• Title/Summary/Keyword: PP Specimen

Search Result 54, Processing Time 0.026 seconds

Measurement of Loss Factor and Young's Modulus of ABS and PP Specimens by Using a Speaker (스피커를 이용한 ABS와 PP의 손실계수 및 영률 측정)

  • Jeon, Byeong Su;Jung, Sung Soo;Lee, Jong Kyu
    • Transactions of the Korean Society for Noise and Vibration Engineering
    • /
    • v.24 no.9
    • /
    • pp.724-730
    • /
    • 2014
  • It is essential to control noise and vibration in various industrial fields. In the automobile industry, various plastics have been developed and replaced metallic materials in order to reduce mass and vibration effectively. In this study, we measured and analyzed the Young's moduli and the loss factors of Acrylonitrile butadiene styrene(ABS) and Polypropylene(PP). In order to solve the fundamental error to determine the two quantities, a loudspeaker was used instead of conventional electromagnetic devices to generate bending motion to the specimens and a laser vibrometer was also used in detection of vibration signal of the specimen. The measured Young's moduli and loss factors of the ABS specimen were nearly constant as the temperature($-10{\sim}60^{\circ}C$) was increased. The loss factor of PP specimen showed peak value at $20^{\circ}C$ and it means that there is glass transition for the PP specimen. Young's modulus of PP specimen was linearly decreased as the temperature was increased.

Spatting and Fire Enduring Properties of High Strength RC Column Subjected to Axial Load Depending on Fiber Contents (중심 축하중을 받는 고강도 RC기둥의 섬유 혼입량에 따른 폭열 및 내화 성상)

  • Han, Cheon-Goo;Hwang, Yin-Seong;Lee, Jae-Sam;Kim, Kyoung-Min
    • Journal of the Korea Concrete Institute
    • /
    • v.18 no.1 s.91
    • /
    • pp.83-90
    • /
    • 2006
  • This paper investigates experimentally the fire resistance performance and spatting resistance of high performance reinforced concrete column member subjected to fire containing polypropylene fiber(PP fiber) and cellulose fiber(CL fiber). An increase in PP fiber and CL fiber contents, respectively resulted in a reduction of fluidity due to fiber ball effect. Air content is constant with m increase in fiber content. Compressive strength reached beyond 50 MPa. Based on fire resistance test, severe failure occurred with control concrete specimen, which caused exposure of reinforcing bar. No spall occurred with specimen containing PP fiber. This is due to the discharge of internal vapour pressure. Use of CL fiber superior to control concrete in the side of spatting resistance, localized failure at comer of specimen was observed. Corner of specimen had deeper neutralization than surface of specimen. Specimen containing PP fiber had the least damaged area due to spatting. Neutralization depth ranged between 6 and 8 mm Residual compressive strength of specimen containing PP fiber maintained 40%, which is larger than control concrete with 20% of residual strength. Specimen containing CL fiber had 25% or residual strength.

Evaluation on Spalling Properties of Specimen Size with PP Fiber and Fireproof Coating

  • Kim, Gyu-Yong;Min, Choong-Siek;Lee, Tae-Gyu;Miyauchi, Hiroyuki;Park, Gyu-Yeon;Lee, Gwang-Jun
    • Journal of the Korea Institute of Building Construction
    • /
    • v.11 no.4
    • /
    • pp.353-362
    • /
    • 2011
  • High Strength Concrete (HSC) has weakness that in a fire, it is spalled and brittles. The phenomenon of spalling is made by water vapor's being confined in watertight concrete. This study is aimed to evaluate explosive spalling properties of high strength concrete with ${\square}100{\times}100{\times}200$ mm specimen and ${\square}400{\times}400{\times}1500$ mm column. To prevent spalling of concrete, fireproof coating and PP fiber are used. As a result, ${\square}400{\times}400{\times}1500$ mm column was prevented spalling likes ${\times}100{\times}100{\times}200$ mm specimen. When concrete protected failure to explosive spalling, quantity heat ratio (which fireproof coating specimen to pp fiber mixed specimen) between ${\square}100{\times}100{\times}200$ mm and ${\square}400{\times}400{\times}1500$ mm was maximum value at 20 minute, but difference of quantity heat ratio decreased and quantity heat ratio of each specimen is almost same at 30 minute.

Evaluation on Spalling Properties of Polypropylene Fiber reinforced Concrete by Restrained Ring-type Test (구속 링형 시험에 의한 PP섬유 혼입 콘크리트의 폭렬 특성 평가)

  • Han, Cherl-Hwan;Kim, Gyu-Yong;Yoon, Min-Ho;Hwang, Eui-Chul;Baek, Jae-Uk;Nam, Jeong-Soo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2017.11a
    • /
    • pp.124-125
    • /
    • 2017
  • In this study, the spalling properties of Polypropylene reinforced concrete were evaluated by the restrained ring-type test. As a result of the experiment with the fiber mixture ratio set at 0, 0.15 vol.%, The PP fiber reinforced specimen showed lower water vapor pressure as a whole than the Plain specimen, but the restraint stress was measured to be higher. This is thought to be due to the fact that higher thermal stresses were applied in the PP fiber reinforced test specimen.

