• Title/Summary/Keyword: UV exposure test

Search Result 68, Processing Time 0.024 seconds

Analysis of Degradation Behaviors of Geomembrane by Accelerated Test under UV Exposure Conditions (자외선 노출조건 하에서 가속시험에 의한 지오멤브레인의 분해거동 해석)

  • Park, Yeong Mog;Khan, Belas Ahmed;Jeon, Han Yong
    • Polymer(Korea)
    • /
    • v.37 no.1
    • /
    • pp.5-14
    • /
    • 2013
  • In this paper the effect of UV (ultraviolet) exposure on HDPE (high density polyethylene)-smooth and f-PP (flexible polypropylene) geomembranes is evaluated under UVB-313 (ultraviolet wavelength 290-315 nm) exposure. Tensile property, melt flow index (MFI), oxidation induction time (OIT), both standard-OIT and high pressure-OIT and Fourier transform infrared spectroscopy/attenuated total reflectance (FTIR/ATR) results are discussed. Although tensile properties of the exposed geomembrane samples remained unchanged, the depletion of antioxidants was found higher for f-PP than for HDPE geomembrane. Arrhenius model by extrapolation was used on the data to predict the antioxidant lifetime to a typical site temperature of $20^{\circ}C$. There was no significant difference between the MFI value of the virgin and UV exposed HDPE geomembrane samples but a decrease in MFI was found in f-PP geomembrane that signifies that crosslinking has occurred. From FTIR spectra, the small peak (near $1750\;cm^{-1}$) observed in the spectrum of UV exposed sample corresponds to a carbonyl (C=O) linkage, which suggests that oxidation has occurred in the polymer structure, and another new band for f-PP between 3100 and $3500\;cm^{-1}$ is attributed to a hydroxyl bond and/or hydroperoxide bond.

Development of Aging Equipment and Testing Method for UV Effected Degradation Characteristics of Silicone Rubber (자외선 열화에 의한 실리콘고무의 열화 특성 연구를 위한 열화장치 및 시험방법의 개발)

  • Lee, Jeong-Heon
    • Proceedings of the KIEE Conference
    • /
    • 2007.11c
    • /
    • pp.93-96
    • /
    • 2007
  • In this paper, the testing equipment for evaluating aging characteristics of outdoor silicone rubber insulator resulting from the environmental aging effect with regards to sunlight(UV) was developed. Influence of sunlight effect aging is seriously increase due to destruction of ozone layer which is occurred by consumption of fossil fuel. For this purpose, silicone rubber was aged under the artificial sunlight by exposure of xenon lamp radiation in the accelerating aging chamber and various test and analysis were performed such as breakdown strength, contact angle. And FT-IR analysis has been followed.

  • PDF

Color stability of thermochromic pigment in maxillofacial silicone

  • Kantola, Rosita;Lassila, Lippo V.J.;Tolvanen, Mimmi;Valittu, Pekka K.
    • The Journal of Advanced Prosthodontics
    • /
    • v.5 no.2
    • /
    • pp.75-83
    • /
    • 2013
  • PURPOSE. Maxillofacial silicone elastomer is usually colored intrinsically with color pigments to match skin colors. The purpose of this study was to investigate the color stability of a maxillofacial silicone elastomer, colored with a thermochromic, color changing pigment. MATERIALS AND METHODS. Disc-shaped maxillofacial silicone specimens were prepared and divided into 3 groups: a conventionally colored control group, one group additionally colored with 0.2 wt% thermochromic pigment, and one group with 0.6 wt% thermochromic pigment. Half of the surface of each specimen was covered with an aluminium foil. All of the specimens were exposed to UV radiation in 6 hour cycles over 46 days. In between the UV exposures, half of the specimens were stored in darkness, at room temperature, and the other half was stored in an incubator, at a humidity of 97% and a temperature of $+37^{\circ}C$. Color measurements were made with a spectrophotometer and registered according to the CIELAB $L^*a^*b^*$ color model system. The changes in $L^*$, $a^*$ and $b^*$ values during artificial aging were statistically analyzed by using paired samples t-test and repeated measures ANOVA. P-values <.05 were considered as statistically significant. RESULTS. The UV exposure resulted in visually noticeable and statistically significant color changes in the $L^*$, $a^*$ and $b^*$ values in both of the test groups containing thermochromic pigment. Storage in the incubator lead to statistically significant color changes in the $a^*$ and $b^*$ values of the specimens containing thermochromic pigment, compared to those stored at room temperature. CONCLUSION. The specimens containing thermochromic pigment were very sensitive to UV radiation, and the thermochromic pigment is not suitable, as such, to be used in maxillofacial prostheses.

