• Title/Summary/Keyword: Strength of bending

Search Result 2,733, Processing Time 0.031 seconds

Hydrophobic property of surface glaze of ceramic tiles by copper powder addition (구리 분말 첨가를 통한 도자타일 표면유약의 소수화 특성)

  • Choi, Cheong-Soo;Han, Kyu-Sung;Hwang, Kwang-Taek;Kim, Jin-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.29 no.5
    • /
    • pp.215-221
    • /
    • 2019
  • Ceramic tiles, which are widely used as interior and exterior materials for construction, have recently been required to have pollution prevention function. In order to remove contaminants, many researches of ceramic tiles with hydrophilic surface property through $TiO_2$ coating and hydrophobic surface property by improving the flow of water droplets have been proceeded. Expecially, it is very important to develop a surface glaze having hydrophobicity through a sintering process above $1000^{\circ}C$ without an additional coating process and the degradation of mechanical properties. In this study, surface glaze with copper powder was applied to manufacture of ceramic tile. Contact angle of ceramic tile according to thickness of surface glaze layer was investigated after the conventional sintering process. The contact angle of the ceramic tile surface without the copper powder was shown to be $25.3^{\circ}$, which is close to hydrophilic surface. However, the contact angle was increased up to $109.8^{\circ}$ when the thickness of surface glaze with the copper powder was $150{\mu}m$. The excellent hydrophobic property of the surface glaze with copper powder was resulted from the cellular structure of copper particles on the glaze surface. In addition, the mechanical properties of the developed hydrophobic ceramic tiles such as bending strength, chemical resistance, abrasion resistance, and frost resistance were well maintained and meet the criteria of 'KS L 1001 Ceramic tile'.

Lodging Pattern of Rice Plant in Broadcast-Seeded and Hand -Transplanted Cultivation (벼 담수표면직파재배와 손이앙재배의 도복발생 발생 양상)

  • Kim, Je-Kyu;Lee, Moon-Hee;Oh, Yun-Jin
    • KOREAN JOURNAL OF CROP SCIENCE
    • /
    • v.38 no.3
    • /
    • pp.219-227
    • /
    • 1993
  • Broadcast-seeded rice in submerged paddy frequently lodge in the field. In general, the causes of lodging in rice cultivation differ with different cultural methods. This study was conducted to investigate the causes of lodging in broadcast-seeded rice (BSR) and hand-transplanted rice (HTR) under four nitrogen (N) levels. Lodging in BSR was mainly a root lodging due to shallow root distribution, while that in HTR showed a bending type owing to deep rooting system. At the upper soil layer (0-5cm from the surface of ground) the root distribution of BSR (65.2%) was much larger than that of HTR (51.6%), whereas at the 5-10cm soil layer the root distribution of BSR (18.5%) was much smaller than that of HTR (28.0%). The depth of buried culm base was much shallower in BSR (1.2cm) than in HTR (4.0cm). The plant height, fresh weight, lodging index, culm diameter and thickness in HTR were much greater than those in BSR, and the breaking strength of lower internode was similar in the two cultivation methods indicating that HTR would have more lodging causes than BSR. In spite of . the more advantages to lodging resistance in BSR it severely lodged in the field. The main lodging-inducing factors of BSR were the shallow root distribution and shallow depth of buried culm base. Besides these, the higher ratio of gravity center of culm was an important factor. This result suggested that for the fundamental prevention of lodging in BSR, an ideotype of rice plant with ' a deep-rooted behavior ' should be developed.

  • PDF

A Study on the Basic Properties of Wood Impregnated with Inorganic Compounds (무기물처리 목재의 기초물성에 관한 연구)

