Journal of the Korean Recycled Construction Resources Institute
/
v.7
no.3
/
pp.194-201
/
2019
This study analyzed the properties of concrete depending on the coal gasification slag(CGS) contents in order to examine the applicability of CGS as the fine aggregate for concrete. Experimental results, trended that the slump and slump flow increased with increasing CGS contents, and air contents has decreased. Evaluation index for segregation of normal strength concrete(EISN) is showed was good from CGS 25% when using crushed sand A(CSa) and CGS 50% when using mixed sand(MS). The compressive strength decreased with increasing CGS contents when CSa was used. However, when MS was used, the maximum value was CGS 50% due to parabolic tendency. Depending on fine aggregates type, compared with compressive strength of CSa was about 8% higher than that of MS, and depending on the use or unuse of CGS, more advantageous at higher strength than low strength. As a result of relative performance study on the quality of concrete according to the CGS contents, it is considered that CGS can be positively contributed to enhancement of workability and strength development when mixed with fine aggregate around 25~50%.
Journal of the Korean Recycled Construction Resources Institute
/
v.5
no.3
/
pp.253-260
/
2017
The aim of research is to investigate various physical properties of ultra high strength concrete of 80MPa class using a combination of limestone aggregate and electronic arc furnace oxidizing slag aggregate. For aggregate combinations, granite and limestone are used for coarse aggregate, granite and limestone are also used for fine aggregate. And also, limestone fine aggregate is replaced by electronic arc furnace oxidizing slag aggregate of 25% and 50%. Test results indicated that flowability and compressive strength increased when limestone fine aggregate was used compared to that using granite fine aggregate due to higher modulus of elasticity by limestone. Also substitution of electronic arc furnace oxidizing slag aggregate resulted in a decrease of compressive strength slightly. It is found that the use of electronic arc furnace oxidizing slag aggregate and limestone aggregate would be favorable for reducing the autogenous shrinkage by as much as 9~25%.
Journal of the Korean Recycled Construction Resources Institute
/
v.8
no.4
/
pp.596-603
/
2020
In this paper, an experimental study was conducted to investigate the applications of bottom ash, which is an industrial by-product obtained from thermal power plants. Bottom ash was used as fine aggregate in this study, and an experiment was conducted to determine the characteristics of the bottom ash aggregate. In addition, 25, 50, 75, and 100% contents of crushed (natural) fine aggregate were replaced with bottom ash aggregate to produce concrete mixture including bottom ash. Thereafter, test results of the unit weight, ultrasonic velocity, compressive strength, and thermal conductivity of bottom ash concrete were obtained. Moreover, the effect of the curing ages of 28 and 91 days on the material characteristics of bottom ash concrete were identified. Test results showed that bottom ash used as fine aggregate had pozzolanic reaction. Finally, based on the extensive experimental results, relationships between thermal conductivity and unit weight, ultrasonic velocity, and compressive strength was suggested.
Ji, Sang-Kyu;Yun, Hyun-Do;Kim, Sun-Woo;Lee, Eon-Young
Journal of the Korea Concrete Institute
/
v.20
no.1
/
pp.43-50
/
2008
This paper presents experimental and analytical results on the long-term behavior of the reinforced recycled aggregate concrete beams under sustained loading. In this experimental program, three beams with different conditions of aggregates replacement (natural aggregate 100%, recycled coarse aggregate 100%, recycled fine aggregate 50%) were subjected to the sustained flexural loading that was a half of the nominal flexural capacity over a period of 1 year. The beam were designed with net span of 2,000 mm and rectangular cross-section of 170 mm width and 170 mm effective depth. The beams were instrumented and monitored to observe the change in the long-term behavior due to creep and shrinkage of concrete under sustained loading. The predictions of long-term deflection by ACI code, Branson, Mayer, Neville, EMM and AEMM were compared with the experimental results. From the experimental results, the reinforced concrete beams with recycled aggregates showed the same performance as that of a beam with natural aggregate. The proposed method to predict the long-term deflections of reinforced recycled aggregate concrete beams gives a good estimation for experimental results.
