• 제목/요약/키워드: Sn-Pb solder

검색결과 271건 처리시간 0.023초

저Pb Sn-5%Pb-1.5%Ag-x%Bi계 솔더 합금의 특성에 관한 연구 (A study on the characteristics of low Pb Sn-5%Pb-1.5%Ag-x%Bi solder alloys)

  • 홍순국;주철홍;강정윤;김인배
    • Journal of Welding and Joining
    • /
    • 제16권3호
    • /
    • pp.157-166
    • /
    • 1998
  • Recently as environmental pollution caused by Pb has posed a serious threat to the global environment, the trend to regulate the usage of Pb in electronic industry is one the rise. Currently, the solder alloy with high Pb content, Sn-37%Pb, is utilized in the electronic assembly therefore, the objective of this study is to develop an alternative solder alloy for the existing Sn-37%Pb solder alloy. First thing, this work choosed Sn-5%Pb-1.5%Ag, Sn-5%Pb-1.5%Ag-x%Bi(x=1~5%) for candidate solder alloys, and examined their properties such as melting range, wettability, microhardness, tensile property, oxidation behavior and microstructure. Wettability was on the same level of Sn-37%Pb. Dissolution of Pb ion in Sn-5%Pb solder was 0.46ppm. This solder alloy revealed cellular dendrite microstructure $\beta$-Sn matrix, Pb-rich phase, Ag/Sn, and Cu/Sn Intermetallic compounds. The range of solidification temperature was within 3$0^{\circ}C$. Also these alloy displayed higher tensile strength and lower elongation than Sn-37%Pb. The resistance of oxidation in Sn-5%Pb-1.5%Ag solder alloy was superior to that of Sn-37%Pb solder alloy. But that of Sn-5%Pb-1.5%Ag-5%Bi solder alloy was equal to that of Sn-37%Pb solder alloy.

  • PDF

Pb Free Sn-2%Ag-x%Bi계 Solder의 특성에 관한 연구 (A study on the characteristics of Pb free Sn-2%Ag-x%Bi solder alloys)

  • 흥순국;박일경;강정윤
    • Journal of Welding and Joining
    • /
    • 제16권3호
    • /
    • pp.148-156
    • /
    • 1998
  • The purpose of this study is to investigate the characteristics of Pb-Free Sn-2%Ag-Bi solder alloys. The solder alloys used in this study is Sn-2%Ag-(3,5,7,9%) Bi It is examined that their properties such as melting range, wettability, microstructure, microhardness, and tensile property. The addition of Bi(3,5,7,9%) lowered the melting point of the solder and the melting range was 196~203$^{\circ}C$. The wettability of the solder as equal to that of Sn-37% Pb solder. The morphology of structure did not change largely by addition of Bi. But the structure of cellular dendrite of linear type displayed. The tensile strength of the solder was superior to that of Sn-37%Pb solder. But the elongation was inferior to that of Sn-37%Pb solder. The hardness of Sn-2%Ag solder was tow times and that of Sn-2%Ag-Bi solder was three times of that in Sn-37%Pb solder. But the effect of increment of Bi content did not change largely.

  • PDF

저 Pb Sn-5%Pb-1.5%Ag-x%In계 솔도 합금의 특성에 관한 연구 (A Study on the Characteristics of Low Pb Sn-5%Pb-1.5%Pb-1.5Ag-x%In Solder Alloys)