  • Kim, Geon Hyoung;Oh, Tae Kyung;Lee, Weon Hee
    • Journal of the Korean Wood Science and Technology
    • /
    • v.34 no.4
    • /
    • pp.15-21
    • /
    • 2006
  • Composite materials were prepared by impregnating water glass into the wood, followed by soaking in solutions of boric acid or phosphoric acid. The effects of these treatments on the physical and mechanical properties of the specimens and especially on its heat resistance were investigated. 1) Weight Percent Gain (WPG)s increased with increase of concentrations of water glass. However, there was little relationship between treatment temperatures and WPG. Generally, WPGs of double treated specimens were higher than single treated ones. 2) Percent shrinkages in each directions of the specimens treated with water glass had higher value than other specimens. Percent shrinkages of the specimens treated with boric acid or phosphoric acid were decreased as compared with untreated specimen. However, the specimens treated with water glass or phosphoric acid showed very high hygroscopicity. 3) The bending strengths of all specimens treated inorganic substances were slightly decreased. However, the values of compressive strength and hardness of most specimens treated with inorganic substances increased or similar to that of untreated specimen except for a phosphoric acid treated specimens. 4) The specimens had good heat resistance. Weight losses of all specimens treated inorganic substances were about 50~70%. In particular, the specimens treated at $300^{\circ}C$ and $400^{\circ}C$ almost kept their shapes.

Measurement of Mechanical Properties of Thin Film Materials for Flexible Displays (플렉서블 디스플레이용 박막 소재 물성 평가)

  • Oh, Seung Jin;Ma, Boo Soo;Kim, Hyeong Jun;Yang, Chanhee;Kim, Taek-Soo
    • Journal of the Microelectronics and Packaging Society
    • /
    • v.27 no.3
    • /
    • pp.77-81
    • /
    • 2020
  • Commercialization of flexible OLED displays, such as rollable and foldable displays, has attracted tremendous interest in next-generation display markets. However, during bending deformation, cracking and delamination of thin films in the flexible display panels are the critical bottleneck for the commercialization. Therefore, measuring mechanical properties of the fragile thin films in the flexible display panels is essential to prevent mechanical failures of the devices. In this study, tensile properties of the metal and ceramic nano-thin films were quantitatively measured by using a direct tensile testing method on the water surface. Elastic modulus, tensile strength, and elongation of the sputtered Mo, MoTi thin films, and PECVD deposited SiNx thin films were successfully measured. As a result, the tensile properties were varied depending on the deposition conditions and the film thickness. The measured tensile property values can be applied to stress analysis modeling for mechanically robust flexible displays.

Structural analysis of an 38 feet diffusion style for high-speed catamaran yacht (38피트급 보급형 고속 카타마란 요트의 구조해석)

  • Park, Joo-Shin;Ko, Jae-Yong;Lee, Kyoung-Woo;Oh, Woo-Jun
    • Journal of Navigation and Port Research
    • /
    • v.33 no.3
    • /
    • pp.167-174
    • /
    • 2009
  • Recently, design technology of has been required such as catamaran yacht with high-speed according to expand a marine leisure industry. The domestic technical development for design and production of yacht is not actively than Canada, USA, Japan etc. However, with further development of yacht design & technology, it is need to develop a key technology related to increase the value of catamaran yacht. In the present paper, new guideline is suggest for catamaran yacht as like kinds of marine leisure ship in order for fundamental structure design and structural analysis for twin-hulled ship yacht and techniques for structural analysis as sea leisure ship in this research. The class of society has not been proposed formally about regulation and methodology for estimation of strength of small hight-speed craft with satisfying two conditions as noted; length less than 50meters, ratio of length to breadth less than 12. In the present study, we were adopted DNV (Yachts, Design Principles, Design Loads, Hull Structural Design) Rule and KR (FRP rule application guide) for scantling of structural members. Furthermore, ABS rule is used for structural calculation about application of loading conditions for catamaran yacht. This study can be available feedback role to manufacture of 38ft diffusion style for catamaran yacht. It is expected that this study will be a good reference in order to design of catamaran yacht with high-speed.

Effect of limestone addition on mechanical properties of ceramic tiles with fly ash (플라이애시가 첨가된 도자타일 성능에 석회석 함량이 미치는 효과)

  • Lee, Jin-Wook;Han, Kyu-Sung;Hwang, Kwang-Taek;Kim, Jin-Ho
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.28 no.6
    • /
    • pp.256-262
    • /
    • 2018
  • A great amount of fly ash, which is a waste from a thermal power plant, has not been appropriately recycled until now. Landfill of flay ash causes environmental pollution and enormous economic costs. In this study, manufacturing of architectural ceramic tile was investigated replacing fly ash with clay raw material. The properties of porcelain tile was analyzed after manufacturing porcelain tile with mineral based glaze and fast firing process. In particular, the effect of the fly ash addition on the properties of ceramic tile was investigated by increasing the amount of limestone addition. Porcelain tile with fly ash showed excellent bending strength, water absorption, warping and abrasion resistance. However, a significant decrease in durability was observed through the autoclave test. Addition of limestone increased the water absorption, twisting and hydration expansion of the ceramic tile, but it was confirmed that the durability of the ceramic tile with fly ash was greatly improved. In conclusion, recycled architectural ceramic tiles, which can meet domestic construction standards, could be manufactured with the addition of fly ash and limestone.

