Analysis of wear properties in Zr alloys with variation of Nb and Sn content (Zr 합금에서 Nb과 Sn의 함량에 따른 마멸특성분석)

  • Lee Young-Ho;Kim Hyung-Kyu
    • Proceedings of the Korean Society of Tribologists and Lubrication Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.64-71
    • /
    • 2003
  • In order to evaluate the effect of alloying elements (Nb and Sn) on the wear resistance of advanced Zr fuel claddings, sliding wear tests have been performed in room temperature air and water and these results were compared with those of commercial alloys such as Zircaloy-4, A and B alloys. As a result, the advanced Zr fuel claddings have a similar wear resistance compared with the commercial alloys. The wear resistance of the advanced Zr fuel claddings is closely releted to the content of Nb and Sn even though the effects of transition elements are involved in deforming wear properties. In the tested specimens with similar Sn content, wear volume became down to a minimum at $0.4\;wt\;\%$ Nb, then rapidly increased at 1.0 wt Nb. This behavior results in the variation of grain size with alloying contents. But Sn did not have a significant effect on the wear volume of advanced Zr fuel claddings below $1.1\;wt\%$. The relationship between alloying elements and wear behaviour was evaluated and discussed using material compatibility factor.

  • PDF

Observation on the Microstructures of Cu-TiB2 Composites with Wear Behavior (Cu-TiB2 복합재료의 마모거동에 따른 미세조직 관찰)

  • Lee, Tae-Woo;Kang, Kae-Myung
    • Korean Journal of Materials Research
    • /
    • v.16 no.8
    • /
    • pp.511-515
    • /
    • 2006
  • The dispersion hardened $Cu-TiB_2$ composites are a promising candidate for applications as electrical contact materials. The $Cu-TiB_2$ composites for electrical contact materials can reduce material cost and resource consumption caused by wear, due to their good mechanical and electrical properties. In this study, we investigated the wear phenomenon for $Cu-TiB_2$ composites fabricated with hot extrusion, by varying particle sizes and volume fractions of $TiB_2$. The wear tests were performed under the dry sliding condition with a fixed total sliding distance of 40 m. The contact loads at a constant speed of 3.5 Hz were 20, 40, 60, and 80 N. The friction coefficients and wear losses were measured during wear tests. Worn surfaces and wear debris after wear tests were investigated using the scanning electron microscope and the optical microscope. The microstructures of interface between Cu matrix and $TiB_2$ particle before and after wear tests were studied by the transmission electron microscope.

Thermal Sprayed AlSiMg/TiC Composite Coatings : Wear Characteristics (II) (AlSiMg/TiC 복합 용사피막 : 마모 특성 (II))

  • 양병모;변응선;박경채
    • Journal of Welding and Joining
    • /
    • v.18 no.5
    • /
    • pp.105-111
    • /
    • 2000
  • The wear behavior of thermal sprayed AlSiMg-40TiC composite coatings were studied as a function of load and sliding velocity under unlubricated conditions. Experiments were performed using a block-on-ring(WC-6wt%/Co, Hv 1500) type. The tests were carried out a various load(30∼ 125.5N) and sliding velocity(0.5∼2.0m/s). Three wear rate regions were observed in the AlSiMg-40TiC composite coatings. The wear rate in region I at low load (less then 8N( were less than 1×{TEX}$10^{-5}${/TEX}㎣/m. Low wear rates in region I resulted from the load-bearing capacity of TiC particles. The transition from region I to II occurred when the applied load exceeded the fracture and pull-out strength of the particles. The TiC fractured particles trapped between the specimen and the counterface acted as third-body abrasive wear. The subsurface layer worn surface in region II was composed of the mechanically mixed layer (MML). The wear rate increase abruptly above a critical load (region III). The high wear rate in region III was induced by frictional temperature and involves massive surface damage.

