• 제목/요약/키워드: Thermal-Stress

검색결과 3,041건 처리시간 0.031초

The effect of thermo-mechanical fatigue on the retentive force and dimensional changes in polyetheretherketone clasps with different thickness and undercut

  • Guleryuz, Aysegul;Korkmaz, Cumhur;Sener, Ayse;Tas, Mehmet Ozan
    • The Journal of Advanced Prosthodontics
    • /
    • 제13권5호
    • /
    • pp.304-315
    • /
    • 2021
  • PURPOSE. Esthetic expectations have increased the use of polyetheretherketone (PEEK) clasps as alternatives to Cr-Co in removable partial dentures (RPDs). The objective of this study was to evaluate the retentive force and dimensional change of clasps with different thickness and undercut made from PEEK by the thermo-mechanical fatigue. MATERIALS AND METHODS. PEEK clasps (N = 48) with thicknesses of 1 or 1.50 mm and 48 premolar monolithic zirconia crowns with undercuts of 0.25 mm or 0.50 mm were fabricated. Samples are divided into four groups (C1-C4) and were subjected to 7200 thermal aging cycles (at 5 - 55℃). The changes in the retentive force and dimensions of the clasps were measured by micro-stress testing and micro-CT devices from five measurement points (M1 - M5). One-way ANOVA, paired t-test, two-way repeated ANOVA, and post-hoc tests were used to analyze the data (P < .05). RESULTS. The retentive forces of C1, C2, C3, and C4 groups in initial and final test were found to be 4.389-3.388 N, 4.67 - 3.396 N, 5.161 - 4.096 N, 5.459 - 4.141 N, respectively. The effects of retentive force of all PEEK clasps groups were significant decreased. Thermo-mechanical cycles caused significant dimensional changes at points with M2, M4, and M5, and abraded the clasp corners and increased the distance between the ends of the clasp, resulting in reduced retentive forces (P* = .016, P* = .042, P < .001, respectively). CONCLUSION. Thermo-mechanical aging decreases the retentive forces in PEEK clasps. Increasing the thickness and undercut amount of clasps decreases the amount of dimensional change. The values measured after aging are within the clinically acceptable limits.

고온 시효 시험에 따른 Epoxy 솔더 접합부의 접합 특성 평가 (Evaluation of Bonding Properties of Epoxy Solder Joints by High Temperature Aging Test)

  • 강민수;김도석;신영의
    • 한국전기전자재료학회논문지
    • /
    • 제32권1호
    • /
    • pp.6-12
    • /
    • 2019
  • Bonding properties of epoxy-containing solder joints were investigated by a high temperature aging test. Specimens were prepared by bonding an R3216 standard chip resistor to an OSP-finished PCB by a reflow process with two basic types of solder (SAC305 & Sn58Bi) pastes and two epoxy-solder (SAC305+epoxy & Sn58Bi+epoxy) pastes. In all epoxy solder joints, an epoxy fillet was formed in the hardened epoxy, lying around the outer edge of the solder joint, between the chip and the Cu pad. In order to analyze the bonding characteristics of solder joints at high temperatures, a high-temperature aging test at $150^{\circ}C$ was carried out for 14 days (336 h). After aging, the intermetallic compound $Cu_6Sn_5$ was found to have formed in the solder joint on the Cu pad, and the shear stress on the conventional solder joint was reduced by a significant amount. The reason that the shear force did not decrease much, even though in epoxy solder, was thatbecause epoxy hardened at the outer edge of the supported solder joints. Using epoxy solder, strong bonding behavior can be ensured due to this resistance to shear force, even in metallurgical changes such as those where intermetallic compounds form at solder joints.

