• 제목/요약/키워드: Small Crack

검색결과 584건 처리시간 0.021초

$2_{1/4}$ Cr-1 Mo강의 평활재상의 미소한 표면피로균열의 성장특성 (Propagation Characteristics of Fatigue Microcracks on Smooth Specimen of $2_{1/4}$ Cr-1 Mo Steel)

  • 서창민;우병철;장희락
    • 한국해양공학회지
    • /
    • 제4권2호
    • /
    • pp.250-250
    • /
    • 1990
  • In this paper, fatigue tests were carried out at stress test levels of 461 MPa, 441 MPa, and 431 MPa by using smooth specimen of$2_{1/4}$ Cr-1 Mo steel with the stress ratio(R) of 0.05. The initiation, growth and coalescense process of the major cracks and sub-cracks among the fatigue cracks on the smooth specimen are investigated and measured under each stress level at a constant cycle ratio by the replica technique with optical microscope. Some of the important results are as follows: In spite of the difference of stress levels, the major crack data gather into a small band in the curve of surface crack length and crack depth against cycle ratio N/Nf. The sub-crack data, however, deviate from the band of the major crack. The growth rates, da/dN, of major and sub-crack plotted against the stress intensity factor range, ${\Delta}K$, have the tendency to be compressed on a relatively small band. But it is more effective to predict fatigue life through major cracks. The propagation behavior of surface microcracks on the smooth specimens coincides with that of the specimen having an artificial small surface defect or through crack.

SiC 입자 강화 알루미늄기 복합재료의 표면미소 피로균열 발생 및 초기진전거동 (Initiation and Growth Behavior of Small Surface Fatigue Crack on SiC Particle Reinforced Aluminum Composite)

  • 이상협;최영근;김상태;이문환
    • Composites Research
    • /
    • 제21권6호
    • /
    • pp.15-22
    • /
    • 2008
  • 본 연구는 SiC입자를 20% 강화된 알루미늄기 복합재료를 이용해서 평면굽힘피로시험을 향했다. 표면미소피로균열의 발생 및 진전거동은 레프리카법으로 연속관찰을 했고 파괴원인과 파괴기구를 규명하기 위해서 주사전자현미경을 이용했다. da/dn-$K_{max}$ 관계에서 저응력 레벨에서는 여러 개의 균열이 진전하고, 합체 등이 일어나는 것으로부터 진전속도는 꽤 분산(흐트러짐)이 심하고, 고응력 레벨에서는 비교적 흐트러짐은 적게 나타나는 것을 알 수 있었다.

증기발생기 전열관에서의 응력부식균열 성장해석 (Simulation of Stress Corrosion Crack Growth in Steam Generator Tubes)

  • 신규인;박재학;김흥덕;정한섭
    • 한국안전학회지
    • /
    • 제15권3호
    • /
    • pp.57-65
    • /
    • 2000
  • The stress corrosion crack growth is simulated assuming a small axial surface crack inside a S/G tube. Internal pressure and residual stresses are considered as applied forces. Stress intensity factors along crack front, variation of crack shape and crack growth rate are obtained and discussed. It is noted that the aspect ratio of the crack is not depend on the initial crack shape but depend on the residual stress distribution.

  • PDF

하중진폭이 작은 인장과대 하중의 균열성장 거동 (Crack Growth Behavior of Tensile Overload for Small Load Amplitude)

  • 유헌일
    • 한국생산제조학회지
    • /
    • 제7권2호
    • /
    • pp.54-61
    • /
    • 1998
  • This paper examines the crack growth behavior of 7075-T651 aluminum alloy for small tensile overload under high-low block loading condition. The cantilever beam type specimen with a chevron notch is used in this study. The crack growth and closure are investigated by compliance method. The applied initial stress ratios are R=-0.5 R=0.0 and R=0.25 Crack length, effective stress intensity factor range, ratio of effective stress intensity factor range and crack growth rate etc, are inspected with fracture mechanics estimate.

  • PDF

모터 베어링의 트레판 형상 수정에 관한 연구 (TREPAN SHAPE MODIFICATION OF MOTOR BEARING)

  • 이경원;반재삼;강형선;조규종
    • 한국정밀공학회:학술대회논문집
    • /
    • 한국정밀공학회 2002년도 추계학술대회 논문집
    • /
    • pp.950-953
    • /
    • 2002
  • Trepan prevents wear of an inside part of a bearing when the initial shaft rotates. It continuously contacts with the eccentric part of the shaft in rotation and is loaded repeatedly. Therefore, even if an early crack of a trepan part is small, a crack progresses by a repeated load. If a crack progresses, very small chips come out. This is pill in the rotor and prevents rotation of the compressor. There can be leaks in a microgroove and extreme wear can occur due to lack of oil on the surface contact pan. Therefore, this study was carried out to compare and investigate trepan strength and deflection characteristics between trepan locations and dimension changes using a finite element method and search a motor bearing for a model with bigger stiffness of a trepan part and the same deflection. And then. five different types of the oil groove model were chosen to prevent small crack and considered also machining ability and the analysis was carried out on oil feeding flow.