Durability Performance Evaluation of PolyUrea for Seismic Retrofitting of RC Structures (구조물 내진 보강용 폴리우레아의 내구 성능 평가)

  • Cho, Chul-Min;Kim, Jang Jay Ho;Lee, Doo-Sung;Kim, Tae-Kyun
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.21 no.3
    • /
    • pp.1-8
    • /
    • 2017
  • An experimental study is needed a reinforcing method for seismic load to apply for RC structures because a lot of earthquakes have frequently happened in the world and those also collapsed infrastructures or damaged human lives. The reinforcing effect of PolyUrea (PU) appeared to be excellent under blast and impact about RC structures. In this study, Stiff Type PolyUrea (STPU) had developed by manipulating the ratio of the components of prepolymer and hardener of PU. And the durability performance evaluation of STPU for deterioration and chemical resistance has been performed. Acid environmental exposure test and ultraviolet (UV) exposure test have been performed as the durability performance evaluation for STPU. Concrete carbonation exposure test and freezing and thawing test for concrete coated with STPU have been performed. The experimental result showed that STPU has high resisting capacity and durability in all tests. Therefore, STPU would be used as seismic reinforcement materials.

Phototoxicity: Its Mechanism and Animal Alternative Test Methods

  • Kim, Kyuri;Park, Hyeonji;Lim, Kyung-Min
    • Toxicological Research
    • /
    • v.31 no.2
    • /
    • pp.97-104
    • /
    • 2015
  • The skin exposure to solar irradiation and photoreactive xenobiotics may produce abnormal skin reaction, phototoxicity. Phototoxicity is an acute light-induced response, which occurs when photoreacive chemicals are activated by solar lights and transformed into products cytotoxic against the skin cells. Multifarious symptoms of phototoxicity are identified, skin irritation, erythema, pruritis, and edema that are similar to those of the exaggerated sunburn. Diverse organic chemicals, especially drugs, are known to induce phototoxicity, which is probably from the common possession of UV-absorbing benzene or heterocyclic rings in their molecular structures. Both UVB (290~320 nm) and UVA (320~400 nm) are responsible for the manifestation of phototoxicity. Absorption of photons and absorbed energy (hv) by photoactive chemicals results in molecular changes or generates reactive oxygen species and depending on the way how endogenous molecules are affected by phototoxicants, mechanisms of phototoxcity is categorized into two modes of action: Direct when unstable species from excited state directly react with the endogenous molecules, and indirect when endogeneous molecules react with secondary photoproducts. In order to identify phototoxic potential of a chemical, various test methods have been introduced. Focus is given to animal alternative test methods, i.e., in vitro, and in chemico assays as well as in vivo. 3T3 neutral red uptake assay, erythrocyte photohemolysis test, and phototoxicity test using human 3-dimensional (3D) epidermis model are examples of in vitro assays. In chemico methods evaluate the generation of reactive oxygen species or DNA strand break activity employing plasmid for chemicals, or drugs with phototoxic potential.

