  • As device size shrinks, contamination will increasingly affect the reliability and yield of device. Therefore, contaminants must be removed from the surfaces of Si wafers prior to each process. But it becomes out increasingly difficult to clean silicon surfaces with finer patterns by the conventional wet treatment because of the viscosity and surface tension of solutions. Hence, a damage less dry cleaning process is needed for the silicon surfaces. For the removal of Si native oxide by UV-enhanced dry cleaning. $F_2$ gas and $F_2/H_2$ mixed gas were applied. As a result of analysis, UV-enhnaced $F_2/H_2$ treatment is more suitable than UV-enhanced $F_2$ treatment for removal of native oxide on the surfaces of Si wafers.

  • PDF

산성 표면절삭결함 제거 공정에 의한 실리콘 태양전지의 텍스쳐링 효과 개선 (Investigation of Improving Texturing Effect by Surface Saw Damage Etching Using Acidic Etchant for Silicon Solar Cells)

  • 박하영;이준성;권순우;윤세왕;임희진;김동환
    • 대한금속재료학회지
    • /
    • 제46권12호
    • /
    • pp.835-840
    • /
    • 2008
  • Texturing for crystalline silicon solar cells is one of the important techniques to increase conversion efficiency by effective photon trapping. Generally, incoming wafers or alkali etched wafers are used for texturing. From this conventional etching process, $7{\sim}10{\mu}m$-sized random pyramids are formed. In this study, acid etching for removal of saw damages was practiced before texturing. This improved the resulting surface morphology, which consisted of $2{\sim}4{\mu}m$-sized pyramids. Because these pyramids covered the surface much more extensively, we obtained reduction of optical losses on the surface. In order to compare with conventional texturing, FE-SEM is used for observing surface morphology and reflectance data is analyzed by UV-VIS spectrophotometer.

다양한 실리콘 웨이퍼 제조를 위한 와이어 전기 방전가공 (Wire Electric Discharge Machining Process of Various Crystalline Silicon Wafers)

  • 문희찬;최선호;박성희;장보윤;김준수;한문희
    • 한국전기전자재료학회논문지
    • /
    • 제30권5호
    • /
    • pp.301-306
    • /
    • 2017
  • Wire electrical discharge machining (WEDM) process was evaluated to slice Silicon (Si) for various applications. Specifically, various Si workpieces with various resistances, such as single and multi crystalline Si bricks and wafers were used. As conventional slicing processes, such as slurry-on or diamond-on wire slicing, are based on mechanical abrasions between Si and abrasive, there is a limitation to decrease the wafer thickness as well as kerf-loss. Especially, when the wafer thickness is less than $150{\mu}m$, wafer breakage increases dramatically during the slicing process. Single crystalline P-type Si bricks and wafers were successively sliced with considerable slicing speed regardless of its growth direction. Also, typical defects, such as microcracks, craters, microholes, and debris, were introduced when Si was sliced by electrical discharge. Also, it was found that defect type is also dependent on resistance of Si. Consequently, this study confirmed the feasibility of slicing single crystalline Si by WEDM.

태양전지용 실리콘 기판의 절삭손상 식각 조건에 의한 곡강도 변화 (Effect of Saw-Damage Etching Conditions on Flexural Strength in Si Wafers for Silicon Solar Cells)

  • 강병준;박성은;이승훈;김현호;신봉걸;권순우;변재원;윤세왕;김동환
    • 한국재료학회지
    • /
    • 제20권11호
    • /
    • pp.617-622
    • /
    • 2010
  • We have studied methods to save Si source during the fabrication process of crystalline Si solar cells. One way is to use a thin silicon wafer substrate. As the thickness of the wafers is reduced, mechanical fractures of the substrate increase with the mechanical handling of the thin wafers. It is expected that the mechanical fractures lead to a dropping of yield in the solar cell process. In this study, the mechanical properties of 220-micrometer-solar grade Cz p-type monocrystalline Si wafers were investigated by varying saw-damage etching conditions in order to improve the flexural strength of ultra-thin monocrystalline Si solar cells. Potassium hydroxide (KOH) solution and tetramethyl ammonium hydroxide (TMAH) solution were used as etching solutions. Etching processes were operated with a varying of the ratio of KOH and TMAH solutions in different temperature conditions. After saw-damage etching, wafers were cleaned with a modified RCA cleaning method for ten minutes. Each sample was divided into 42 pieces using an automatic dicing saw machine. The surface morphologies were investigated by scanning electron microscopy and 3D optical microscopy. The thickness distribution was measured by micrometer. The strength distribution was measured with a 4-point-bending tester. As a result, TMAH solution at $90^{\circ}C$ showed the best performance for flexural strength.

