• Title/Summary/Keyword: Passive Current Density

Search Result 124, Processing Time 0.031 seconds

Effects of Sulfuric Acid Concentration and Alloying Elements on the Corrosion Resistance of Cu-bearing low Alloy Steels

  • Kim, Ki Tae;Kim, Young Sik
    • Corrosion Science and Technology
    • /
    • v.17 no.4
    • /
    • pp.154-165
    • /
    • 2018
  • During the process of sulfur dioxide removal, flue gas desulfurization equipment provides a serious internal corrosion environment in creating sulfuric acid dew point corrosion. Therefore, the utilities must use the excellent corrosion resistance of steel desulfurization facilities in the atmosphere. Until now, the trend in developing anti-sulfuric acid steels was essentially the addition of Cu, in order to improve the corrosion resistance. The experimental alloy used in this study is Fe-0.03C-1.0Mn-0.3Si-0.15Ni-0.31Cu alloys to which Ru, Zn and Ta were added. In order to investigate the effect of $H_2SO_4$ concentration and the alloying elements, chemical and electrochemical corrosion tests were performed. In a low concentration of $H_2SO_4$ solution, the major factor affecting the corrosion rate of low alloy steels was the exchange current density for $H^+/H_2$ reaction, while in a high concentration of $H_2SO_4$ solution, the major factors were the thin and dense passive film and resulting passivation behavior. The alloying elements reducing the exchange current density in low concentration of $H_2SO_4$, and the alloying elements decreasing the passive current density in high concentration of $H_2SO_4$, together play an important role in determining the corrosion rate of Cu-bearing low alloy steels in a wide range of $H_2SO_4$ solution.

Transdermal Delivery of Ketoprofen and the Effect of Electroosmosis (케토프로펜의 경피전달 및 전기삼투압의 영향)

  • Oh, Seaung-Youl
    • Journal of Pharmaceutical Investigation
    • /
    • v.34 no.6
    • /
    • pp.491-497
    • /
    • 2004
  • We investigated some important factors which affect the transdermal flux of ketoprofen, a nonsteroidal anti-inflammatory agent, as a first step to provide some basic knowledge for the development of a iontophoretic transdermal patch system. Factors such as current density, polarity, buffer (HEPES) and electrolyte concentration and pH were studied using hairless mouse skin. The effect of poly(L-lysin), which is known to affect the electro-osmotic flow through skin, on flux was also studied. Passive flux was about $20\;{\mu}g/cm^2hr$ at pH 4.0, but was negligible at pH 7.4 where all ketoprofen molecules dissolved are ionized (ketoprofen pKa=5.94). At pH 4.0, application of anodal current increased the flux further above the passive level, however anodal flux at pH 7.4 was much smaller than passive flux at pH 4.0. The application of cathodal current at pH 4.0 increased the average flux to $30-40\;{\mu}g/cm^2hr$, depending on the current density applied. At pH 7.4, cathodal flux was only about $5\;{\mu}g/cm^2hr$. Decrease in buffer and electrolyte concentration increased this cathodal flux about 10 fold. However decrease in HEPES buffer concentration 100 fold did not affect the flux. Anodal flux of acetaminophen was much larger than cathodal flux, indicating that electroosmotic flow can be playing an important role in the flux. Poly(L-lysin) increased the cathodal flux at pH 7.4. These results provide some important insights into the mechanism of transdermal flux of ketoprofen and the role of electroosmotic flow.

Study on the new development of combined electrochemical processes using pulse current (마이크로 펄스 전해 복합가공에 관한 연구)

  • 박정우;이은상;문영훈
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2002.05a
    • /
    • pp.918-921
    • /
    • 2002
  • Some investigators who have tried to achieve the highly smooth surface finish using electrochemical processes have reported that high current density produced lustrous surfaces while the opposite conditions produced a passive layer and had a tendency to produce a black surface. However, processing at a low current density may produce a non-lustrous surface but the improvement of dimensional accuracy of the surface is significant. The surface with pulse process was a bit more lustrous than with continuous current but the black passive layer still could be found at grooved surface. There are two ways to achieve highly smooth surface finish. One is brushing it with a brush the other is electrochemical machining (ECM) with high current. The former method is the most common polishing practice, but not only may the surface obtained differ from operator to operator, but precision smooth surface on micro grooves are difficult to obtain. The latter one recently has been used to produce a highly smooth surface after EDM process. However, the material removal rate in ECM with high current is relatively high. Hence the original shape of the micro grooves, which was formed by electrochemical micro-machining (EMM) process, may be destroyed. In this study, an electrochemical polishing process using pulse current is adopted as a possible alternative process when micro grooves formed by EMM process should be polished. Mirror-like micro grooves with lustrous and smooth surface can be produced electrochemically with pulse current because the voltage and current used can be lower than the case of continuous current. This study will discuss the accurate control of physical and electrical conditions so as to achieve mirror-like micro grooves with lustrous and smooth surface without destroying the original shape of micro grooves.

