• Title/Summary/Keyword: Strength Ratio

Search Result 7,461, Processing Time 0.039 seconds

Spalling Properties of 80MPa High Strength Concrete with Fiber (복합섬유(PP,NY)를 혼입한 설계강도 80MPa 3성분계 고강도콘크리트의 폭렬특성)

  • Kim, Seong-Deok;Lee, Bum-Sik;Bae, kee-Sun;Kim, Sang-yun;Park, Su-Hee
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2009.11a
    • /
    • pp.51-54
    • /
    • 2009
  • In this study, the fire resistance test was carried out with a parameter such as fiber(PP+NY) mixed ratio on high strength concrete with 80MPa, and the spalling resistance property was evaluated. Concrete material test was carried out with a parameter such as fiber(PP+NY) mixed ratio(0%, 0.05%, 0.1%, 0.2%) of high strength concrete with 80MPa. Although the flowability and the strength capacity were delicately decreased with a increase of fiber mixed ratio, they satisfied the target limits. As the spalling resistance property after the fire resistance test of 3 hours, the spalling was partly shown on the high strength concrete with fiber(PP+NY) mixed ratio of 0% but, wasn't shown on the high strength concrete with fiber(PP+NY) mixed ratio of 0.05% ~ 0.2%.

  • PDF

A Study on the Remicon B/P Application and Properties of High Strength Concrete using Crushed Sand (부순모래를 사용한 고강도콘크리트의 특성 및 레미콘 B/P 적용에 관한 연구)

  • Choi, Se-Jin;Lee, Seong-Yeon;Lee, Sang-Soo
    • Journal of the Korea Institute of Building Construction
    • /
    • v.7 no.1 s.23
    • /
    • pp.57-62
    • /
    • 2007
  • Generally, the strength of concrete depends on factors of materials, mix proportions, compaction, manufacturing methods and curing and so on. And recently, it has increased the using of crushed sand for concrete due to the exhaustion of good natural aggregate. In case of Korea, in 2004, the using ratio of crushed sand occupies about 28% of whole fine aggregate. This is an experimental study to compare and analyze the influence of W/B ratio and replacement ratio of crushed sand on the fluidity and compressive strength of high strength concrete. For this purpose, the mix proportions of concrete according to the W/B (31.5, 27.5, 23.5%) and replacement ratio of crushed sand (0, 20, 40%) was selected. And then air content, slump-flow, a-lot, compressive strength test were performed.

Influence of Process Parameters on the Breathable Film Strength of Polymer Extrusion (고분자압출의 공정변수가 통기성필름강도에 미치는 영향)

  • Choi, Man-Sung
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.21 no.4
    • /
    • pp.625-632
    • /
    • 2012
  • Optimization of process parameters in polymer extrusion is an important task to reduce manufacturing cost. To determine the optimum values of the process parameters, it is essential to find their influence on the strength of polymer breathable thin film. The significance of six important process parameters namely, extruder cylinder temperature, extruder speed, extruder dies temperature, cooling roll temperature, stretching ratio, stretching roll temperature on breathable film strength of polymer extrusion was determined. Moreover, this paper presents the application of Taguchi method and analysis of variance (ANOVA) for maximization of the breathable film strength influenced by extrusion parameters. The optimum parameter combination of extrusion process was obtained by using the analysis of signal-to-noise ratio. The conclusion revealed that extruder speed and stretching ratio were the most influential factor on the film strength, respectively. The best results of film strength were obtained at higher extruder speed and stretching ratio.

An Experimental Study on the Shear Behavior of High Strength Concrete Deep Beam (고강도 철근 콘크리트 깊은 보의 전단거동에 관한 실험적 연구)

  • 함영삼;양근혁;이영호;정헌수
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.11a
    • /
    • pp.897-902
    • /
    • 2001
  • The purpose of this experimental study is to investigate the shear behavior of high-strength concrete deep beam and to grasp the conservatism of ACI Building Code. Experimental results on 12 deep beams under two equal symmetrically placed point loads are reported. Main variables are vertical and horizontal web reinforcement and shear span-to-overall depth ratio. Test results indicated that web reinforcement dose not affect on formation of inclined cracks but shear span-to-overall depth ratio affect on inclined shear cracks and ultimate shear strength. Addition of vertical web reinforcement improves ultimate shear strength of H.S.C. deep beams that shear span-to-overall depth ratio is 1.0. Considerable increase in ultimate shear strength of H.S.C. deep beams with increasing horizontal web reinforcement that shear span-to-overall depth ratio is 0.5. Especially with increasing concrete strength($f_{ck}$) the ACI code is conservative in estamating the ultimate shear strength of deep beams.

