• Title/Summary/Keyword: Pre-film

Search Result 388, Processing Time 0.031 seconds

Influence of the nitrogen gas addition in the Ar shielding gas on the erosion-corrosion of tube-to-tube sheet welds of hyper duplex stainless steel (질소 보호 가스 첨가가 하이퍼 듀플렉스 스테인리스 밀봉용접재의 마모부식 저항성에 미치는 영향)

  • Kim, Hye-Jin;Jeon, Soon-Hyeok;Kim, Soon-Tae;Lee, In-Sung;Park, Yong-Soo
    • Corrosion Science and Technology
    • /
    • v.13 no.2
    • /
    • pp.70-80
    • /
    • 2014
  • Duplex stainless steels with nearly equal fraction of the ferrite(${\alpha}$) phase and austenite(${\gamma}$) phase have been increasingly used for various applications such as power plants, desalination facilities due to their high resistance to corrosion, good weldability, and excellent mechanical properties. Hyper duplex stainless steel (HDSS) is defined as the future duplex stainless steel with a pitting resistance equivalent (PRE=wt.%Cr+3.3(wt.%Mo+0.5wt.%W)+30wt.%N) of above 50. However, when HDSS is welded with gas tungsten arc (GTA), incorporation of nitrogen in the Ar shielding gas are very important because the volume fraction of ${\alpha}$-phase and ${\gamma}$-phase is changed and harmful secondary phases can be formed in the welded zone. In other words, the balance of corrosion resistance between two phases and reduction of $Cr_2N$ are the key points of this study. The primary results of this study are as follows. The addition of $N_2$ to the Ar shielding gas provides phase balance under weld-cooling conditions and increases the transformation temperature of the ${\alpha}$-phase to ${\gamma}$-phase, increasing the fraction of ${\gamma}$-phase as well as decreasing the precipitation of $Cr_2N$. In the anodic polarization test, the addition of nitrogen gas in the Ar shielding gas improved values of the electrochemical parameters, compared to the Pure Ar. Also, in the erosion-corrosion test, the HDSS welded with shielding gas containing $N_2$ decreased the weight loss, compared to HDSS welded with the Ar pure gas. This result showed the resistance of erosion-corrosion was increased due to increasing the fraction of ${\gamma}$-phase and the stability of passive film according to the addition $N_2$ gas to the Ar shielding gas. As a result, the addition of nitrogen gas to the shielding gas improved the resistance of erosion-corrosion.

Low-Power Discrete-Event SoC for 3DTV Active Shutter Glasses (3DTV 엑티브 셔터 안경을 위한 저전력 이산-사건 SoC)

  • Park, Dae-Jin;Kwak, Sung-Ho;Kim, Chang-Min;Kim, Tag-Gon
    • Journal of the Institute of Electronics Engineers of Korea SP
    • /
    • v.48 no.6
    • /
    • pp.18-26
    • /
    • 2011
  • Debates concerning the competitive edge of leading 3DTV technology of the shutter glasses (SG) 3D and the film-type patterned retarder (FPR) are flaring up. Although SG technology enables Full-HD 3D vision, it requires complex systems including the sync transmitter (emitter), the sync processor chip, and the LCD lens in the active shutter glasses. In addition, the transferred sync-signal is easily affected by the external noise and a 3DTV viewer may feel flicker-effect caused by cross-talk of the left and right image. The operating current of the sync processor in the 3DTV active shutter glasses is gradually increasing to compensate the sync reconstruction error. The proposed chip is a low-power hardware sync processor based discrete-event SoC(system on a chip) designed specifically for the 3DTV active shutter glasses. This processor implements the newly designed power-saving techniques targeted for low-power operation in a noisy environment between 3DTV and the active shutter glasses. This design includes a hardware pre-processor based on a universal edge tracer and provides a perfect sync reconstruction based on a floating-point timer to advance the prior commercial 3DTV shutter glasses in terms of their power consumption. These two techniques enable an accurate sync reconstruction in the slow clock frequency of the synchronization timer and reduce the power consumption to less than about a maximum of 20% compared with other major commercial processors. This article describes the system's architecture and the details of the proposed techniques, also identifying the key concepts and functions.