비정질 인듐-갈륨-아연 산화물 기반 박막 트랜지스터의 NBIS 불안정성 개선을 위한 연구동향 (Research Trends for Improvement of NBIS Instability in Amorphous In-Ga-ZnO Based Thin-Film Transistors)

  • 윤건주;박진수;김재민;조재현;배상우;김진석;김현후;이준신
    • 한국전기전자재료학회논문지
    • /
    • 제32권5호
    • /
    • pp.371-375
    • /
    • 2019
  • Developing a thin-film transistor with characteristics such as a large area, high mobility, and high reliability are key elements required for the next generation on displays. In this paper, we have investigated the research trends related to improving the reliability of oxide-semiconductor-based thin-film transistors, which are the primary focus of study in the field of optical displays. It has been reported that thermal treatment in a high-pressure oxygen atmosphere reduces the threshold voltage shift from -7.1 V to -1.9 V under NBIS. Additionally, a device with a $SiO_2/Si_3N_4$ dual-structure has a lower threshold voltage (-0.82 V) under NBIS than a single-gate-insulator-based device (-11.6 V). The dual channel structure with different oxygen partial pressures was also confirmed to have a stable threshold voltage under NBIS. These can be considered for further study to improve the NBIS problem.

Thermal and light impacts on the early growth stages of the kelp Saccharina angustissima (Laminariales, Phaeophyceae)

  • Augyte, Simona;Yarish, Charles;Neefus, Christopher D.
    • ALGAE
    • /
    • 제34권2호
    • /
    • pp.153-162
    • /
    • 2019
  • Anthropogenic disturbances, including coastal habitat modification and climate change are threatening the stability of kelp beds, one of the most diverse and productive marine ecosystems. To test the effect of temperature and irradiance on the microscopic gametophyte and juvenile sporophyte stages of the rare kelp, Saccharina angustissima, from Casco Bay, Maine, USA, we carried out two sets of experiments using a temperature gradient table. The first set of experiments combined temperatures between $7-18^{\circ}C$ with irradiance at 20, 40, and $80{\mu}mol\;photons\;m^{-2}\;s^{-1}$. The second set combined temperatures of $3-13^{\circ}C$ with irradiance of 10, 100, and $200{\mu}mol\;photons\;m^{-2}\;s^{-1}$. Over two separate 4-week trials, in 2014 and again in 2015, we monitored gametogenesis, the early growth stages of the gametophytes, and early sporophyte development of this kelp. Gametophytes grew best at temperatures of $8-13^{\circ}C$ at the lowest irradiance of $10-{\mu}mol\;photons\;m^{-2}\;s^{-1}$. Light had a significant effect on both male and female gametophyte growth only at the higher temperatures. Temperatures of $8-15^{\circ}C$ and irradiance levels of $10-100{\mu}mol\;photons\;m^{-2}\;s^{-1}$ were conditions for the highest sporophyte growth. Sporophyte and male gametophyte growth was reduced at both temperature extremes-the hottest and coldest temperatures tested. S. angustissima is a unique kelp species known only from a very narrow geographic region along the coast of Maine, USA. The coupling of global warming with high light intensity effects might pose stress on the early life-history stages of this kelp, although, as an intertidal species, it could also be better adapted to temperature and light extremes than its subtidal counterpart, Saccharina latissima.

간헐 압축응력완화 시험법과 시간-온도 중첩 이론을 이용한 NBR 오링의 노화 거동 분석 연구 (Study on the Degradaion Behavior of Acrylonitrile Rubber(NBR) O-ring by Intermittent CSR and Time-Temperature Superposition Principle)

  • 이진혁;배종우;최명찬;윤유미;김원호;박성한;조남주
    • 한국추진공학회지
    • /
    • 제23권1호
    • /
    • pp.46-51
    • /
    • 2019
  • Intermittent CSR 측정법을 이용하여 NBR 오링의 노화 거동과 수명 예측에 관하여 연구하였다. Intermittent CSR jig는 오링의 실제 사용 환경을 고려하여 설계 제작하였다. 오링의 노화 거동은 $40{\sim}120^{\circ}C$에서의 가속 노화 연구를 통하여 관찰하였다. 오링은 $80^{\circ}C$ 이하에서 비선형 노화 거동을 나타내었다. 오링의 수명은 고장 조건 20%에 대하여 Arrhenius plot으로부터 32.5년, WLF plot으로 부터 22.6년으로 나타났다.

