temperature were 0.41% and 0.38% respectively. Small changes of water content and hardness of rice were observed by solvent treatment. Cooking characteristics; that is, water-uptake ratio. extended volume, total solid, and starch-iodine blue test of rice was markedly changed by ethanol treatment, while little changes were observed by hexane treatment. No considerable differences in moisture sorption isotherm of rice were observed by both solvent treatments. Changes in TBA number and stale flavor appearance of rice treated with or without solvent immersion during storage at $60^{\circ}C$ showed that rice treated with hexane had best storage stability compared to ethanol treatment, while ethanol treatment of rice had better storage stability than no treatment. Similar results were noted in changes of the flavor score of cooked rice samples which were freeze dried.

  • PDF

Effects of Exercise Training and Selenium on MCT1 and MCT4 Protein Levels in Skeletal Muscles of Diabetic Goto-Kakizaki Rats (지구성 운동과 셀레니움 투여가 당뇨 Goto-kakizaki 쥐의 골격근의 MCT1과 MCT4단백질 발현수준에 미치는 효과)

  • Kim, Seung-Seok;Kang, Eun-Bum;Eum, Hyun-Sub;Kim, Bum-Su;Lim, Yea-Hyun;Park, Joon-Young;Cho, In-Ho;Oh, Yoo-Sung;Kwak, Yi-Sub;Cho, Joon-Yong
    • Journal of Life Science
    • /
    • v.18 no.1
    • /
    • pp.1-8
    • /
    • 2008
  • The purpose of this study was to determine the possible additive effects of endurance exercise training (EXER) and selenium (SELE) on the improvements of glucose and lactate transport capacities in diabetic Goto-kakizaki rats. Animals either remained sedentary control (SED) or performed EXER or received SELE [$5{\mu}mol$ kg body wt (-1) day (-1)], or underwent both EXER and SELE (COMBI), which lasted for 6 wk. Compared with sedentary control, EXER alone or the SELE alone group, or the combined treatment group had significant reduction in glucose response measured at 90 min and 120 min during an intraperitoneal glucose tolerance test (IPGTT) and body weight after 6week treatment. EXER alone, or combined group individually had significantly higher glycogen contents in liver compared with SED or SELE groups. EXER alone increased glycogen content in soleus and plantaris compared with SED, and this parameter was increased to greatest extent in the combined treatment groups compared with SED or SELE groups. EXER alone, SELE alone or COMBI, caused significant decreases in the plasma lactates, serum glucose, insulin, total cholesterol and HOMA-IR along with a significant increase in high-density lipoprotein cholesterol compared with SED. In addition, EXER or COMBI individually had significantly lower serum triacylglycerol compared with SED or SELE. With respect to protein expression related to glucose and lactate transport capacities, EXER alone, SELE alone, or COMBI increased in MCT1 and MCT4 protein level in soleus and plantaris. Furthermore, EXER alone, SELE alone or COMBI caused significant increases in mt MCT1 protein level in soleus and plantaris. The findings of the current study suggest that endurance exercise training and selenium treatment may provide therapeutic values to type II diabetic patients with peripheral insulin resistance and hyperlactatecemia by improving glucose and lactate transport capacities, leading to improvements in plasma lactate, serum glucose, insulin and lipid profiles (TC, TG, HDL).

The Study on the Methylmercury Analysis and the Monitoring of Total Mercury and Methylmercury in Fish (어류 중 메틸수은 분석법 확립 및 모니터링)