투명 면상 발열체 응용을 위한 하이브리드 스퍼터 ITO / Ag / ITO 박막의 물성평가

  • Kim, Jae-Yeon;Park, So-Yun;Song, Pung-Geun
    • Proceedings of the Korean Vacuum Society Conference
    • /
    • 2016.02a
    • /
    • pp.252-252
    • /
    • 2016
  • 최근 학계나 산업계에서 indium tin oxide (ITO)의 높은 전기 전도도 및 광투과율을 이용하여 줄 발열을 기초로 하는 투명 면상 발열체에 대한 연구가 활발히 진행 되고 있다. 하지만 단일 ITO 박막으로 제작한 투명 면상 발열체는 온도가 상승함에 따라 균일하게 발열 되지 않으며, 글라스의 곡면 부분에서 유연성이 부족하여 크랙이 발생하는 다양한 문제점들을 가지고 있다. 이를 해결하기 위해 ITO의 결정화 온도 $160^{\circ}C$ 이상의 고온공정 또는 증착 후 열처리가 필요 하는 추가적인 공정이 필요하다. 따라서 본 연구에서는 단일 ITO 박막의 단점을 개선하는 ITO/Ag/ITO 하이브리드 구조의 투명 면상 발열체를 제작하여 전기적, 광학적 특성을 비교하고 발열량, 온도 균일성, 발열 유지 안정도를 조사하였다. 본 연구에서는 $50{\times}50mm$ 크기의 non-alkali glass (Corning E-2000) 기판 상에 마그네트론 스퍼터링 공정으로 상온에서 ITO/Ag/ITO 박막을 연속적으로 증착 하여 다층구조의 하이브리드 형 투명 면상 발열체를 제조하였다. 박막 증착 파워는 DC (Ag) power 100 W, RF (ITO) power 200 W로 하였으며 ITO박막두께는 40 nm로 고정 시키고 Ag박막 두께는 10 ~ 20 nm로 변화를 주었다. 증착원은 3인치 ITO 단일 타깃(SnO2, 10 wt.%)과 Ag 금속 타깃 (순도 99.99%)을 사용하였으며, 고순도 Ar을 이용하여 방전하였으며 총 주입량은 20 sccm, working pressure는 1.0 Pa을 유지하였다. 증착전 타깃 표면의 불순물 제거와 방전의 안정성을 유지하기 위해 10분간 pre-sputtering을 진행하고 증착하였다. 증착한 박막의 전기적, 광학적 특성은 각각 Hall-effect measurements system (ECOPIA, HMS3000), UV-Vis spectrophotometer (UV-1800, SHIMADZU)으로 측정하였으며, 하이브리드 표면의 구조 및 형상은 field emission-scanning electron microscopy (FE-SEM, Hitachi S-4800)으로 관찰하였다. 또한 투명 면상 발열체의 성능은 0.5 ~ 3 V/cm의 다양한 전압을 power supply (Keithly 2400, USA)를 통해서 시편 양 끝단에 인가한 후 시간에 따른 투명면상 발열체의 표면 온도변화를 infrared thermal imager (IR camera, Nikon)를 이용하여 관찰하였다. 하이브리드 구조를 가진 ITO박막의 두께는 40 nm로 고정 시키고 Ag박막의 두께는 10, 15, 20 nm로 변화를 주었다. 이들 박막의 면저항 값은 각각 5.3, 3.2, $2.1{\Omega}/{\Box}$였으며, 투과도는 각각 86.9, 81.7, 66.5 %였다. 이에 비해 두께 95 nm의 단일 ITO박막의 면저항 값은 $59.5{\Omega}/{\Box}$였으며, 투과도는 89.1 %였다. 하이브리드 구조의 전기적특성은 금속층의 두께가 증가할수록 캐리어 농도 값이 증가함에 따라 비저항 값이 감소되어 면저항 값도 감소된 것이며, 금속 삽입층의 전도특성이 비저항에 큰 영향을 주고 있음을 보여준다. 하지만 금속 층의 두께가 증가할수록 Ag층이 연속적인 막을 형성하여 반사율이 증가함에 따라 투과도가 감소하였다. 따라서 하이브리드 구조를 가진 투명 면상 발열체에 금속 삽입층의 두께 조절은 매우 중요한 인자임을 확인 할 수 있었다. 또한 발열성능을 평가 하기 위해 시편 양 끝단에 3 V전압을 인가한 결과, 금속 삽입층의 두께가 10 nm에서 5 nm씩 증가한 하이브리드 구조를 가진 투명면상 발열체의 최고 온도는 각각 98, 150, $167^{\circ}C$ 였으며, 단일 ITO의 최고 온도는 $32^{\circ}C$였다. 이 것은 동일한 두께 (95 nm)의 단일 ITO 박막과 비교하여 면저항이 낮은 하이브리드 박막의 발열량은 약 $120^{\circ}C$로 발열효율이 매우 우수한 것을 확인 할 수 있었다.

