Corrosion Behavior of Ti-13Nb-13Zr and Ti-6Al-4V Alloys for Biomaterial Application

  • Saji, Viswanathan S.;Jeong, Yong-Hoon;Yu, Jin-Woo;Choe, Han-Cheol
    • Corrosion Science and Technology
    • /
    • 제9권1호
    • /
    • pp.12-15
    • /
    • 2010
  • Ti-13Nb-13Zr (TNZ) alloy has attracted considerable research attention in the last decade as a suitable substitute for the commercially used Ti-6Al-4V (TAV) alloy for orthopedic and dental implant applications. Hence, in the present work, a comparative evaluation has been performed on the electrochemical corrosion behavior of TNZ and TAV alloys in 0.9 wt.% NaCl solution. The result of the study showed that both the alloys had similar electrochemical behavior. The corrosion resistance of TAV alloy is found to be marginally superior to that of TNZ alloy.

Ti-13Nb-13Zr 합금의 저 변형량에서 초미세 결정립 형성 및 기계적 적합성 향상 (Formation of submicrocrystalline in Ti-13Nb-13Zr alloy without severe deformation and enhanced mechanical compatibility)

  • 박찬희;염종택;전영수;이종수
    • 한국소성가공학회:학술대회논문집
    • /
    • 한국소성가공학회 2009년도 추계학술대회 논문집
    • /
    • pp.328-331
    • /
    • 2009
  • Microstructural evolution of alpha and beta phases during dynamic globularization of near-beta Ti-13Nb-13Zr alloy was investigated to determine the optimum processing conditions. The submicrocrystalline alloy sheet with ${\sim}80%$ of high-angle grain boundaries was produced utilizing dynamic globularization at temperature of $600^{\circ}C$, equivalent strain rate of $10^{-1}\;s^{-1}$ and strain of 1.4. The refined structure with the gain size of ${\sim}0.4{\mu}m$ showed 25-60% enhanced mechanical compatibility as compared to those of the conventional mill-annealed or solution treated and aged microstructures.

  • PDF

넓은 과냉각 액체영역을 가지는 Ni-Nb-Ti-Zr계 비정질 합금의 제조 (Fabrication of Ni-Nb-Ti-Zr Amorphous Alloys with Wide Supercooled Liquid Region)

  • 김성규
    • 한국주조공학회지
    • /
    • 제22권5호
    • /
    • pp.252-256
    • /
    • 2002
  • Ni-Nb-Ti-Zr amorphous alloys were manufactured using melt-spinning methods. Amorphous formability, the supercooled liquid region before crystallization and mechanical properties were examined. The value of the reduced glass transition temperature and the supercooled liquid region of $Ni_{62}Nb_{10}Ti_{13}Zr_{15}$ alloy were relatively high and were 0.612 and 76 K respectively. However, amorphous bulk alloy rod was not formed using the Cu-mold die casting. The mechanical properties were in the range of $800{\sim}900DPN$ of hardness and $2.5{\sim}2.8$ GPa of tensile strength in the whole composition range.

Pb($Zn_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-$PbZrO_3$계 세라믹의 유전특성에 관한 연구 (Study on Dielectric Characteristics of Pb($Zn_{1/3}Nb_{2/3}$)$O_3$-$PbTiO_3$-$PbZrO_3$Ceramics))

  • 최창문;박정철;소대화
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1994년도 추계학술대회 논문집
    • /
    • pp.13-16
    • /
    • 1994
  • In this paper, xPb(Zn$_{1/3}Nb_{2/3}$)$O_3$-yPbTiO$_3$-zPbZrO$_3$-(0.5wt%)MnO$_2$ ceramics were fabricated by the mixed oxide method sintered at $1250^{\circ}C$ for 2[hr] and then the deielectric, electromechanical coupling factor($K_{p}$ and mechanical coupling factor(Qm) properties were investigated. In 0.1PZN-0.45PT-0.45PZsample, dielectric properties and electromechanical coupling factor were 829 and 29%. In the case of 0.5PZN-0.45PT-0.50PZ sample, that was 101 according to mechanical quality facotr. molphotropic phase boundary(MPB) certained area which $PbTiO_3$addition quatity 40∼50[㏖%].

