Microstructure and Mechanical Properties of Mg-Zn-Y-Yb Alloys Produced by Consolidation of Rapidly Solidified Ribbons

  • Sakamoto, Yoshihito;Yamasaki, Michiaki;Kawamura, Yoshihito
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1045-1047
    • /
    • 2006
  • Fabrication of $Mg_{95.75}Zn_1Y_3Yb_{0.25}$ bulk alloy has been performed through the consolidation of rapidly solidified ribbons. The $Mg_{95.75}Zn_1Y_3Yb_{0.25}$ bulk alloy exhibited excellent mechanical properties, high tensile yield strength of 530 MPa, and large elongation of 3 %. Microstructure of the alloy was characterized by equiaxed fine grains that consist of -Mg, long period ordered (LPO) structure phase, and $Mg_5RE$-type cubic compound. The strengthening of the alloys may be due to fine grains with LPO structure phase and $Mg_5RE$-type compound.

  • PDF

MAI체제하의 효율적인 FDI전략 (The Effective FDI Strategies under the MAI System)

  • 채점길
    • 한국항만경제학회지
    • /
    • 제19권1호
    • /
    • pp.139-159
    • /
    • 2003
  • This study deals sith some problems of foreign direct investment and seeks for the ways of activating foreign direct investment (hereafter F.D.I.) by analyzing the Korean economic structure that is faced with the neo-protectivism and nationalism of the advanced or foreign countries currently. During a transformational process in the transitional period of world trade environment, it is necessary for Korea not only to learn the higher technology for advanced countries, but also to apply techonology to their economic structure in order to enter into competition with the advanced countries. Based on the experiences and accomplishments from their investments, Korean enterprises should turn their business into F.D.I. and act appropriately in order to keep the balance between indoor and outdoor investment. Looking through the ways to activate F.D.I., we may make conclusions as follows: 1. Government policy transparency 2. Prudential Macro Economic policy 3. International policy coorperation system 4. Solidification of Foreign Commercial intercourse to Developing countries 5. Globalixation base of domestic coorperation 6. High efficiency- low cost of business coorperation enterprise 7. Attacktive investiestment strategies on conclusive competive advantage 8. Multilateral investment Area 9. New recognixation on marketing investment etc. F.D.I. strategies

  • PDF

불순 Fe를 함유한 A356 주조합금에서 미세조직 형성에 관한 Mn과 Cr의 효과 (The Effects of Mn and Cr Additions on the Microstructure of A356 Alloys Containing Impure Fe)

  • 한상원
    • 한국주조공학회지
    • /
    • 제25권3호
    • /
    • pp.128-133
    • /
    • 2005
  • The effects of Mn and Cr on the crystallization behaviors of Fe-bearing intennetallics in A356 alloy were studied. Coarse and acicular ${\beta}-Al_{5}$FeSi phase in A356-0.20wt.%Fe alloy was modified into small ${\alpha}$-Al(Fe,Mn)Si and ${\alpha}$-Al(Fe,Cr)Si phases in response to Mn and Cr addition, respectively. Increasing of Mn addition amount elevates the crystallizing temperature of ${\alpha}$-Al(Fe,Mn)Si and the Mn/Fe ratio in the ${\alpha}$-Al(Fe,Mn)Si. Cr is more effective to modify ${\beta}-Al_{5}$FeSi in comparison with Mn. ${\alpha}$-Al(Fe,Mn)Si phase had BCC/SC dual structure.

저탄소성 용접금속의 응고균열에 미치는 탄소함량의 영향 (The effect of carbon content on hot cracking of low carbon steel weld)

  • 정호신;엄동석
    • Journal of Welding and Joining
    • /
    • 제6권4호
    • /
    • pp.16-26
    • /
    • 1988
  • The effect of carbon content on hot cracking of welded carbon steel was investigated Eight steel plates whose carbon content range from 0.02 to 0.23 percent were welded by autogeous gas tungsten are process. Constant strain was applied to the hot crack test specimen under the strain rate of 0.15 mm per second during welding. The hot cracking susceptibility ws high in the rnage of 0.02-0.05 and 0.12-0.23 percent carbon contents. The critical carbon content immune to hot cracking is in the range from 0.07 to 0.12 percent carbon. By electron probe microanalyser, amanganese segregation was not seen significantly in the whole carbon range. But segregation of silicon was higher in the region of low carbon contents. However, sulphur was segregated remarkably in the region betwen 0.18 and 0.23 percent carbon by peritectic reaction. Very smal lamount of dnedritic structure was observed in the region from 0.02 to 0.05 percent carbon by peritectic reaction. Very small amount of dendritic structure was observed in the region from 0.02 to 0.05 percent carbon but the predominant solidification structure was smooth by cellular growth. The higher the carbon content is, the more the columnar dendritic structure was observed.

