Spray Dry한 ${\beta}$-SiC-$TiB_2$ 도전성(導電性) 세라믹 복합체(複合體)의 특성(特性) (Properties of ${\beta}$-SiC-$TiB_2$ Electrocondutive Ceramic Composites by Spray Dry)

  • 신용덕;주진영;최광수;오상수;이동윤;임승혁
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2003년도 하계학술대회 논문집 C
    • /
    • pp.1538-1540
    • /
    • 2003
  • The composites were fabricated respectively 61vol.% ${\beta}$-SiC and 39vol.% $TiB_2$ spray-dried powders with the liquid forming additives of 12wt% $Al_2O_3+Y_2O_3$ by pressureless annealing at $1700^{\circ}C,\;1750^{\circ}C\;1800^{\circ}C$ for 4 hours. The result of phase analysis of composites by XRD revealed ${\alpha}$-SiC(6H), $TiB_2$, and YAG($Al_5Y_3O_{12}$) crystal phase. The relative density, the Young's modulus and fracture toughness showed respectively the highest value of 92.97%, 92.88Gpa and $4.4Mpa{\cdot}m^{1/2}$ for composites by pressureless annealing temperature $1700^{\circ}C$ at room temperature. The electrical resistivity showed the lowest value of $8.09{\times}10^{-3}{\Omega}{\cdot}cm$ for composite by pressureless annealing tempe rature $1700^{\circ}C$ at $25^{\circ}C$. The electrical resistivity of the SiC-$TiB_2$ composites was all positive temperature cofficient resistance (PTCR) in the temperature ranges from $25^{\circ}C$ to $700^{\circ}C$.

  • PDF

$MoSi_2$ 금속간화합물 복합재료의 미세구조와 방전가공특성 (Microstructure and EDM Processing of $MoSi_2$ Intermetallic Composite)

  • 윤한기;이상필;윤경욱;김동현
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2002년도 춘계학술대회 논문집
    • /
    • pp.23-28
    • /
    • 2002
  • This paper describes the machining characteristics of the $MoSi_2$ based composites by electric discharge drilling with various tubular electrodes, besides, Hardness characteristics and microstructures of $Nb/MoSi_2$ laminate composites were evaluated from the variation of fabricating conditions such as preparation temperature, applied pressure and pressure holding time. $MoSi_2$ -based composites has been developed in new materials for jet engine of supersonic-speed airplanes and gas turbine for high- temperature generator. Achieving this objective may require new hard materials with high strength and high temperature-resistance. However, With the exception of grinding, traditional machining methods are not applicable to these new materials. Electric discharge machining (EDM) is a thermal process that utilizes a spark discharge to melt a conductive material, the tool electrode being almost non-unloaded, because there is no direct contact between the tool electrode and the workpiece. By combining a nonconducting ceramics with more conducting ceramic it was possible to raise the electrical conductivity. From experimental results, it was found that the lamination from Nb sheet and $MoSi_2$ powder was an excellent strategy to improve hardness characteristics of monolithic $MoSi_2$. However, interfacial reaction products like (Nb, Mo)$SiO_2$ and $Nb_2Si_3$ formed at the interface of $Nb/MoSi_2$ and increased with fabricating temperature. $MoSi_2$ composites which a hole drilling was not possible by the conventional machining process, enhanced the capacity of ED-drilling by adding $NbSi_2$ relative to that of SiC or $ZrO_2$ reinforcements.

  • PDF

탄소섬유가 혼합된 세라믹 복합재 제동마찰재의 마찰·마모 특성 (Tribological Properties of Ceramic Composite Friction Materials Reinforced by Carbon Fibers)

  • 구병춘;김민수
    • Tribology and Lubricants
    • /
    • 제33권1호
    • /
    • pp.15-22
    • /
    • 2017
  • Because the running speed of vehicles is increasing and a shorter braking distance is required, high heat-resistant brake pads are needed to satisfy the requirements of customers and car makers. In the near future, hazardous materials such as Cu, Cr, Zn, and Sb will be restricted from use in friction materials. Ceramic composites reinforced by carbon fibers are good candidates for eco-friendly friction materials. In this study, we develop ceramic composite friction materials. The friction materials are composed of carbon fibers, Si, SiC, graphite, and phenol resin and are prepared by hot forming and heat treatment at high temperatures. The density, void ratio, and compressive strength are $1.59-1.66g/cm^3$, 16.6-20, and 70-90 MPa, respectively. Friction and wear tests are performed using a pin-on-plate-type reciprocating friction tester at 25, 100, and $200^{\circ}C$. The counterpart material is a CrMoV steel extracted from a KTX brake disc. Friction coefficient, wear amount, and wear mechanism are measured and examined. We determine that the friction coefficients depend on the temperature and the fluctuation of the friction coefficients is larger at higher temperatures. The amount of wear increases with the surface temperatures of the specimens. The tribological properties of the developed composites are similar to those of a Cu-based sintered friction material. Through this study, it is confirmed that ceramic composite materials can be used as friction materials.

