Characterization of Acetylene Plasma-Polymer Films: Recovery of Surface Hydrophobicity by Aging

  • Kim, Jeong-Ho;Kim, Tae-Hyung;Oh, Jung-Geun;Noh, Seok-Hwan;Lee, Jeong-Soo;Park, Kyu-Ho;Ha, Sam-Chul;Kang, Heon
    • Bulletin of the Korean Chemical Society
    • /
    • v.30 no.11
    • /
    • pp.2589-2594
    • /
    • 2009
  • Aging phenomena of plasma polymer films were studied by using the surface analysis techniques of contact angle measurement, X-ray photoelectron spectroscopy (XPS), time-of-flight secondary ion mass spectrometry (TOFSIMS), and atomic force microscopy (AFM). The polymer films were grown on an aluminum substrate by using a plasma polymerization method from a gas mixture of acetylene and helium, and the films were subsequently modified to have a hydrophilic surface by oxygen plasma treatment. Aging of the polymer films was examined by exposing the samples to water and air environments. The aging process increased the hydrophobicity of the surface, as revealed by an increase in the advancing contact angle of water. XPS analysis showed that the population of oxygen-containing polar groups increased due to the uptake of oxygen during the aging, whereas TOF-SIMS analysis revealed a decrease in the polar group population in the uppermost surface layer. The results suggest that the change in surface property from hydrophilic to hydrophobic nature results from the restructuring of polymer chains near the surface, rather than compositional change of the surface. Oxidative degradation may enhance the mobility and the restructuring process of polymer chains.

Effects of direct and indirect bonding techniques on bond strength and microleakage after thermocycling (직접 부착법과 간접 부착법이 열순환 후 부착강도와 미세누출에 미치는 영향에 대한 연구)

  • Ozturk, Firat;Babacan, Hasan;Nalcaci, Ruhi;Kustarci, Alper
    • The korean journal of orthodontics
    • /
    • v.39 no.6
    • /
    • pp.393-401
    • /
    • 2009
  • Objective: The purpose of this study was to compare the shear bond strength (SBS) of brackets and microleakage of a tooth-adhesive-bracket complex bonded with a direct and an indirect bonding technique after thermocycling. Methods: Fifty non-carious human premolars were divided into two equal groups. In the direct bonding group a light-cured adhesive and a primer (Transbond XT) was used. In the indirect-bonding group, a light-cured adhesive (Transbond XT) and chemical-cured primer (Sondhi Rapid Set) were used. After polymerization, the teeth were kept in distilled water for 24 hours and thereafter subjected to thermal cycling (500 cycles). For the microleakage evaluation, 10 teeth from each group were further sealed with nail varnish, stained with 0.5% basic fuchsin for 24 hours, and examined under a stereomicroscope. Fifteen teeth from each group were used for SBS testing with the universal testing machine and adhesive remnant index (ARI) evaluation. Data were analyzed using the Mann-Whitney U test, Chi-square test, and Fisher's exact test. Results: There were no statistical differences on SBS and microleakage between the two bonding techniques. The indirect bonding group had a significantly lower ARI score. Bracket failures were obtained between enamel-resin interfaces. Conclusions: The type of bonding technique did not significantly affect the amount of microleakage and SBS.

Comparative Study on Mechanical Properties and Dimensional Stability of Staypak and Wood-Polymer Composites from Populus alba × P. Glandulosa wood (현사시나무로 제조(製造)된 열압축목재(熱壓縮木材)와 목재(木材)-고분자(高分子) 복합체(複合體) 재질(材質)의 비교연구(比較硏究))