  • Kim, Hee-Yun;Chung, So-Young;Sho, You-Sub;Oh, Geum-Soon;Park, Seong-Soo;Suh, Jung-Hyuk;Lee, Eun-Ju;Lee, Yoon-Dong;Choi, Woo-Jeong;Eom, Ji-Yoon;Song, Min-Soo;Lee, Jong-Ok;Woo, Gun-Jo
    • Korean Journal of Food Science and Technology
    • /
    • v.37 no.6
    • /
    • pp.882-888
    • /
    • 2005
  • Procedure for analysis of methylmercury in fish was developed, involving addition of HCl, extraction with toluene, and clean-up using L-cystein solution. Obtained extract is analyzed by gas chromatography with electron capture detector using Ulbon HR-Thermon-Hg column. Detection limit and recovery of the method were 0.005mg/kg (expressed as Hg), 98-107 (103%), respectively. Total mercury and methylmercury concentrations in 175 commercial fish samples ranged from [mean-max (mean), unit: mg/kg]: 0.014-1.200 (0.270) and 0.006-0.901 (0.168) in tuna-fish, 0.020-0.934 (0.323) and 0.012-0.553 (0.149) in martin-fish, 0.082-0.782 (0.391) and 0.040-0.436(0.201) in shark, 0,023-0.031 (0.026) and 0,013-0.018 (0.015) in salmon, 0.098-0.193 (0.133) and 0.031-0.015(0.090) in tilefish, and 0,031-0.214 (0.089) and 0.016-0.093 (0.042) in canned tuna respectively. No sample of analyzed fish exceeded 1.0mg/kg wet wt., limit for methylmercury established by Codex. In all species examined, estimated weekly intake was lower than Provisional Tolerable Weekly Intake recommended by the JECFA (the Joint FAO/WHO Expert Committee on Food Additives).

Changes in $A_{1}$, Adenosine Receptor-Adenylyl Cyclase System of Rat Adipocytes Fellowing Induction of Experimental Diabetes by Streptozotocin Treatment (Streptozotocin으로 당뇨병을 유발시킨 쥐의 지방세포에 나타나는 $A_{1}$, Adenosine Receptor-Adenylyl Cyclase System의 변화)

  • Park, Kyung-Sun;Lee, Myung-Soon;Kim, Kyung-Hwan
    • The Korean Journal of Pharmacology
    • /
    • v.29 no.1
    • /
    • pp.97-105
    • /
    • 1993
  • Adenosine receptors in rat adipose tissues have been reported to be of $A_{1}$ subclass, and their stimulation leads to inhibition of adenylyl cyclase, resulting in inhibition of lipolysis. In the present study we investigated changes in $A_{1}$ adenosine receptor-adenylyl cyclase system of adipocytes following induction of experimental diabetes in rats. One week following experimental diabetes were induced by intravenous injection of streptozotocin (50 mg/kg body wt.), adipocytes from rats $(170{\sim}230g)$ fed ad libitum were isolated using collagenase. When adipocytes were incubated for 1 h with 1 unit/ml adenosine deaminase and $1\;{\mu}M$ isoproterenol, and assayed for glycerol formation, it was found that the inhibition of lipolysis in diabetic adipocytes by $(-)-N^{6}-(R-phenylisopropyl)adenosine$ (PIA), an $A_{1}$, adenosine receptor agonist, was twice that of control adipocytes. In an effort to delineate the mechanism(s), $[^{3}H]PIA$ binding to adipocytic membranes from diabetic and control rats were determined. Neither the affinities nor numbers of $A_{1}$ adenosine receptor were significantly different from each other (Best fit parameters for the one-site model are: $K_{d}=0.51{\pm}0.09nM$ and $B_{max}=1.60{\pm}0.12\;pmoles/mg$ protein for control membranes; $K_{d}=0.54{\pm}0.21\;nM$ and $B_{max}=1.72{\pm}0.31\;pmoles/mg$ protein for diabetic membranes). However, the inhibiton by PIA of the isoproterenol-stimulated adenylyl cyclase activities was found to be 1.9 times higher in adipocytic membranes from diabetic rats than those from controls. These results suggest that the increased sensitivity of inhibition of lipolysis to PIA in adipocytic membranes from diabetic rats is due to changes in signal transduction pathways, rather than alterations of $A_{1}4 adenosine receptor molecules themselves.

  • PDF