  • PDF

Shear Strength of High Strength Concrete Beams with Steel Fibrous (강섬유를 혼입한 고강도 콘크리트 보의 전단강도)

  • 곽계환;박종건;정태영
    • Journal of the Korea Concrete Institute
    • /
    • v.12 no.4
    • /
    • pp.23-30
    • /
    • 2000
  • The purpose of this paper is to study on the shear strength of high strength concrete beams with steel fibrous. In general, the shear strength of reinforced concrete beams is affected by the compressive strengths of concrete( c), the shear span-depth ratio(a/d), the longitudinal steel ratio($\rho$ $\omega$), and shear reinforcement. An experimental investigation of the shear strength of high strength concrete beams with steel fibrous was conducted. In each series the shear span-depth ratio(a/d) was held constant at 1.5, 2.8, or 3.6, while concrete strengths were varied from 320 to 520, to 800kgf/$\textrm{cm}^2$. To verify the proposed equations the experimental results were compared with those from other researches such as equation of ACI code 318-95 or equation of Zsutty. To deduce equation for shear strength from experimental data carried out MINITAP program. According to the experimental results, the addition of steel fibrous has increased the deflection and strain at failure load, improving the brittleness of the high strength concrete.

On Reliability and Comparison of $J_{Rice}$-Resistance considering Optimal Strength Ratio and $J_{\delta}$-Resistance Curves converted from CTOD using Appropriate Strength chosen according to Strain Hardening Level (강도비를 적용한 Rice-저항곡선과 변형경화를 고려한 $J_{\delta}$-저항곡선과의 비교)

  • 장석기
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.26 no.1
    • /
    • pp.59-67
    • /
    • 2002
  • The comparison of $J_{Rice}$-resistance considering a few strength ratio in Rice J-integral formula and $J_{\delta}$-resistance curves converted from experimental CTOD using appropriate strength chosen according to strain hardening level, n=10.6 (A533B steel) and n=8.1 (BS4360 steel) is carried out. The optimal dimensionless strength ratio like the factor of revision, (see full text)reflecting strain hardening level in Rice\`s experimental formula is found out and the reliability of appropriate reference strength chosen according to strain hardening level in different materials is investigated through doing that CTOD is transformed from $J_{\delta}$-integral using relationship between J-integral and CTOD. The results are as follows; 1) The optimal factor of revision is when m equals to 3 in (see full text) for Rice's and the above optimal factor of revision multiplies by coefficient, η in Rice's experimental formula instead of n=2, 2) and the pertinent reference strength for high strain hardening material like BS4360 steel is ultimate strength, $\sigma_{u}$ and for material like A533B steel is ultimate-flow strength, $\sigma_{u-f}$. The incompatible of the behavior of both experimental J-resistance curves using Rice's formula and CTOD-resistance curves for A533B and BS4360 steel by Gordon, et al., could be corrected using the optimal factor of revision in Rice\`s and the pertinent reference strength in J=$m_{j}$${\times}$$\sigma_{i}$${\times}$CTOD.

An Experimental Study on the Strength of Recycled Concrete with Steam Curing (증기양생 재생콘크리트의 강도특성에 관한 실험연구)

  • Lee, Myung-Kue;Kim, Kwang-Seo;Lee, Keun-Ho;Jung, Sang-Hwa
    • Journal of the Korea Institute of Building Construction
    • /
    • v.5 no.2 s.16
    • /
    • pp.89-95
    • /
    • 2005
  • Various tests are performed with the recycled concrete including compressive strength, flexural strength, splitting tensile strength, bonding strength and chloride ion penetration test. The basic data obtained from the presented test could be accumulated for the purpose of utilization in concrete structure. Most of the strength tests show that strength decrease a little extent with increasing substitution ratio of recycled coarse aggregate except splitting tensile test for the concrete with $100\%$ recycled fine aggregate. But in case of the $50\%$ substitution of recycled coarse aggregate, compressive strength, flexural strength and bonding strength are almost equal to the normal concrete. Chloride ion penetration test shows that the penetration amounts of chloride ion becomes more in proportion to the substitution ratio of recycled aggregate. But most of the results show that the permeability of recycled concrete is proper to use. The results of present study nay imply that the use of recycled aggregate for steam curing concrete is possible but the substitution ratio of recycled aggregate should be determined through further studies.

