Leakage Current of Capacitive BST Thin Films (BST 축전박막의 누설전류 평가)

  • 인태경;안건호;백성기
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.8
    • /
    • pp.803-810
    • /
    • 1997
  • Ba0.5Sr0.5TiO3 thin films were deposited by RF magnetron sputliring method in order to clarify the anneal condition and doping effect on loakage current Nb and Al were selected as electron donor and acceptor dopants respectively, in the BST films because they have been known to have nearly same ionic radii as Ti and thought to substitute Ti sites to influence the charge carrier and the acceptor state adjacent to the gram boundary. BST thin films prepared in-situ at elevated temperature showed selatively high leakage current density and low breakdown voltage. In order to achieve smooth surface and to improve electrical properties, BST thin films were deposited at room temperature and annealed at elevated temperature. Post-annealed BST thin films showed smoother surface morphology and lower leakage current density than in-situ prepared thin films. The leakage current density of Al doped thin films was measured to be around 10-8A/cm2, which is much lower than those of undoped and Nb doped BST films. The result clearly demonstrates that higher Schottky barrier and lower mobile charge carrier concentration achieved by annealing in the oxygen atmosphere and by Al doping are desirable for reducing leakage current density in BST thin films.

  • PDF

Electrical Properties of $V_{1.9}W_{0.1}O_5$ Thin Films for the uncooled Infrared Detector (비냉각 적외선 감지소자 응용을 위한 $V_{1.9}W_{0.1}O_5$ 박막의 전기적 특성)

  • Nam, Sung-Pill;Lee, Sung-Gap;Bea, Seon-Gi;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 2008.07a
    • /
    • pp.1248-1249
    • /
    • 2008
  • The $V_{1.8}W_{0.2}O_5$ thin films deposited on $Pt/Ti/SiO_2/Si$ substrates by RF sputtering method exhibited fairly good TCR and dielectric properties. It was found that film crystallinity, dielectric properties, and TCR properties were strongly dependent upon the annealing temperature. The dielectric constants of the $V_{1.8}W_{0.2}O_5$ thin films annealed at 400$^{\circ}C$ were 38.11, with a dielectric loss of 0.134, respectively. Also, the TCR values of the $V_{1.8}W_{0.2}O_5$ thin films annealed at 400$^{\circ}C$ were about -3.15%/K.

  • PDF

Chemical Solution Deposition 방법으로 증착된 $Bi_{0.8}A_{0.2}FeO_3$ (A=Pb, Co) 박막의 자기적 특성에 대한 연구

  • Cha, Jeong-Ok;An, Jeong-Seon
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2011.08a
    • /
    • pp.245-245
    • /
    • 2011
  • $BiFeO_3$ (BFO)박막에 전위금속 Pb와 Co를 각각 치환환 박막을 chemical solution deposition 방법으로 Pt/Ti/SiO2/Si(100) 기판위에 증착하였다. Bi 자리에 Pb와 Co를 20 at.% 치환하였으며, 치환된 $Bi_{0.8}Pb_{0.2}FeO_3$ (BPFO), $Bi_{0.8}Co_{0.2}FeO_3$ (BCFO) 박막의 구조적, 자기적 특성 변화를 BFO 박막과 비교하여 조사하였다. XRD 패턴을 분석한 결과 BPFO, BCFO 박막들은 모두 rhombohedrally distorted perovskite 구조였으며 불순물인 pyrochlore 상이 약하게 관측되었다. 치환이 이루어진 BPFO, BCFO 박막들의 자기 이력곡선은 안정된 포화곡선을 나타냈으며 BFO의 포화값(5 emu/$cm^3$)에 비해 크게 증가된 55 emu/$cm^3$, 35 emu/$cm^3$의 값을 나타냈다. 또한 보자력장(coercive field, Hc)값도 BFO의 500 Oe보다 크게 증가된 1,200 Oe, 800 Oe의 값을 보였다.

  • PDF

Microstructure and Electrical Properties of Pb[(Mg,Mn)Nb]O3-Pb(Zr,Ti)O3 Piezoelectric Ceramics