  • PDF

Quantum Dot-Sensitized Solar Cells Based on Mesoporous TiO2 Thin Films (메조포러스 이산화티타늄 박막 기반 양자점-감응 태양전지)

  • Lee, Hyo Joong
    • Journal of the Korean Electrochemical Society
    • /
    • v.18 no.1
    • /
    • pp.38-44
    • /
    • 2015
  • This review article summarizes the recent progress of quantum dot (QD)-sensitized solar cells based on mesoporous $TiO_2$ thin films. From the intrinsic characteristics of nanoscale inorganic QDs with various compositions, it was possible to construct a variety of 3rd-generation thin film solar cells by solution process. Depending on preparation methods, colloidal QD sensitizers are pre-prepared for later deposition onto the surface of $TiO_2$ or in-situ deposition of QDs from chemical bath is done for direct growth of QD sensitizers over substrates. Recently, colloidal QD sensitizers have shown an overall power conversion efficiency of ~7% by a very precise control of composition while a representative CdS/CdSe from chemical bath deposition have done ~5% with polysulfide electrolytes. In the near future, it is necessary to carry out systematic investigations for developing new hole-conducting materials and controlling interfaces within the cell, thus leading to an enhancement of both open-circuit voltage and fill factor while keeping the current high value of photocurrents from QDs towards more efficient and stable QD-sensitized solar cells.

A Study on the strengthening of Watching the Children's Musicals in the early childhood Education Institutions (유아교육기관에서의 뮤지컬 관람 실태와 활성화 개선 방안 연구)

  • Oh, Sun-Keun
    • Journal of the Korea Academia-Industrial cooperation Society
    • /
    • v.16 no.7
    • /
    • pp.4441-4449
    • /
    • 2015
  • The purpose of this study is to find out how children's musical is done in the early childhood education field. To find out the realities of children's musical watching, seek problems and way to improve, educationally new alternative, we selected subjects of study as follows. First, how children's musical of the early childhood education center is done? Second, how the education related children's musical of the early childhood education center is done? Third, what is the problem and way to improve of watching children's musical? To find out these, the result of the teachers(159 people) who are working the kidergarten and the early childhood education center is as follows. First, Children were very interested in watching musical and could get new, various experience and culture. Second, when watching musical, kindergarten and the early education center did pre-exploration everytime except same place. second, Of post-education activity, drawing activity related with musical content, story-making activity, developing to child's act are educationally effective. Third, whey watching musical, there is much pressure about danger and safety. So it is hard to control when children is moving. This significant result shows the importance of educational effects of the musical watching and the proposed expansion of the opportunity to experience a musical watching of the various educational approaches.