  • Pak, Sang-Bum;Ahn, Won-Yung
    • Journal of the Korean Wood Science and Technology
    • /
    • v.13 no.2
    • /
    • pp.14-34
    • /
    • 1985
  • One of the techniques for altering the properties of wood that has received considerable attention in the last twenty years is the formation of a wood-polymer composite (WPC) by irradiation and heat-catalyst polymerization of a monomer incorporated into the wood matrix. Wood-polymer composites are the new products having the superior mechanical and physical properties and the combinated characteristics of wood and plastic. The purpose of this experiment was to obtain the basic data for the improvement of wooden materials by manufacturing WPC and Staypak. The species examined was Hyunsasi-Namoo (Populus alba ${\times}$ P. glandulosa) which had not been utilized yet. Methylmethacrylate (MMA) as monomer, benzoyl peroxide (BPO) as initiator and methyl alcohol as bulking agent were used. The monomer containing BPO was impregnated into wood pieces by the dipping and the vacuum process for 2 hours. After impregnation, the treated samples were polymerized on the hot press with pressure and heat-catalyst methods. The results obtained were summarized as follows 1. The monomer loading into wood by the dipping process was 12.13 percent and 29.99 percent by the vacuum. The polymer loading into wood by the dipping process was 6.79 percent and 15.44 percent by the vacuum. 2. Comparing with Staypak, antishrink efficiency (ASE) of WPC was 12.5 to 13.6 percent on the radial direction and 14.70 to 18.63 percent on the tangential. Antiswelling efficiency (AE) was 14.40 to 17.22 percent on the radial direction and 17.18 to 42.1 8 to 42.14 percent on the tangential. Reduction in water absorptivity (RWA) was 8.19 to 15.5 percent. As a whole, the vacuum process was better than the dipping. 3. The specific gravity of control, Staypak and WPC were 0.44, 0.66 and 0.61 to 0.62, respectively. 4. In the bending strength test, the strength in case that the load direction is on the radial surface was greater than that which the load direction is on the tangential. 5. Increasing rate of stress at proportional limit in compression perpendicular to grain was 72.26 percent in case of WPC by the dipping process, 78.93 percent by the vacuum and 99.09 percent in case of Staypak.

  • PDF

Material Properties of Polymer-Impregnated Concrete and Nonlinear Fracture Analysis of Flexural Members (폴리머 침투콘크리트의 재료특성과 휨부재의 비선형 파괴해석)

  • 변근주;이상민;최홍식;노병철
    • Magazine of the Korea Concrete Institute
    • /
    • v.6 no.2
    • /
    • pp.97-107
    • /
    • 1994
  • The objective of this study is to develop polymer-impregnated concrete(PIC), which is a newly developed composite material made by impregnating polymer impregnanls into hardened normal concrete, and to develop analytical techniques for its proper applications. Crystalline methyl methacrylate(MMA) is chosen as a monomer of polymer impregnants. The corrlpositions of polymer impregnants and producing processes are developed by analyzing the effects of penetration, polymerization, thermal safety, and strengthening characteristics. On t he basis of experimental results of this study, various strength characteristics and stress strain constitutive relations are formulated in terms of the compressive strength of normal concrete and the polymer loadings, which can be applied for analysis and design of PIC members. In order to provide a model for fracture analysis of flexural members, fracture toughness, fracture energy, critical crack width, and tension softening relations near crack tip are also formulated in terms of member depth, initial notch depth, and the flexural strength of normal concrete. The structural analysis procedure and the finite element computer program developed in the study are applicable to evaluate elastic behavior, ultimate strength, and tension softening behavior of MMA type PIC structural members subject to various loading conditions. The accuracy and effectiveness of the developed computer program is examined by comparing the anal ytical results with the experimental results. Therefore, it is concluded that the developed structural analysis procedure and the finite element computer program are applicable to analysis and design of in-situ and precast PIC structural members.

COMPARISON OF MECHANICAL PROPERTIES IN 4 INDIRECT COMPOSITE RESIN (4종의 간접법용 복합 레진의 기계적 특성 비교)