Design of a shoe rack for effective sterilization and deodorization of the shoes contaminated by various bacteria (오염된 신발의 효율적인 살균과 탈취를 위한 신발장의 설계)

  • Lee, Sam-Cheol;Jang, Yong-Seok
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.17 no.6
    • /
    • pp.199-206
    • /
    • 2016
  • The aim of this study was to establish the optimal conditions to design a shoe rack that could effectively sterilize and deodorize shoes contaminated by various bacteria. The manufacture and evaluation of a shoe rock was conducted for one year from October 2014 to September 2015. The antibacterial efficacies were evaluated using Escherichia coli and Staphylococcus aureus by JIS Z 2801:2010. The deodorization efficiency was identified by the standard method for deodorization efficiency evaluation of an indoor air cleaner established by Korea Air Cleaning Association, SPS-KACA002-132:2006. The results showed that antibacterial evaluation showed more than 99.9% of the sterilization effects on Escherichia coli and Staphylococcus aureus after exposure to ultraviolet (UV) light for 30 seconds. The average deodorization efficiency for the test gases was 42.5%. The temperature in the shoes and in the shoe rack was lower than $40^{\circ}C$ and $25^{\circ}C$, respectively, when the UV lamp was turned on for 5 minutes and off for 25 minutes repeatedly. This was controlled by turning the UV lamp on and off to maintain the appropriate temperature in the shoes. In conclusion, the real deodorization efficiency is expected to be higher than the measured value because the internal volume of the shoe rack was smaller than the test chamber used to measure the deodorization efficiency. The deodorization effect could be increased further by the sterilization of bacteria causing bad odors in shoes. Further studies will be needed to determine the temperature deviations within the shoe rack to provide constant conditions.

Anti-Reflective Coating with Hydrophilic/Abraion-Resistant Properties using TiO2/SiOxCy Double-Layer Thin Film (TiO2/SiOxCy 이중 박막을 이용한 투명 친수성/내마모성 반사방지 코팅)

  • Lee, Sung-jun;Lee, Min-kyo;Park, Young-chun
    • Journal of the Korean institute of surface engineering
    • /
    • v.50 no.5
    • /
    • pp.345-351
    • /
    • 2017
  • A double-layered anti-reflective coating with hydrophilic/abrasion-resistant properties was studied using anatase titanium dioxide($TiO_2$) and silicon oxycarbide($SiO_xC_y$) thin film. $TiO_2$ and $SiO_xC_y$ thin films were sequentially deposited on a glass substrate by DC sputtering and PECVD, respectively. The optical properties were measured by UV-Vis-NIR spectrophotometer. The abrasion-resistance and the hydrophilicity were observed by a taber abrasion tester and a contact angle analyzer, respectively. The $TiO_2/SiO_xC_y$ double-layer thin film had an average transmittance of 91.3%, which was improved by 10% in the visible light region (400 to 800 nm) than that of the $TiO_2$ single-layer thin film. The contact angle of $TiO_2/SiO_xC_y$ film was $6.9^{\circ}$ right after UV exposure. After 9 days from the exposure, the contact angle was $10.2^{\circ}$, which was $33^{\circ}$ lower than that of the $TiO_2$ single-layer film. By the abrasion test, $SiO_xC_y$ film showed a superior abrasion-resistance to the $TiO_2$ film. Consequently, the $TiO_2/SiO_xC_y$ double-layer film has achieved superior anti-reflection, hydrophilicity, and abrasion resistance over the $TiO_2$ or $SiO_xC_y$ single-layer film.