투광성 Ba(La1/2Nb1/2)O3-PbZrO3-PbTiO3세라믹의 강유전 및 전기광학특성에 관한 연구 (A Study on the Ferroelectic and Electrooptical Properties of the Transparent Ba(LaS11/2TNbS11/2T)OS13T-PbZrOS13T-PbTiOS13T Ceramics)

  • 김준수;류기원;박영희;박창엽
    • 대한전기학회논문지
    • /
    • 제41권8호
    • /
    • pp.858-868
    • /
    • 1992
  • 0.085Ba(LaS11/2TNbS11/2T)OS13T-0.915Pb(ZrS1yTTiS11-yT)OS13T (0.45$\leq$y$\leq$0.65) transparent electrooptic ceramics were fabricated by two-stage sintering method. The structural, ferroelectric and electrooptic properties were investigated varying composition and second sintering time. Also the possibility of application to electrooptic device was studied. If we increase the PbZrOS13T contents, dielectric constants were increased and Curie temperature was decreased. In the composition of 0.55[mol] PbZrOS13T, electromechanical coupling factor and piezoelectric charge constant were the highest values of 43[%] and 173x10S0-12T[C/N], respectively. Mechanical quality factors were decreased with the increasing PbZrOS13T contents. Light transmittance was increased with wavelength when measured from 300[nm] to 900[nm], and with PbZrOS13T contents in the range of 0.50[mol]-0.65[mol], and had the highest value of 67[%] in the composition of 0.65[mol] PbZrOS13T. From the results of ferroelectric hysteresis loop and transmitted light intensity with electric field, the specimens with compositions of 0.65,0.60,0.55[mol] PbZrOS13T were applicable to electrooptic memory device and those with compositions of 0.50,0.45[mol] PbZrOS13T were applicable to linear electrooptic device.

플라즈마질화처리에 의한 13Cr 스테인리스강의 표면경화특성에 미치는 질화물형성원소첨가의 영향 (Effects of Alloying Elements on Hardening of 13Cr Stainless Steels Using Plasma Nitriding Process)

  • 박화순;조희정;박봉규;강정윤
    • Journal of Welding and Joining
    • /
    • 제16권1호
    • /
    • pp.88-97
    • /
    • 1998
  • The surface characteristics of 13Cr stainless steel systems by plasma nitriding were investigated. The plasma nitriding for the 13Cr steels, in which the nitriding forming elements such as Ti, V, W, Nb, Al, Zr and Si were added about 2~3wt.%, respectively, was performed. In all nitrided specimens, .epsilon.-F $e_{2-3}$N, UPSILON.'-F $e_{4}$N and CrN were detected as the nitrides with the a-Fe in the nitrided layer. VN and .betha.- $W_{2}$N were also detected in 13Cr-3V and 13Cr-3W alloys. The growth of the nitrided layer was controlled by the diffusion process. The thickness of the nitrided layer was similar in the 13Cr-2Nb and 3Zr specimens to that of 13Cr(BM) specimen, while the others exhibited the thinner layer. The activation energy for the growth of the nitrided layer in the temperature range of 773-873K was about 130kJ/mol in 13Cr(BM), 13Cr-2Ti, 3W, 3Al, 3Zr and 3Si alloys. The hardness of the nitrided specimens was significantly increased above Hv1000, comparing to the non-nitrided specimen. The specimens with the nitrided forming elements revealed much higher hardness values and, especially, 13Cr-3Al, 3V and 3Si specimens were significantly hardened up to Hv1300.v1300.0.