BCB 수지로 본딩한 웨이퍼의 본딩 결합력에 관한 연구 (A Study on the Bond Strength of BCB-bonded Wafers)

  • 권용재;석종원
    • Korean Chemical Engineering Research
    • /
    • 제45권5호
    • /
    • pp.479-486
    • /
    • 2007
  • BCB 수지를 이용하여 본딩한 웨이퍼의 BCB 두께, 본딩 촉진제의 사용여부 및 이웃하는 적층 물질의 종류에 따른 본딩 결합력에 대한 영향을 4-점 굽힘방법을 이용하여 규명한다. 실험결과 본딩 결합력은 BCB 두께에 선형 비례하는데, 이는 BCB의 소성 변형의 정도가 두께에 비례하는 반면에 BCB의 항복 강도에는 영향을 미치지 않기 때문이다. 본딩한 BCB의 두께가 각각 $2.6{\mu}m$$0.4{\mu}m$인 경우에 대하여 본딩 촉진제를 사용 했을 때, 본딩 촉진제와 본딩된 물질의 표면에서는 공유 결합이 형성되기 때문에 본딩 결합력이 증가한다. 산화 규소막이 증착된 실리콘 웨이퍼와 BCB 사이 계면에서의 본딩 결합력은 글래스 웨이퍼와 BCB 사이의 계면에서 보다 약 3배 정도 높다. 이러한 본딩 결합력의 차이는 각 계면에서 Si-O 본드의 본딩 밀도 및 본드 파단 에너지의 차이에 기인한다. PECVD 산화 규소막을 증착한 실리콘 웨이퍼와 BCB 사이 계면의 경우, 기 측정된 $18J/m^2$$22J/m^2$의 본드 파단 에너지를 얻기 위해 각각 약 $12{\sim}13bonds/nm^2$$15{\sim}16bonds/nm^2$의 Si-O 본드 밀도가 필요하다. 반면에, 글래스 웨이퍼와 BCB 사이 계면의 경우에는 기 측정된 $5J/m^2$의 본드 파단 에너지를 얻기 위해 약 $7{\sim}8bonds/nm^2$의 Si-O 본드 밀도가 필요하다.

다층 다공성 실리콘의 합성과 그 광학적 특성 조사 (Synthesis and Optically Characterization of Bragg Structure Porous Silicon)

  • 김성기
    • 통합자연과학논문집
    • /
    • 제2권1호
    • /
    • pp.45-49
    • /
    • 2009
  • Electrochemical etching of heavily doped p-type silicon wafers (boron doped, <100> orientation, resistivity; $0.8-1.2m{\Omega}/cm$) with different current density resulting two different refractive indices resulted in DBR (Distributed Bragg Reflectors) porous silicon, which exhibited strong in-plane anisotropy of refractive index (birefringence). Dielectric stacks of birefringent porous silicon acting as distributed Bragg reflectors have two distinct reflection bands depending on the polarization of the incident linearly polarized light. This effect is caused by a three-dimensional (in plane and in depth) variation of the refraction index. Optical characteristics of DBR porous silicon were investigated.