A Study on the Laser Direct Imaging for FPD ( I ) (평판 디스플레이용 Laser Direct Imaging에 관한 연구( I ))

  • Kang, H.S.;Kim, K.R.;Kim, H.W.;Hong, S.K.
    • Proceedings of the Korean Society of Laser Processing Conference
    • /
    • 2005.11a
    • /
    • pp.37-41
    • /
    • 2005
  • When screen size of the Flat Panel Display (FPD) becomes larger, the traditional photo-lithography using photomasks and UV lamps might not be possible to make patterns on Photo Resist (PR) material due to limitation of the mask size. Though the maskless photo-lithography using UV lasers and scanners had been developed to implement large screen display, it was very slow to apply the process for mass-production systems. The laser exposure system using 405 nm semi-conductor lasers and Digital Micromirror Devices (DMD) has been developed to overcome above-mentioned problems and make more than 100 inches FPD devices. It makes very fine patterns for full HD display and exposes them very fast. The optical engines which contain DMD, Micro Lens Array (MLA) and projection lenses are designed for 10 to 50 ${\mu}m$ bitmap pattern resolutions. The test patterns for LCD and PDP displays are exposed on PR and Dry Film Resists (DFR) which are coated or laminated on some specific substrates and developed. The fabricated edges of the sample patterns are well-defined and the results are satisfied with tight manufacturing requirements.

  • PDF

Effects and permeation property of anti-aging material from tinged autumnal leaves of Maple tree in the skin

  • Kim, Jin-Hwa;Lee, Jeong-Jae;Park, Sung min;Lee, Bum chun;Pyo, Hyeong-Bae
    • Proceedings of the SCSK Conference
    • /
    • 2003.09b
    • /
    • pp.464-478
    • /
    • 2003
  • Free radicals and reactive oxygen species (ROS) caused by UV exposure or other environmental facts play critical roles in cellular damage and aging. The extract of tinged autumnal leaves of maple tree(Acer palmatum) has proven to be a powerful antioxidant. The Acer palmatum extract is very effective on the stabilization of biological membranes( containing unsaturated fatty acid). We studied photoprotective effect of the extract against UVB-induced cytotoxicity in human keratinocytes. The extract improved cell viability comparing to control after UVB irradiation. In the determination test of pro inflammatory cytokines the extract decreased expression of interleukin 1 a and 6, which play an important role in inflammation and skin erythema caused by UV. We also studied property of varying cosmetic formulations on the percutaneous absorption of the extract. After 24 hour in vitro penetration study, the content of the extract was more highly detected in skin residue part. This result showed the extract had relatively high compatibility of skin in our emulsion system. On human skin, after appling the product containing the extract we obtained a good result of antiwrinkle effect by skin visiometer. In conclusion, the Acer palmatum extract is a photoprotective and very effective in stressed and aged skin care. And we can predict the extract mainly affects on the skin cell and tissue in our emulsion system.

  • PDF

The Corrosion Behavior of Anti-Graffiti Polyurethane Powder Coatings

  • Rossi, S.;Fedel, M.;Deflorian, F.;Feriotti, A.
    • Corrosion Science and Technology
    • /
    • v.17 no.6
    • /
    • pp.257-264
    • /
    • 2018
  • Anti-graffiti coatings have become more important. These layers must guarantee excellent corrosion protection properties, and graffiti must be easily removable, without reducing protection and aesthetic properties. In this study, anti-graffiti and corrosion behavior of two anti-graffiti polyurethane powder coatings were studied. These layers were deposited on aluminum substrate, with two different surface finishes, smooth, and wrinkled. The action of four different removers are investigated. Graffiti were drawn on coatings by means of red acrylic spray paint. Methyl-ethyl-ketone (MEK) and a "commercial" remover were the most effective solvents, in terms of graffiti removal capability, producing limited change in aesthetical surface aspect for smooth finishing. The wrinkled surface was less resistant. Corrosion protection properties, after removal action and contact with the remover, were evaluate by electrochemical impedance spectroscopy. After approximately 5 hours, coatings were no longer protective due to formation of defects. To simulate the weathering effect, UV-B cyclic test (4 hours of UV exposure followed by 4 hours of saturated humidity at $50^{\circ}C$) were performed for 2000 hours. Gloss and color changes were measured, and electrochemical impedance spectroscopy measurements were performed after aging and graffiti removal.