  • 홍순국;주철홍;강정윤;김인배
    • 한국재료학회지
    • /
    • 제8권11호
    • /
    • pp.1011-1019
    • /
    • 1998
  • Pb의 환경오염 문제를 발생하지 않는 저농도 Pb 솔도합금을 개발하기 위하여, 새로운 Sn-5%Pb-1.5%Ag-x%In계 합금 조성을 설계하고, 이 합금의 융점, 젖음성, 상분석, 경도, 인장강도, 드로스성을 평가하여, Sn-37%Pb 솔더오 대체 가능성을 타진하였다. Sn-37%Pb 솔도 합금의 Pbdldhs 용출농도는 국제규제치인 3ppm보다 훨씬 적은 0.46ppm이었고, 환경문제를 유발하지 않는 것으로 확인되었다. 이 합금계의 융점은 $183-192^{\circ}C$이고, 응고온도범위도 $5^{\circ}C$내외로 매우 좁았다. 젖음성은 In의 첨가양에 따라 큰 차이가 거의 없었으며, Sn-375Pb와 비슷하였다. 융점 및 젖음성 측면에서 Sn-37%Pb와 대체 가능한 것으로 판단되었다. 경도는 Sn-37%Pb의 약 1.5배이고, 인장강도는 Sn-37%Pb의 것보다 높고, In의 첨가량에 따라 증가하였지만, 연신율은 감소하였다. In이 1% 첨가된 합금에서는 수지 상정 경계에 Ag3Sn과 Pb가 정출되고, 3% 이상에서는 $Ag_3Sn$$Ag_3In$ 및 Pb가 정출되었다. 드로스 생성속도는 Sn-37%Pb 합금이 Sn-5%Pb-1.5%Ag 합금보다 빠르고, In을 첨가할수록 느리고 2%의 In을 첨가한 합금은 180분에서도 거의 드로스가 발생하지 않았다.

  • PDF

A:V Ratio 변화에 따른 Sn-37Pb, Sn-4.0Ag-0.5Cu Solder 접합부의 특성 연구 (A Study on Characteristics of Sn-37Pb and Sn-4.0Ag-0.5Cu Solder Joints as Various A:V Ratio)

  • 한현주;임석준;문정탁;이진
    • 한국마이크로전자및패키징학회:학술대회논문집
    • /
    • 한국마이크로전자및패키징학회 2001년도 추계 기술심포지움
    • /
    • pp.67-73
    • /
    • 2001
  • To investigate the relationships of solder joint characteristics with solder composition and A:V ratio (solder volume per pad area), Sn-37Pb and Sn-4.0Ag-0.5Cu solder balls with 330, 400, 450 and $457{\mu}{\textrm}{m}$ size were reflowed on same substrate. Sn-37Pb and Sn-4.0Ag-0.5Cu was reflowed at $220^{\circ}C$ and $240^{\circ}C$ respectively by IR-type soldering machine. As a result of reflowed solder- ball diameter(D) and height(H) measurement, D/H was decreased with solder ball size increment in range of 330~450 ${\mu}{\textrm}{m}$. But, D/H was increased in the solder joint for 457 ${\mu}{\textrm}{m}$ size, it was caused possibly by decrement of solder ball height increment compared with solder volume increment. As a result of shear and pull test, joint strength with A:V ratio was high. Joint strength of Sn-4.0Ag-0.5Cu was higher than Sn-37Pb. However, Sn-37Pb had more stable solder joint of small standard deviation. A thick and clean scallop type Ni-Cu-Sn intermetallic compound layer was formed in high A:V ratio and Sn-4.0Ag-0.5Cu solder joint interface.

  • PDF

진공 증발법에 의해 제조된 플립 칩 본딩용 솔더의 미세 구조분석 (Microstructure Characterization of the Solders Deposited by Thermal Evaporation for Flip Chip Bonding)

  • 이충식;김영호;권오경;한학수;주관종;김동구
    • 한국표면공학회지
    • /
    • 제28권2호
    • /
    • pp.67-76
    • /
    • 1995
  • The microstructure of 95wt.%Pb/5wt.%Sn and 63wt.%Sn/37wt.%Pb solders for flip chip bonding process has been characterized. Solders were deposited by thermal evaporation and reflowed in the conventional furnace or by rapid thermal annealing(RTA) process. As-deposited films show columnar structure. The microstructure of furnace cooled 63Sn/37Pb solder shows typical lamellar form, but that of RTA treated solder has the structure showing an uniform dispersion of Pb-rich phase in Sn matrix. The grain size of 95Pb/5Sn solder reflowed in the furnace is about $5\mu\textrm{m}$, but the grain size of RTA treated solder is too small to be observed. The microstructure in 63Sn/37Pb solder bump shows the segregation of Pb phase in the Sn rich matrix regardless of reflowing method. The 63Sn/37Pb solder bump formed by RTA process shows more uniform microstructure. These result are related to the heat dissipation in the solder bump.