Fracture Behavior and Crack Growth of Concrete by The Nonlinear Fracture Mechanics (비선형 파괴역학에 의한 콘크리트의 파괴거동과 균열성장에 관한 연구)

  • 배주성;나의균
    • Magazine of the Korea Concrete Institute
    • /
    • v.2 no.2
    • /
    • pp.81-92
    • /
    • 1990
  • Concrete, a mixed material, has heterogeniety, anisotrophy and nonlinearity. Therefore, in its 'racture analysis, it is more reasonable to evaluate its fracture toughness by applying the concept of 'racture mechanics rather than the strength concept. Up to the present the concepts of fracture mechanics which were applied to concrete have been divided into two main classes. The one is the concept of linear elastic fracture mechanics and the other is the concept of elastic-plastic fracture mechanics. But it has been pointed out that there are many problems and irrationalities in applying the concept of linear elastic fracture mechanics to concrete. In this study, the J -integral method and the COD method mainly used in the analysis of nonlinear fracture mechanics, were introduced and the three point bending test was carried out for investigating the effects of the variation of the maximum aggregate size and notch depth on the fracture behavior and the crack growth of concrete, and the relationships of fracture energy and crack opening displacement. According to the results of this study the more the maximum aggregate size and the notch depth increased, the more the nonlinearity of load-deflection behavior was remarkable. The increase of the coarse aggregate size created the more ductility of concrete. Thus concrete showed the more stable fracture. As for the path of the crack growth, the more the coarse aggregate size increased, the more it was irregulary deviated from the straight line but it was not almost affected by the variation of the notch depth. Also, the fracture energy increased according as the coarse aggregate size increased and the notch depth decreased.

On the dimensional stabilization of woods with treatment of Polyethylene Glycol-400 (폴리에치렌 글리콜-400에 의한 목재(木材)의 칫수안정화(安定化))

  • Cho, Nam-Seok;Jo, Jea-Myeong;Bae, Kyu-Yong
    • Journal of the Korean Wood Science and Technology
    • /
    • v.3 no.1
    • /
    • pp.3-15
    • /
    • 1975
  • How to stabilize wood against shrinking and swelling in variable atmospheric moisture conditions is important to the wood-using industry and a challenge to research. Polyethylene glycol stabilize wood by bulking the fiber. PEG also serve as a chemical seasoning agent, suppress decay in high concentrations, and have slight effect on physical properties, gluing or finishing. The study designed to determine the effect of PEG-400 on the dimensional stabilization of local hardwoods for wood carvings that could supply a greatly expanding tourist trade and making curved furniture parts, lamp stands and other decorative objects, and possible gunstock. The species examined were 6 species, Seo-Namoo (Carpinus laxiflora), Cheungcheung-Namoo (Cornus controversa), Gorosae-Namoo (Acer mono), Karae-Namoo (Juglans mandshurica), Jolcham-Namoo (Quercusserrata) and Sanbud-Namoo (Prunus sargentii), used as block of 5cm thick radially to the grain, 7cm wide tangentially, and 70cm long parallel to the wood grain. All these test piecies were conditioned above the fiber saturation point before impregnation. The stabilization effects were determined for PEG-400 treated woods in a 50 percent solution for 20 days. The following conclusions were obtained. PEG retentions increased with treating time. It was more effective to treat at 60$^{\circ}C$ than at room temperature. In degree of PEG-400 impregnation on species, Cheungcheung-Namoo havinglow specific gravity had the highest retentions, 68.77% but the lowest, 56.33% was shown in Jolcham-Namoo with high specific gravity. Specific gravity of treated wood increased considerably with effectiveness of polymer loading. The increases in specific gravity were 5.36 to 13.16 percent. The highest was Jolcham-Namoo, the lowest Karae-Namoo. On the dimensional stability, a 40 percent of effectiveness of polymer loading was just as effective as 60 percent in reduction in water absorptivity (RWA), antishrinkage efficiency (ASE) and antiswelling efficiency (AE), and from over 60 percent they increased more rapidly. Also species response varied considerably. ASE was 30.12 to 69.97 percent tangentially and 27.86 to 56.37 percent radially, AE 34.06 to 73.76 percent tangentially and 30.11 to 70.12 percent radially, and RWA 42.31 to 65.32 percent. No differences in volume swelling among the 6 species were observed. Its values were ranged from 14.98 to 19.55 percent and also increased with PEG retentions. On the mechanical properties, the strengths very much decreased with PEG-400 loadings as shown in Figure 12; that were 11.41 to 22.90 percent in compression, 21.61 to 34.35 percent in bending and 22.83 to 36.83 percent in tensile strength. PEG retention in cell wall was less than 1 percent and the most of PEG were immersed in cell lumen. Except for Korae-Namoo, effectivenesses of polymer loading were as much high as 61.58 to 75.02 percent. This is believed to be due to the effect of PEG-400 on excellant dimensional stability of treated woods.

