• 제목/요약/키워드: Pb foil

검색결과 7건 처리시간 0.02초

전해콘덴사용 알루미늄박의 피막형성 거동에 관한 연구 (Anodizing Mechanism of Aluminum Foil Electrolytic Capactor.)

  • 김기호
    • 한국표면공학회지
    • /
    • 제22권2호
    • /
    • pp.62-68
    • /
    • 1989
  • Pb2+ ino, added in ctching sohing, is electrodeposited on a alumiunm foil for electrolycic condenser to promote its capacitance. In addition, several factoral factors in etching process are varied to examine how they change the capacitance of the condenser. The capacitance of the condenser made of 0.1 ppm pb electrodeposited aluminum foil is enhanced about 20% than of conventional ane. It is thought out that the enhanement is the result of the act of PbO2, which existed for the conveting of electrodeposited Pb, as a promoter tunnel etching of aluminum foil.

  • PDF

솔더 포일을 이용한 무플럭스 솔더링에 관한 연구 (A Study on Fluxless Soldering using Solder Foil)

  • 신영의;김경섭
    • Journal of Welding and Joining
    • /
    • 제16권5호
    • /
    • pp.100-107
    • /
    • 1998
  • This paper describes fluxless soldering of reflow soldering process using solder foil instead of solder pastes. There is an increasing demand for the reliable solder connection in the recent high density microelectronic components technologies. And also, it is problem fracture of an Ozone layer due to freon as which is used to removal of remained flux on the substrate. This paper discussed joining phenomena, boudability and joining processes of microelectronics devices, such as between outer lead of VLSI package and copper pad on a substrate without flux. The shear strength of joints is 8 to 13 N using Sn/Pb (63/37 wt.%) solder foil with optimum joining conditions, meanwhile, in case of using Sn/In (52/48 wt.%) solder foil, it is possible to bond with low heating temperature of 550 K, and accomplish to high bonding strength of 25N in condition heating temperature of 650K. Finally, this paper experimentally shows fluxless soldering using solder foil, and accomplishes key technology of microsoldering processes.

  • PDF

Development of the Copper Core Balls Electroplated with the Solder of Sn-Ag-Cu

  • Imae, Shinya;Sugitani, Yuji;Nishida, Motonori;kajita, Osamu;Takeuchi, Takao
    • 한국분말야금학회:학술대회논문집
    • /
    • 한국분말야금학회 2006년도 Extended Abstracts of 2006 POWDER METALLURGY World Congress Part2
    • /
    • pp.1207-1208
    • /
    • 2006
  • We developed the copper core ball electroplated with Sn-Ag-Cu of the eutectic composition which used mostly as Pb free solder ball with high reliability. In order to search for the practicality of this developed copper core ball, the evaluation was executed by measuring the initial joint strength of the sample mounted on the substrate and reflowed and by measuring the joint strength of the sample after the high temperature leaving test and the constant temperature and the humidity leaving test. This evaluation was compered with those of the usual other copper core balls electroplated with (Sn,Sn-Ag,Sn-Cu,Sn-Bi) and the Sn-Ag-Cu solder ball.

  • PDF

Electrochemical Synthesis of Octahedral Nanostructured PbF2

  • Lee, Joon-Ho;Choi, Jin-Sub
    • Bulletin of the Korean Chemical Society
    • /
    • 제32권2호
    • /
    • pp.463-466
    • /
    • 2011
  • In this work, we investigate anodization of Pb in ethylene glycol containing small amount of $NH_4F$, demonstrating that ${\beta}-PbF_2$ particles with octahedral morphology can be prepared by adjusting the applied potential and anodizing time. FE-SEM images and XRD measurements of anodic nanostructures as a function of anodizing time clearly show that PbO is first formed on Pb. Subsequently, a local dissolution of PbO leads to formation of skeleton structure of PbO, releasing $Pb^{2+}$ ions in the electrolyte. The lead ions can be precipitated on the walls or intersection of the skeleton walls when the concentration of lead ions is saturated. The method described in this article shows the feasibility of formation of metal fluoride crystal by anodization of metal in a fluoride containing solution.

