• Title/Summary/Keyword: Solution Mixing Method

Search Result 238, Processing Time 0.026 seconds

Fabrication of Al2O3/ZrO2Ceramics by the Polymerization Dispersion Process (ZrO2의 고분자화 분산법을 이용한 Al2O3/ZrO2요업체의 제조)

  • Cho, Myung-Je;Hwang, Kyu-Hong;Lee, Jong-Kook
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.4
    • /
    • pp.284-288
    • /
    • 2004
  • To improve mechanical properties of $Al_2$O$_3$/ZrO$_2$composites have been controlled dispersion of ultra low size ZrO$_2$ particles in $Al_2$O$_3$ ceramics by polymeric precursor method (Pechini process). In case of coprecipitation or mechanical mixing of ZrO$_2$ powders with $Al_2$O$_3$, homogeneous dispersion and controlling the ZrO$_2$ size were relatively difficult due to high sintering temperature. So the polyesterization process of Zr/Y(NO$_3$)$_3$-citric acid solution in ethylene glycol with the commercial sub-micron sized o(-alumina powder (Sumitomo AES-11(0.4 ${\mu}{\textrm}{m}$)) was adopted in order to obtain homogeneous dispersion of ZrO$_2$ in A1203. By this partial polyesterization process, the homogeneous dispersion of relatively low sized ZrO$_2$in $Al_2$O$_3$/ZrO$_2$composites was achieved at 1450∼1$600^{\circ}C$ of sintering temperature range and their mechanical properties were measured.

Variations in Electrical Conductivity of CNF/PPy Films with the Ratio of CNF and Application to a Bending Sensor (탄소나노섬유의 함량에 따른 CNF/PPy 필름의 전기전도도 및 굽힘센서로 응용)

  • Kim, Cheol;Zhang, Shuai;Kim, Seon-Myeong
    • Composites Research
    • /
    • v.23 no.3
    • /
    • pp.31-36
    • /
    • 2010
  • A new material, carbon-nanofiber/polypyrrole (CNF/PPy) composite films, with different CNF weight ratios were fabricated electrochemically. Compared to the fabrication process based on simple physical mixing, the flexibility of the new film has been improved much better than the previous similar material. Pure PPy films were also fabricated by the new electrochemical process for the comparison of difference. Several SEM images were taken at two locations (electrode-side and solution-side) and at the cross section of the samples. Electrical conductivity of the composite films was measured by the four-probe method. The conductivity of the pure PPy film 0.013cm thick was 79.33S/cm. The CNF/PPy composite film with 5% CNF showed a conductivity of 93S/cm. One with 10% CNF showed a conductivity of 126 S/cm. The conductivity of PPy improves, as the CNF weight ratio increases. The good conductivity of CNF/PPy composites makes them a candidate for a small bending actuator. A bending sensor consists of PPy and PVDF, which can be operated in the air, was designed and the bending deflection was calculated using FEM.

Study on the Selection of Solvent for Purificatino of p-Dioxanone by Crystallization Method (결정화에 의한 파라디옥산온의 정제를 위한 용매선정에 관한 연구)

  • kim, Sung-Il;Koh, Joo-young;Kim, Chul-Ung;Koh, Jae-Cheon;Park, So-Jin;Seo, Young-Jong;Choi, Byung-Ryul
    • Applied Chemistry for Engineering
    • /
    • v.16 no.4
    • /
    • pp.581-587
    • /
    • 2005
  • In order to obtain a highly purified p-dioxanone (PDX) as monomer of biodegradable polymer, suitable solvent must be selected. The selection was based on the solubility of impurities, and partial layer melt crystallization were carried out under the presence of solvent. The solubility of PDX in various solvents such as ethyl acetate, tetrahydrofuran, acetone, alcohols (methanol, ethanol, 1-propanol, 1-butanol and 1-pentanol) were measured over the temperature range of $-10{\sim}15^{\circ}C$. As solubility parameters, the mixing and dissolution enthalpy between the PDX and the solvents was studied based on empirical equations and the regular solution theory. The solubility and the temperature dependency of the solubility with the solvents of acetone, ethylacetate, and tetrahydrofuran of PDX were shown to have relatively high values compared to the alcohol type solvents. Also, in same alcohols, the smaller molecules and higher polarity gave higher solvency. In partial layer melt crystallization, small amount of ethylacetate selectively dissolved impurities and gave highly purified p-dioxanone, over 99.9% purity.

