Distribution Characteristics of Radionuclies (60Co, 137Cs) During the Melting of Radioactive Metal Waste (방사성 금속폐기물의 용융시 방사성 핵종(60Co, 137Cs)의 분배특성)

  • Min, Byung Youn;Choi, Wang Kyu;Oh, Won Zin;Jung, Chong Hun;Kang, Yong
    • Korean Chemical Engineering Research
    • /
    • v.45 no.6
    • /
    • pp.627-632
    • /
    • 2007
  • A fundamental study on the melt decontamination of metal wastes generated by dismantling the nuclear facility, the melting of metal wastes such as stainless steel and carbon steel have been carried out to investigate the distribution phenomena of the radioisotopes such as $^{60}Co$ and $^{137}Cs$ into the ingot, slag and dust phases by using the various slag types, slag concentration and basicity in an arc furnace. The $^{60}Co$ remained homogeneously in the ingot phase above 90 % and it was barely present in the slag below 10 %. The effect of the slag composition on the distribution for Co-60 was not considerable, but a basic slag former with high fluidity showed effective. $^{137}Cs$ was completely eliminated from the melt of the stainless steel as well as the carbon steel and distributed to the slag and the dust phase.

Preparation of Porous Ceramics Sound Absorbent Material Using Sewage Sludge Slag (하수슬러지 슬래그를 이용한 다공성 세라믹스 흡음재료 제조)

  • 신대용;한상목
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.3
    • /
    • pp.273-278
    • /
    • 2003
  • The effects of content and particle size of sewage sludge slag on the sound absorption was investigated and the physical$.$mechanical properties of porous ceramics for sound absorbent material was studied. The physical$.$mechanical properties of specimens have depended on sintering temperature and slag content without particle size effect of slag. As water glass content increase and particle size of slag decrease at the same slag content, physical$.$mechanical properties of them have been improved. The bulk density and compressive strength of specimens with the batch composition of 77∼89 wt% of slag content and particles with 1∼3 mm, and sintered at 1,050$^{\circ}C$ for 2 h were 1.48∼1.71 and 86∼163 kgf/$\textrm{cm}^2$, respectively. The specimens with 1∼3 mm and <1 mm of particles size showed good sound absorption property at low frequency and high frequency region. With increasing thickness of specimens, sound absorption properties at low frequency region were increased.

Flowing and Setting Properties of High Flowing$\cdot$High Strength Concrete using Blast-Furnace Slag according to the Chemical Agent (고로슬래그 미분말을 사용한 고유동고$\cdot$강도 콘크리트의 혼화제에 따른 유동 및 응결 특성)

  • Kim, Yong-Ro;Shim, Jae-Hyung;Kang, Suk-Pyo;Kim, Sang-Yun;Baik, Chul;Kim, Moo-Han
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2000.10b
    • /
    • pp.1242-1247
    • /
    • 2000
  • Results from a study on the effect of the chemical agent on the flowing and setting properties of high flowing.high strength concrete using blast-furnace slag are presented in this paper. The flowing and setting properties of concrete are investigated by slump, slump-flow, flowing velocity, L-flow, velocity of V-funnel, L-spatial passability and setting time. In addition, kinds of chemical agent were composed of naphthalene type, of naphthalene and melamine and melamine type. The results indicate that dispersive capacity can be increased by naphthalene composition. Also, it shows that viscosity and early strength can be increased by melamine composition.

  • PDF

Characteristics of Basalt Materials Derived from Recycling Steel Industry Slags (철강산업 슬래그를 이용하여 제조한 바잘트 소재의 특성)