The amount of the waste foundry sand(WFS) produced in Korea is over 700,000 ton per year, but most WFS buries itself and only 5~6% or total WFS is recycled in the way or mixing as fine aggregate for construction materials. A bY-product, WFS produced from a foundry may affect our environmental contamination if it is discharged without proper waste disposal in Korea. Therefore in this study, we performed the fundamental research about specific gravity, absorption, grading curve, finesse modulus of WFS, different aggregates and the flow and the compressive strength of mortar with WFS replaced as fine aggregate, the workability and compressive strength of concrete with WFS as fine aggregate aimed at the specified strength of 270 kgf/$\textrm{cm}^2$, and then optimum mix proportion of concrete was determined
Journal of the Korean Recycled Construction Resources Institute
/
v.1
no.2
/
pp.107-113
/
2013
This study is the study desiring to solve the problem by utilizing the kinds of recycled resources considered to be troubled complementarily. Namely the reaction of potential hydraulicity of Blast Furnace Slag Powder (BS) shall be reacted with the alkali of Recycled Fine Aggregates Coarse Aggregate, it has been experimented to obtain the optimum value with the replacement ratio of incineration plant ash (WA) treated with the slaked lime as the experiment variable by solving the alkali of shortage with the Ordinary Portland Cement (OPC). As a result, the liquidity and the air volume are declined slightly as the replacement ratio of incineration plant ash WA increases, the mixture of incineration plant ash WA 1% has been analyzed to be the most suitable considering the viewpoint of effective handling of waste as the compression and the tensile strength showed the maximum value before and after 1% even though it was disadvantageous with the increase of chloride content.
Kim, Ho-Kyu;Kim, Young-Ahn;Choi, Seung-Yong;Cho, Young-Keun
Journal of the Korean Recycled Construction Resources Institute
/
v.6
no.3
/
pp.167-173
/
2018
In general, calcium is required for the reaction of blast furnace slag fine powder and fly ash. The by-products generated during the process of producing recycled aggregates have different calcium contents depending on the crushing stage and the possibility of using the process by-product as a concrete mixture is also different. In this study, the effect of the calcium content of the by-products on the compressive strength was investigated and the block was fabricated by using this. To utilize the by-products as an admixture, the calcium content was analyzed and the bending strength and surface temperature were measured according to the shape of the water storage block. As a result of this study, the possibility of making a block using recycled aggregate by-products was verified and arch type block was constructed to secure storage capacity and bending strength. Also, the surface temperature of the water storage block was reduced by $9^{\circ}C$ or more than that of the general permeable block.
Journal of the Korean Recycled Construction Resources Institute
/
v.8
no.4
/
pp.562-570
/
2020
This study explores manufacturing technology and basic properties of high strength cement composites at 2,000kg/㎥ of specific weight. It is suggested that lightweight-high strength cement composites can be produced by substituting silica sand in ulta-high performance concrete mixture with lightweight materials such as solid bubbles and lightweight fine aggregates. The 28-day compressive strengths of cement composites with solid bubbles were from 116MPa to 141MPa at below 2.0g/㎤ of unit density while the cement composites with lightweight aggregates possessed lower compressive strength and higher unit density. The specific weight calculated from mixture proportions did not have significant difference with unit density of hardened cement composites, indicating that unit density of hardened cement composites can be estimated from the specific weight in mixture proportions.
Journal of the Korean Recycled Construction Resources Institute
/
v.12
no.3
/
pp.246-253
/
2024
When concrete with slag powder or fly ash is under an accelerated carbonation test at early age, a very complicated carbonation behavior occurs since several reactions covering cement hydration, pozzolanic reaction, and carbonation reaction occu simultaneously. In particular, fine and coarse aggregates with poor quality were used, the trend with strength development and carbonation behavior was not clear. In this study, concrete samples with three design strength grade(24 MPa, 27 MPa, and 30 MPa) were manufactured with different aggregates site(A, B, and C). Compressive strength test were performed considering curing ages(7 and 28 days), and the accelerated carbonation tests were performed for 8 weeks for evaluating carbonation rate. The relationship between compressive strength and carbonation rate was analyzed considering mix properties and the aggregate site conditions. In addition, the minimum cover depth satisfying intended service life was obtained through carbonation design based on Domestic Design Code, and the necessities for improving design parameters (direction coefficient and effective water-binder ratio) were suggested.
Journal of the Korean Recycled Construction Resources Institute
/
v.2
no.4
/
pp.321-327
/
2014
Structural light weight aggregate concrete are made with both coarse and fine light weight aggregates, but it is common with the high strength concrete to replace all or part with normal weight sand be called class 1 structural light weight aggregate concrete. Fire resistance of structural light weight aggregate concrete are determined by properties of high water content ratio and explosive spalling. Especially, structural light weight aggregate concrete is occurred serious fire performance deterioration by explosive spalling stem from thermal stress and water vapor pressure. This study is concerned with experimentally investigating fire resistance of class 1 structural light weight concrete. From the test result, class 1 structural light weight concrete is happened explosive spalling. The decrease of cross section caused by explosive spalling made sharp increasing gradient of inner temperature.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.