  • Kim, Kil-Soo;Yoon, Tae-Ho;Song, Kwang-Yeob;Ahn, Seung-Geun
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.45 no.1
    • /
    • pp.21-33
    • /
    • 2007
  • Statement of problem: The esthetic component of dental care has become increasingly more important, while new tooth-colored materials are continually marketed. Various new indirect composite materials have been developed with required advantages. The most recent development in the indirect composites has been the introduction of the second-generation laboratory composite or poly-glass materials. They are processed by different laboratory techniques based on combinations of heat, pressure, vacuum and light polymerization. Although, second generation products became available in 1995, their characteristics and clinical performance have not been adequately investigated. Purpose: The aim of this study was to measure the mechanical properties of the second generation indirect resin system and compare these with an existing universal direct composite resin. Material and method: In this study four indirect composite material (Adoro LC, BelleGlass HP, Tescera, Synfony) were tested for flexural strength, wear resistance, hardness and their degree of conversion against Z250, a light cure direct composite. Results: Within the limitations of this study, the following conclusions were drawn: 1. From the abrasion wear result, Adoro showed the least volume loss while Synfony showed the greatest volume loss. Z250 and BelleGlass HP didn't show significant difference (p>0.05), but they showed significant difference with other groups (p<0.05). From the attrition wear, BelleGlass HP showed the least volume loss and it didn’t show significant difference with Tescera (p>0.05). While Synfony showed the greatest volume loss that it showed significant difference with other groups (p>0.05). 2. Mean values of flexural strength by means of three point bending test was in the order of Z250, Adoro, Belleglass HP, Tescera and Synfony. Mean elastic modulus was in the order of Z250, BelleGlass HP, Tescera, Adoro and Synfony. 3. The result of Vicker‘s microhardness value showed that significantly higher value in Z250 (p<0.05), and is in the order of BelleGlass HP, Tescera, Adoro and Synfony. 4. The degree of conversion measured by FT-IR showed significantly higher value in BelleGlass HP (p<0.05), and is in the order of Adoro, Synfony, Tescera and Z250. Conclusion: Significant differences were found in the flexural strength, wear resistance, hardness and their degree of conversion.

MECHANICAL PROPERTIES AND MICROLEAKAGE OF COMPOSITE RESIN MATERIALS CURED BY VARIABLE LIGHT INTENSITIES (가변 광도에 따른 복합레진의 기계적 물성 및 변연누출도 변화)

  • Han, Seung-Ryul;Min, Kyung-San;Shin, Dong-Hoon
    • Restorative Dentistry and Endodontics
    • /
    • v.28 no.2
    • /
    • pp.134-145
    • /
    • 2003
  • Mechanical properties and microleakage of two composites [conventional hybrid type DenFil (VERICOM Co., Anyang, Korea) / micro matrix hybrid type Esthet X (Dentsply Caulk, Milford, DE, U.S.A.)] were evaluated to assess whether variable light intensity curing is better than conventional curing technique. Curing was done for 40 seconds in two ways of 2 step soft-start technique and 5 step ramping technique. Three kinds of light intensities of 50, 100, $200{\;}mW/\textrm{cm}^2$ were initially used for 10, 20, 30 seconds each and the maximum intensity of $600 {\;}mW/\textrm{cm}^2$ was used for the rest of curing time in a soft-start curing tech nique. In a ramping technique, curing was done with the same initial intensities and the light intensity was increased 5 times with the same rate to the maximum intensity of $600{\;}mW/\textrm{cm}^2$. After determining conditions that showed no different mechanical properties with conventional technique, Esthet X composite was filled in a class V cavity, which dimension was $4{\times}3{\times}1.5{\;}mm$ and cured under those conditions. Microleakage was evaluated in two ways of dye penetration and maximum gap estimation through SEM observation. ANOVA and Spearman's rho test were used to confirm any statistical significance among groups. The results were as follows : 1 Several curing conditions of variable light intensities resulted in the similar mechanical properties with a conventional continuous curing technique, except conditions that start curing with an initial light intensity of $50{\;}mW/\textrm{cm}^2$. 2. Conventional and ramping techniques were better than soft-start technique in mechanical properties of microhardness and compressive strength. 3. Soft-start group that started curing with an initial light intensity of $100{\;}mW/\textrm{cm}^2$ for 10 seconds showed the least dye penetration. Soft-start group that started curing with an initial light intensity of $200{\;}mW/\textrm{cm}^2$ for 10 seconds showed the smallest marginal gap, if there was no difference among groups. 4. Soft-start technique resulted in better dye-proof margin than conventional technique(p=0.014) and ramping technique(p = 0.002). 5. There was a very low relationship(p=0.157) between the methods of dye penetration and marginal gap determination through SEM evaluation. From the results of this study, it was revealed that ramping technique would be better than conventional technique in mechanical properties, however, soft-start technique might be better than conventional one in microleakage. It was concluded that much endeavor should be made to find out the curing conditions, which have advantages of both aspects or to solve these kinds of problems through a novel idea of polymerization.

