• 제목/요약/키워드: Piezoelectric ceramics

검색결과 828건 처리시간 0.031초

BNKZ치환된 (Na,K)NbO3계 세라믹스의 미세구조 및 압전 특성 (Microstructure and Piezoelectric Properties of (Na,K)NbO3 System Ceramics Substituted with BNKZ)

  • 한종대;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제30권10호
    • /
    • pp.637-640
    • /
    • 2017
  • In this study, $(1-x)(Na_{0.52}K_{0.443}Li_{0.037})(Nb_{0.883}Sb_{0.08}Ta_{0.037})O_3-x(Bi_{0.5}(Na_{0.7}K_{0.3})_{0.5}ZrO_3$ ceramics were fabricated by BNKZ substitution using a conventional solid-state method to develop excellent lead-free piezoelectric ceramics for piezoelectric actuators; their dielectric and piezoelectric properties were then investigated. All specimens were in the orthorhombic phase. $NKL-NSTO_3$ ceramics with x=0.01 showed excellent piezoelectric properties. The density (${\rho}$), piezoelectric charge constant ($d_{33}$), planar piezoelectric coupling coefficient ($k_p$), mechanical quality factor ($Q_m$), and dielectric constant (${\varepsilon}_r$) had optimized values of $4.56g/cm^3$, 208 pC/N, 0.43, 96, and 975, respectively.

Nb 변화에 따른 KNN 세라믹스의 압전 및 전기적 특성 (Piezoelectric and Electrical properties of KNN ceramics as a function of the Variation of Nb)

  • 이갑수;류주현;김인성;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2010년도 하계학술대회 논문집
    • /
    • pp.302-302
    • /
    • 2010
  • The lead-free piezoelectric ceramics must have high piezoelectric properties and electrical properties for the applications of piezoelectric devices. Therefore, KNN ceramics were investigated as a function of the variation of Nb. The density was increased with the increase of Nb. The density was saturated above 0.8895 mol Nb. The maximum value of electromechanical coupling coefficient(kp) was obtained 0.428 at 0.8895mol Nb. This result can be attributed to the well sintered of specimens. Also, The maximum value of mechanical quality factor(Qm) showed 1554 at 0.8895mol Nb. Therefore, this composition can be used for application of piezoelectric device such as piezoelectric transformer and piezoelectric actuator.

  • PDF

PZT-PMNS 세라믹의 공진특성 및 압전 정수의 전계의존성 (The Electric Field Dependence of the Resonance Characteristics and Piezoelectric Constant of the PZT-PMNS Ceramics)

  • 오진헌;임기조;강성화;김현후
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2008년도 Techno-Fair 및 합동춘계학술대회 논문집 전기물성,응용부문
    • /
    • pp.179-180
    • /
    • 2008
  • In this paper, the variable tendency piezoelectric constant and resonance characteristics piezoelectric ceramics due to the electric field is studied. The practical application of piezoelectric ceramics is not only applied in field of small signal. For example, in case of an ultrasonic motor, $120{\sim}130Vrms$ of driving voltage is needed and that of an piezoelectric pump, $200{\sim}220Vrms$ of voltage is required. Therefore, to examine the characteristics of piezoelectric ceramics in large signal contributes to reducing the susceptibility to the multifarious application and securing the ease of the production of control circuit. These contributions may be connected to the expansion of industrial application. We fabricated disk-type piezoelectric ceramic samples by using conventional method and measured the resonance characteristics of these samples under from low to high voltage driving conditions. According to increasing the value of the input voltage, we measured the resonance frequency of the piezoelectric ceramic, and inquired into the cause of these phenomena.

  • PDF

K5.4Cu1.3Ta10O29 첨가에 따른 (Na,K)NbO3계 세라믹스의 압전특성 (Piezoelectric Properties of (Na,K)NbO3 Ceramics as a Function of K5.4Cu1.3Ta10O29 Addition)

  • 노정래;류주현;정영호
    • 한국전기전자재료학회논문지
    • /
    • 제23권5호
    • /
    • pp.379-382
    • /
    • 2010
  • In this study, in order to develop the lead-free piezoelectric ceramics with high piezoelectric and dielectric properties, $(K_{0.5}Na_{0.5})(Nb_{0.97}Sb_{0.03})O_3$ ceramics were fabricated using a conventional mixed oxide process and their piezoelectric and dielectric characteristics were investigated according to the $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition. $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition enhanced density, electromechanical coupling factor($k_p$) piezoelectric constant $d_{33}$ and mechanical quality factor($Q_m$). At the 0.9 mol% $K_{5.4}Cu_{1.3}Ta_{10}O_{29}$ addition, density, electromechanical coupling factor($k_p$), dielectric constant(${\varepsilon}_r$) and piezoelectric constant($d_{33}$) of specimen showed the optimum values of 0.46, 471, and 148 pC/N, respectively.