  • PDF

평활 및 노치재의 미소피로균열측정과 성장특성 (Small Fatigue Crack Measurement and Crack Growth Characteristics for Smooth and Notch Specimens)

  • 이종형
    • 대한기계학회논문집
    • /
    • 제17권9호
    • /
    • pp.2145-2152
    • /
    • 1993
  • The objective of this paper is to examine the detection limit, growth characteristics and notch curvature radius in short crack problem. Measurement techniques such as ultrasonic method and back-face strain compliance method were adopted. The fatigue crack growth rate of the short crack is slower than that of a long crack for a notched specimen. The characteristic of crack growth and crack closure is same as the case of a delay of crack growth caused by constant amplitude load for an ideal crack or single peak overload for a fatigue crack. The short crack is detected effectively by ultrasonic method. A short surface crack occurs in the middle of specimen thickness and is transient to a through crack depth is larger than the notch curvature radius.

304 스테인리스 鋼의 高溫에서의 表面균열 成長特性에 관한 硏究 (Surface crack growth behaviors of 304 stainless steel at elevated temperatures)

  • 서창민;신형섭;권영태
    • 대한기계학회논문집
    • /
    • 제11권3호
    • /
    • pp.355-361
    • /
    • 1987
  • 본 연구에서는 고온기기의 부재로 널리 사용되는 304스테인리스강을 사용하여 기기의 사용조건을 고려한 538.deg. C(1000.deg. F), 593.deg. C(1100.deg. F)및 650.deg. C(1200.deg. F)의 세가지 온도레벨하의 대기중에서 크리이프-피로시험을 실시하여 작은 인공표면결함으로부터 발생.성장하는 표면균열의 성장거동을 조사 연구하였다. 또한 주파수의 영향을 조사 하기 위하여 538.deg. C에서 고온피로시험을 실시하여 이 결과를 크리이프 및 크리이프피로 시험의 결과와 비교.검토하였다.

파괴역학을 이용한 차륜과 레일의 마모에 관한 연구 (A Study on the Wear of Rail by Fracture Mechanics)

  • 구병춘
    • 한국철도학회:학술대회논문집
    • /
    • 한국철도학회 1998년도 창립기념 춘계학술대회 논문집
    • /
    • pp.315-322
    • /
    • 1998
  • A two dimensional elasto-plastic finite element program taking into account contact between crack surfaces if developed in order to analyze subsurface cracking in rolling contact. But the friction between upper and lower surface of the crack is not considered. Under the assumptions of small deformation and small displacement, the incremental theory of plasticity is used to describe plastic deformation. J-integral is computed as the applied Hertzian load slides over the surface with friction. J-integral is correlated with wear rate of the rail. The propagation rate of the right tip of the surface crack is fast by 45% than that of the left side.

  • PDF

A Modified Two-Parameter Solution for Crack-Tip Field in Bending Dominated Specimens

  • Jang Seok-Ki;Zhu Xian Kui
    • Journal of Advanced Marine Engineering and Technology
    • /
    • 제30권4호
    • /
    • pp.494-504
    • /
    • 2006
  • It is well known that the two-parameter $J-A_2$ solution can well characterize the crack-tip fields and quantify the crack-tip constraint for different flawed geometries in variety of loading conditions. However, this solution fails to do so for bending dominated specimens or geometries at large deformation because of the influence of significant global bending stress on the crack-tip field. To solve this issue, a modified $J-A_2$ solution is developed in this paper by introducing an additional term to address the global bending influence. Using the $J_2$ flow theory of plasticity and within the small-strain framework detailed finite element analyses are carried out for the single edge notched bend (SENB) specimen with a deep crack in A533B steel at different deformation levels ranging from small-scale Yielding to large-scale Yielding conditions. The numerical results of the crack-tip stress field are then compared with those determined from the $J-A_2$ solution and from the modified $J-A_2$ solution at the same level of applied loading Results indicate that the modified $J-A_2$ solution largely improves the $J-A_2$ solution, and match very well with the numerical results in the region of interest at all deformation levels. Therefore, the proposed solution can effectively describe the crack-tip field and the constraint for bending dominated specimens or geometries.

Behavioral Characteristics of Fatigue Cracks in Small Hole Defects Located on Opposite Sides of the Shaft Cross Section

  • Sam-Hong;Il-Hyuk;Jeong-Moo
    • International Journal of Precision Engineering and Manufacturing
    • /
    • 제5권4호
    • /
    • pp.36-42
    • /
    • 2004
  • The shaft with the circular cross section has symmetric structural combination parts to keep the rotating balance. Hence the crack usually initiates from symmetric combination parts due to the stress concentration of these parts. In this study to estimate the fatigue behavior of symmetric cracks, the fatigue test was performed by using a rotary bending tester and the specimen with symmetric defects in circular cross section. The characteristics of crack initiation and propagation on the symmetric surface cracks in circular cross section were examined. We also observed the internal crack using the oxidation coloring method and investigated the fatigue behavior using the relationship between the surface crack and the internal crack. As a result, the fatigue life of symmetric cracks was reduced by 35% compared to that of a single crack. We examined the characteristics of fatigue behavior of elements with symmetric cracks using internal crack propagation rate and maximum stress intensity factor range that were obtained from an approximation method.