• Title/Summary/Keyword: Thermal Cracks

Search Result 443, Processing Time 0.03 seconds

Reliability evaluation of brittle structures under thermal shocks (열충격이 작용하는 취성구조의 신뢰성 평가)

  • 이치우;장건익;김종태
    • Journal of Ocean Engineering and Technology
    • /
    • v.12 no.1
    • /
    • pp.58-64
    • /
    • 1998
  • An analysis method for the reliability of ceramic structures subjected to thermal shocks is presented. Flaws with the size of given probability distribution function are assumed to be distributed at random with a certain density per unit volume in the structures. Criterions for crack instability are derived for brittle solids under general thermal stresses. A probabilistic failure model is presented to study the probability of crack instability for brittle solids containing cracks with uncertain size. The reliabilities of brittle structures are evaluated based on the weakest-link hypothesis, which states that a structure fails when the cracks in any differential volume become unstable. A numerical example is given to demonstrate the application of the proposed method.

  • PDF

A Feasibility Study on the Use of Autogeneous GTAW for Correction of Distortions in Welded Aluminum Alloy Structures (알루미늄 熔接構造物의 變形橋正을 위한 Autogeneous GTAW의 適用 可能性 硏究)

  • 하용훈;강춘식;유순영
    • Journal of Welding and Joining
    • /
    • v.10 no.1
    • /
    • pp.20-34
    • /
    • 1992
  • Characteristics of two correcting methods, a new Autogeneous GTAW heating (TIG) method and the conventional GMAW bead-on plate welding(MIG) method, for distorted aluminum fabrication structures were studied. As a result of microscopic study of Autogeneous GTAW heating and GMAW bead-on plate welding areas, porosities in weld metal and surface cracks in local heating zone were found. Through the mechanical tests, it was verified that porosities decrease tensile strength and surface of distortion, angular displacement and transeverse shrinkage were measures and compared. In order to investigate changes of material properties in heating area and cause of defects such thermal stresses were calculated by ADINA. Through the computations of transient thermal stresses and microscopic observation of fracture surface, thermal stress was found to be the cause of crack during Autogeneous GTAW heating.

  • PDF

Thermal Behavior Analysis in Continuous Bloom Casting Mold (Bloom용 연속주조 몰드의 열거동 해석)

  • 정영진;김성훈;김영모;강충길
    • Transactions of Materials Processing
    • /
    • v.13 no.4
    • /
    • pp.319-325
    • /
    • 2004
  • Continuous casting machine has been experienced a rapid development to increase productivity with high casting speed and to meet consumer's strict demands for high quality. However, because most of defects and cracks are initially formed in mold and grown into surface cracks during the post process, more specific and clear investigations upon heat transfer mechanism between mold and solidified shell are necessarily needed. In this study heat transfer coefficients which shows the characteristic of heat transfer mechanism are calculated with temperatures measured in bloom mold using optimal algorithm, and thermal analysis are investigated using the calculated heat transfer coefficients. Finally uniformity of solidified shell is investigated for high carbon steel, 0.187%C from thermal analysis.

Reliability Evaluation of Ceramic Structures Under Thermal Shocks (열충격이 작용하는 세라믹구조의 신뢰성 평가)

  • 김종태;심확섭;장건익;이치우;이환우
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 1996.11a
    • /
    • pp.954-958
    • /
    • 1996
  • An analysis method for the reliability of ceramic structures subjected to thermal shocks is presented, Flaws with the size of given probability distribution function are assumed to be distributed at random with a certain density per unit volume in the structures. Criterions for crack instability are derived for brittle solids under general thermal stresses. A probabilistic failure model is presented to study the probability of crack instability for blittle solids containing cracks with uncertain crack size. The reliabilities of brittle structures are evaluated based on the weakest-link hypothesis, which states that a structure fails when the cracks in any differential volume become unstable. A numerical example is given to demonstrate the application of the proposed method.

  • PDF

Regularity and coupling correlation between acoustic emission and electromagnetic radiation during rock heating process

  • Kong, Biao;Wang, Enyuan;Li, Zenghua
    • Geomechanics and Engineering
    • /
    • v.15 no.5
    • /
    • pp.1125-1133
    • /
    • 2018
  • Real-time characterization of the rock thermal deformation and fracture process provides guidance for detecting and evaluating thermal stability of rocks. In this paper, time -frequency characteristics of acoustic emission (AE) and electromagnetic radiation (EMR) signals were studied by conducting experiments during rock continuous heating. The coupling correlation between AE and EMR during rock thermal deformation and failure was analyzed, and the microcosmic mechanism of AE and EMR was theoretically analyzed. During rock continuous heating process, rocks simultaneously produce significant AE and EMR signals. These AE and EMR signals are, however, not completely synchronized, with the AE signals showing obvious fluctuation and the EMR signals increasing gradually. The sliding friction between the cracks is the main mechanism of EMR during the rock thermal deformation and fracture, and the AE is produced while the thermal cracks expanding. Both the EMR and AE monitoring methods can be applied to evaluate the thermal stability of rock in underground mines, although the mechanisms by which these signals generated are different.