  • PDF

Improved Photoluminescence from Light-Emitting Silicon Material by Surface Modification

  • 김동일;이치우
    • Bulletin of the Korean Chemical Society
    • /
    • 제16권11호
    • /
    • pp.1019-1023
    • /
    • 1995
  • A light-emitting silicon material was prepared by electrochemical etching of n-Si single crystal wafers in a solution of hydrofluoric acid and ethanol. Visible photoluminescence from the silicon was inhomogeneous and decayed rapidly in the ambient laboratory conditions or with photoirradiation. Substantial improvements in photoluminescence which include little-dependent luminescence peak energy with excitation energy variation and longer-lasting room temperature visible photoluminescence were achieved when the surface of photoluminescent silicon material was derivatized with the surface modifier of octadecylmercaptan. Surface modification of the photoluminescent silicon was evidenced by the measurements of contact angles of static water drops, FT-IR spectra and XPS data, in addition to changed photoluminescence. Similar improvements in photoluminescence were observed with the light-emitting silicon treated with dodecylmercaptan, but not with octadecane. The present results indicate that sulfurs of octadecylmercaptans or dodecylmercaptans appear to coordinate the surface Si atoms of LESi and perturb the surface states to significantly change the luminescent characteristics of LESi.

Structural and Optical Properties of Porous Silicon Prepared by Electrochemical Etching

  • Lee, Jeong-Seok;Cho, Nam-Hee
    • 한국세라믹학회지
    • /
    • 제39권2호
    • /
    • pp.109-112
    • /
    • 2002
  • The structural and optical features of Porous Silicon(PS) were investigated; the porous silicon was prepared by electrochemical etching of silicon wafers in HF solution. The morphologies and Photoluminescece(PL) features of the PS were investigated in terms of etching time, current density and aging conditions. The average pore diameter and pore depth were determined by current density and etching time, respectively. As-prepared PS exhibited the maximum PL peak at the wavelength of ∼ 450 nm. The degree of deviation from as-prepared PS during aging treatment seemed to depend on the microstructure as well as morphology of the PS. It is found that etching current density played an important role on the microstructural features of the PS.

12" 웨이퍼 Spin etcher용 실시간 박막두께 측정장치의 개발 (Development of Real Time Thickness Measurement System of Thin Film for 12" Wafer Spin Etcher)

  • 김노유;서학석
    • 반도체디스플레이기술학회지
    • /
    • 제2권2호
    • /
    • pp.9-15
    • /
    • 2003
  • This paper proposes a thickness measurement method of silicon-oxide and poly-silicon film deposited on 12" silicon wafer for spin etcher. Halogen lamp is used as a light source for generating a wide-band spectrum, which is guided and focused on the wafer surface through a optical fiber cable. Interference signal from the film is detected by optical sensor to determine the thickness of the film using spectrum analysis and several signal processing techniques including curve-fitting and adaptive filtering. Test wafers with three kinds of priori-known films, polysilicon(300 nm), silicon-oxide(500 nm) and silicon-oxide(600 nm), are measured while the wafer is spinning at 20 Hz and DI water flowing on the wafer surface. From experiment results the algorithm presented in the paper is proved to be effective with accuracy of maximum 0.8% error.rror.

  • PDF

Solid-Phase crystallization of amorphous silicon films deposited by plasma-enhanced chemical vapor deposition

  • Lee, Jung-Keun
    • Journal of Korean Vacuum Science & Technology
    • /
    • 제2권1호
    • /
    • pp.49-54
    • /
    • 1998
  • The effect of deposition paratmeters on the solid-phase crystallization of amorphous silicon films deposited by plasma-enhanced chemical vapor deposition has been investigated by x-ray diffraction. The amorphous silicon films were prepared on Si(100) wafers using SiH4 gas with and without H2 dilution at the substrate temperatures between 12$^{\circ}C$ and 38$0^{\circ}C$. The R. F. powers and the deposition pressures were also varied. After crystallizing at $600^{\circ}C$ for 24h, the films exhibited (111), (220), and (311) x-ray diffraction peaks. The (111) peak intensity increased as the substrate temperature decreased, and the H dilution suppressed the crystallization. Increasing R.F. powers within the limits of etching level and increasing deposition pressures also have enhanced the peak intensity. The peak intensity was closely related to the deposition rate, which may be an indirect indicator of structural disorder in amorphous silicon films. Our results are consistent with the fact that an increase of the structural disorder I amorphous silicon films enhances the grain size in the crystallized films.