Preparation and characterization of Ga-doped TiO2 nanofibers by electrospinning (전기방사를 이용한 Ga이 첨가된 나노섬유의 제작 및 특성평가)

  • Song, Chan-Geun;Kang, Won Ho;Yoon, Jong-Won
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.22 no.6
    • /
    • pp.274-278
    • /
    • 2012
  • $TiO_2$ can be used optically and is applied on many areas such as gas sensor, solar cell and photocatalysis. Electrospun nanofibers have received great interest for development and utilization in some novel applications, such as chemical sensors, dye-sensitized solar cell and photo catalysis. In this study, pure $TiO_2$ and Ga-doped $TiO_2$ nanofibers synthesized by a modified electrospinning method. The Ga doped $TiO_2$ solution is prepared by mixing poly vinyl pyrrolidone, ethyl alcohol, and titanium (IV) isopropoxide. By electrospinning these sols, nanofibers were fabricated. These fibers are heat-treated at $800^{\circ}C$ in air. The prepared pure $TiO_2$ and Ga-doped $TiO_2$ nanofibers samples were characterized by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), scanning electron microscopy (SEM), transmission electron microscopy (TEM) and Raman spectroscopy.

The effects of novel biodegradable amorphous Calcium Phosphate on bone regeneration in rat calvarial defects (새롭게 개발된 비정질의 Calcium Phosphate가 백서두개골의 골재생에 미치는 영향)

  • Choi, Jung-Yoo;Chae, Gyung-Joon;Kim, Chang-Sung;Lee, Yong-Keun;Cho, Kyoo-Sung;Chai, Joong-Kyu;Kim, Chong-Kwan;Choi, Seong-Ho
    • Journal of Periodontal and Implant Science
    • /
    • v.37 no.4
    • /
    • pp.871-879
    • /
    • 2007
  • Purpose: The purpose of this study was to evaluate the bone regeneration of novel biodegradable amorphous calcium phosphate. Materials and Method: An 8-mm, calvarial, critical-size osteotomy defect was created in each of 20 male Sprague-Dawley rats(weight $250{\sim}300g$). The animals were divided into two groups of 10 animals each and allowed to heal for 2 weeks(10 rats). The first group was the control group and the other group was the experimental group which received the novel biodegradable calcium phosphate. Results: The healing of the calvarium in the control group was uneventful. The histologic results showed little bone formation in the control group. The experimental group which received the novel biodegradable calcium phosphate showed a normal wound healing. There were a lot of new bone formation around the biomaterial in 2 weeks. The bone formation increased in 8 weeks when compared to 2 weeks and there was a significant bone increase as well(P<0.01). The nobel biodegradable calcium phosphate showed statistical significance when compared to the control group (P<0.05). The novel biodegradable calcium phosphate in 8 weeks showed a significant increase in bone formation when compared to 2 weeks $(40.4{\pm}1.6)$(%). The biodegradable calcium phosphate which is made from mixing calcium phosphate glass(CPG), NaCO and NaOH solution, is biocompatible, osteoconductive and has a high potency of bone formation. Conclusion: We can conclude that the novel biodegradable calcium phosphate can be used as an efficient bone graft material for its biodegradability and osteoconductivity.

Precipitation-Filtering Method for Reuse of Uranium Electrokinetic Leachate (우라늄 오염 동전기 침출액의 재이용을 위한 침전-여과 방법)

