• Title/Summary/Keyword: Thin/thick film

Search Result 491, Processing Time 0.033 seconds

A New process for the Solid phase Crystallization of a-Si by the thin film heaters (박막히터를 사용한 비정질 실리콘의 고상결정화)

  • 김병동;정인영;송남규;주승기
    • Journal of the Korean Vacuum Society
    • /
    • v.12 no.3
    • /
    • pp.168-173
    • /
    • 2003
  • Recently, according to the rapid progress in Flat-panel-display industry, there has been a growing interest in the poly-Si process. Compared with a-Si, poly-Si offers significantly high carrier mobility, so it has many advantages to high response rate in Thin Film Transistors (TFT's). We have investigated a new process for the high temperature Solid Phase Crystallization (SPC) of a-Si films without any damages on glass substrates using thin film heater. because the thin film heater annealing method is a very rapid thermal process, it has very low thermal budget compared to the conventional furnace annealing. therefore it has some characteristics such as selective area crystallization, high temperature annealing using glass substrates. A 500 $\AA$-thick a-Si film was crystallized by the heat transferred from the resistively heated thin film heaters through $SiO_2$ intermediate layer. a 1000 $\AA$-thick $TiSi_2$ thin film confined to have 15 $\textrm{mm}^{-1}$ length and various line width from 200 to 400 $\mu\textrm{m}$ was used as the thin film heater. By this method, we successfully crystallized 500 $\AA$-thick a-Si thin films at a high temperature estimated above $850^{\circ}C$ in a few seconds without any thermal deformation of g1ass substrates. These surprising results were due to the very small thermal budget of the thin film heaters and rapid thermal behavior such as fast heating and cooling. Moreover, we investigated the time dependency of the SPC of a-Si films by observing the crystallization phenomena at every 20 seconds during annealing process. We suggests the individual managements of nucleation and grain growth steps of poly-Si in SPC of a-Si with the precise control of annealing temperature. In conclusion, we show the SPC of a-Si by the thin film heaters and many advantages of the thin film heater annealing over other processes

Thickness Dependence of the Crystallization of FePt/MgO(001) Magnetic Thin Films (FePt/MgO(001) 자성박막 결정화의 두께의존성)

  • Jeung, Ji-Wook;Yi, Min-Soo;Cho, Tae-Sik
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.23 no.2
    • /
    • pp.153-158
    • /
    • 2010
  • The crystallization of FePt/MgO(001) magnetic thin films of various thicknesses has been studied using synchrotron x-ray scattering, atomic force microscope, and vibrating sample magnetometer. In film with a 499-$\AA$-thick, face-centered tetragonal, ordered FePt phase was dominantly crystallized into perpendicular (001) grains keeping the magnetically easy c-axis normal to the film plane during annealing. In film with a 816-$\AA$-thick, however, longitudinal (110) grains keeping the c-axis parallel to the film plane were grown on top of the perpendicular (001) grains. The behavior of the magnetic properties was consistent with the thickness dependence of the crystallization. We attribute the thickness dependence of the crystallization to the substrate effect, which prefers the growth of the c-axis oriented perpendicular grains near the film/substrate interfacial area.

Effect of the Cu Bottom Layer on the Properties of Ga Doped ZnO Thin Films

  • Kim, Dae-Il
    • Transactions on Electrical and Electronic Materials
    • /
    • v.13 no.4
    • /
    • pp.185-187
    • /
    • 2012
  • Ga doped ZnO (GZO)/copper (Cu) bi-layered film was deposited on glass substrate by RF and DC magnetron sputtering and then the effect of the Cu bottom layer on the optical, electrical and structural properties of GZO films were considered. As-deposited 100 nm thick GZO films had an optical transmittance of 82% in the visible wavelength region and a sheet resistance of 4139 ${\Omega}/{\Box}$, while the GZO/Cu film had optical and electrical properties that were influenced by the Cu bottom layer. GZO films with 5 nm thick Cu film show the lower sheet resistance of 268 ${\Omega}/{\Box}$ and an optical transmittance of 65% due to increased optical absorption by the Cu metallic bottom layer. Based on the figure of merit, it can be concluded that the thin Cu bottom layer effectively increases the performance of GZO films as a transparent and conducting electrode without intentional substrate heating or a post deposition annealing process.

