Kim, Seong-Hwan;Kim, Dong-Ho;Kim, Hyun-Oh;Lee, Bong-Hak
Journal of Industrial Technology
/
v.23
no.A
/
pp.149-156
/
2003
The development and maintenance of a sound bond are essential requirements of concrete repair and replacement. The bond property of a overlay to its substrate concrete during the lifetime is one of the most important performance requirements which should be quantified. A standard or a verified bond strength measurement method is required at field for screening, selecting materials and quality control for overlay or repair materials, but no test method has been adopted as a standard. In this study, a concrete pull off bond strength measurement method for field application is proposed and evaluated. This study compares the splitting tensile test, slant shear test, nipple pipe direct tensile test, flexural adhesion test, briquette tensile test, jumbo nail pull-out test and core pull-off test with their test procedures. From these comparison and investigation, core pull-off test is selected as a main topic of this study because of it's suitability for in situ testing, simplicities in field application and clearness at interface boundary condition. Thus, the proposed core pull off test is evaluated to be the most appropriate method for field application in a simple manner. The fracture surface and fracture mode could be easily determined by visual observation of failure surface of the field specimen. The core pull off test was found to be sensitive to surface condition and latex contents at latex modified concrete.
Journal of the Korean Institute of Landscape Architecture
/
v.33
no.2
s.109
/
pp.32-47
/
2005
This study was carried out to investigate and propose a green-wall system with evergreen plants for urban greening of Tongyeong City. To achieve these goals, the requirements and possibilities for wall greening were investigated and evaluated considering the location, topography, and climate of Tongyeong City. Existing walls were analyzed and then a suitable green wall system is proposed. Tongyeong City and its 151 islands covers the central and the southern parts of the Goseong peninsula. Most of the land is covered with hills and mountains; $43.9\%$ of the land area has a slope greater than $15\%$ and most hills and mountains near the urban area have a slope of more than $30\%$. As a result of the topographical properties, concrete retaining walls can often be seen along the streets in urbanized areas. These retaining walls are not only unattractive, but they also create environmental problems, and thus should be replaced with native evergreen plants. Options for replacing the retaining walls include evergreen vine-plants such as Hedaa spp. and Euonymus radicans, but native evergreen shrubs such as Pittosporum tobira, Nandina domestica, Raphiolepis umbellata, Ilex cornuta, flex crenata, Fatsia japonic, and Aucuba japonica may be a more attractive option. Current wall conditions are unsuitable for planting vines, therefore, a reservoir-drainage-type plant box filled with a light artificial substrate is required for greening these concrete retaining walls. These might be irrigated in the dry season and fertilized annually by an appropriate system. These plant boxes could be attached along the entire walls. An experiment investigating effects of substrates and bark-chip mulching on the growth of Hedera spp. showed that the mixture of cerasoil and field soil(v/v, 4:6) was superior to field soil alone and to the mixture of perlite small grain, large grain, and field soil(v/v/v, 2:2:6). Bark-chip mulching tended to increase the growth of Hedera spp..
Several techniques have been developed for shear strengthening of reinforced concrete (RC) members by using fiber reinforced polymer (FRP) composites. However, debonding of FRP retrofits from concrete substrate still deemed as a challenging concern in their application which needs to be scrutinized in details. As a result, this paper reports on the results of an experimental investigation on shear strengthening of RC beams using near surface mounted (NSM) FRP reinforcing bars. The main objective of the experimentation was increasing the efficiency of shear retrofits by precluding/postponing the premature debonding failure. The experimental program was comprised of six shear deficient RC beams. The test parameters include the FRP rebar spacing, inclination angle, and groove shape. Also, an innovative modification was introduced to the conventional NSM technique and its efficiency was evaluated by experimental observation and measurement. The results testified the efficiency of glass FRP (GFRP) rebars in increasing the shear strength of the test specimens retrofitted using conventional NSM technique. However, debonding of FRP bars impeded exploiting all retrofitting advantages and induced a premature shear failure. On the contrary, application of the proposed modified NSM (MNSM) technique was not only capable of preventing the premature debonding of FRP bars, but also could replace the failure mode of specimen from the brittle shear to a ductile flexural failure which is more desirable.
Proceedings of the Korean Institute of Building Construction Conference
/
2017.05a
/
pp.77-78
/
2017
Although many waterproofing materials and techniques have been developed and applied, there is still a leakage in concrete structures. The main reason for the failure of waterproofing is due to the lack of consideration of the environmental conditions and the inconsistent performance requirement of the waterproofing materials in response to the complexity of the environmental conditions., and materials that are unsuitable to the environment are still being selected for usage due to their low price. Moreover, there is no valid test assessment for waterproofing materials to be used prior to actual application in the construction site. The development of a testing method and apparatus that can evaluate the composite waterproofing method is proposed in this paper and an interpretation method that can analyze the results of the evaluation.