  • PDF

급냉응고된 비정질 실리콘 분말의 원자구조에 관한 연구 (Characterization of Atomic Structure in Rapidly Solidified Amorphous Silicon)

  • 김연옥
    • 한국재료학회지
    • /
    • 제4권6호
    • /
    • pp.644-650
    • /
    • 1994
  • Electrohydrodynamic Atomization 급냉응고장치를 이용하여 고순도 실리콘 미세분말을 제조하여 투과전자현미경으로 미세조직과 그 응고상을 조사한 결과 직경이 60nm 이하인 분말에서 비장질상이 발견되었다. 비정질 실리콘의 원자구조를 분석하기 위하여 비정질 분말에서 얻은 전자회절 데이타를 이용하여 radial distribution function을 계산하여 해석한 결과, 실리콘의 결정구조인 다이아몬드 입방격자에서 발견되는 기본적 정사면체 배열이 비정질 실리콘의 2번째 근접원자간 거기까지 유지됨을 알 수 있었으며 이로부터 비정질 실리\ulcorner이 단범위 규칙성을 갖는 tetrahedrally coordinated random network 원자배열로 이루어짐을 알았다.

  • PDF

Development of High Aperture Ratio 2.1” QVGA LTPS (Low Temperature Poly Si) LCD Using SLS (Sequential Lateral Solidification) Technology

  • Kang, Myung-Koo;Lee, Joong-Sun;Park, Jong-Hwa;Zhang, Lintao;Joo, Seung-Yong;Kim, Chul-Ho;Kim, Il-Kon;Kim, Sung-Ho;Park, Kyung-Soon;Yoo, Chun-Ki;Kim, Chi-Woo
    • 한국정보디스플레이학회:학술대회논문집
    • /
    • 한국정보디스플레이학회 2005년도 International Meeting on Information Displayvol.II
    • /
    • pp.1033-1034
    • /
    • 2005
  • High resolution 2.1” QVGA LTPS LCD (190ppi) having high aperture ratio of 65% could be successfully developed using state-of-the-art SLS technology and active/gate storage structure. Cost effective P-MOS 6-Mask structure was used. Full gate and transmission gate circuits are integrated in the panel. The high aperture ratio was obtained by using active/gate capacitance structure, which can reduce storage capacitance area. The aperture ratio was increased to 65% from 49% of conventional gate/data capacitance structure. The brightness was increased from 180cd to 270cd without any degradation of optical properties such as contrast ratio, flicker or crosstalk.

  • PDF

급속응고된 Fe-6.5wt% Si 강판의 미세조직과 자기적 특성에 미치는 열처리의 영향 (Effect of Heat Treatment on Microstructures and Magnetic Properties of Rapidly Solidified Fe-6.5wt % Si sheet)

  • 황동하;이갑호;이태행;구자명
    • 열처리공학회지
    • /
    • 제8권2호
    • /
    • pp.149-154
    • /
    • 1995
  • The alloying of 6.5wt % Silicon in iron decreases the magnetization and the anisotropy and minimizes the iron loss noticeably. But it is very difficult to make thin sheets because of its poor ductility which is due to an ordering reaction (body centered cubic to CsCI type crystal structure). However the ordering reaction can be suppressed by rapid solidification method. The cooling rate of rapidly solidified Fe-6.5wt % Si alloy is about $10^3K/s$ and rapidly solidified structure are fine structure, cellular structure, dendrite and equiaxed grain from surface. The precipitates of $DO_3$ Phase emerges on $B_2$ matrix and the coercive force was 0.51 Oe (50cycle, 15KGauss) in Fe-6.5wt% Si alloy which was processed by heat treatment of $1150^{\circ}C$ for 1hr in high vacuum.