Axial behavior of the steel reinforced lightweight aggregate concrete (SRLAC) short columns

  • Mostafa, Mostafa M.A.;Wu, Tao;Liu, Xi;Fu, Bo
    • Steel and Composite Structures
    • /
    • v.39 no.5
    • /
    • pp.583-598
    • /
    • 2021
  • The composite steel reinforced concrete (SRC) columns have been widely used in Structural Engineering due to their good performances. Many studies have been done on the SRC columns' performances, but they focused on the ordinary types with conventional configurations and materials. In this study, nine new types of steel reinforced lightweight aggregate concrete (SRLAC) short columns with cross-shaped (+shaped and X-shaped) steel section were tested under monotonically axial compressive load; the studied parameters included steel section ratio, steel section configuration, ties spacing, lightweight aggregate concrete (LWAC) strength, and longitudinal bars ratio. From the results, it could be found that the specimens with larger ties ratio, concrete strength, longitudinal bars ratio, and steel section ratio achieved great strength and stiffness due to the excellent interaction between the concrete and steel. The well-confined concrete core could strengthen the steel section. The ductility and toughness of the specimens were influenced by the LWAC strength, steel section ratio, and longitudinal bars ratio; in addition, larger ties ratio with smaller LWAC strength led to better ductility and toughness. The load transfer between concrete and steel section largely depends on the LWAC strength, and the ultimate strength of the new types of SRLAC short columns could be approximately predicted, referring to the codes' formulas of ordinary types of steel reinforced concrete (SRC) columns. Among the used codes, the BS-5400-05 led to the most conservative results.

Effects of Anisotropic Consolidation on Strength of Soils (이방압밀이 흙의 강도에 미치는 영향)

  • 강병희
    • Proceedings of the Korean Geotechical Society Conference
    • /
    • 2000.11a
    • /
    • pp.3-14
    • /
    • 2000
  • Anisotropic consolidation, shear, a transportational component during or after deposition each may produce anisotropic fabrics, which result in the anisotropic properties of soils. Nevertheless, the isotropically consolidated compression triaxial tests are commonly used in practice to determine the strength of the anisotropically consolidated soils because of their practicality and simplicity. In this paper the effects of anisotropic consolidation on the strength properties of soils are discussed. For the sandy soils consolidated under a constant vertical consolidation pressure, the deformation modulus decreases with decreasing consolidation pressure ratio($\sigma$$\sub$3c/'/$\sigma$ sub 1c/'), but the liquefaction resistance increases. For the saturated cohesive soils, both the undrained shear strength and undrained creep strength decrese with decreasing the consolidation pressure ratio. When the in-situ strength properties of the anisotropically and normally consolidated soils are determined by the isotropically consolidated tests, the undrained shear strength and creep strength of saturated cohesive soils as well as the deformation modulus of sandy soils are measured to be higher than the rear in-situ values. This, therefore, could lead to a dangerous judgement in stability analysis

  • PDF

Optimum Mix Proportion of the High Strength and Self Compacting Concrete Used Above-Ground LNG Storage Tank (지상식 LNG 저장탱크용 고강도 자기충전 콘크리트의 최적배합에 관한 연구)

  • Kwon, Yeong-Ho
    • Journal of the Korea Concrete Institute
    • /
    • v.23 no.1
    • /
    • pp.99-107
    • /
    • 2011
  • This study is to performed to find the optimum mix proportion of the high strength and self compacting concrete for the above-ground LNG storage tank construction and field application. If LNG storage tank wall thicknesscan be reduced, the construction cost and quality can be improved by using self-compacting high strength concrete with compressive strength 60~80 MPa. For this purpose, low heat cement (Type IV) and class F fly ash are used in concrete mix to control hydration heat, flowability, and viscosity. Mix design variables of unit water, fly ash replacement ratio, water-binder ratio, and fine aggregate ratio are selected and tested for material properties and manufacturing cost of the concrete. Also, fly ash replacement ratio is considered using confined water ratio test. The test results showed that the optimum mix proportion of the self-compacting high strength concrete characteristics are as follows. 1) In case of the concrete with specified compressive strength of 60 MPa, the optimum mix proportion is fly ash replacement ratio of 20% and water- binder ratio of 27~30%. 2) In case of the concrete with the strength of 80 MPa, the optimum mix proportion is fly ash replacement ratio of 10% and water-binder ratio 25%. But unit water and fine aggregate ratio are 165 $kg/m^3$ and $51{\pm}2%$, respectively, regardless of the traget concrete compressive strength range. Also, test results showed that concrete manufacturing cost of 60 MPa and 80 MPa concrete require additional costs of 14~22% and 33%, respectively, compared to the manufacturing cost of 40 MPa concrete. Therefore, application of the self-compacting high strength concrete has proven to be economical in the perspective of the material cost, quality control, and site management.