Permanent Magnet Excitation in Small Axial Flux Driver with MR Sensor and Thin Film Multilayer Winding

  • 최도순
    • Journal of Korea Society of Industrial Information Systems
    • /
    • v.6 no.1
    • /
    • pp.70-76
    • /
    • 2001
  • The disc type driver with Nd-Fe-B magnet is one of the servo drivers, which have many applications in various fields. For efficient and easy, it is desirable to be small and thin in its size. However, the driver which uses a conventional wire reel is very difficult to be reduced in its volume. one of alternatives to achieve the above goal is the thick film multilayer winding. The winding method will significantly reduce the total volume of the driver. Therefor this paper proposed the thick film multilayer winding methods and consists of parts: design manufactures, properties and applications.

  • PDF

Preparation of a PVDF (Polyvinylidene Fluoride) Thin Film Grown by Using the Method of Electric Field Application (전계인가법을 이용한 PVDF 박막의 제작과 특성에 대한 연구)

  • 장동훈;강성준;윤영섭
    • Proceedings of the IEEK Conference
    • /
    • 2000.06b
    • /
    • pp.76-79
    • /
    • 2000
  • The 3$\mu\textrm{m}$-thick PVDF (Polyvinyiidene fluoride) thin film have been prepared using physical vapor deposition with electric field, and its FT-IR specrum, dielectric property and electric conduction phenomenon have been investigated. Since the characteristic peaks ate detected at 509.45 and 1273.6〔cm〕 in the FT-IR spectrum, we are confirmed that the ${\beta}$ -phase is dominant in the PVDF thin film. In the results of dielectric properties, the PVDF thin film shows anomalous dispersion, i.e. gradual decrease of dielectric constant with increase of frequency, and also that the dielectric absorption point changes from 200Hz to 7000Hz with increasing temperature of thin film, which is consistent with the Debye's theory. The activation energy (ΔH) obtained from temperature dependence of dielectric loss is 21.64 ㎉/㏖. We confirm that the electric conduction mechanism of PVDF thin film is dominated by ionic conduction by investigating the dependence of the leakage current of the thin film on the temperature and the electric field.

  • PDF

Fabrication and Characterization of High Temperature Superconducting Thin Film on Metallic Substrate Using Laser Ablation (레이저 증착법을 이용한 금속기판상 고온초전도 박막증착 및 특성분석)

  • Lee, Sang-Yeol
    • Proceedings of the KIEE Conference
    • /
    • 1995.11a
    • /
    • pp.329-331
    • /
    • 1995
  • Laser ablation was used to fabricate superconducting $YBa_2Cu_3O_{7-x}$ (YBCO) thin films on metallic substrates with an YSZ buffer layer. An ArF excimer laser with an wavelength of 193 nm was used to deposit both YSZ buffer layer and superconducting thin film. The characterizations of thin films were performed and compared. With a 200 nm YSZ buffer layer, c-axis orientation and $T_c$=85 K were obtained for a 200 nm-thick YBCO film.

  • PDF

Study of Stress Changes in Nanocrystalline CoW Thin/Thick Film Alloys Eletrodeposited from Citrate Baths (Citrate Baths로부터 전기도금된 나노결정립 CoW 합금 박막/후막의 응력변화에 대한 연구)

