• 제목/요약/키워드: Silk-I

검색결과 273건 처리시간 0.023초

BTCA에 의한 실크/면 교직물의 DP 가공 (I) - 물리적 특성에 미치는 처리 조건의 영향 - (Durable Press Finishing of Silk/Cotton Fabrics with BTCA ( I ) - Effect of Treating Conditions on Physical Properties -)

  • 이문철;조석현
    • 한국염색가공학회지
    • /
    • 제14권1호
    • /
    • pp.43-50
    • /
    • 2002
  • Silk/Cotton fabrics were treated with butanetetracarboxylic acid(BTCA) to improve crease recovery and anti-shrinking properties at various curing temperatures and pH values. We investigated the effects of finishing conditions on add-on of BTCA, bending property(E, 2HB), wrinkle recovery angle, shrinkage, and dyeing properties. The Add-on of BTCA increased with increasing curing temperature and concentration. Crease recovery was improved with decreasing shrinkage. Maximum add-on of BTCA was showed at pH 2.5. In case of dyeing and mercerization, silk side treated with BTCA was more flexible than untreated, whereas cotton side was more stiff. In dyeing after mercerization, B and 2HB values were higher and K/S values were doubled nearly. The hand of fabric improved with decreasing B and 2HB by the BTCA treatment. BTCA treatment after reactive dyeing improved crease recovery, and caused no change of color difference. However, BTCA treatment after reactive dyeing didn't improve crease recovery, whereas B and 2HB were decreased considerably by the treatment.

호장근 추출액에 의한 염색성(I) (The Dyeing Properties of Polygonum cuspidatum Extract( I ))

  • 김미숙;최석철
    • 한국염색가공학회지
    • /
    • 제13권1호
    • /
    • pp.45-54
    • /
    • 2001
  • The Purpose of this studs was to investigate dyeing properties of silk and nylon fabrics by Polygonum cuspidatum extract. The properties were evaluated by it's extracting condition, dyeing condition, mordants variables, methods of mordanting and color fastness. Silk fabric showed the highest K/S value at $50-70^\circ{C}$, while Nylon fabric showed at $90^\circ{C}$. Surface color of dyed fabrics were various by the used mordants ; none-, and Al-mordanted fabrics were yellow, Cu-mordanted fabrics were redish yellow, Fe-mordanted fabrics were olive green. Fe-mordanted silk fabrics showed excellent laundering fastness and light fastness. Both silk and nylon fabric showed excellent laundering and dry cleaning fastness.

  • PDF

삼백초의 염색성 및 항균성(I) (The Dyeability and Antimicrobial Activity of Saururus Chinensis(I))

  • 김병희;송화순
    • 대한가정학회지
    • /
    • 제38권3호
    • /
    • pp.1-9
    • /
    • 2000
  • Saururus-chinensis was used for the natural due stuff extraction and concentration to produce the condensed dye liquid. Using this liquid, the silk and the cotton fabrics were dyed. And then the K/S value, color difference were measured in order to determine the dye ability and the antimicrobial activity. The K/S values of silk were much higher than those of cotton. In terms of the silk fabric, the Al, Cr-premordanting and Fe, Cu-simmordanting method was most efficient of the mordanting method. The various suface colors on the dyed fabric were resulted according to used mordants and mordanting methods. The dye fastness was significantly improved when mordants were added. Among them, Al-mordant improved more than 1 level. The Cu, Fe-mordants showed the greatest antimicrobial activity on both of mordant treat silk and cotton.

  • PDF

밤송이 추출액을 이용한 견 및 면직물 염색(I) (A Study on the Dyeing Properties of Chestnut Bur Extract on Silk and Cotton(I))

  • 장재철;전동원;김애순
    • 한국염색가공학회지
    • /
    • 제12권5호
    • /
    • pp.280-287
    • /
    • 2000
  • For thousands of years, dyes were obtained from natural sources, such as plants and animals. Although synthetic dyes have replaced many natural dyes for commercial use but natural dyes with their fascinating color are still used extensively by some people. To investigate the dyeing properties of chestnut bur, which is most widely found in our country, some experiments were performed under the several dyeing conditions with silk and cotton fabrics. It was found that $\lambda_{max}$ of chestnut but extract was 410nm and the color of the fabric dyed is Yellow Red. The K/S value of silk and cotton fabrics increased when the dyeing temperature was higher than $60^\circ{C}$ and the dyeing time was more than 30 minutes. Optimal dyeing pH was between 5 and 6, and repetition of dyeing increased K/S value of the sample fabrics. K/S value of silk fabric dyed with chestnut bur extract was higher than that of cotton. Post-mordanting method showed higher color yield compared with pre-mordanting, and higher temperature and increased time in mordanting increased the dye-uptake.