  • PDF

MnO$_2$가 첨가된 Pb(Sn$_{1}$2/Nb$_{1}$2/)O$_3$-PbTiO$_3$-PbZrO$_3$ 세라믹의 유전 및 초전특성에 관한 연구 (A Study on the Dielectric and Pyroelectric Properties of the Pb(Sn$_{1}$2/Nb$_{1}$2/)O$_3$-PbTiO$_3$-PbZrO$_3$ Ceramics doped with MnO$_2$)

  • 함영욱;이능헌;이덕출
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 1993년도 추계학술대회 논문집
    • /
    • pp.10-13
    • /
    • 1993
  • ln this study, x PSN - y PT - z PZ ceramics doped with w MnO$_2$were fabricated by the mixed oxide method at 1250[$^{\circ}C$] for 2[hr] and then the dielectric and pyroelectric properties were investigated. In the 0.05 PSN - 0.4 PT - 0.55 PZ specimen with 0.5[wt.%] MnO$_2$, the pyroelectric coefficient was 6.6${\times}$10$\^$-8/[C/cm$^2$$.$$^{\circ}C$], respectibly.

  • PDF

강구조물(鋼構造物) 진단(診斷)을 위한 초음파(超音波) 센서 (Ultrasonic Sensors for Steel Structure Inspection)

  • 신병철
    • 한국구조물진단유지관리공학회 논문집
    • /
    • 제2권2호
    • /
    • pp.170-176
    • /
    • 1998
  • The team mixed PbO, $ZrO_2$, $TiO_2$, $Nb_2O_5$ and $MnCO_3$, to make $Pb[(Zr_{0.54}\;Ti_{0.46})\;Nb_{0.005}]O_3+4%MnCO_3$. The electroded PZT ceramics were poled by 3 kV/mm at $110^{\circ}C$ for 600 s. We assembled the 0.4mm thick PZT slices into ultrasonic transducers. Central frequency of the probe is 5 MHz, which is proper to the thickness gauge for steel pipes and for flaw detector. The probe can detect a disk shape defect of 1mm diameter at 15cm deep in steel block. The new probe's Fresnel zone that the ultrasonic beam do not broaden is 13mm. Over the Fresnel zone, the ultrasonic beam spreads. Half of the beam spread angle of the probe is $4.3^{\circ}-4.6^{\circ}$. This probe can be used for the ultrasonic transducers for non-destructive testing of steel bridges.

  • PDF

Piezoelectric Properties of PMN-PNN-PZT Ceramics and the Simulation of Ultrasonic Cleaner

  • Sujin Kang;Ju Hyun Yoo;Sun A Whang;Jae Gyu Lee;Jong Hyeon Lee;Ji Hoon Lee;Dae Yeol Hwang;Sua Kim;Seong Min Lee;Han Byeol Kim
    • 한국전기전자재료학회논문지
    • /
    • 제36권2호
    • /
    • pp.191-196
    • /
    • 2023
  • In this paper, for the application of ultrasonic cleaners for cleaning dentures and transparent braces, Pb(Mn1/3Nb2/3)O3-Pb(Ni1/3 Nb2/3)O3-Pb(Zr,Ti)O3 [PMN-PNN-PZT] system ceramics were manufactured and their dielectric and piezoelectric properties were investigated. Overall the best properties suitable for the device applications such as ultrasonic cleaner were obtained from the ceramics sintered at 920℃: bulk density of 7.8 g/cm3, the dielectric constant (εr) of 1,689, piezoelectric charge constant (d33) of 433 pC/N, planar electromechanical coupling factor (kp) of 0.64, mechanical quality factor (Qm) of 835, S11E of 13.37 (10-12 N/m2), and Curie temperature of 315℃ By using the physical properties of this composition, the ultrasonic cleaner was designed and simulated using the commercial ATILA software. For the three-layered ceramics with the dimension of 25 mm × 25 mm × 2.5mm, an excellent displacement of 8.998 10-3 m) and the sound pressure of 147.68 dB were recorded.