폴리카보실란 전구체로부터 고온 산화성분위기서 기계적물성이 우수한 파이롯-규모의 탄화규소섬유 제조공정 개발 (Development of Pilot-Scale Manufacturing Process of SiC Fiber from Polycarbosilane Precursor with Excellent Mechanical Property at Highly Oxidation Condition and High Temperature)

  • 윤병일;최우철;김정일;김재성;강홍구;김명주
    • Composites Research
    • /
    • 제30권2호
    • /
    • pp.116-125
    • /
    • 2017
  • 본 연구의 목적은 고온 산화성 분위기하에서 기계적물성이 우수한 탄화규소섬유(SiC Fiber)를 파일롯-규모로의 생산 제조공정을 개발하는 것이다. 프리세라믹 전구체로서 폴리카보실란(PCS)을 사용하여 탄화규소섬유를 제조하였다. 연속성의 PCS 섬유는 $300{\sim}350^{\circ}C$에서 PCS를 용융한 후에 용융방사로부터 얻었다. 열처리 전에 섬유의 불융화를 위하여 공기 분위기하에서 경화를하였다. 경화 전, 후에 측정한 FT-IR 스펙트라 피크로 부터 경화도를 계산하였다. 탄화규소섬유의 물성은 경화도에 따라 크게 영향을 받았다. 본 개발에서 열처리 중 섬유의 장력 조절로 우수한 물성을 갖는 탄화규소섬유를 얻었다. 탄화규소섬유의 화학조성과 기계적물성은 안정화섬유의 열처리시의 이송속도에 영향을 받았다. 탄화규소섬유를 공기분위기하 $1000^{\circ}C$에서 1분부터 50시간까지 노출한 후에 인장시험을 수행하였다. 그 결과 인장강도는 약 60%까지 감소함을 보여주었다. 장시간 노출시험시 낮은 인장 강도값을 나타내는 섬유는 화학성분 분석시 섬유의 표면에 많은 탄소량을 함유하고 있었다.

비접촉 초음파 탐상 기법을 이용한 항공기 브레이크 디스크의 신뢰성 평가 (Reliability Evaluation of Aircraft Brake Disk using the Non-contact Air-coupled Ultrasonic Transducer Method)

  • 곽남수;김재열;고가진;박대광
    • 한국기계가공학회지
    • /
    • 제15권3호
    • /
    • pp.36-43
    • /
    • 2016
  • Carbon fiber-reinforced silicon carbide (Cf-SiC) and SiC / SiC composites have high thermal conductivity, and excellent corrosion and wear resistance, a low coefficient for thermal expansion and are lightweight. This is why they are commonly used in parts of the aerospace industry to develop an aircraft thrust deflector, jet vane, combustion chamber, elevens, body flap, and a shingle. So, understanding how this state-of-the-art Cf-SiC affects both internal and external crack detection and determining issues during the manufacturing process of composite materials, should be evaluated according to valuation techniques in the external environment. In this paper, we apply a non-contact air ultrasonic technique of non-destructive testing techniques to perform a study on internal defect detection identification and assessment of carbon-fiber reinforced silicon carbide composites to perform basic research and applied research.

Al2O3와 SiC 강화재가 첨가된 Al-Cu 기지 복합재료의 소결, 재압축 및 기계적 특성에 관한 연구 (Study on the Sintering, Repressing and Mechanical Properties of Al2O3 and Al-Cu-SiC Composites)

  • 박정수;이성규;안재환;정형식
    • 한국분말재료학회지
    • /
    • 제11권2호
    • /
    • pp.171-178
    • /
    • 2004
  • Effects of liquid phase and reinforcing particle morphology on the sintering of Al-6 wt%Cu-10 vol% $Al_2O_3$ or SiC particles were studied in regards to densification, structure and transverse rupture properties. The Al-Cu liquid phase penetrated the boundaries between the aluminum matrix powders and the interfaces with reinforcing particles as well, indicating a good wettability to the powders. This enhanced the densification during sintering and the resulting strength and ductility. Since most of the copper added, however, was dissolved in the liquid phase and formed a brittle $CuAl_2$ phase upon cooling rather than alloyed with the aluminum matrix, the strengthening effect by the copper was not fully realized. Reinforcing particles of agglomerate type were found less suitable for the liquid phase sintering than solid type particles. $Al_2O_3$ and SiC particles protluced little difference on the sintering behavior but their size had a large effect. Repressing of the sintered composites increased density and bending properties but caused debonding at the matrix-particle interfaces and also fracturing of the particles.