  • PDF

Low molecular weight silk fibroin increases alkaline phosphatase and type I collagen expression in MG63 cells

  • Kim, Jwa-Young;Choi, Je-Yong;Jeong, Jae-Hwan;Jang, Eun-Sik;Kim, An-Sook;Kim, Seong-Gon;Kwon, Hae-Yong;Jo, You-Young;Yeo, Joo-Hong
    • BMB Reports
    • /
    • 제43권1호
    • /
    • pp.52-56
    • /
    • 2010
  • Silk fibroin, produced by the silkworm Bombyx mori, has been widely studied as a scaffold in tissue engineering. Although it has been shown to be slowly biodegradable, cellular responses to degraded silk fibroin fragments are largely unknown. In this study, silk fibroin was added to MG-63 cell cultures, and changes in gene expression in the MG-63 cells were screened by DNA microarray analysis. Genes showing a significant (2-fold) change were selected and their expression changes confirmed by quantitative RT-PCR and western blotting. DNA microarray results showed that alkaline phosphatase (ALP), collagen type-I alpha-1, fibronectin, and transforming growth factor-${\beta}1$ expressions significantly increased. The effect of degraded silk fibroin on osteoblastogenic gene expression was confirmed by observing up-regulation of ALP activity in MG-63 cells. The finding that small fragments of silk fibroin are able to increase the expression of osteoblastogenic genes suggests that controlled degradation of silk fibroin might accelerate new bone formation.

견/합성섬유 혼방품의 일욕염색(III) ―산성염료/분산염료 염욕에서의 견/PET의 염착거동― (On Bath Dyeing of silk/synthetic Fibre Blends(III) ―Adsorption Behavior of Acid Dyes/Disperse Dyes on Silk/PET―)

  • Gwag, In Jun;Yoon, Kyung Sup;Kim, Ae Soon;Kim, Gong Ju
    • 한국염색가공학회지
    • /
    • 제5권4호
    • /
    • pp.67-78
    • /
    • 1993
  • In one bath dyeing system of silk/PET fiber blend fabric with acid/disperse dyes, adsorption behavior of disperse dyes and acid dyes on silk and PET fabrics were examined. In the dyeing of PET with C.I.Disperse Red 19(Red 19) and C.I.Disperse Red 60(Red 60) at 10$0^{\circ}C$(carrier dyeing) and 13$0^{\circ}C$, dye uptake with Red 60 was higher than that with Red 19. When the silk/PET dyed with Red 19 and Red 60 at 10$0^{\circ}C$(carrier dyeing) and 13$0^{\circ}C$, dye uptake on PET was influenced by affinity of the dye to the silk fabric dyed together. When the silk/PET dyed with Blue 80/Red 19 and Blue 80/Red 60 at 10$0^{\circ}C$(carrier dyeing) and 13$0^{\circ}C$ for 60 minutes, color of PET dyed with Red 19 and Red 60 was little influenced by Blue 80 but silk dyed with Blue 80 was influenced. Interrelation of K/S value and Munsell value was scarcely any but showed the change tendency of K/S value.

  • PDF

딥코팅에 의한 실크 피브로인막으로 제조한 바이오 압전발전기 (Bio-Piezoelectric Generator with Silk Fibroin Films Prepared by Dip-Coating Method)

  • 김민수;박상식
    • 한국전기전자재료학회논문지
    • /
    • 제34권6호
    • /
    • pp.487-494
    • /
    • 2021
  • Piezoelectric generators use direct piezoelectric effects that convert mechanical energy into electrical energy. Many studies were attempted to fabricate piezoelectric generators using piezoelectrics such as ZnO, PZT, PVDF. However, these various inorganic/organic piezoelectric materials are not suitable for bio-implantable devices due to problems such as brittleness, toxicity, bio-incompatibility, bio-degradation. Thus, in this paper, piezoelectric generators were prepared using a silk fibroin film which is bio-compatible by dip-coating method. The silk fibroin films are a mixed state of silk I and silk II having stable β-sheet type structures and shows the d33 value of 8~10 pC/N. There was a difference in output voltages according to the thickness. The silk fibroin generators, coated 10 times and 20 times, revealed the power density of 16.07 μW/cm2 and 35.31 μW/cm2 using pushing tester, respectively. The silk fibroin generators are sensitive to various pressure levels, which may arise from body motions such as finger tapping, foot pressing, wrist shaking, etc. The silk fibroin piezoelectric generators with bio-compatibility shows the applicability as a low-power implantable piezoelectric generator, healthcare monitoring service, and biotherapy devices.

