2004
In this study, in order to develop the low temperature sintering ceramics for ultrasonic vibrator, Pb(Sb$\_$$\frac{1}{2}$/Nb$\_$$\frac{1}{2}$/) O$_3$-Pb(Ni$\_$1/3/Nb$\_$2/3/)O$_3$-Pb(Zr$\_$0.48/Ti$\_$0.52/)O$_3$ ceramics were manufactured as a function of the amount of CuO addition, and their dielectric and piezoelectric characteristics were investigated. With increasing CuO addition, the grain size and density increased up to 0.3 wt% CuO addition. Taking into consideration electromechanical coupling factor(k$\_$p/) of 0.53, mechanical quality factor(Q$\_$m/) of 423, dielectric constant($\varepsilon$$\_$r/) of 1,759 and piezoelectric constant(d$\_$33/) of 362pC/N, it could be concluded that 0.5 wt% CuO added composition ceramic sintered at 920$^{\circ}C$ was suitable for ultrasonic vibrator application.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.24
no.5
/
pp.416-421
/
2011
Nowadays, the increasing demands upon mobile devices such as wireless sensor networks and the recent advent of low power electrical devices such as MEMS make such renewable power sources attractive. A vibration-driven MEMS lead zirconate titanate $Pb(Zr,Ti)O_3$ (PZT) cantilever device is developed for energy harvesting application. This paper presents a piezoelectric based energy harvester which is suitable for power generating from conventional vibration and has in providing energy for low power electron ic devices. The PZT cantilever is used d33 mode to get the electrical power. The PZT cantilever based energy harvester with the dimension of 7 mm${\times}$3 mm${\times}$0.03 mm is fabricated using micromachining technologies. This PZT cantilever has the mechanical resonance frequency with a 900 Hz. With these conditions, we get experimentally the 37 uW output power from this device with the application of 1g acceleration using the 900 Hz vibration. From this study, we show the feasibility of one of energy harvesting candidates using PZT based structure. This PZT energy harvester could be used for various applications such a batteryless micro sensors and micro power generators.
The Transactions of the Korean Institute of Electrical Engineers C
/
v.55
no.9
/
pp.429-433
/
2006
PZT(80/0) powder was prepared by a sol-gel method and PZT thick films were fabricated by the screen-printing method on the alumina substrates. The coating and drying procedure was repeated 4 times. And then the PZT(20/80) precusor solution was spin-coated on the PZT thick films. A concentration of a coating solution was 0.5mol/L and the number of coating was varied from 0 to 6. The porosity decreased and the grain size increased with increasing the number of coatings. The thickness of the PZT-6(6: number of coatings) films was about $60{\mu}m$. The relative dielectric constant increased and the dielectric loss decreased with increasing the number of PZT(20/80) sol coatings. The relative dielectric constant and dielectric loss of the PZT-6 thick film were 275 and 3.5%, respectively. The remanent polarization, coercive field and breakdown strength of the PZT-6 film were $19.8{\mu}C/cm^2$, 13.7kV/cm and 130kV/cm, respectively.
Pb(Zr,Ti)$O_3$ (PZT) based ceramics with superior piezoelectric properties have been extensively used in various domestic and industrial appliances. However, PZT ceramics causing environmental contamination and health problems need to be eventually replaced by any of Pb-free materials. $(Na_{0.53}K_{0.47})(Nb_{1-x}Ta_x)O_3$ (NKNT), one of Pb-free piezoelectric ceramics, has long been known but its properties are not fully understood and developed. In this study, dielectric and piezoelectric properties of Pb-free NKNT ceramics were studied with Ta substitution for B-site at x = 0~0.6. It was found that polymorphic phase transition (PPT) between orthorhombic and tetragonal phases was notably influenced by Ta substitution. The highest piezoelectric coefficient ($d_{33}$) of 284 pC/N was occurred at x = 0.45.
Journal of the Korean Institute of Electrical and Electronic Material Engineers
/
v.25
no.4
/
pp.286-289
/
2012
In this paper, we have proposed piezoelectric energy harvester employing the pillar structure with the diameter size of 500 um. So we have selected the Su-8 photo-resist and modified lithography process to manufacture the pillar structure with height above the $500{\mu}m$. Simultaneously, we tried to make a comparative study to use ceramic bulk - polymer structure In this paper, we will report the process and properties of micro pillar structure based on the PMN-PZT ($Pb(Mg_{1/3}Nb_{2/3})O_3-PbZrTiO_3$) materials. Finally, We will propose a method for generating electrical energy with a piezoelectric element using vibration, an energy source can be obtained from the "clean" energy.