  • PDF

Effects of Alloying Elements on the Surface Characteristics of Fe-38Al Intermetallic Compounds (Fe-38 at.% Al계 금속간화합물의 표면특성에 미치는 합금원소의 영향)

  • 최한철
    • Journal of the Korean institute of surface engineering
    • /
    • v.37 no.2
    • /
    • pp.128-136
    • /
    • 2004
  • Effects of alloying elements on the surface characteristics of Fe-38Al intermetallic compounds were investigated using potentiostat. The specimens were casted by the vacuum arc melting. The subsequent homogenization and the stabilization led to the homogeneous DO$_3$ structure of the specimen. After the corrosion tests, the surface of the tested specimen was observed by the optical microscopy and scanning electron microscopy(SEM). For Fe-38 at.% Al intermetallic compound, the addition of Cr and Mo proved to be beneficial in decreasing the grain boundary attack by decreasing the active current density. Addition of Band Nb resulted in a higher active current density and also a higher passive current density. These results indicated the role of Cr and Mo in improving the pitting corrosion resistance of Fe-38 at.%Al intermetallic compound. Band Nb addition to Fe-38 at.%Al accelerated the granular corrosion. Fe-38 at.%Al containing Cr and Mo showed remarkably improved pitting corrosion resistance in comparison with Band Nb addition to Fe-38 at. %Al.

Comparison with Polarization Characteristic of Polymers

  • Choi, Chil-Nam;Yabg, Hyo-Kyung
    • Proceedings of the Korean Environmental Sciences Society Conference
    • /
    • 2001.11a
    • /
    • pp.188-190
    • /
    • 2001
  • We carried out to measure the variations of potential with current density polymers. The results were particularly examined to identify the influences on corrosion potential and corrosion rate of various factors including temperature and pH. The Tafel slope for anodic dissolution was determined by the polarization effect depending on these conditions. The optimum conditions were established for each case. The second anodic current density peak and maximum passive current density were designated as the relative corrosion sensitivity($I_{r}I_{f}$). The mass transfer coefficient value (${\alpha}$) was determined with the Tafel slope for anodic dissolution based on the polarization effect with optimum conditions.

  • PDF

A Study on the Flow-Accelerated Corrosion Characteristics of Galvanically Coupled Dissimilar Metals. (이종금속 연결에 따른 침부식(FAC) 특성에 관한 연구)

  • Kim, Jung-Gu
    • Proceedings of the KIEE Conference
    • /
    • 2000.11a
    • /
    • pp.269-272
    • /
    • 2000
  • The flow accelerated galvanic corrosion characteristics of a carbon steel coupled to stainless steel were investigated in deaerated alkaline-chloride solutions as a function of flow velocities(0, 0.2, 0.4 and 0.6 m/s), pH(8, 9, and 10) and temperature(25, 50 and $75^{\circ}C$). The electrochemical properties of specimens were investigated by potentiodynamic test and galvanic corrosion test using RCE(Rotating Cylinder Electrode). Carbon steel did not show passive behavior in the alkaline-chloride solution. The galvanic current density increases with increasing flow velocity and temperature, but decreased with increasing pH. Flow velocity had a small effect on the galvanic current density at $25^{\circ}C$, whereas the flow velocity increased galvanic current density significantly at $50^{\circ}C$ and $75^{\circ}C$. This might be due to the increased solubility of magnetite at the higher temperature.

  • PDF

A Study on the IR Drop in Crevice of AISI 304 Stainless Steel by Temperature Variation (온도변화에 따른 AISI 304SS의 틈내 전위강하에 관한 연구)

  • 나은영
    • Journal of Advanced Marine Engineering and Technology
    • /
    • v.27 no.7
    • /
    • pp.872-878
    • /
    • 2003
  • As the results of recent industrial development, many industrial plants and marine structures are exposed to severe corrosion environment than before. Especially, under the wet environment, crevice corrosion damage problems necessarily occur and encourage many interests to prevent them. In this study, the electrochemical polarization test was carried out to study characteristics of crevice corrosion for AISI 304 stainless steel in various solution temperatures. The results are as follows ; 1) as the solution temperature increased in IN $\textrm{H}_2\textrm{SO}_4$, the passive current density and critical current density were increased, whereas corrosion potential and break down potential were nearly constant, 2) as the solution temperature increased. the induced time for initiation of crevice corrosion was shortened. 3) The potential range in the crevice was -220mV/SCE to -380mV/SCE according to the distance from the crevice opening, which is lower than that of external surface of -200mV/SCE.