  • Kim, Jin-Ho;Kim, Jong-Hwa;Baik, Seung-Woo
    • Transactions on Electrical and Electronic Materials
    • /
    • v.6 no.5
    • /
    • pp.202-209
    • /
    • 2005
  • Phase evolution, microstructure and the electrical properties such as $k_p$ and $Q_m$ of $Pb(Mg_{1/3}Nb_{2/3})O_3[PMN]-Pb(Mn_{1/3}Nb_{2/3})O3[PM'N]-PbZrO_3[PZ]-PbTiO_3[PT]$ quaternary system were investigated within the compositional ranges $0{\leq}y{\leq}0.125$, y+z=0.125, and $0.39{\leq}x{\leq}0.54$ of the formula $Pb_{0.97}Sr_{0.03}[Mg_{1/3}Nb_{2/3})_y\;(Mn_{1/3}Nb_{2/3})_z\;(Zr_{x}Ti_{1-x})_{1-(y+z)}]O_3$. In the case of increasing Mn/(Mg+Mn) ratio for a fixed Zr/Ti ratio of 47.5/52.5, phase relation remained unchanged but the grain size drastically decreased, and the electrical properties changed as following: both $k_P$ and $Q_m$ reached the peak values at $Mn/(Mg+Mn)\cong0.3l7$ and gradually decreased; $\varepsilon33^T$ showed a monotonic decrease; P-E hysteresis loop gradually changed to asymmetrical one, and $E_i$ increased in correspondence. With increasing Zr/Ti ratio for a fixed Mn/(Mg+Mn) ratio of 0.317, on the contrary, the cell parameter $(\alpha^2c)^{1/3}$ gradually increased, and tetragonal-rhombohedral morphotropic phase boundary appeared in the range of $51/49{\leq}Zr/Ti{\leq}54/46$. the meantime, the grain size substantially increased, and the electrical properties changed as following: $k_P$ and $\varepsilon33^T$ reached peak values at Zr/Ti=51/49 and 48/52, respectively, and then gradually decreased; change of $Q_m$ was adverse to $k_P$; both $E_C\;and\;E_i$ considerably decreased while $P_S$ moderately increased. For the system 0.125(PMN+PM'N)-0.875PZT studied, the composition Mn/(Mg+Mn)=0.3l7 and Zr/Ti=51/49 revealed some promising electrical properties for piezoelectric transformer application such as $k_P=0.58,\;Q_m\cong1000$, and $\varepsilon^T_{33}=970$, as well as dense and fine-grained microstructure.

Fabrication of 3-Dimensional LiMn2O4 Thin Film

  • Park, Bo-Gun;Ryu, Jea Hyeok;Choi, Won Youl;Park, Yong-Joon
    • Bulletin of the Korean Chemical Society
    • /
    • v.30 no.3
    • /
    • pp.653-656
    • /
    • 2009
  • 3-Dimensionally ordered macroporous $LiMn_2O_4$ thin film was prepared by a sol-gel and dip coating method on Pt/Ti/$SiO_2$/Si substrate. An opal structure consisting of mono dispersed polystyrene beads (300 nm) was used as a template. After solution containing Mn and Li precursors was coated on the template-deposited substrate, the template and organic materials in the precursors was removed by calcination at 400 ${^{\circ}C}$. And then the 3-dimensional $LiMn_2O_4$ thin film with spinel structure was fabricated by heat treatment at 700 ${^{\circ}C}$. The structural and electrochemical property was investigated by XRD, SEM and charge-discharge cycler.

Smart Solid State Syntheses of Well-Crystallized Phase Pure Mixed Oxides for Electroceramics

  • Sennat, Mamoru
    • Journal of the Korean Ceramic Society
    • /
    • v.43 no.11 s.294
    • /
    • pp.680-687
    • /
    • 2006
  • An overview is given to optimize the solid state processes toward phase pure and well-crystallized fine particulates of mixed oxides, serving as electroceramic materials in various genres. Elevation of the reactivity and preservation of stoichiometry of the starting mixture are of universal importance. Mechanical activation is versatile for these purposes, particularly when an oxygen atom as a hinge promotes formation of hetero-bridging bonds between dissimilar cationic species prior to calcination. Case studies carried out recently in the author's laboratory are displayed and compared for ferroelectric materials, i.e. $PbMg_{1/3}Nb_{2/3}O_3$ $xPbTiO_3$(PMN-PT), $(1-y)Pb(Zn_xMg{1-x})_{1/3}$ $yNb_{2/3}O_3$ (PZN-PMN), $BaBi_2Ta_2O_9$ (BBT), $Ba(Mg_{1/3}Ta_{2/3})O_3$ (BMT), and ferromagnetics, i.e. M-, Y-, and Z-phases of Ba-hexaferrites.

Effect of Seed-layer on the Crystallization and Electric Properties of SBN60 Thin Films (SBN60 박막의 결정화 및 전기적 특성에 관한 씨앗층의 영향)

  • Jang, Jae-Hoon;Lee, Dong-Gun;Lee, Hee-Young;Jo, Sang-Hee
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.07b
    • /
    • pp.723-727
    • /
    • 2003
  • [ $Sr_xBa_{1-x}Nb_2O_6$ ] (SBN, $0.25{\leq}x{\leq}0.75$) ceramic is a ferroelectric material with tetragonal tungsten bronze (TTB) type structure, which has a high pyroelectric coefficient and a nonlinear electro-optic coefficient value. In spite of its advantages, SBN has not been investigated well compared to other ferroelectric materials with perovskite structure. In this study, SBN thin film was manufactured by ion beam sputtering technique using the prepared SBN target in $Ar/O_2$ atmosphere. SBN30 thin film of $1000{\AA}$ was pre-deposited as a seed layer on $Pt(100)/TiO_2/SiO_2/Si$ substrate followed by SBN60 deposition up to $3000{\AA}$ in thickness. As-deposited SBN60/SBN30 layer was heat-treated at different temperatures of 650, 700, 750, and $800^{\circ}C$ in air, respectively The crystallinity and orientation behavior as well as electric properties of SBN60/SBN30 multi-layer were examined. The deposited layer was uniform and the orientation was shown primarily along (001) plane from XRD pattern. There was no difference in the crystal structure with heat-treatment temperature, but the electric properties depended on the heating temperature and was the best at $750^{\circ}C$. In electric properties of Pt/SBN60/SBN30/Pt thin film capacitor prepared, the remnant polarization (2Pr) value was $15{\mu}C/cm^2$, the coercive field (Ec) 75 kV/cm, and the dielectric constant 1075, respectively.