  • Kim, Gye-Nam;Shon, Dong-Bin;Park, Hye-Min;Kim, Ki-Hong;Lee, Ki-Won;Moon, Jeik-kwon
    • Journal of Nuclear Fuel Cycle and Waste Technology(JNFCWT)
    • /
    • v.9 no.2
    • /
    • pp.63-71
    • /
    • 2011
  • A large volume of uranium electrokinetic leachate has been generated during the electrokinetic decontamination to remove uranium from contaminated soil. The treatment technology for the reuse of the uranium leachate was developed. The concentration of uranium in the generated uranium leachate was 180 ppm and concentrations of Mg(II), K(I), Fe(II), and Al(III) ions ranged from 20 ppm to 1,210 ppm. The treatment process for uranium leachate consisted mainly of mixing and cohesion, precipitation, concentration, and filtration. In order to obtain the pH=11 of a precipitate solution, the calcium hydroxide needs to be 3.0g/100ml and the sodium hydroxide needed to be 2.7g/100ml. The results of several precipitation experiments showed that a mixture of NaOH+0.2g alum+0.15g magnetite was an optimal precipitant for filtration. The average particle size of precipitate with NaOH+alum+0.15g magnetite was $600\;{\mu}m$. Because the total value of metal concentrations in supernatant at pH=9 was the smallest, sodium hydroxide should be added with 0.2g alum and 0.15g magnetite for pH=9 of leachate.

Characteristics of Eco-friendly Porous Concrete for Seawater Purification Using By-Products of Steel Industry (철강산업 부산물을 활용한 해수정화용 친환경 다공질콘크리트의 특성)

  • Han, Woonwoo;Lee, Byungjae
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.24 no.1
    • /
    • pp.1-7
    • /
    • 2020
  • As of 2018, Steel slag was generated approximately 24.23 million tons. Howeve, except blast furnace slag, steel slag is a typical by-product which does not have a clearly defined purpose in recycling. Thus, countries around the world are putting great efforts into developing a purpose for the recycling of steel slag. The vast habitat foundation of marine life has been destroyed due to recent reckless marine development and environment pollution, resulting in intensification of the decline of marine resources, and a solution to this issue is imperative. In order to propose a method to recycle large amounts of by-product slag into a material that can serve as an alternative to natural aggregate, the engineering properties and applicability for each mixing factor of environment friendly porous concrete as a material for the composition of seawater purification were in this study. Regarding the nutrient elution properties, it was clear that the nutrients continuously flowed out up to an immersion time by 8 months in natural seawater; the nitrogenous fertilizer displayed excellent elution properties in this regard.

Preparation of Heterogeneous Bipolar Membranes Using Poly (phenylene oxide, PPO) Polyelectrolyte and Their Water Splitting Properties (Poly (phenylene oxide, PPO) 고분자 전해질을 이용한 불균질 바이폴라막 제조 및 물분해 특성)

  • Kim, In Sik;Hwang, Seong Yeon;Kang, Byung Gwan;Hwang, Taek Sung
    • Korean Chemical Engineering Research
    • /
    • v.57 no.1
    • /
    • pp.65-72
    • /
    • 2019
  • In this study, heterogeneous ion exchange membranes were prepared by casting method with various mixing ratios of PPO ion-selective solution and ion exchange resin. Then heterogeneous bipolar membranes were prepared by using this. The water content of heterogeneous cation and anion exchange membranes were 60~80% respectively, the ion exchange capacity was 2.81~3.26 meq/g, 2.31~2.74 meq/g and electrical resistances were $1.65{\sim}1.45{\Omega}{\cdot}cm^2$ and $1.55{\sim}1.05{\Omega}{\cdot}cm^2$. The tensile strength of heterogeneous bipolar membrane was lower than that of PPO resin before functionalization ($700Kg_f/cm^2$). The tensile strength of heterogeneous bipolar membrane with catalyst layer was lower than that of non-catalytic heterogeneous bipolar membrane. The water splitting voltage of the heterogeneous bipolar membrane with catalyst layer was low and stable at a minimum of 1.7~1.8 V, maximum 3.9~4.0 V, and the water splitting voltage of the non-catalytic heterogeneous bipolar membrane was constant at 3.8~4.0 V.