  • Jung, Woo-Gwang;Back, Gu-Seul;Yoon, Mi-Jung;Lee, Jee-Wook
    • Korean Journal of Materials Research
    • /
    • v.27 no.5
    • /
    • pp.281-288
    • /
    • 2017
  • In this study, Fe-Ni slag, converter slag and dephosphorization slag generated from the steel industry, and fly ash or bottom ash from a power plant, were mixed at an appropriate mixing ratio and melted in a melting furnace in a mass-production process for glass ceramics. Then, glass-ceramic products, having a basalt composition with $SiO_2$, $Al_2O_3$, CaO, MgO, and $Fe_2O_3$ components, were fabricated through casting and heat treatment process. Comparison was made of the samples before and after the modification of the process conditions. Glass-ceramic samples before and after the process modification were similar in chemical composition, but $Al_2O_3$ and $Na_2O$ contents were slightly higher in the samples before the modification. Before and after the process modification, it was confirmed that the sample had a melting temperature below $1250^{\circ}C$, and that pyroxene and diopside are the primary phases of the product. The crystallization temperature in the sample after modification was found to be higher than that in the sample before modification. The activation energy for crystallization was evaluated and found to be 467 kJ/mol for the sample before the process modification, and 337 kJ/mol for the sample after the process modification. The degree of crystallinity was evaluated and found to be 82 % before the process change and 87 % after the process change. Mechanical properties such as compressive strength and bending strength were evaluated and found to be excellent for the sample after process modification. In conclusion, the samples after the process modification were evaluated and found to have superior characteristics compared to those before the modification.

A Study of Effecting Factor in the Reology and Physical Properties of Cements (시멘트 유동성과 물성에 미치는 영향인자에 관한 연구)

  • 엄태선;최상흘
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.10
    • /
    • pp.1027-1036
    • /
    • 1997
  • The reology and several physical properties of cements are studied by varying the different mineral composition and particle size distribution(PSD) of cements with closed circuit ball mill for high workability, low heat of hydration, and high strength. In this study, we found that the workability of concretes is related to the viscosity of cement, and affects to strength. Here, this workability is affected by mineral composition (C3A) and the PSD. Especially, rosin-rammer index and 44${\mu}{\textrm}{m}$ residue in the PSD of cements are affected to water demand, casting property, slump loss, strength of cements. From the above results, the conditions of cement for high workability, low heat of hydration and high strength are to use low C3A clinker, 5-10% slag addition, and to grind cement below 0.7 rosin-rammer index, above 3.5-4.5% 44 ${\mu}{\textrm}{m}$ residue, 4000$\pm$100 $\textrm{cm}^2$/g blaine. Such cements are, therefore, supurior to super low heat cement and slag-blended cement in comparing the physical properties of strength, slump, slump-flow, adiabetic temperature, etc.

  • PDF

Viscosity Change of Al2O3-SiO2-CaO Slag System with Used Electronic Scrap (산화처리된 PCB 스크랩을 첨가한 Al2O3-SiO2-CaO 3성분계 슬래그의 점도)

  • Kwon, Eui-Hyuk;Han, Sin-Suk;Ji, Jae-Hong;Han, Jeong-Whan;You, Byung-Don;Kim, Byung-Soo;Lee, Jae-Chun
    • Korean Journal of Materials Research
    • /
    • v.13 no.4
    • /
    • pp.239-245
    • /
    • 2003
  • In order to explore the possibility to extract precious metals from PCB(Printed Circuit Board) scrap by gravity separation, a high temperature melting process was adopted, from the recycling view point, to investigate the influence of viscosity on A1$_2$$O_3$-CaO$-SiO_2$ slag system composed of PCB scrap. For optimizing the pre-treatment process of PCB scrap, an experimental condition for the complete calcination and oxidation of organic materials in PCB scrap was established and a quantitative analysis of oxidized PCB scrap was also carrie out. It was found that 6 hours were enough for the complete oxidation of PCB scrap at 1273 K in an atmosphere condition. A slag, l5wt%$A1_2$$O_3$-45wt%CaO-40wt%SiO$_2$, was chosen as a basic slag composition which is determined based on the quantitative analysis of PCB scrap. Viscosities were measured in slag systems both made from pure fluxes and from PCB scrap with additional fluxes. Slag viscosities composed of pure fluxes were measured to be 5.29 poise and 30.52 poise at temperatures of 1773 and 1573 K, whereas that of PCB scrap with additional fluxes were 3.37 poise and 69.89 poise, respectively.