Jo, Seo-Hyeon;Nam, Sung-Pil;Lee, Sung-Gap;Lee, Seung-Hwan;Lee, Young-Hie;Kim, Young-Gon
Transactions on Electrical and Electronic Materials
/
v.12
no.5
/
pp.193-196
/
2011
Lead zirconate titanate (PZT)/ bismuth ferrite (BFO) multilayer thin films have been fabricated by the spin-coating method on Pt(200 nm)/Ti(10 nm)/$SiO_2$(100 nm)/p-Si(100) substrates using $BiFeO_3$ and $Pb(Zr_{0.52}Ti_{0.48})O_3$ metal alkoxide solutions. The PZT/BFO multilayer thin films show a uniform and void-free grain structure, and the grain size is smaller than that of PZT single films. The reason for this is assumed to be that the lower BFO layers play an important role as a nucleation site or seed layer for the formation of homogeneous and uniform upper PZT layers. The dielectric constant and dielectric losses decreased with increasing number of coatings, and the six-layer PZT/BFO thin film has good properties of 162 (dielectric constant) and 0.017 (dielectric losses) at 1 kHz. The remnant polarization and coercive field of three-layer PZT/BFO thin films were 13.86 ${\mu}C/cm^2$ and 37 kV/cm respectively.
This paper was to measure the structure, piezoelectric properties of $0.03Pb(Mg_{0.5}W_{0.5})O_3$ - $0.12Pb(Sb_{0.5}Nb_{0.5})O_3$ - $0.85Pb(Zr_{0.52}Ti_{0.48})O_3$ + $0.5[wt%]MnO_2$ ceramics dropped with additive CuO after manufacturing the specimens with a general method. It is shown that X-ray diffraction pattern variation of lines (211) have tendency to move minutely by addition of additive CuO. According to dropping with Cu, the dielectric constant at 20[$^{\circ}C$] reduced to CuO 3.0[wt%]. In case of sintering at 1050[$^{\circ}C$], dielectric constant was maximum value 623.59 at CuO 1.0[wt%]. Dielectric loss was maximum value 2.7[%] at Cu 2.0[wt%] in case of sintering at 1050[$^{\circ}C$].
Transactions on Electrical and Electronic Materials
/
v.2
no.3
/
pp.18-23
/
2001
For the piezoelectric transformer application, Pb(Sb$\_$1/2/ Nb$\_$1/2/)O$_3$-Pb(Zr,Ti)O$_3$ ceramics were produced by attrition milling. Microstructural, dielectric and piezoelectric characteristics of the ceramics were investigated as a function of milling time. The particle size and grain size decreased while dielectric constant, density and mechanical quality factor (Q$\_$m/) increased with milling time. Temperature coefficient of resonant frequency (TCf$\_$r/) was shifted to positive side with increasing milling time. The attrition milling process proved to be one of the effective routes to produce transformers for high power application.
Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
/
2002.07b
/
pp.746-748
/
2002
The effect of $MnO_2$ addition in $0.05Pb(Sn_{0.5}Sb_{0.5})O_3-0.8PbZrO_3-0.15PbTiO_3$(0.05PSS-0.8PZ-0.15PT) ceramics on crystal structure and electrical properties were studied. The sintering temperature and time were $1230^{\circ}C{\sim}1270^{\circ}C$ and 2hr, respectively. Then crystal structure, dielectric and pyroelectric properties were investigated. All the poled specimens showed the lower dielectric constant and $tan{\delta}$ than the unpoled specimens. Dielectric constant at 1kHz of the 0.05PSS-0.8PZ-0.15PT(MnO2 0.3wt%) system specimen sintered at $1250^{\circ}C$ for 2hr were 270 and showed the lowest $tan{\delta}$ of 0.2% after poling of $2kV_{DC}/mm$ at $150^{\circ}C$ for 30 minutes. Pyroelectric coefficient was maximum value of $50nC/cm^2K$ and Curie temperature was $224^{\circ}C$.
Journal of the Korean institute of surface engineering
/
v.31
no.4
/
pp.209-216
/
1998
It is well knownthat electroledd plating is the desirable surface treatment method which is being widely used to all kinds of material such as requiring corrosing resistance, wear resistance and conductivity, especially nonconductivity materials' surface plating. However, it is suggested that there are some problems that must be solved, for exaple, rate of plating, corrosion resistance, thickness of plating film etc. Therefore in this paper, when electroless nickel plating was performed on the PZT(Pb(Zr,Ti))with varying of solution composition such as NaOH, and $H_2NCH_2COOH$, the effect of the rate of plating and corrosion resistance were investigated.
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.