물/유기용매 불혼합 이성분계에서의 반응염색(Ⅱ) - C. I. Reactive Blue 203을 이용한 견섬유의 염색 - (Reactive Dyeing in Immiscible Two-phase System of Water/Organic Solvent(Ⅱ) - The Dyeing of Silk with C. I. Reactive Blue 203 -)

  • 김태경;김미경;임용진;조광호
    • 한국염색가공학회지
    • /
    • 제13권2호
    • /
    • pp.42-42
    • /
    • 2001
  • Following the prior studs regarding that 1.0g of cotton fabric cound be dyed uniformly with a reactive dye in the solvent mixture of 2㎖ of water and 23㎖ of dichloromethane, silk fabric was dyed with C. I. Reactive Blue 203 in the water/dichloromethane two-phase immiscible solvent media. In order to minimize dye loss due to its hydrolysis, the reactive dyeing was carried out in dichloromethane containing a small amount of water. With only 3㎖ of water in 22㎖ of dichloromethane, 1.0g of silk fabric could be dyed perfectly. The uptake ratio was increased greatly, compared with that of normal reactive dyeing in a water medium. It would seem that the one of hydrophobic solvents, dichloromethane, can assist the even dyeing as it disperses a small amount of dye-dissolved water phase and conveys this water phase to the fabric entirely and uniformly.

물/유기용매 불혼합 이성분계에서의 반응염색(II) - C. I. Reactive Blue 203을 이용한 견섬유의 염색 - (Reactive Dyeing in Immiscible Two-phase System of Water/Organic Solvent (II) - The Dyeing of Silk with C. I. Reactive Blue 203 -)

  • 김태경;김미경;임용진;조광호
    • 한국염색가공학회지
    • /
    • 제13권2호
    • /
    • pp.128-134
    • /
    • 2001
  • Following the prior studs regarding that 1.0g of cotton fabric round be dyed uniformly with a reactive dye in the solvent mixture of $2m\ell$ of water and $23m\ell$ of dichloromethane, silk fabric was dyed with C. I. Reactive Blue 203 in the water/dichloromethane two-phase immiscible solvent media. In order to minimize dye loss due to its hydrolysis, the reactive dyeing was carried out in dichloromethane containing a small amount of water. With only $3m\ell$ of water in $22m\ell$ of dichloromethane, 1.0g of silk fabric could be dyed perfectly. The uptake ratio was increased greatly, compared wish that of normal reactive dyeing in a water medium. It would seem that the one of hydrophobic solvents, dichloromethane, can assist the Even dyeing as it disperses a small amount of dye-dissolved phase and conveys this water phase to the fabric entirely and uniformly.

  • PDF

중성염이 견의 반응염색에 미치는 영향(I) - 양이온의 영향- (Effect of Neutral Salts on the Reactive Dyeing of Silk(I) -Effect of Cations-)

  • 도성국;박찬헌;권지윤
    • 한국염색가공학회지
    • /
    • 제12권6호
    • /
    • pp.372-379
    • /
    • 2000
  • Four kinds of neutral salts with different cations, LiCl, NaCl, KCl, and CsCl, were added to the dye bath to accurately understand the effect of cations on the reactive dyeing of silk with C. I. Reactive Black 5. The cations of salts added lowered the negative surface potential of the silk, improving equilibrium adsorption and the accessibility of the dyestuff to the fiber greatly and speeding up the dyeing rate in the order of $Li^+>Na^+>K^+>Cs^+$. The activation energy$(E_a)$ for the dyeing was in the order of$Li^+>Na^+>K^+>Cs^+$ but the activation free energy$(\Delta{G}^*)$, or the real energy barrier for the reaction, was in the order of $Li^+>Na^+>K^+>Cs^+$ because the degree of the contribution of E$^{a}$ to the activation entropy$(\Delta{S}^*)$ was $Li^+>Na^+>K^+>Cs^+$. It was found from this result that LiCl had the strongest lowering effect on the negative surface potential of silk. The decrease in $\Delta{S}^*$ should be attributed to the loosely bonded activated complex of dyestufffs, cations and fiber molecules at transition state. It was clarified from the Bronsted equation that salts had the ionic strength effect and the specific salt effect on the reactive dyeing.

  • PDF