This study was performed to develop repair and reinforcing materials in sewage drain pipe by using 40% of CAC(Calcium Aluminate Cement) and 4% of Polymer Powder. Regarding reinforcing materials to enhance load-bearing capacity, polyester textile and wire mesh were adopted and then they were evaluated by the measurement of deflection and Stress-strain Relationship. Two types of drain pipe made by concrete and PE were considered as plain specimens and then loading test were performed after repaired by CAC mortar impregnated reinforcing materials. As the test results of the load-bearing test on both drain pipe, there was higher load-bearing capacity on the specimen adopted wire mesh but debonding of repair mortar was found due to stiffness of wire mesh. By the way, repair system using CAC mortar impregnated polyster textile without wire mesh showed satisfactory results including bonding and load-bearing capacity regardless substrate, so this repair system using by mixture of CAC mortar and polyster textile is suggested as the reasonable repairing method within this experimental scope.
Ji, Sung-Jun;Pyeon, Su-Jeong;Choi, Byung-Cheol;Kim, Jae-Hwan;Kim, Do-Su;Nam, Jeong-Soo
Journal of the Korea Institute of Building Construction
/
v.24
no.1
/
pp.35-42
/
2024
This research explores the potential of methyl methacrylate(MMA) as a material for road repair applications. It specifically examines two MMA formulations, referred to as type A and type B, in relation to their performance on concrete substrates. The evaluation criteria included drying time, tensile bond strength, and resistance to alkali. The condition of the substrate surface was varied across three curing environments: constant temperature and humidity(R), immersion in water(W), and immersion in water with chloride ions(N). The findings indicate that type B MMA exhibits a quicker drying time and superior resistance to alkali compared to type A. While type A demonstrated greater tensile bond strength, it failed to maintain adhesion with the concrete base. Based on the parameters tested in this study, type B MMA emerges as the more favorable option for road repair contexts. Nonetheless, the study underscores the necessity for additional testing on asphalt substrates to fully assess the material's durability and applicability for long-term road maintenance.
Proceedings of the Korean Institute of Building Construction Conference
/
2002.11a
/
pp.23-27
/
2002
Waterproofing is one of the important factor to improve performance of building elements. But existing repair system for waterproofing have many problems like a damage of waterproof layer due to movement of concrete substrate, blistering effect and moisture condition. So waterproofing layer can not play an important part to improve waterproofing function and performance of building. Therefore, new waterproofing system to solve these problems of existing waterproofing system is developed. In this paper, new waterproofing system in water-leakage repair for remodeling is introduced
Proceedings of the Korean Institute of Building Construction Conference
/
2006.11a
/
pp.61-65
/
2006
Urethane, epoxy, acrylic have common property to adhere on the concrete dried surface in the waterproofing materials at present. In the wet condition, however, the materials such as urethane, epoxy, acrylic need a long hardening time and it become a reason of water leakage as the materials breaking down. it is one of the problem to adhere to the substrate. Therefore, in this thesis, I focused to assure the structural safety and durability and quality for waterproofing and safe of construction cost by cut down the cost of labor and reduce the term of works as searching the application of field condition for hish adhesive spray type of degenerated and rubberized asphalt membrane material.
Proceedings of the Korean Institute of Building Construction Conference
/
2017.11a
/
pp.219-220
/
2017
Current domestic waterproofing market in Korea mainly uses single-ply waterproofing materials comprised of coatings or waterproof sheets and two or more-ply composite waterproofing methods. In order to evaluate these types of composite waterproofing systems, a new test equipment and method that incorporates various deterioration conditions (joint displacement, chemical exposure, water pressure etc) was developed. In a comparison testing, the results showed that flexible type materials have higher response performance towards joint displacement than the hardened material. Furthermore, the importance of securing the stability of the waterproofing method in the vulnerable over-lap joint areas of waterproofing sheets is emphasized.
In this paper, the dynamic characteristics of a composite cylindrical beam made of a mechanism of carbon dioxide absorption coated on the tube core are investigated based on the classical beam theory coupled with the modified couple stress theory. The composite tube structures are assumed to be uniform along the tube length, and the energy method regarding the Hamilton principle is utilized for generating the governing equations. A powerful numerical solution, the generalized differential quadrature method (GDQM), is employed to solve the differential equations. The carbon dioxide trapping mechanism is a composite consisting of a polyacrylonitrile substrate and a cross-link polydimethylsiloxane gutter layer. Methacrylate, poly (ethylene glycol), methyl ether methacrylate, and three pedant methacrylates are all taken into account as potential mechanisms for capturing carbon dioxide. The application of the present study is helpful in the design and production of microelectromechanical systems (MEMS) and the different valuable parameters, such as the length-scale parameter, rate of section change, aspect ratio, etc., are presented in detail.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.