Modeling the Density and Hardness of AA2024-SiC Nanocomposites

  • Jeon, A-Hyun;Kim, Hong In;Sung, Hyokyung;Reddy, N.S.
    • 한국분말재료학회지
    • /
    • 제26권4호
    • /
    • pp.275-281
    • /
    • 2019
  • An artificial neural network (ANN) model is developed for the analysis and simulation of correlation between flake powder metallurgy parameters and properties of AA2024-SiC nanocomposites. The input parameters of the model are AA 2024 matrix size, ball milling time, and weight percentage of SiC nanoparticles and the output parameters are density and hardness. The model can predict the density and hardness of the unseen test data with a correlation of 0.986 beyond the experimental data. A user interface is designed to predict properties at new instances. We have used the model to simulate the individual as well as the combined influence of parameters on the properties. Moreover, we have analyzed the calculated results from the powder metallurgical point of view. The developed model can be used as a guide for further composite development.

$MoSi_2$/W 복합재료의 합성과 성질에 관한 연구 (Synthesis and Properties of In-situ $MoSi_2$/W Composites)

  • 장대규
    • 한국재료학회지
    • /
    • 제8권10호
    • /
    • pp.938-944
    • /
    • 1998
  • $MoSi_2$에 W분말을 첨가하여 $MoSi_2$/W 복합재료를 $1600^{\circ}C$에서 3시간 동안 유지하면서 30MPa의 조건하에서 고온진공 가압기를 이용하여 제조하였으며, 텅스텐 분말의 첨가량이 $(Mo)Si_2$의 미세조직과 기계적 성질에 미치는 영향을 조사하였다. 텅스텐은 몰리브덴과 치환하면서 고용체 합금을 이루었으며, 입자의 크기는 텅스텐 분말의 첨가량이 증가할수록 감소하였다. 비커스경도는 텅스텐 분말의 첨가량이 증가할수록 향상되었으나, 반면에 압흔파단 강도는 오히려 감소되었다. 10%정도의 텅스텐 분말을 첨가하였을 때, 압흔파단 강도가 $4.5MPa$\sqrt{m}$로서 순수 $MoSi_2$$2.7MPa\sqrt{m}$에 비하여 향상되었음을 알 수 있었다.

  • PDF

와이블 통계 해석에 의한 ZrO2 복합 세라믹스의 기계적 특성 (Determining Mechanical Properties of ZrO2 Composite Ceramics by Weibull Statistical Analysis)

  • 김선진;김대식;남기우
    • 대한기계학회논문집A
    • /
    • 제39권10호
    • /
    • pp.955-962
    • /
    • 2015
  • 비커스 경도 시험은 모든 재료에 적용할 수 있으며, 경도 시험 중에서 가장 광범위하게 사용된다. 경도는 기계적 성질을 평가하는 하나의 확률변수로 볼 수 있다. 본 연구는 $ZrO_2$ 단상 세라믹스와 $TiO_2$ 첨가량에 따르는 $ZrO_2/SiC$ 복합 세라믹스의 굽힘강도와 비커스 경도의 통계적 성질을 조사하였다. 굽힘강도와 비커스 경도는 와이블 확률 분포를 잘 따랐다. 척도 및 형상 파라메터는 $ZrO_2$ 모재 세라믹스, $ZrO_2/SiC/TiO_2$ 모재 세라믹스 및 이들을 열처리한 세라믹스를 사용하여 평가하였다. 또한 압입하중의 증가에 따른 영향도 평가하였다.

반용융 성형가공한 SiCp/AZ91HP Mg복합재료의 피로 및 내마모 특성 (Fatigue and Wear Properties of Semi-Liquid Formed SiCp/AZ91HP Mg Composites)

  • 하홍수;김명균;안선규;임병수;김영직
    • 한국주조공학회지
    • /
    • 제17권5호
    • /
    • pp.472-479
    • /
    • 1997
  • The effect of size and mass fraction of SiC particulate on the fatigue and wear have been investigated for semi-liquid formed SiCp/AZ91HP Mg composites. In the study, different particulate sizes of 7, 20, $50 {\mu}m$ were prepared with various mass fraction for sample preparation. By tension-tension fatigue tests, whose procedures are standardized in ASTM standard 647E-93, the da/dN vs. ${\Delta}K$ curves were obtained. Also, the crack propagation paths were observed by optical microscope. As a result of wear test, specific wear loss is decreased with increasing mass fraction and particulate size. Specific wear loss of 30 mass% $50 {\mu}m$ SiC reinforced Mg composite is compared to SKD11.

  • PDF