  • PDF

3 차원 형상의 미소제품 제작을 위한 마이크로 광 조형시스템의 개발 (Development of micro-stereolithography system for the fabrication of three-dimensional micro-structures)

  • 이인환;조윤형;조동우;이응숙
    • 한국정밀공학회지
    • /
    • 제21권2호
    • /
    • pp.186-194
    • /
    • 2004
  • Micro-stereolithography is a newly proposed technology as a means that can fabricate a 3D micro-structure of free form. It makes a 3D micro-structure by dividing the shape into many slices of relevant thickness along horizontal surfaces, hardening each layer of slice with a focused laser beam, and stacking them up to a desired shape. In this technology, differently from the conventional stereolithography, scale effect is dominant. To realize micro-stereolithography technology, we developed the micro-stereolithography apparatus which is composed of an Ar+ laser, x-y-z stages. controllers. optical devices and scan path generation software. Related processes were developed, too. Using the system, a number of micro-structures were successfully fabricated. Some of these samples are shown for prove this system. Laser scan path generation algorithm and software considering photopolymer solidification phenomena as well as given 3D model were developed. Sample fabrication of developed software shows relatively high dimensional accuracy compared to the uncompensated result.

정역 회전법에 의한 고순도 알루미늄의 응고 및 정련에 관한 연구 (A Study on the Solidification and Purification of High Purity Aluminium Alternate Stirring Method)

  • 김욱;이종기;백홍구;허성강
    • 한국주조공학회지
    • /
    • 제12권3호
    • /
    • pp.220-229
    • /
    • 1992
  • The degree of purification and the macrostructure of high purity aluminium were studied through the alternate stirring method in order to improve the nonuniformity of solute concentration in the unidirectional stirring method. The $2^3$ factorial design was done to examine the effects of experimental factors more qualitatively. In the relatively low stirring speed of 1500 rpm with alternate stirring mode, the uniform solute profile and refined grain structure were obtained due to strong washing effect and turbulent fluid flow. It was induced by the transition of the momentum boundary layer by alternation of the stirrer. It was concluded from this study that the alternate stirring mode was more effective to obtain the uniformity of solute even in the stirring speed of 1500 rpm. But the degree of purification decreased below the critical alternating period. When 2N(99.8wt.%) aluminium was used as the starting material the morphology of solid-liquid showed the cellular shape and the columnar grains were inclined to the direction of rotation. This inclined grain growth resulted from the difference of relative velocities of solid and liquid. The inclined angle was increased as the stirring speed increased and solidification proceeded. In the case of 4N aluminium, there was no inclined grain growth and it was confirmed from the macrostructure and SEM work that the morphology of solid-liquid interface was planar. From the factorial design, it was found that the alternate stirring mode showed poorer purification effect than that of unidirectional stirring mode at low speed(500 rpm). In addition, the factor that had the most significant effect on the degree of purification was the stirring speed.

  • PDF

과전류에 의해 단락된 전선의 결정성장 특성에 관한 연구 (Study of the Characteristics and Crystal Growth of a shorted Wire by Overcurrent)

  • 박진영;방선배;고영호
    • 한국화재소방학회논문지
    • /
    • 제31권6호
    • /
    • pp.83-90
    • /
    • 2017
  • 전선에 정격이상의 과전류가 흐르게 되면 온도가 상승하고 전선피복이 열화되어 단락현상이 발생한다. 과전류의 크기에 따라 전선의 온도 상한치는 변화하며, 각각의 온도 상한치에서 단락이 발생할 때, 단락온도와 전선표면온도간 온도차로 인해 응고과정에서 냉각속도 차이가 발생한다. 이때 용융단면에 형성되는 수지상 조직의 패턴특징이 상이하게 된다. 본 논문에서는 과전류 크기에 따라 변화하는 전선온도의 상한치를 측정하고, 이때 단락을 발생시켜 수지상의 2차 가지 간격(Dendrite Arm Spacing : DAS)을 분석하여 수치를 정량화 하였다. 실험결과, 과전류 크기가 커짐에 따라 전선온도의 상한치는 증가하였으며, 전선온도가 높아질수록 2차 가지 간격이 증가하는 것을 확인하였다.