Analytical Estimation of the Performance of Marine Concrete with Mineral Admixture (광물질 혼화재를 혼합한 해양 콘크리트의 해석적 성능 평가)

  • Lee, Bang-Yeon;Kwon, Seung-Jun;Kang, Su-Tae
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.4
    • /
    • pp.301-306
    • /
    • 2015
  • For the purpose of developing high performance marine concrete with improved crack resistance and durability, this analytical study aimed to estimate strength, hydration heat characteristics, and chloride attack resistance of concrete with mineral admixture. Ground granulated furnace slag and fly ash were considered for mineral admixture. The replacement of ground granulated furnace slag and fly ash considered in the analysis was in the range of 0~70% and 0~40 %, respectively. The analysis results indicated that both ground granulated furnace slag and fly ash decreased compressive strength, and the effect of adding ground granulated furnace slag on mitigation of hydration heat was limited whereas fly ash had an noticeable influence on it. It was also found that the replacement with ground granulated furnace slag enhanced the chloride attack resistance but fly ash deteriorated the resistance. From the analytical studies, It could be expected that a ternary blended cement composition with proper amount of ground granulated furnace slag and fly ash might be effective to control crack resistance as well as chloride attack resistance of marine concrete.

Study on the Remelting of Titanium Scrap by DC-ESR Process (DC-ESR법(去)을 이용한 타이타늄 스크랩의 재용융(再熔融)에 관한 연구(硏究))

  • Seo, Yeung-Deuk;Lee, Ho-Seong;Sohn, Ho-Sang
    • Resources Recycling
    • /
    • v.16 no.4
    • /
    • pp.33-39
    • /
    • 2007
  • Titanium scrap was re-melted and refined by using a DC-ESR (Direct Current Electro Slag Remelting) apparatus. A graphite rod was used as an anode. The used slag was $CaF_2-TiO_2-CaO$ slag system. The effect of slag composition on the shape and oxygen content of re-melted ingot was studied. The titanium ingot was produced very well from the $CaF_2-TiO_2$ slag system, and the oxygen content of the ingot was less than that of titanium scrap. The addition of CaO into $CaF_2-TiO_2$ slag system made the bad shape of titanium ingot. The oxygen content of the ingot was also higher than that of titanium scrap.

Development of a User-Friendly Automatic Control System for Electro-Slag Remelting Process

  • Lim, Tae-Gyoon;Reeu, Chang-Woo;Boo, Kwang-Suk
    • 제어로봇시스템학회:학술대회논문집
    • /
    • 2001.10a
    • /
    • pp.97.5-97
    • /
    • 2001
  • This paper presents development of a user-friendly automatic control system for ESR(Electro-Slag Remelting or Refining) process. It is a second-phase refining one, commonly applied to production of high-purity specialty steel. A primarily refined castingot acts as a consumable electrode and melts by the electric resistance heat generated when high current is induced through a slag bath. The quality of product is evaluated by its chemical composition, purity, micro-structure, uniformity, mechanical property, etc. To meet the standards, above all things, the process should be kept sound and the melt rate should track the optimum profile irrespective of environment variations. Current ESR system is manually operated ...

  • PDF

Characteristics of Electro Slag Strip overlaied weldments on the 1.25Cr-0.5Mo Steel (1.25Cr-0.5Mo 강에서의 Electro Slag Strip 육성 용접부 특성)

  • Seong, Hui-Jun;Ju, Myeong-Su;Ju, Jeong-Gwon;Kim, Yeong-Il
    • Proceedings of the KWS Conference
    • /
    • 2005.11a
    • /
    • pp.65-66
    • /
    • 2005
  • In order to evaluate disbonding properties caused by hydrogen on the Electro Slag Strip Welding for 1.25Cr-0.5Mo steel, two kinds of welding consumables were selected and tested under the disbonding condition of $97.2kgf/cm^{2}$ at $425^{\circ}C$. Chemical composition of the welds showed that they have similar chemical compositions. The microsturucture investigation, however, indicated that 'A' weld has high ratio of coarse grain area, while B weld has low. Disbonding results showed that high ratio coarse grain welds showed unacceptable, while low ratio coarse grain welds showed acceptable.

  • PDF