Comparative accuracy of implant impression techniques with different splinting materials (임플란트 인상채득 방법과 인상용 코핑 연결 고정에 따른 정확성 비교)

  • Ki-Yoon Hong;Soo-Yeon Shin
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.39 no.1
    • /
    • pp.9-20
    • /
    • 2023
  • Purpose: We investigated the effect of open tray impression using pick-up impression coping and close tray impression using transfer impression coping on the accuracy of impression in edentulous patients on their mandibular parts. the effect of material types of pick-up type impression copings for splinting in open tray impression on the accuracy of impression was also evaluated. Materials and Methods: Two implant fixtures were implanted in parallel in the left molar of the mandibular in the shape of a mandibular partial edentulous model. The 40 individual trays were fabricated using 3D printer. The prepared individual trays were classified into 4 groups (i.e., PN, PG, PH, and TN groups), and a total of 40 impression-takings were conducted. A master cast was connected to a Scan Body. The converted STL file was super-imposed on the scan images of the various groups. Results: The order of standard deviation values decreased as follows: PN (0.2343 ± 0.0844 mm), TN (0.2192 ± 0.0840 mm), indicating that the high accuracy of impression for TN group. In addition, for the comparison results between the material types used in splinting the open tray impression, the PH group showed a relatively lower standard deviation (0.1910 ± 0.1176 mm) than that of the PN group (0.2343 ± 0.0844 mm), PG group (0.2556 ± 0.1082 mm). Conclusion: The acrylic resin synthesized by light-induced polymerization exhibited a higher accuracy of impression taking than that of autopolymerizing acrylic resin. Meanwhile, the accuracy of impression taking was not dependent on the implant impression taking method or the presence of connection/fixation of impression copings.

The effects of polishing technique and brushing on the surface roughness of acrylic resin (연마 방법과 칫솔질이 아크릴릭 레진의 표면 거칠기에 미치는 영향)

  • Lee, Ju-Ri;Jeong, Cheol-Ho;Choi, Jung-Han;Hwang, Jae-Woong;Lee, Dong-Hwan
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.48 no.4
    • /
    • pp.287-293
    • /
    • 2010
  • Purpose: This study evaluated the effect of polishing techniques on surface roughness of polymethyl methacrylate (PMMA), as well as the influence of light-cured surface glaze and subsequent brushing on surface roughness. Materials and methods: A total of 60 PMMA specimens ($10{\times}10{\times}5\;mm$) were made and then divided into 6 groups of 10 each according to the polymerization methods (under pressure or atmosphere) and the surface polishing methods (mechanical or chemical polishing) including 2 control groups. The mechanical polishing was performed with the carbide denture bur, rubber points and then pumice and lathe wheel. The chemical polishing was performed by applying a light-cured surface glaze ($Plaquit^{(R)}$; Dreve-Dentamid GmbH). Accura $2000^{(R)}$, a non-contact, non-destructive, optical 3-dimensional surface analysis system, was used to measure the surface roughness (Ra) and 3-dimensional images were acquired. The surface roughness was again measured after ultrasonic tooth brushing in order to evaluate the influence of brushing on the surface roughness. The statistical analysis was performed with Mann-Whitney test and t-test using a 95% level of confidence. Results: The chemically polished group showed a statistically lower mean surface roughness in comparison to the mechanically polished group (P = .0045) and the specimens polymerized under the atmospheric pressure presented a more significant difference (P = .0138). After brushing, all of the groups, except the mechanically polished group, presented rougher surfaces and showed no statistically significant differences between groups. Conclusion: Although the surface roughness increased after brushing, the chemical polishing technique presented an improved surface condition in comparison to the mechanical polishing technique.