Corrosion Characteristics of Amorphous Alloy Ribbon ($Fe_{70}Cr_5Si_{10}B_{15}$ and $Co_{70}Cr_5Si_{10}B_{15}$) in Hydrochloric Acid Aqueous Solution

  • Choi, Chil-Nam;Hyo, Kyung-Yang;Yang, Myung-Sun
    • Proceedings of the Korean Environmental Sciences Society Conference
    • /
    • 2001.05a
    • /
    • pp.236-237
    • /
    • 2001
  • In this study, experiments were carried out to measure the variations in the corrosion potential and current density of polarization curves with amorphous $Fe_{70}Cr_5Si_{10}B_{15}$ and $Co_{70}Cr_5Si_{10}B_{15}$ alloy ribbon. The results were particularly examined to identify the influences of corrosion potential including various conditions such as hydrochloric acid, temperature, salt, pH, and oxygen. The optimum conditions were established with variations including temperature, salt, pH, oxygen, corrosion rate, and resistance of corrosion potential. The mass tranfer coefficient(${\alpha}$) value was determined with the Tafel's slope for the anodic dissolution based on the polarization effect with optimum conditions. The second anodic current density peak and maximum passive current density were designated as the critical corrosion sensitivity($I_{r}/I_{f}$).

  • PDF

Iontophoretic Delivery of Vitamine C 2-Phosphate (이온토포레시스를 이용한 2-인산 비타민 C의 피부투과)

  • Kim, Su-Youn;Oh, Seaung-Youl
    • Journal of Pharmaceutical Investigation
    • /
    • v.34 no.3
    • /
    • pp.201-207
    • /
    • 2004
  • In order to develop an optimum formulation for iontophoretic flux of vitamine C 2-phosphate (VCP), we have prepared three different hydrogels containing VCP, using carbopol, HPMC and poloxamer, and iontophoretic flux through hairless mouse skin from these hydrogels was carried out. Drug stability in phosphate buffer (PBS) solution (pH 7.4) with and without current application was studied. The effect of various factors, such as drug concentration, current density, and current profile on skin flux was also investigated. Stability study indicated that VCP in PBS (pH 7.4) solution was stable under the experimental condition, irrespective of the presence of current. Cathodal delivery increased the flux markedly, whereas the anodal and passive flux was negligible. Thus, cathodal delivery was used in all experiments. Flux increased as the drug concentration (2.5, 5.0, 7.5%) and current density $(0.2,\;0.4,\;0.6\;mA/cm^2)$ increased. Pulsed application of the current showed lower flux than constant current application. The results obtained suggest that VCP can be delivered into the skin and the amount delivered can be controlled by varying hydrogel, current density, drug concentration and current application profile.

Orientation Dependent Directed Etching of Aluminum

  • Lee, Dong Nyung;Seo, Jong Hyun
    • Corrosion Science and Technology
    • /
    • v.8 no.3
    • /
    • pp.93-102
    • /
    • 2009
  • The direct-current electroetching of high purity aluminum in hot aqueous-chloride solution produces a high density of micrometer-wide tunnels whose walls are made up of the {100} planes and penetrate aluminum in the <100> directions at rates of micrometer per second. In the process of the alternating-current pitting of aluminum, cathodic polarization plays an important role in the nucleation and growth of the pits during the subsequent polarization. The direct-current tunnel etching and alternating-current etching of aluminum are basically related to the formation of poorly crystallized or amorphous passive films. If the passive film forms on the wall, a natural misfit exists between the film and the aluminum substrate, which in turn gives rise to stress in both the film and the substrate. Even though the amorphous films do not have directed properties, their stresses are influenced by the substrate orientation. The films on elastically soft substrate are likely to be less stressed and more stable than those on elastically hard substrate. The hardest and softest planes of aluminum are the {111} and {100} planes, respectively. Therefore, the films on the {111} substrates are most likely to be attacked, and those on the {100} substrates are least likely to be attacked. For the tunnel etching, it follows that the tunnel walls tend to consist of the {100} planes. Meanwhile, the tunnel tip, where active corrosion takes place, tend to be made of four closely packed {111} planes in order to minimize the surface energy, which gives rise to the <100> tunnel etching.