  • PDF

Effect of Seed-layer thickness on the Crystallization and Electric Properties of SBN Thin Films. (SBN 박막의 결정화 및 전기적 특성에 관한 씨앗층 두께의 영향)

  • Jang, Jae-Hoon;Lee, Dong-Gun;Lee, Hee-Young;Cho, Sang-Hee
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2003.11a
    • /
    • pp.271-274
    • /
    • 2003
  • [ $Sr_xBa_{1-x}Nb_2O_6$ ] (SBN, $0.25{\leq}x{\leq}0.75$) ceramic is a ferroelectric material with tetragonal tungsten bronze (TTB) type structure, which has a high pyroelectric coefficient and a nonlinear electro-optic coefficient value. In spite of its advantages, SBN has not been investigated well compared to other ferroelectric materials with perovskite structure. In this study, SBN thin film was manufactured by ion beam sputtering technique using the prepared SBN target in $Ar/O_2$ atmosphere. SBN30 thin films of different thickness were pre-deposited as a seed layer on $Pt(100)/TiO_2/SiO_2/Si$ substrate followed by SBN60 deposition up to $4500\;{\AA}$ in thickness. As-deposited SBN60/SBN30 layer was heat-treated at different temperatures of 650, 700, 750, and $800\;^{\circ}C$ in air, respectively, The crystallinity and orientation behavior as well as electric properties of SBN60/SBN30 multi-layer were examined. The deposited layer was uniform and the orientation was shown primarily along (001) plane from XRD pattern. There was difference in the crystal structure with heat-treatment temperature, and the electric properties depended on the heating temperature and the seed-layer thickness. In electric properties of Pt/SBN60/SBN30/Pt thin film capacitor prepared, the remnant polarization (2Pr) value was $15\;{\mu}C/cm^2$, the coercive field (Ec) 65 kV/cm, and the dielectric constant 1492, respectively.

  • PDF

A Study on the Switching and Retention Characteristics of PLT(5) Thin Films (PLT(5) 박막의 Switching 및 Retention 특성에 관한 연구)

  • Choi Joon Young;Chang Dong Hoon;Kang Seong Jun;Yoon Yung Sup
    • Journal of the Institute of Electronics Engineers of Korea SD
    • /
    • v.42 no.1
    • /
    • pp.1-8
    • /
    • 2005
  • We fabricate PLT(5) thin film on Pt/TiO/sub x/SiO₂/Si substrate by using sol-gel method and investigate leakage current, switching and retention properties. The leakage current density of PLT(5) thin film is 3.56×10/sup -7/A/㎠ at 4V. In the examination of switching properties, pulse voltage and load resistance were 2V~5V and 50Ω~3.3kΩ, respectively. Switching time has a tendency to decrease from 0.52㎲ to 0.14㎲ with the increase of pulse voltage, and also the time increases from 0.14㎲ to 13.7㎲ with the increase of load resistance. The activation energy obtained from the relation of applied pulse voltage and switching time is about 135kV/cm. The error of switched charge density between hysteresis loop and experiment of polarization switching is about 10%. Also, polarization in retention decreases as much as about 8% after l0/sup 5/s.

Electrical properties of $V_{2-x}W_xO_5$ thin film doped Tungsten contents (텅스텐을 첨가한 $V_{2-x}W_xO_5$ 박막의 전기적 특성)

  • Nam, Sung-Pill;Noh, Hyun-Ji;Lee, Sung-Gap;Bea, Seon-Gi;Lee, Young-Hie
    • Proceedings of the KIEE Conference
    • /
    • 2009.07a
    • /
    • pp.1322_1323
    • /
    • 2009
  • The $V_{1.85}W_{0.15}O_5$ thin films deposited on Pt/Ti/$SiO_2$/Si substrates by RF sputtering method exhibited fairly good TCR and dielectric properties. It was found that film crystallinity, dielectric properties, and TCR properties were strongly dependent upon the annealing temperature. The dielectric constants of the $V_{1.85}W_{0.15}O_5$ thin films annealed at $400^{\circ}C$ were 38.11, with a dielectric loss of 1%, respectively. Also, the TCR values of the $V_{1.85}W_{0.15}O_5$ thin films annealed at $400^{\circ}C$ were about -3.45%/K.