(Na,K,Li)(Nb,Sb,Ta)O3계 세라믹스의 소성시간이 압전특성에 미치는 영향 (Effect of Sintering Time on the Piezoelectric Properties of (Na,K,Li)(Nb,Sb,Ta)O3 Ceramics)

  • 김승원;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제30권4호
    • /
    • pp.218-222
    • /
    • 2017
  • In this paper, in order to develop excellent composition ceramics for a piezoelectric energy- harvesting device, we synthesized $0.99(Na_{0.52}\;K_{0.443}\;Li_{0.037})(Nb_{0.883}\;Sb_{0.08}\;Ta_{0.037})O_3$ + $0.01(Sr_{0.95}Ca_{0.05})TiO_3$ + $0.3\;wt%\;Bi_2O_3\;+\;0.3\;wt%\;Fe_2O_3\;+\;0.3\;wt%\;CuO$ (abbreviated as NKN-SCT) ceramics with different sintering times, using the ordinary solid-state reaction method. The effect of sintering time on the microstructure and piezoelectric properties was investigated. The ceramics with the sintering time of 7 h have the optimum values of the piezoelectric constant ($d_{33}$), piezoelectric voltage constant ($g_{33}$), planar piezoelectric coupling coefficient (kp), mechanical quality factor (Qm), and dielectric constant (${\varepsilon}r$): $d_{33}=314[pC/N]$, $g_{33}=20.07[10^{-3}mV/N]$, kp = 0.442, Qm = 93, ${\varepsilon}r=1,768$, all being suitable for a piezoelectric energy-harvesting device.

저온소결 PMN-PNN-PZT 세라믹스의 WO3 첨가에 따른 압전 및 유전특성 (Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT Ceramics with the amount of WO3 Addition)

  • 류주현;김국진;이석태
    • 한국전기전자재료학회논문지
    • /
    • 제20권2호
    • /
    • pp.130-134
    • /
    • 2007
  • In this study, in order to. develop the low temperature sintering ceramics for multilayer piezoelectric actuator, PMN-PNN-PZT ceramics using CuO, $Bi_{2}O_{3}\;and\;Li_{2}CO_{3}$ as sintering aids were manufactured with the amount of $WO_{3}$ addition. The ceramics were sintered at $900,\;930,\;960^{\circ}C$, respectively. Thereafter, their microstructural, dielectric and piezoelectric properties were investigated. The $WO_{3}$ was proved to lower the sintering temperature of piezoelectric ceramics due to the effects of PbO and $WO_{3}$ liquid phase. At 0.3 wt% $WO_{3}$ added specimen sintered at $930^{\circ}C$, electromechanical coupling factor($k_{p}$), mechanical quality factor($Q_{m}$), dielectric constant and $d_{33}$ showed the optimum values as the values of 0.60, 1,402, 1,440 and 360 pC/N, respectively, for multilayer piezoelectric actuator application.

ZnO와 CuO 첨가에 따른 NKN-LST 세라믹스의 압전 특성 (Piezoelectric Properties of NKN-LST Ceramics with ZnO and CuO Addition)

  • 이승환;이성갑;이영희
    • 한국전기전자재료학회논문지
    • /
    • 제24권8호
    • /
    • pp.632-635
    • /
    • 2011
  • Additions (ZnO, CuO) doped $0.98(Na_{0.5}K_{0.5})NbO_3-0.02Li(Sb_{0.17}Ta_{0.83})O_3$ (0.98NKN-0.02LST-x) lead free piezoelectric ceramics have been fabricated by ordinary sintering technique. The effects of additions doping on the dielectric, piezoelectric, and ferroelectric properties of the ceramics were mainly investigated. X-ray diffraction of the sample appeared orthorhombic phase. The specimen doped with additions exhibits enhanced electrical properties ($d_{33}$= 153 pC/N). These results indicate that the 0.98NKN-0.02LST-x ceramics is a promising candidate for lead-free piezoelectric ceramics for applications such as piezoelectric actuators, harmonic oscillator and so on.