Berberine Alleviates Paclitaxel-Induced Neuropathy

  • Rezaee, Ramin;Monemi, Alireza;SadeghiBonjar, Mohammad Amin;Hashemzaei, Mahmoud
    • 대한약침학회지
    • /
    • 제22권2호
    • /
    • pp.90-94
    • /
    • 2019
  • Objectives: Paclitaxel (PTX) as an anticancer drug used against solid cancers, possesses adverse reactions such as neuropathic pain which has confined its use. PTX-induced neuropathic pain is mediated via activation of oxidative stress. Berberine (BER), an isoquinoline phytochemical found in several plants, exerts strong antioxidant and painkilling properties. In the current study, we aimed to evaluate pain-relieving effect of BER in a mouse model of PTX-induced neuropathic pain. Methods: This study was done using 42 male albino mice that were randomly divided into 6 groups (n = 7) as follow: Sham-operated (not treated with PTX), negative control group (PTX-treated mice receiving normal saline), BER 5, 10, and 20 mg/kg (PTX-treated mice receiving BER) and positive control group (PTX-treated mice receiving imipramine 10 mg/kg). Neuropathic pain was induced by intraperitoneal administration of four doses of PTX (2 mg/kg/day) on days 1, 3, 5 and 7. Then, on day 7, hot plate test was done to assess latency to heat to measure possible anti-neuropathic pain effect of BER. Results: Four doses of PTX 2 mg/kg/day induced neuropathy that was reduced by BER at all time-points (i.e. 0, 30, 60, 90 and 120 min) after injection (P < 0.001 in comparison to control). The statistical analysis of data showed significant differences between groups (P < 0.001 in comparison to negative control), at 30, 60, 90 and 120 min after injection of BER 5, 10 and 20 mg/kg; in other words, 30, 60, 90 and 120 min after BER administration, neuropathic pain was significantly reduced as compared to normal saline-treated mice. Conclusion: Altogether, our results showed that PTX could induce neuropathic pain as reflected by hyperalgesia and BER could alleviate PTX-induced thermal hyperalgesia.

마그네슘 합금 표면의 지르코니아 분말 레이저 소결과정에서 조사 패턴이 접합 계면 품질에 미치는 영향 (Effect of Laser Processing Patterns on the Bonding Interface Quality during Laser Sintering of Magnesium Alloys with Zirconia)

  • 윤상우;김주한
    • 한국기계가공학회지
    • /
    • 제20권2호
    • /
    • pp.51-57
    • /
    • 2021
  • The quality of the ceramic sintered coating on a metal surface through laser surface treatment is affected by the laser irradiation pattern. Depending on the laser irradiation pattern, the amount of residual stress and heat applied or accumulated on the surface increases or decreases, affecting the thickness attained in the ceramic sintering area. When the heat energy accumulated in the sintering area is high, the ceramic and the metal alloy melt and sufficiently mix to form a homogeneous and thick bonding interface. In this study, the thermal energy accumulation in the region sintered with zirconia was controlled using four types of laser processing patterns. The thickness of the diffusion region is analyzed by laser-induced breakdown spectroscopy of Mg-ZrO2 generated by laser sintering zirconia powder on the magnesium alloy surface. On the basis of the analysis of the Mg and Zr present in the sintered region through LIBS, the effect of the irradiation pattern on the sintering quality is confirmed by comparing and analyzing the heat and mass transfer tendency of the diffusion layer and the degree of diffusion according to the irradiation pattern. The derived diffusion coefficients differed by up to 9.8 times for each laser scanning pattern.

FTIR 분자구조 해석을 통한 에폭시-실리카 나노복합소재의 열기계적 물성 연구 (Study on the Thermomechanical Properties of Epoxy-Silica Nanocomposites by FTIR Molecular Structure Analyses)