Vibration analysis of carbon nanotubes with multiple cracks in thermal environment

  • Ebrahimi, Farzad;Mahmoodi, Fatemeh
    • Advances in nano research
    • /
    • v.6 no.1
    • /
    • pp.57-80
    • /
    • 2018
  • In this study, the thermal loading effect on free vibration characteristics of carbon nanotubes (CNTs) with multiple cracks is studied. Various boundary conditions for nanotube are taken in to account. In order to take the small scale effect, the nonlocal elasticity of Eringen is employed in the framework of Euler-Bernoulli beam theory. This theory states that the stress at a reference point is a function of strains at all points in the continuum. A cracked nanotube is assumed to be consisted of two segments that are connected by a rotational spring which is located in the position of the cracked section. Hamilton's principle is used to achieve the governing equations. Influences of the nonlocal parameter, crack severity, temperature change and the number of cracks on the system frequencies are investigated. Also, it is found that at room or lower temperature the natural frequency for CNT decreases as the value of temperature change increases, while at temperature higher than room temperature the natural frequency of CNT increases as the value of temperature change increases. Various boundary conditions have been applied to the nanotube.

Consideration of Constraint Effect of Surface Cracks Under PTS Conditions Using J-Q Approach (PTS 사고하에서 J-Q해석법을 이용한 표면균열의 구속효과 고찰)

  • Kim, Jin-Su;Choe, Jae-Bung;Kim, Yun-Jae;Kim, Yeong-Jin
    • Transactions of the Korean Society of Mechanical Engineers A
    • /
    • v.26 no.1
    • /
    • pp.105-112
    • /
    • 2002
  • In recent years, the integrity of reactor Pressure Vessel(RPV) under pressurized thermal shock (PTS) accident has been treated as one of the most critical issues. Under PTS condition, the combination of thermal and mechanical stress by steep temperature gradient and internal pressure causes considerably high tensile stress at the inside of RPV wall. As a result, cracks on inner surface of RPV may experience elastic-plastic behavior which can be characterized by J-integral. In such a case, however, J-integral may possibly lose its vapidity due to the constraint effect. The degree of constraint effect is influenced by the loading mode, crack geometry and material properties. In this paper, in order to investigate the effect of clad thickness and crack geometry on constraint effect, three dimensional finite element analyses were performed for various surface cracks. Total of 27 crack geometries were analyzed and results were presented by a two-parameter characterization based on the J-integral and the f-stress.

Comparison of Degradation Behaviors for Titanium-based Hard Coatings by Pulsed Laser Thermal Shock

  • Jeon, Seol;Lee, Heesoo
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.6
    • /
    • pp.523-527
    • /
    • 2013
  • Ti-based coatings following laser ablation were studied to compare degradation behaviors by thermomechanical stress. TiN, TiCN, and TiAlN coatings were degraded by a Nd:YAG pulsed laser with an increase in the laser pulses. A decrease in the hardness was identified as the pulses increased, and the hardness levels were in the order of TiAlN > TiCN > TiN. The TiN showed cracks on the surface, and cracks with pores formed along the cracks were observed in the TiCN. The dominant degradation behavior of the TiAlN was surface pore formation. EDS results revealed that diffusion of substrate atoms to the coating surface occurred in the TiN. Delamination occurred in the TiN and TiCN, while the TiAlN which has higher thermal stability than the TiN and TiCN maintained adhesion to the substrate. It was considered that the decrease in the hardness of the Ti-based hard coatings is attributed to surface cracking and the diffusion of substrate atoms.

Interfacial degradation of thermal barrier coatings in isothermal and cyclic oxidation test

  • Jeon, Seol;Lee, Heesoo;Choi, Youngkue;Shin, Hyun-Gyoo;Jeong, Young-Keun
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.24 no.4
    • /
    • pp.151-157
    • /
    • 2014
  • The degradation mechanisms of thermal barrier coatings (TBCs) were investigated in different thermal fatigue condition in terms of microstructural analyses. The isothermal and cyclic oxidation tests were conducted to atmospheric plasma sprayed-TBCs on NIMONIC 263 substrates. The delamination occurred by the oxide layer formation at the interface, the Ni/Cr-based oxide was formed after Al-based oxide layer grew up to ${\sim}10{\mu}m$ in the isothermal condition. In the cyclic oxidation with dwell time, the failure occurred earlier (500 hr) than in the isothermal oxidation (900 hr) at same temperature. The thickness of Al-based oxide layer of the delaminated specimen in the cyclic condition was ${\sim}4{\mu}m$ and the interfacial cracks were observed. The acoustic emission method revealed that the cracks generated during the cooling step. It was considered that the specimens were prevented from the formation of the Al-based oxide by cooling treatment, and the degradation mode in the cyclic test was dominantly interfacial cracking by the difference of thermal expansion coefficients of the coating layers.

Thermal Stress Intensity Factors for Rigid Inclusions of Cusp Crack Shape (커스프균열형 강체함유물의 열응력 세기계수에 관한 연구)

  • 이강용;최흥섭
    • Transactions of the Korean Society of Mechanical Engineers
    • /
    • v.12 no.3
    • /
    • pp.497-504
    • /
    • 1988
  • The steady state thermal stress intensity factors (TSIF's) are analyzed for hypocycloid, symmetric airfoil and symmetric lip type rigid inclusions embedded in infinite elastic solids, using Boganoff's complex variable approach in plane thermoplasticity. Two thermal conditions are considered, one with an uniform heat flow disturbed by an insulated rigid inclusion of cusp crack shape and the other with an uniform heat flow disturbed by a rigid inclusion of cusp crack shape with fixed boundary temperature. The tendencies of TSIF's for rigid inclusions of cusp crack shape are somewhat different from those of traction free cusp cracks. However, if k=-1, the non-dimensionalized TSIF's for rigid inclusions of cusp crack shape become those of traction free cusp cracks like the tendencies of the SIF's under mechanical loading conditions. The thermal stress and displacement components for a rigid circular inclusion of radius Ro are drived from the results of a hypocycloid crack type rigid inclusion.