  • PDF

A Study on the High Temperature Deformation and the Cavity Initiation of Gamma TiAl Alloy ($\gamma$-TiAl 합금의 고온변형 및 Cavity 형성 연구)

  • Kim J. H.;Ha T. K.;Chang Y. W.;Lee C. S.
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 2001.05a
    • /
    • pp.172-175
    • /
    • 2001
  • The high temperature deformation behavior of two-phase gamma TiAl alloy has been investigated with the variation of temperature and ${\gamma}/{\alpha}_2$ volume fraction. For this purpose, a series of load relaxation tests and tensile tests have been conducted at temperature ranging from 800 to $1050^{\circ}C$. In the early stage of the deformation as in the load relaxation test experimental flow curves of the fine-grained TiAl alloy are well fitted with the combined curves of two processes (grain matrix deformation and dislocation climb) in the inelastic deformation theory. The evidence of grain boundary sliding has not been observed at this stage. However, when the amount of deformation is large (${\epsilon}{\approx}$ 0.8), flow curves significantly changes its shape indicating that grain boundary sliding also operates at this stage, which has been attributed to the occurrence of dynamic recrystallization during the deformation. With the increase in the volume fraction of ${\alpha}_2$-phase, the flow stress for grain matrix deformation increases since ${\alpha}_2$-Phase is considered as hard phase acting as barrier for dislocation movement. It is considered that cavity initiation is more probable to occur at ${\alpha}_2/{\gamma}$ interface rather than at ${\gamma}/{\gamma}$ interface.

  • PDF

Effect of Contact Load on Wear Property of (TiB+TiC) Particulates Reinforced Titanium Matrix Composites ((TiB+TiC) 입자강화 Ti기 복합재료의 접촉하중에 따른 내마모 특성)

  • Choi, Bong-Jae
    • Journal of Korea Foundry Society
    • /
    • v.37 no.4
    • /
    • pp.115-122
    • /
    • 2017
  • The aim of this research is to evaluate the wear properties of (TiB+TiC) paticulate reinforced titanium matrix composites (TMCs) by in-situ synthesis. Different particle sizes (1500, $150{\mu}m$) and contents (0.94, 1.88 and 3.76 mass% for Ti, 1.98 and 3.96 mass% for the Ti6Al4V alloy) of boron carbide were added to pure titanium and to a Ti6Al4V alloy matrix during vacuum induction melting to provide 5, 10 and 20 vol.% (TiB+TiC) particulate reinforcement amounts. The wear behavior of the (TiB+TiC) particulate reinforced TMCs is described in detail with regard to the coefficient of friction, the hardness, and the degree of reinforcement fragmentation during sliding wear. The worn surfaces of each sliding wear condition are shown for the three types of wear studied here: transfer layer wear, particle cohesion wear and the development of abrasive areas. The fine reinforcements of TMCs were easily fragmented from the Ti matrix as compared to coarse reinforcements, and fragmented debris accelerated the decrease in the wear resistance.

Friction Characteristics of the Tip Seal in a Scroll Compressor (스크롤 컴프레서 팁실의 마찰특성)

  • Jeong, Bong Soo
    • Tribology and Lubricants
    • /
    • v.30 no.6
    • /
    • pp.370-377
    • /
    • 2014
  • The basic elements in a rotary-type scroll compressor are two identical spiral scrolls containing refrigerant gas. The pressure variations in the compression pockets of a scroll compressor change the forces acting on the orbiting scroll, and these forces affect the dynamic behavior of the compression mechanism parts. To achieve high efficiency, using a self-sealing mechanism as a tip seal mechanism is very effective. Tip seals, which are placed on top of the scroll wraps, accomplish thrust sealing. This study calculates the friction force between the tip seal and the side plate of a scroll compressor using the numerical model considered in the Reynolds equation. The calculated friction force is verified by an experiment using a pin-on-disk apparatus. A hydraulic servo valve that controls the pressure of the oil hydraulic cylinder applies the normal load for the test, and a DC servo motor controls the sliding velocity of the disk. The friction force and normal load are measured by the force sensors attached to the supporting parts. The results show that the theoretical and experimental results are similar and that the friction is influenced by the viscosity of the oil and the sliding velocity of the scroll.

A Study on the Wear Behavior of the Cu-TiB2 Composites (Cu-TiB2 복합재료의 마모거동에 관한 연구)

  • Kim Jung-Nam;Choi Jong-Un;Kang Kae-Myung
    • Korean Journal of Materials Research
    • /
    • v.15 no.1
    • /
    • pp.61-65
    • /
    • 2005
  • The titanium $diboride(TiB_2)$ has high strength(750MPa), high melting point $(3225^{\circ}C)\;and\;10\%$ IACS electrical conductivity. On this account, the dispersion hardening $Cu-TiB_2$ composites(MMCs) are a promising candidate for applications as electrical contact materials. MMCs for electrical contact materials can reduce material cost and resource consumption caused by wear, due to its good mechanical and electrical property. In this study, we attempt to prepare MMCs with various volume fraction and particle size of $TiB_2$ by means of hot extruded and cold drawn process. Dry sliding wear tests were performed on a pin-on-disk type wear tester, sliding against SM45C under the different applied loads. After wear testing, the microstructures of the worn surfaces were observed by SEM and the microhardnesses of the subsurface zone were measured.