  • 장서현;한유수;황도순;정주원;김영국
    • 마이크로전자및패키징학회지
    • /
    • 제28권2호
    • /
    • pp.51-57
    • /
    • 2021
  • 이 연구에서는 에폭시 수지에 포함된 나노 실리카 입자의 농도가 재료의 열/기계적 물성에 미치는 영향에 대해 알아보았다. 약 12 nm 크기의 나노 입자를 에폭시 수지에 다섯가지 무게비로 섞은 나노복합소재를 제작하였다. DMA와 TMA 방법을 이용하여 유리전이온도, 응력이완, 열팽창 거동을 측정하였다. 이를 통해 나노입자가 재료의 점탄성 거동에 어떠한 영향을 미치는지 보였다. 실리카 입자의 함량이 증가할수록 순수 에폭시 재료 대비 탄성 물성은 증가하였고, 유리전이온도는 감소하였다. FTIR 결과는 분자구조의 관점에서 충진제 함량에 따른 물성변화의 원인을 찾고 나노입자가 에폭시 분자 구조에 어떠한 영향을 미치는지를 규명하는데 중요한 역할을 하였다.

리튬용융염에서 플라즈마 용사된 부분안정화 지르코니아 코팅층의 고온부식 거동 (Hot Corrosion Behavior of Plasma-Sprayed Partially Stabilized Zirconia Coatings in a Lithium Molten Salt)

  • 조수행;홍순석;강대승;박병흥;허진목;이한수
    • 대한금속재료학회지
    • /
    • 제46권10호
    • /
    • pp.646-651
    • /
    • 2008
  • The electrolytic reduction of spent oxide fuel involves the liberation of oxygen in a molten LiCl electrolyte, which results in a chemically aggressive environment that is too corrosive for typical structural materials. It is essential to choose the optimum material for the process equipment handling molten salt. IN713LC is one of the candidate materials proposed for application in electrolytic reduction process. In this study, yttria-stabilized zirconia (YSZ) top coat was applied to a surface of IN713LC with an aluminized metallic bond coat by an optimized plasma spray process, and were investigated the corrosion behavior at $675^{\circ}C$ for 216 hours in the molten salt $LiCl-Li_2O$ under an oxidizing atmosphere. The as-coated and tested specimens were examined by OM, SEM/EDS and XRD, respectively. The bare superalloy reveals obvious weight loss, and the corrosion layer formed on the surface of the bare superalloy was spalled due to the rapid scale growth and thermal stress. The top coatings showed a much better hot-corrosion resistance in the presence of $LiCl-Li_2O$ molten salt when compared to those of the uncoated superalloy and the aluminized bond coatings. These coatings have been found to be beneficial for increasing to the hot-corrosion resistance of the structural materials for handling high temperature lithium molten salts.

냉각 성능 향상을 위한 고속철도 제동 디스크 허브의 해석 연구 (Analytical Study of High Speed Railway Braking Disc-hub for Enhancement of Cooling Performance)

  • 이용우;김장훈
    • 한국산학기술학회논문지
    • /
    • 제22권3호
    • /
    • pp.199-207
    • /
    • 2021
  • 본 연구는 한국형고속철도(KTX)의 제동장치의 국산화를 통한 성능 개선을 위한 목적으로 수행되었다. 본 연구에서 기존 수입에 의존하고 있는 고속철도용 제동 디스크 허브를 국산화하기 위하여 유한요소 해석을 통해 성능을 분석하고 제동 시험결과와 상관도 분석을 통해 모델의 검증을 수행하였다. 또한, 제동시 발생할 수 있는 기계적인 특성을 검토하기 위하여 마찰열에 의한 열전달-열응력 해석, 고유진동해석 및 강도해석을 수행하였다. 디스크 허브 국산화 신규 모델의 개발을 위해 형상에 따른 설계 인자를 도출하고 파라미터 해석을 수행하여 방열성능을 향상시키고 경량화를 위한 최적 사양을 도출하고자 하였다. 개발 모델을 기존 모델과 비교한 결과 기존 모델 대비 제동시 발생하는 허브의 최고 온도가 낮아졌으며, 냉각 효율이 향상되었음 확인할 수 있었다. 또한, 고유진동수 및 강도 특성 또한 동등 수준 이상의 성능을 확보한 설계임을 확인하였다. 본 연구 결과는 철도차량 및 수송기기 분야의 제동 디스크 시스템 개발에 활용될 수 있을 것으로 기대된다.