  • PDF

An Experimental Study on Flexural Behavior of Steel Fiber Reinforced Ultra High Performance Concrete Prestressed Girders (강섬유 보강 초고성능 콘크리트 프리스트레스트 거더의 휨거동 실험 연구)

  • Yang, In-Hwan;Joh, Chang-Bin;Kim, Byung-Suk
    • Journal of the Korea Concrete Institute
    • /
    • v.22 no.6
    • /
    • pp.777-786
    • /
    • 2010
  • This paper examines the flexural behavior of full-scale prestressed concrete girders that were constructed of steel fiber reinforced ultra high performance concrete (UHPC). This study is designed to provide more information about the bending characteristics of UHPC girders in order to establish a reasonable prediction model for flexural resistance and deflection for future structural design codes. Short steel fibers have been introduced into prestressed concrete T-girders in order to study their effects under flexural loads. Round straight high strength steel fibers were used at volume fraction of 2%. The girders were cast using 150~190 MPa steel fiber reinforced UHPC and were designed to assess the ability of steel fiber reinforced UHPC to carry flexural loads in prestressed girders. The experimental results show that steel fiber reinforced UHPC enhances the cracking behavior and ductility of beams. Moreover, when ultimate failure did occur, the failure of girders composed of steel fiber reinforced UHPC was observed to be precipitated by the pullout of steel fibers that were bridging tension cracks in the concrete. Flexural failure of girders occurred when the UHPC at a particular cross section began to lose tensile capacity due to steel fiber pullout. In addition, it was determined that the level of prestressing force influenced the ultimate load capacity.

Physico-mechanical Properties and Optimum Manufacturing Conditions of Bi-Sn Metal Alloy Impregnated Wood Composites (Bi-Sn 용융합금주입 목재복합체의 최적제조조건 및 물리·기계적 특성)

  • Park, Kye-Shin;Lee, Hwa-Hyoung;Kang, Seog Goo
    • Journal of the Korean Wood Science and Technology
    • /
    • v.42 no.6
    • /
    • pp.691-699
    • /
    • 2014
  • In order to improve the dimensional stability and durability of wood, this study attempted to impregnate bismuth (Bi) - tin (Sn) alloy metal with low melting temperature into solid woods of three species such as radiata pine, red oak and white oak, and investigated to determine an optimum condition of manufacturing the metal alloy-wood composites with natural wood grains. These Bi-Sn alloys were chosen for this study because they were harmless to human and melting at low temperatures. The composites resulted in high dimensional stability and low thickness swelling, and also showed much improved performance such as high bending strength, high hardness, high electric conductivity, and high thermal conductivity as floor materials. A proper impregnating condition of all specimens was determined as 10 minutes of the preliminary vacuum time, and $185^{\circ}C$ of the heating temperature. The proper processing condition for radiata pine wood was 2.5 minutes of the pressuring time at the pressure of $10kgf/cm^2$. For red oak wood, 10 minutes of the pressuring time at the pressure of $30kgf/cm^2$ were the proper condition. The proper manufacture conditions for white oak wood was determined as 10 minutes of the pressuring time at the pressure of $50kgf/cm^2$.