Dependence of the Diamond Coating Adhesion on the Microstructure of WC-Co Substrates (WC-Co계 미세조직에 따른 CVD 다이아몬드 코팅막의 접착력 변화)

  • Lee, Dong-Beum;Chae, Ki-Woong
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.10 s.269
    • /
    • pp.728-734
    • /
    • 2004
  • The effect of microstructure of WC-Co substrates which have different WC grain sizes from submicron to 5 $\mu$m on the diamond-substrate adhesion strength was investigated. The substrates were pre-treated by two methods : chemical etching with Murakami's solution and subsequently with $H_2SO_4$, and thermal heat-treatment. The adhesion strength was estimated by degree of peeling after Rockwell indentation. Diamond films of 20 $\mu$m thickness deposited on the heat-treated substrates showed an excellent adhesion strength at the load of 100 kg, which ascribed to the large and elongated WC grains. However, the cutting edge of insert was deformed after heat treatment and the surface morphology of heat treated substrate strongly affected on the surface roughness of the deposited diamond films. On the contrary, the diamond film of 10 $\mu$m in thickness on the chemically etched substrates of average WC grain size over 2 $\mu$m showed good adhesion strength enough not to peel-off under a load of 60 kg. Especially, the substrate of average WC grain size over 5 $\mu$m exhibited much improved reliability of adhesion comparing with the substrate of average grain size under 2 $\mu$m. No substrate deformation was observed in this case after the chemical etching, which is more advantageous and more practical in terms of precious machining than the heat treatment case.

Performance Improvement of ZnO Thin Films for SAW Bandpass Filter (SAW 대역 통과 필터용 ZnO 박막의 특성 개선 연구)

  • Lee, Seung-Hwan;Kang, Kwang-Yong;Yu, Yun-Sik
    • The Journal of Korean Institute of Electromagnetic Engineering and Science
    • /
    • v.25 no.12
    • /
    • pp.1219-1227
    • /
    • 2014
  • For development of the surface acoustic wave bandpass filter(SAW-BPF), we fabricated the high quality ZnO thin films through the step-by-step(double) deposition using two different deposition methods which are pulsed laser deposition(PLD) and RF sputtering techniques. The second growth of ZnO thin films was completed by RF sputtering method on the first ZnO thin films pre-deposited by PLD method. The characteristics of ZnO thin films were analyzed by XRD, SEM and AFM systems. The FWHM of ${\omega}$-scan analysis and the minimum RMS value of surface roughness of step-by-step grown ZnO thin films were $0.79^{\circ}$ and 1.108 nm respectively. As a result, the crystallinity and the preferred orientation of the grown ZnO thin films were kept good quality and the surface roughnesses of those were improved by post-annealing process as comparison with ZnO thin film fabricated by the conventional PLD technique only. Using these proposed ZnO thin films, we demonstrated the RF device such as SAW-BPF, built by the proposed ZnO thin films, shows that it has the bandwidth of 2.98 MHz and the insertion loss of 36.5 dB at the center frequency of 260.8 MHz, respectively.

Growth and Postharvest Freshness of $Tah$ $Tasai$ Chinese Cabbage ($Brassica$ $campestris$ var. $narinosa$) Baby Leaf Vegetable as Affected by Brushing Treatment during Cultivation (재배 시 brushing 처리에 따른 어린잎 채소 다채의 생육과 수확 후 선도 차이)

  • Lee, Jung-Soo;Do, Kyung-Ran
    • Food Science and Preservation
    • /
    • v.19 no.1
    • /
    • pp.19-25
    • /
    • 2012
  • An experiment was conducted to find out the effect of brushing treatment during cultivation on the postharvest quality of the baby leaf vegetable, specifically tah tasai Chinese cabbage (Brassica campestris var. narinosa). The effect of mechanical brushing during cultivation on the postharvest quality was determined in terms of the quality changes in weight loss, gas partial pressure, leaf color, and appearance during storage using a 30-${\mu}m$-thick polypropylene film at $16^{\circ}C$. The brushing treatment included brushing with A4 paper back and forth 50 times a day. The study revealed that the growths on the brushing-treated plant group were less than those on the control group. The structure of the leaf tissue of the brushing-treated plant also tended to be less compact than that of the non-treated plant. The brushing treatment resulted in less growth and denser plant tissues as well as in differences in the gas $O_2$ consumption and $CO_2$ accumulation after packaging. For the gas partial pressure, the $O_2$ consumption and $CO_2$ accumulation of the brushing-treated plant tended to be less than those of the non-treated plant. There were no differences, however, between the brushing-treated plant and control groups in the SPAD value and appearance. The study results also suggested that after packaging, the effects of the brushing treatment during cultivation on the quality of the tah tasai Chinese cabbage baby leaf vegetable was not significant. As such, it is recommended that effective post-harvest methods of improving the product quality of the baby leaf vegetable be further investigated.