  • PDF

Immersion Ag가 도금된 Cu기판을 가진 Pb-free solder 접합부의 신뢰성 평가 (Reliability evaluation of Pb-free solder joint with immersion Ag-plated Cu substrate)

  • 윤정원;정승부
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2006년도 춘계 학술대회 개요집
    • /
    • pp.30-32
    • /
    • 2006
  • The interfacial reaction and reliability of eutectic Sn-Pb and Pb-free eutectic Sn-Ag ball-grid-array (BGA) solders with an immersion Ag-plated Cu substrate were evaluated following isothermal aging at $150^{\circ}C$. During reflowing, the topmost Ag layer was dissolved completely into the molten solder, leaving the Cu layer exposed to the molten solder for both solder systems. A typical scallop-type Cu-Sn intermetallic compound (IMC) layer was formed at both of the solder/Cu interfaces during reflowing. The thickness of the Cu-Sn IMCs for both solders was found to increase linearly with the square root of isothermal aging time. The growth of the $Cu_3Sn$ layer for the Sn-37Pb solder was faster than that for the Sn-3.5Ag solder, In the case of the Sn-37Pb solder, the formation of the Pb-rich layer on the Cu-Sn IMC layer retarded the growth of the $Cu_6Sn_5$ IMC layer, and thereby increased the growth rate of the $Cu_3Sn$ IMC layer. In the ball shear test conducted on the Sn-37Pb/Ag-plated Cu joint after aging for 500h, fracturing occurred at the solder/$Cu_6Sn_5$ interface. The shear failure was significantly related to the interfacial adhesion strength between the Pb-rich and $Cu_6Sn_5$ IMC layers. On the other hand, all fracturing occurred in the bulk solder for the Sn-3.5Ag/Ag-plated Cu joint, which confirmed its desirable joint reliability.

  • PDF

솔더볼 조성에 의한 피로강도의 영향 (Effects of Fatigue Strength by Solder Ball Composition)

  • 김경수;김진영
    • 한국진공학회지
    • /
    • 제13권3호
    • /
    • pp.127-131
    • /
    • 2004
  • BGA(ball grid array) package에서 솔더볼의 피로강도에 대한 솔더 조성에 대한 영향을 조사하기 위하여 패키지 신뢰성 시험을 실시하였다. 공정조성 솔더 63Sn/37Pb, 62Sn/36Pb/2Ag, 63Sn/34.4Pb/2Ag/0.5Sb 솔더를 이용하여 제조된 시편을 MRT Lv3 (moisture resistance test level) 조건에서 전처리 후 T/C(temperature cycle test) 실험을 수행하였다. 각각의 신뢰성 시험에 대하여 전단강도를 측정하였으며, 미세 조직 사진을 얻었다. 또한, SEM (scanning electron microscope)과 EDX (energy dispersive X-ray)를 이용하여 파괴 기구에 대한 분석을 실시하였다. Sn63Pb34.5Ag2Sb0.5 솔더에서 Au-Sn 성장비는 63Sn/37Pb, 62Sn/36Pb/2Ag 솔더에 비해 느리다 솔더 조성에 따른 솔더볼의 전단응력 저하에 대하여 논의하였다.