  • Cho, Ik-Jong;Park, Deok-Yong;Ihn, Hyun-Man
    • Journal of the Korean Electrochemical Society
    • /
    • v.9 no.4
    • /
    • pp.141-150
    • /
    • 2006
  • Nanocrystalline CoW thin/thick film alloys were electodeposited from citrate baths to investigate the influences of metal ion concentration, current density and solution pH on chemical composition, current efficiency, residual stress, surface morphology, and microstructure of the film. Deposit W (tungsten) content in CoW thin/thick film increased with increasing W ion concentration, current density, and solution pH in the plating bath. It was observed that residual stress in CoW thin/thick film decreased with increasing W ion concentration and solution pH. CoW thin film exhibited mixed phases of hop Co [(100) and (002)] and hcp $Co_3W$ [(002) and (201)] at W ion concentration with 0.02 to 0.08 M. The microstructure of CoW thin film at W ion concentration of 0.1 to 0.2 M was close to amorphous phase. The dominant phases were found to be hop Co (002) and hop $Co_3W$ [(200), (002) and (201)] at the current densities of 5, 10, 25, and $100mA{\cdot}cm^{-2}$ CoW thin film at the current densities of 50 and $75mA{\cdot}cm^{-2}$ was close to amorphous phase. At solution pH 8.7, CoW thin film exhibited hcp Co (002) and hop $Co_3W$ [(200), (002) and (201)]. Below solution pH 8.7, CoW thin film exhibited amorphous microstructure. The optimum electrodeposition conditions for CoW thin/thick film were found to be W ion concentration of 0.08 M, current density of $10mA{\cdot}cm^{-2}$, and solution pH 8.7.

Characteristics of $\pi$-type attenuators using Ti(N) thin film resistors

  • Cuong, Nguyen Duy;Kim, Dong-Jin;Kang, Byoung-Don;Yoon, Soon-Gil
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2007.06a
    • /
    • pp.50-50
    • /
    • 2007
  • We report the effect of the film thickness on electrical properties of Ti(N) film resistors. The applications of titanium nitride thin film resistor in $\Pi$-type attenuators are also characterized. As film thickness decreases from 100 to 30 nm, temperature coefficient of resistance significantly decreases from -60 to -148 ppm/K, while sheet resistance increases from 37 to $270\;{\Omega}/{\square}$. The characterizations of 20dB-attenuators using thin film resistors are improved in comparison with those using thick film resistors. The $\Pi$-type attenuators using Ti(N) thin film resistors exhibit a attenuation of -19.94 dB and voltage standing wave ratio of 1.16 at a frequency of 2.7 GHz.

  • PDF

Electrical property of polyvinylalcohol (Polyvinylalcohol의 전기적 특성)

  • 김현철;구할본
    • Electrical & Electronic Materials
    • /
    • v.8 no.2
    • /
    • pp.184-189
    • /
    • 1995
  • The electrical property of ultra thin PVA films(several hundreds .angs.-several .mu.m in thickness) formed by sphere bulb blowing technique, has been studied. The electrical conductivity of relatively thick films(>several thousands .angs.) has been very high and enhanced by the exposure either to high humidity of air or $NH_3$, which can be explained in terms of the role of ionic transport. The use of PVA films as NH$_{3}$ sensor is also proposed. In ultra thin PVA films less than 1500.angs., two conducting states ; high conducting and low conducting states, are observed. The nonlinear current-voltage characteristics in the low conducting state and the switching between these two states are also confirmed. These properties are discussed in terms of electronic conduction processes. The breakdown strength of the ultra thin PVA film is found to be very high(-30MV/cm), supporting the electron avalanche process in a thick polymer films.

  • PDF

Crystallization of FePt/MgO(100) magnetic thin films (FePt/MgO(100) 자성박막의 결정화 연구)

  • Jeung, Ji-Wook;Cho, Tae-Sik;Yi, Min-Soo
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2005.07a
    • /
    • pp.278-279
    • /
    • 2005
  • The crystallization of FePt/MgO(100) magnetic thin films of various thicknesses has been studied using synchrotron x-ray scattering, atomic force microscope, and vibrating sample magnetometer. In film with a 500-${\AA}$-thick, ordered (fct) FePt phase was dominantly crystallized into perpendicular (001) grains keeping the magnetically easy c-axis normal to the film plane during annealing. In film with a 812-${\AA}$-thick, however, longitudinal (110) grains keeping the c-axis parallel to the film plane were grown on top of the perpendicular (001) grains. The behavior of the magnetic properties was consistent with the thickness dependence of the crystallization. We attribute the thickness dependence of the crystallization to the substrate effect, which prefers the growth of the c-axis oriented perpendicular grains near the film/substrate interfacial area.

  • PDF