A Study on Chloride Binding Capacity of Various Blended Concretes at Early Age (초기재령에서 각종 혼합콘크리트의 염소이온 고정화능력에 관한 연구)

  • Song, Ha-Won;Lee, Chang-Hong;Lee, Kewn-Chu
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.12 no.5
    • /
    • pp.133-142
    • /
    • 2008
  • This paper studies the early-aged chloride binding capacity of various blended concretes including OPC(ordinary Portland cement), PFA(pulversied fly ash), GGBFS(ground granulated blast furnace slag) and SF(silica fume) cement paste. Cement pastes with 0.4 of a free water/binder ratio were cast with chloride admixed in mixing water, which ranged from 0.1 to 3.0% by weight of cement and different replacement ratios for the PFA, GGBFS and SF were used. The content of chloride in each paste was measured using water extraction method after 7 days curing. It was found that the chloride binding capacity strongly depends on binder type, replacement ratio and total chloride content. An increase in total chloride results in a decrease in the chloride binding, because of the restriction of the binding capacity of cement matrix. For the pastes containing maximum level of PFA(30%) and GGBFS(60%) replacement in this study, the chloride binding capacity was lower than those of OPC paste, and an increase in SF resulted in decreased chloride binding, which are ascribed to a latent hydration of pozzolanic materials and a fall in the pH of the pore solution, respectively. The chloride binding capacity at 7 days shows that the order of the resistance to chloride-induced corrosion is 30%PFA > 10%SF > 60%GGBFS > OPC, when chlorides are internally intruded in concrete. In addition, it is found that the binding behaviour of all binders are well described by both the Langmuir and Freundlich isotherms.

Runoff and Erosion of Alachlor, Ethalfluralin, Ethoprophos and Pendimethalin by Rainfall Simulation (인공강우에 의한 alachlor, ethalfluralin, ethoprophos 및 pendimethalin의 토양표면 유출)

  • Kim, Chan-Sub;Ihm, Yang-Bin;Lee, Young-Deuk;Oh, Byung-Youl
    • Korean Journal of Environmental Agriculture
    • /
    • v.25 no.4
    • /
    • pp.306-315
    • /
    • 2006
  • Two different experiments, adsorption/desorption and runoff by rainfall simulation of four pesticides, such as alachlor, ethalfluralin, ethoprophos and pendimethalin were undertaken their runoff and erosion losses from sloped land and to assess the influence of their properties and environmental factors on them. The mobility of four pesticides and which phase they were transported by were examined in adsorption study, and the influence of rainfall pattern and sloping degree on the pesticide losses were evaluated in simulated rainfall study. Freundlich adsorption parameters (K) by the adsorption and desorption methods were 1.2 and 2.2 for ethoprophos, 1.5 and 2.6 for alachlor, respectively. And adsorption distribution coefficients (Kd) by the adsorption and desorption methods were 56 and 94 for ethalfluralin, and 104 and 189 for pendimethalin, respectively. K or Kd values of pesticides by the desorption method which were desorbed from the soil after thoroughly mixing, were higher than these ones by the adsorption method which pesticides dissolved in water were adsorbed to the soil. Another parameter (1/n), representing the linearity of adsorption, in Freundlich equation for the pesticides tested ranged from 0.96 to 1.02 by the desorption method and from 0.87 to 1.02 by the adsorption method. Therefore, the desorption method was more independent from pesticide concentration in soil solution than the adsorption method. By Soil Survey and Land Research Center (SSLRC)'s classification for pesticide mobility, alachlor and ethoprophos were classified into moderately mobile $(75{\leq}Koc<500)$, and ethalfluralin and pendimethalin were included to non-mobile class (Koc > 4000). Runoff and erosion loss of pesticides by three rainfall scenarios were from 1.0 to 6.4% and from 0.3 to 1.2% for alachlor, from 1.0 to 2.5% and from 1.7 to 10.1% for ethalfluralin, from 1.3 to 2.9% and from 3.9 to 10.8% for pendimethalin, and from 0.6 to 2.7% and from 0.1 % 0.3% for ethoprophos, respectively. Distribution of pesticides in soil profile were investigated after the simulated rainfall study. Alachlor and ethoprophos were leached to from 10 to 15 cm of soil layer, but ethalfluralin and pendimethalin were mostly remained at the top 5 cm of soil profile. The losses of the pesticides at 30% of sloping degree were from 0.2 to 1.9 times higher than those at 10%. The difference of their runoff loss was related with their concentration in runoff water while the difference of their erosion loss must be closely related with the quantity of soil eroded.