효율적인 광전기화학적 태양에너지 전환과 저장을 위한 Solar Water Battery의 최적화 (Optimization of Solar Water Battery for Efficient Photoelectrochemical Solar Energy Conversion and Storage)

  • 고현주;박이슬
    • 청정기술
    • /
    • 제27권1호
    • /
    • pp.85-92
    • /
    • 2021
  • 태양에너지를 활용하여 전력을 생산하는 시스템인 Solar water battery는 광전기화학전지와 에너지저장시스템을 결합한 것으로 추가적인 외부 전압 없이 태양에너지의 전환과 저장을 동시에 할 수 있다. Solar water battery는 광전극, 저장전극 그리고 상대전극으로 구성되어 있고, 이들의 선택과 조합은 시스템의 성능과 효율에 있어 중요한 역할을 한다. 본 연구에서는 Solar water battery의 구성요소들을 변화시켜 시스템에 미치는 영향을 알고자 하였다. 상대전극이 방전 시 미치는 영향, 광전극과 저장전극의 전극 재료, 전해질의 종류에 따른 태양에너지 전환 효율과 저장 용량에 미치는 영향에 대해 연구하였다. 이들의 최적화된 구성(TiO2 : NaFe-PB : Pt foil)에서 15시간동안의 광조사 후의 방전 용량이 72.393 mAh g-1으로 시스템 구성 조건에 따라 광전환/저장 효율이 크게 영향을 받음을 확인 할 수 있었다. 또한, 유기 오염물질을 광전극 반응조내 전해질에 첨가하여 광전하를 효율적으로 분리시킴으로써 광전류 증가시켰으며, 이로 인해 저장용량이 향상되고, 동시에 오염물질도 분해시킬 수 있음을 확인하였다. 이처럼 Solar water battery는 추가적인 외부 전압이 필요없는 새로운 친환경 태양에너지 전환/저장 시스템이며, 나아가 수처리에도 활용할 수 있을 것으로 기대된다.

비파괴 분석법을 통한 안성 청룡사 금동관음보살좌상 내부구조 및 금박층 조사 (Investigation of the Internal Structure and Gold-thin Layer of the Gilt-bronze Seated Avalokitesvara Bodhisattva at Anseong Cheonryong Temple through the Non-destructive Analysis)

  • 최정은;최학
    • 보존과학회지
    • /
    • 제37권6호
    • /
    • pp.670-678
    • /
    • 2021
  • <안성 청룡사 금동관음보살좌상>을 봉안하고 있는 청룡사(靑龍寺)는 경기도 안성시 서운면 서운산 자락에 있는 사찰이며, 대한불교조계종 제2교구 본사인 용주사의 말사이다. 안성 청룡사 금동관음보살좌상의 바닥면 XRF 분석 결과는 Cu-27.2 wt%, Sn-12.6 wt%, Pb-48 wt%이며, 과거 여러 전란으로 인해 소지금속 성분과 차이가 있을 것으로 예상된다. 불상의 내부를 확인하기 위해 감마선(γ-ray, Ir-192)으로 촬영하였으며, 파손된 배면 부분과 후대에 나무로 덧대어 수리한 위치를 확인하였다. γ-ray 촬영 결과와 XRF 분석을 이용하여 확인한 좌, 우의 수리 경계면은 허벅지 중간부터 목 아랫부분까지로 청동과 나무로 분리된다. 안성 청룡사 금동관음보살좌상의 금박 두께를 추정하기 위해 표준시료를 이용해 계산한 결과 얼굴과 가슴과 같은 육신 부분의 금박 두께가 20.7 ㎛와 21 ㎛로 가장 두꺼웠으며, 나무를 소지 재료로 한 부분이 평균 11.9 ㎛, 마지막으로 소지금속이 청동인 부분이 평균 7.4 ㎛로 금박 두께가 가장 얇음을 확인할 수 있었다.

굽힘 시험에 의한 플렉시블 CZTS 태양전지의 I-V 특성 변화에 관한 연구 (Change of I-V Properties of Flexible CZTS Solar Cell Through Mechanical Bending Test)

  • 김성준;김제하
    • 한국융합학회논문지
    • /
    • 제13권3호
    • /
    • pp.197-202
    • /
    • 2022
  • CZTS 태양전지는 Cu, Zn, Sn, Se, S으로 구성된 흡수층을 사용하는 박막 태양전지로, In, Ga이 사용되는 CIGS 태양전지보다 저렴하며 Pb, Cd이 사용된 페로브스카이트, CdTe 태양전지보다 친환경적이다. 본 연구에서 우리는 유연기판인 Mo foil 위에 제작된 유연 CZTS 태양전지를 지정된 곡률만큼 휘게 하는 bending test를 진행하였다. 태양전지에 압축응력이 가해지는 inner benidng과 인장응력이 가해지는 outer bending의 방향에서 실험은 진행되었으며, 50 mmR의 곡률 반경으로 진행된 1,000 회의 굽힘 횟수 동안 태양전지의 효율은 최고 12.7%까지 감소하였으며, 두 방향 모두에서 효율 감소의 가장 큰 원인은 병렬저항의 큰 감소로 나타났다.