Phase Transformation of Sn-Pb-Bi Solder for Photovoltaic Ribbon: A Real-time Synchrotron X-ray Scattering Study

  • Cho, Tae-Sik
    • Transactions on Electrical and Electronic Materials
    • /
    • 제15권3호
    • /
    • pp.155-158
    • /
    • 2014
  • The phase transformation of Sn-Pb-Bi solder for photovoltaic ribbon during soldering was studied using real-time synchrotron x-ray scattering. At room temperature, Sn and Pb crystal phases in the solder existed separately. By heating to $92^{\circ}C$, a new PbBi alloy crystal phase was formed, which grew further up to $160^{\circ}C$. The Sn crystal phase first started to melt at $160^{\circ}C$, and was mostly melted at $165^{\circ}C$. In contrast, the Pb and PbBi crystal phases started to melt at $165^{\circ}C$, and were mostly melted at $170^{\circ}C$. The useful result was obtained, that the solder's melting temperature decreased from $183^{\circ}C$ to $170^{\circ}C$ by addition of a small amount of Bi atoms to the eutectic Sn62-Pb38 (wt%) solder. Our study first revealed the detailed in-situ phase transformation of Sn-Pb-Bi solder during heating to the eutectic temperature. Considering the results of peel strength and hardness, adding 1 wt% of Bi atoms to the Sn62-Pb38 (wt%) solder produced an appropriate composition.

Sn-37mass%Pb 솔더 및 Sn-3.5mass%Ag 무연솔더를 이용한 ${\mu}BGA$ 솔더접합부의 열피로수명 예측 (Thermal Fatigue Life Prediction of ${\mu}BGA$ Solder Joint Using Sn-37mass%Pb Solder and Sn-3.5mass%Ag Lead-free Solder)

  • 신영의;이준환;하범용;정승부;정재필
    • Journal of Welding and Joining
    • /
    • 제19권4호
    • /
    • pp.406-412
    • /
    • 2001
  • This study is focussed on the numerical prediction of the thermal fatigue life of a ${\mu}BGA$(Micro Ball Grid Array) solder joint. Numerical method is used to perform three-dimensional finite element analysis for Sn-37mass%Pb. Sn-3.5mass%Ag solder alloys during the given thermal cycling. Strain values, along with the result of mechanical fatigue tests for solder alloys were then used to predict the solder joint fatigue life using the Coffin-Manson equation. In this study, a practical correlation for the prediction of the thermal fatigue life is suggested by using the dimensionless variable $\gamma$. As a result. it could be found that Sn-3.5mass%Ag has longer fatigue life than Sn-37mass%Pb in low cycle fatigue. In addition. the result with ${\gamm}ashow$a good agreement with the FEA results.

  • PDF

전단펀치-크리프 시험에 의한 리플로우 시간별 Pb-free 솔더 합금 접합부에 대한 고온 크리프 물성 평가 (Material Property Evaluation of High Temperature Creep on Pb-free Solder Alloy Joint to Reflow Time by Shear Punch-creep Test)

  • 함영필;허우진;유효선;양성모
    • 한국자동차공학회논문집
    • /
    • 제21권1호
    • /
    • pp.145-153
    • /
    • 2013
  • In this study, shear punch-creep (SP-Creep) at Sn-4Ag/Cu pad the joint was tested by using environment-friendly Pb-free solder alloy Sn-4Ag of electronic components. Pb eutectic alloy (Sn-37Pb) joints limited to environmental issues with reflow time (10sec, 30sec, 100sec, 300sec) according to two types of solder alloy joints are compared and evaluated by creep strain rate, rupture time and IMC (Intermetallic Compound) behavior. As the results, reflow time increases with increasing thickness of IMC can be seen at overall 100sec later in case of two solder joints on the IMC thickness of Sn-4Ag solder joints thicker than Sn-37Pb solder joints. In addition, when considering creep evaluation factors, lead-free solder alloy Sn-4Ag has excellent creep resistance more than Pb eutectic alloy. For this reason, the two solder joints, such as in the IMC (Cu6Sn5) was formed. However, the creep resistance of Sn-4Ag solder joints was largely increased in the precipitation strengthening effect of dispersed Ag3Sn with interface more than Sn-37Pb solder joints.