Molecular Simulation of Influence of Surface Energy on Water Lubrication (표면 에너지가 물 윤활 현상에 미치는 영향에 대한 분자시뮬레이션 연구)

  • Hyun-Joon Kim
    • Tribology and Lubricants
    • /
    • v.39 no.6
    • /
    • pp.273-277
    • /
    • 2023
  • This paper presents a molecular dynamics simulation-based numerical investigation of the influence of surface energy on water lubrication. Models composed of a crystalline substrate, half cylindrical tip, and cluster of water molecules are prepared for a tribological-characteristic evaluation. To determine the effect of surface energy on lubrication, the surface energy between the substrate and water molecules as well as that between the tip and water molecules are controlled by changing the interatomic potential parameters. Simulations are conducted to investigate the indentation and sliding processes. Three different normal forces are applied to the system by controlling the indentation depth to examine the influence of normal force on the lubrication of the system. The simulation results reveal that the solid surface's surface energy and normal force significantly affect the behavior of the water molecules and lubrication characteristics. The lubrication characteristics of the water molecules deteriorate with the increasing magnitude of the normal force. At a low surface energy, the water molecules are readily squeezed out of the interface under a load, thus increasing the frictional force. Contrarily, a moderate surface energy prevents expulsion of the water molecules due to squeezing, resulting in a low frictional force. At a high surface energy, although squeezing of the water molecules is restricted, similar to the case of moderate surface energy, dragging occurs at the soil surface-water molecule interface, and the frictional force increases.

The Effect of Si Content on the Tribological Behaviors of Ti-Al-Si-N Coating Layers (Ti-Al-Si-N 코팅막의 마모거동에 미치는 Si 함량의 영향)

  • Jin, Hyeong-Ho;Kim, Jung-Wook;Kim, Kwang-Ho;Yoon, Seog-Young
    • Journal of the Korean Ceramic Society
    • /
    • v.42 no.2 s.273
    • /
    • pp.88-93
    • /
    • 2005
  • Ti-AI-Si-N coating layers were deposited on WC-Co substrates by a hybrid system of arc ion plating and sputtering techniques. The coatings were prepared with different Si contents to investigate the effect of Si content on their mechanical properties and microstructures. The dry sliding wear experiments were conducted on Ti-AI-Si-N coated WC-Co discs at constant load, 3N, and sliding speed, 0.1 m/s with two different counterpart materials such as steel ball and zirconia ball using a conventional ball-on-disc sliding wear apparatus. In the case of steel ball, the friction coefficient of Ti-AI-Si-N coating layers became lower than that of Ti-AI­N coating layers. The friction coefficient decreased with increasing of Si content due to adhesive wear behavior between coating layer and steel ball. On the contrary, in the case of zirconia ball, the friction coefficient increased with increasing of Si content, indicating that abrasive wear behavior was more dominant when the coating layers slid against zirconia ball.

Thermal Behavior and Structral Efficiency of Rahmen with Sliding-Girder (슬라이딩 거더를 가진 라멘의 온도거동과 구조효율)

  • Jeong, Dal-Yeong;Jeong, Chang-Hyun;Yhim, Sung-Soon
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.21 no.1
    • /
    • pp.1-7
    • /
    • 2020
  • Although the temperature load is an important load among the various loads affecting the behaviors of general rahmen-type temporary bridges (GRTB), no study of the thermal load has been carried out. In the case of GRTB, horizontal displacement should be free, and the generated internal force should be minimized to reduce stress due to a temperature load. Sliding girder type bridge (SGTB) allows the axial deformation due to thermal load, and decreases the axial stress and delivers bending stress. This study examined the temperature behavior of an SGTB. Structural analysis was carried out for four types of spans (eq, 10, 20, 30, and 40m) and three types of pier heights (eq, 2, 4, and 6m) along with the GRTB. The applied loads were a fixed vertical load and an axial temperature load. The friction coefficient was 0.4, which is a representative value of a steel girder. Consequently, the stress of the SGTB increased with increasing span length, regardless of the temperature load. The stress of the GRTB increased with increasing temperature and span length. Compared to the GRTB, the stress of the SGTB decreased by 20% to 50% at the center of the girder and by 50% to 90% at the bottom of the pier. This could secure the structural efficiency compared to the GRTB with the same specifications.