• 제목/요약/키워드: Pb-free 솔더

검색결과 159건 처리시간 0.022초

SnPb와 무연 플립칩 솔더의 유효전하수와 임계전류밀도 (Effective Charge Number and Critical Current Density in Eutetic SnPb and Pb Free Flip Chip Solder Bumps)

  • 채광표
    • Journal of Welding and Joining
    • /
    • 제23권5호
    • /
    • pp.49-54
    • /
    • 2005
  • The effective charge number and the critical current density of electromigration in eutetic SnPb and Pb Free $(SnAg_{3.8}Cu_{0.7)$ flip chip solder bumps are studied. The effective charge number of electromigration in eutectic SnPb solder is obtained as 34 and the critical current density is $j=0.169{\times}({\delta}_{\sigma}/{\delta}_x})\;A/cm^2,\;where\;({\delta}_{\sigma}/{\delta}_x})$ is the electromigration-induced compressive stress gradient along the length of the line. While the effect of electromigration in Pb free solder is much smaller than that in eutectic SnPb, the product of diffusivity and effective charge number $DZ^{\ast}$ has been assumed as $6.62{\times}10^{-11}$. The critical length for electromigration are also discussed.

무연솔더페이스트의 신뢰성 규격 제정 (Standardization of reliability specification for lead free solder paste)

  • 강종태;박재현;김영섭;이중주
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.73-74
    • /
    • 2004
  • Sn-Pb계 유연 솔더는 오랜 기간동안 전자기기의 가장 유효한 접합재료로 사용되어 왔다 그러나, 근년. 솔더를 사용한 전자기기의 폐기 시에 산성비에 의해 솔더중에 함유된 납(Pb) 성분이 용출되어 지하수를 오염시키고 이것이 인체에 흡수되면 지능저하, 생식기능저하 등 인체에 해를 미치는 환경오염 물질로 지적되고 있다. (중략)

  • PDF

BGA 솔더 접합부의 기계적.전기적 특성에 미치는 리플로우 횟수의 효과 (Effect of Reflow Number on Mechanical and Electrical Properties of Ball Grid Array (BGA) Solder Joints)

  • 구자명;이창용;정승부
    • 마이크로전자및패키징학회지
    • /
    • 제14권4호
    • /
    • pp.71-77
    • /
    • 2007
  • 본 연구에서는 리플로우 횟수를 달리하여 Sn-37Pb, Sn-3.5Ag와 Sn-3.5Ag-0.75Cu (all wt.%) BGA 솔더 접합부들을 OSP가 코팅된 Cu 패드 상에 형성시킨 후, 기계적 전기적 특성을 연구하였다. 주사전자현미경 분석 결과, 접합 계면에 생성된 $Cu_6Sn_5$ 금속간화합물 층의 두께는 리플로우 횟수가 증가함에 따라 증가하였다. Sn-Pb와 Sn-Ag-Cu 솔더 접합부의 경우, 3회 리플로우 후 최대 전단 강도를 나타내었으며, Sn-Ag 솔더 접합부의 경우 4회 리플로우 후 최대 전단 강도를 나타내었다. 이후 리플로우 횟수가 10회까지 증가함에 따라 전단 강도는 점차 감소하였다. 리플로우 횟수가 증가함에 따라 전기적 특성은 점차 감소하였다.

  • PDF

BGA 접합부에서 Sn-Ag-X 계 solder의 soldering성 특성에 관한 연구 (A study on soldering Characteristics between Sn-Ag-X system and BGA joints)

  • 김봉균;박종현;오은주;이규하;서창제
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2004년도 춘계 학술발표대회 개요집
    • /
    • pp.81-83
    • /
    • 2004
  • 최근 대두되고 있는 환경오염문제로 인해 전자산업에서는 전 세계적으로 Pb 솔더에 관한 규제가 진행중에 있다. 이에 Pb free 솔더에 관한 연구가 활발히 진행 중에 있으며 그 중 Sn-Ag계 solder는 유력한 대체 solder로 대두되고 있다. (중략)

  • PDF

자동차 전장용 무연 솔더 기술 (Lead-free Solder Technology and Reliability for Automotive Electronics)

  • 이순재;정재필
    • 마이크로전자및패키징학회지
    • /
    • 제22권3호
    • /
    • pp.1-7
    • /
    • 2015
  • In this study, properties of Pb-free solders for automotive electronics parts were discussed. Lead-free solders for electronics became important after RoHS (Restriction of the use of certain Hazardous Substances) to avoid environmental pollution. Also the growing electronic rate in automotive parts and ELV (End-of Life Vehicles) make Pb-free solder for automotive electronics to be inevitable trend. Definitely, Pb-free solder for automotive electronics should have good wettability, basic strength, but need more reliability than other solders, since it has harsh condition like high temperature, humidity and engine vibration. Thus, shear strength test, thermal shock, drop test and many others are needed to ensure the high reliability. This study describes the properties and requirements of Pb-free solders for automotive electronics.

Sn8Zn3Bi 솔더를 이용한 1608 칩 솔더링부의 고온고습 신뢰성 평가 (Reliability evaluation of 1608 chip joint using Sn8Zn3Bi solder under high temperature and high humidity)

  • 김규석;이영우;홍성준;정재필;문영준;이지원;한현주;김미진
    • 대한용접접합학회:학술대회논문집
    • /
    • 대한용접접합학회 2005년도 추계학술발표대회 개요집
    • /
    • pp.228-230
    • /
    • 2005
  • Sn-8wt%Zn-3wt%Bi (이하, Sn-8Zn-3Bi) 솔더의 장기 신뢰성을 평가하기 위하여 고용고습시험을 행하였다. 고온 고습 시험은 $85^{\circ}C$/85RH 조건에서 1000 시간 동안 하였다. 접합 기판으로는 각각 OSP (Organic Solderability Preservative), Sn 그리고 Ni/Au 처리를 한 PCB(Printed Circuit Board) 패드를 사용하였다. 접합에 사용한 부품은 1608Chip 으로 MLCC(Multi Layer Ceramic Capacitor 이하, 1608C) 와 Chip Resister(이하, 1608R)을 사용하였으며, 이 두 부품의 전극부위에 Sn-10wt%Pb(이하 Sn-l0PB), Sn을 각각 도금하였다. 솔더링 후 1608C 와 1608R의 전단 접합 강도와 솔더링부에서 Zn상의 변화를 관찰하였다. 측정결과, Sn-8Zn-3Bi 솔더의 초기 전단 접합 강도는 기판의 표면처리에 상관없이 약 40N 이었다. 그러나 고온 고습 시험 1000 시간 후에는 기판의 표면처리에 상관없이 약 30N 까지 감소하였다. 하지만 이는 reference인 Sn-37Pb 솔더의 강도값과 거의 유사하며, 이는 Sn-8Bi-3Zn 솔더의 고온 고습 시험 후 전단강도 특성은 기존 유연솔더와 비교하여 동등이상이라고 평가할 수 있다.

  • PDF