PNN 치환에 따른 PMW-PNN-PZT-BF 세라믹스의 미세구조와 압전 특성 (Microstructure and Piezoelectric Properties of Low Temperature Sintering PMW-PNN-PZT-BF Ceramics According to PNN Substitution)

  • 신상훈;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제29권2호
    • /
    • pp.90-94
    • /
    • 2016
  • In this work, [$Pb(Mg_{1/2}W_{1/2})_{0.03}(Ni_{1/3}Nb_{2/3})_x(Zr_{0.5}Ti_{0.5})_{0.97-x}O_3-BiFeO_3$] (x=0.02 to 0.12) composition ceramics were fabricated by the conventional soild state reaction method and their microstructure and piezoelectric properties were investigated according to PNN substitution. The addition of small amount of $BiFeO_3$, $Li_2CO_3$, and $CaCO_3$ were used in order to decrease the sintering temperature of the ceramics. The XRD (x-ray diffraction patterns) of all ceramics exhibited a perovskite structure. The sinterability of PMW-PNN-PZT-BF ceramics was remarkably improved using liquid phase sintering of $CaCO_3$, $Li_2CO_3$. However, it was identified from of the X-ray diffraction patterns that the secondary phase formed in grain boundaries decreased the piezoelectric properties. According to the substitution of PNN, the crystal structure of ceramics is transformed gradually from a tetragonal to rhombohedral phase. The x=0.10 mol PNN-substituted PMW-PNN-PZT-BF ceramics sintered at $920^{\circ}C$ showed the optimum values of piezoelectric constant($d_{33}$), piezoelectric figure of merit($d_{33{\cdot}}g_{33}$), planar piezoelectric coupling coefficient($k_p$) and density : $d_{33}=566$ [pC/N], $g_{33}=29.28[10^{-3}mV/N]$, $d_{33{\cdot}}g_{33}=16.57[pm^2/N]$, $k_p=0.61$, density=7.82 [$g/cm^3$], suitable for duplex ultrasonic sensor application.

저온소결 PMN-PNN-PZT세라믹스의 $WO_3$첨가에 따른 압전 및 유전특성 (Piezoelectric and Dielectric Characteristics of Low Temperature Sintering PMN-PNN-PZT ceramics with the amount of $WO_3$ addition)

  • 김국진;류주현;정영호
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2006년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.61-62
    • /
    • 2006
  • In this study, in order to develop the low temperature sintering ceramics for multilayer piezoelectric actuator, PMN-PNN-PZT ceramics using ${Fe_2}{O_3}$ and $WO_3$ as sintering aids were manufactured with the amount of $WO_3$ addition, and the specimens were sintered at 900, 930, $960^{\circ}C$, respectively. Thereafter, their dielectric and piezoelectric properties were investigated. The sintering aids were proved to lower the sintering temperature of piezoelectric ceramics due to the effects of ${Fe_2}{O_3}$ and $WO_3$ liquid phase. At 0.3wt% $WO_3$ added specimen sintered at $930^{\circ}C$, kp, Qm, dielectric constant and $d_{33}$ showed the optimum values of 0.60, 1402, 1440 and 360[pC/N], respectively, for multilayer piezoelectric actuator application.

  • PDF

Columbite법으로 제조된 (Na,K,Li)(Nb,Ta,Sb)O3 세라믹스의 하소온도에 따른 유전 및 압전 특성 (Dielectric and Piezoelectric Properties of (Na,K,Li)(Nb,Ta,Sb)O3 Ceramics Manufactured Using Columbite Methods with Calcination Temperature)

  • 라철민;류주현
    • 한국전기전자재료학회논문지
    • /
    • 제29권3호
    • /
    • pp.159-163
    • /
    • 2016
  • In this paper, in order to develop optimum composition ceramics with excellent piezoelectric properties, $(Na_{0.525}K_{0.443}Li_{0.037})(Nb_{0.823}Sb_{0.08}Ta_{0.037})O_3+0.3wt%Bi_2O_3+0.4wt%Fe_2O_3$ lead-free piezoelectric ceramics were synthesized by conventional soild-state method. The calcination temperature of columbite precursors were fabricated at temperature range from $950^{\circ}C$ to $1,150^{\circ}C$ and sintering aids with low melting point were added to densify these ceramics. Effect of calcination temperature on dielectric and piezoelectric properties of ceramics were investigated. the ceramics with B-site columbite precursors at temperature of $1,100^{\circ}C$ obtained the optimal values of $d_{33}=272$ [pC/N], $k_p=0.51$, $Q_m=102$, ${\varepsilon}_r=978$.