Practical Virtual Compensator Design with Dynamic Multi-Leaf Collimator(dMLC) from Iso-Dose Distribution

  • Song, Ju-Young;Suh, Tae-Suk;Lee, Hyung-Koo;Choe, Bo-Young;Ahn, Seung-Do;Park, Eun-Kyung;Kim, Jong-Hoon;Lee, Sang-Wook;Yi, Byong-Yong
    • Proceedings of the Korean Society of Medical Physics Conference
    • /
    • 2002.09a
    • /
    • pp.129-132
    • /
    • 2002
  • The practical virtual compensator, which uses a dynamic multi-leaf collimator (dMLC) and three-dimensional radiation therapy planning (3D RTP) system, was designed. And the feasibility study of the virtual compensator was done to verify that the virtual compensator acts a role as the replacement of the physical compensator. Design procedure consists of three steps. The first step is to generate the isodose distributions from the 3D RTP system (Render Plan, Elekta). Then isodose line pattern was used as the compensator pattern. Pre-determined compensating ratio was applied to generate the fluence map for the compensator design. The second step is to generate the leaf sequence file with Ma's algorithm in the respect of optimum MU-efficiency. All the procedure was done with home-made software. The last step is the QA procedure which performs the comparison of the dose distributions which are produced from the irradiation with the virtual compensator and from the calculation by 3D RTP. In this study, a phantom was fabricated for the verification of properness of the designed compensator. It is consisted of the styrofoam part which mimics irregular shaped contour or the missing tissues and the mini water phantom. Inhomogeneous dose distribution due to the styrofoam missing tissue could be calculated with the RTP system. The film dosimetry in the phantom with and without the compensator showed significant improvement of the dose distributions. The virtual compensator designed in this study was proved to be a replacement of the physical compensator in the practical point of view.

  • PDF

Preparation of Activated Carbon Fiber-Ceramic Composites and Its Physical Properties (활성탄소섬유-세라믹복합체의 제조 및 물성)

  • 이재춘;박민진;김병균;신경숙;이덕용
    • Journal of the Korean Ceramic Society
    • /
    • v.34 no.1
    • /
    • pp.56-62
    • /
    • 1997
  • The PAN (Polyacrylonitrile) based carbon fiber-ceramic composites (CFCC) were prepared from mixtures of short carbon fibers, phenolic resin and ceramic binder. The effects of carbonization temperature of a pre-cursor fiber, the stabilized PAN fiber, on the specific surface area and the bending strength of the activated CFCC were studied in this work. The precursor fiber was carbonized at 80$0^{\circ}C$ and 100$0^{\circ}C$, respectively. The CFCC were activated at 85$0^{\circ}C$ in carbon dioxide for 10~90 minutes. As the burn-off of the activated CFCC made of the precursor fiber carbonized at 80$0^{\circ}C$ was increased from 37% to 76%, the specific surface area in-creased from 493m2/g to 1090m2/g, and the bending strength decreased from 4.5MPa to 1.4MPa. These values were about two times larger than those of the activated CFCC of which precursor fiber was car-bonized at 100$0^{\circ}C$. The effects of carbonization temperature of a precursor fiber on the specific surface area and bending strength of the activated CCFC were explained by bonding force between carbon fiber and car-bonized phenolic resin as well as by relative shirnkage between carbon fiber and ceramic film.