  • PDF

Combustion Properties of Ethylene-propylene diene monomer/polypropylene/Clay Nanocomposites Based on EDPM/PP (EPDM/PP에 바탕을 둔 에칠렌-프로필렌 디엔 모노머/폴리프로필렌/클레이 나노복합체의 연소특성)

  • Chung, Yeong-Jin
    • Journal of the Korean Applied Science and Technology
    • /
    • v.28 no.4
    • /
    • pp.410-417
    • /
    • 2011
  • Effects of ethylene-propylene diene monomer (EPDM)/polypropylene (PP), zinc oxide, stearic acid, and clay on the combustive properties based on EDPM/PP were investigated. The EDPM/PP/clay nanocomposites was compounded to prepare specimen for combustive analysis by cone calorimeter (ISO 5660-1). It was found that the specific mass loss rate (SMLR) in the nanocomposites decreased due to the fire resistance compared with unfilled EDPM/PP, while the nanocomposites showed the higher total heat release (THR), higher CO production release, and higher specific extinction area (SEA) than those of virgin EPDM/PP. The stearic acid for softening ruber increased the THR and amount of smoke by itself, combustible.

A study on deformation and strength of polymer composites using automobiles (자동차용 폴리머 복합재료의 변형과 강도에 관한 연구)

  • Shin, Je-Hoon;Lim, Jae-Kyoo;Park, Han-Ju
    • Proceedings of the KSME Conference
    • /
    • 2000.11a
    • /
    • pp.238-243
    • /
    • 2000
  • The effect of the temperature, the fatigue and the test speed on DEN(double edged notch) specimen which was made by the pp-rubber composites during fracture was stuied. DEN specimen was made on PP-rubber composites through the injection molding. With increasing temperature the fracture strength is linearly decrease and the fracture energy is first increase by $0^{\circ}C$ and after that decrease. In the same temperature the fracture strength during increasing the notch radius is hardly increase. The fracture behaviour at low and high test speed is different entirely. At high test speed plastic region is small and fracture behaviour was seen to brittle fracture tendency. The deformation mechanism of polypropylene-rubber composites during fracture was studied by SEM fractography. A strong plastic deformation of the matrix material ahead of the notch/crack occured. The deformation seem to be enhanced by a thermal blunting of the notch/crack.

  • PDF

Spalling Properties of High Performance Concrete Designed with the Various Types of Coarse Aggregate (굵은골재 종류 변화에 따른 고성능 콘크리트의 폭렬특성)

  • Heo, Young-Sun;Park, Yong-Kyu;Jin, Hu-Lin;Jee, Suk-Won;Yang, Seong-Hwan;Han, Cheon-Goo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2006.11a
    • /
    • pp.95-98
    • /
    • 2006
  • This study investigates spalling properties of high performance concrete, 60MPa clan, made with the various types of coarse aggregate and adding ratio of polypropylene(PP) fiber. As experimental parameters, totally sixteen specimens of ${\phi}100{\times}200mm$ in size are prepared: one specimen for control without fiber, ten specimens with different coarse aggregate types, along with 0.05, 0.1, 0.15 percent of PP fiber in each. 1 hour fire test is conducted and then spalling appearance, spalling degree and residual compressive strength are examined. In addition, sit specimens made with two types of coarse aggregate site, along with same adding ratio of fiber are supplementally done, and only spalling properties is examined. Test results showed that control concrete and most specimens containing 0.05% of PP fiber exhibited 4 to 3 level of spalling degree, resulting severe explosive spalling, except for the specimen using basalt aggregate(Bc) showing 2 to 3 level of that. Especially, the Bc specimen containing 0.1% of the fiber exhibited that residual compressive strength value was 32%, which is 10% higher than other specimens using limestone or granite. Spalling resistance performance was also effective as aggregate size increase.

  • PDF

A Study on the Dynamic Properties of Cement Mortar with Recycled PET Fiber (폐PET섬유를 혼입한 시멘트모르터의 역학적 특성에 관한 연구)

  • 김영근;김상철;김명훈
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2002.11a
    • /
    • pp.77-86
    • /
    • 2002
  • In this study we intended to investigate properties of cement mortar with recycled PET fiber, PE fiber, and PP fiber such as slump flow, compressive strength, tensile strength, and flexural strength. As results of experiment, several properties of specimen with recycled PET fiber were little low comparing those of specimen with PE fiber and PP fiber. But if we see from point of economy and recycle of industrial wastes, it has enough reason to be used. Compressive strength of specimen with recycled PET fiber at 56 days was about 10% higher, but tensile strength and flexural strength were lower than that of no-fiber.

  • PDF

A Study on the Dynamic Properties of Cement Mortar with Recycled PET Fiber (폐PET섬유를 혼입한 시멘트모르터의 역학적 특성에 관한 연구)

  • Kim, Young-geun;Kim, Sang-cheol;Kim, Myung-hoon
    • Journal of the Korea Institute of Building Construction
    • /
    • v.2 no.4
    • /
    • pp.113-122
    • /
    • 2002
  • In this study we intended to investigate properties of cement mortar with recycled PET fiber, PE fiber. and PP fiber such as slump flow, compressive strength, tensile strength, and flexural strength. At results of experiment. several properties of specimen with recycled PET fiber were little low comparing those of specimen with PE fiber and PP fiber. But if we see from point of economy and recycle of industrial wastes, it has enough reason to be used. Compressive strength of specimen with recycled PET fiber at 55 days was about 10% higher. but tensile strength and flexural strength were lower than that of no-fiber.

Fundamental Properties and Spalling Resistance of High Strength Concrete Containing Hybrid Organic fiber (복합유기섬유를 사용한 고강도 콘크리트의 기초특성 및 폭렬방지)

  • Pei, Chang-Chun;Han, Dong-Yeop;Lee, Jin-Woo;Han, Chang-Pyung;Yang, Seong-Hwan;Han, Cheon-Goo
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2006.11a
    • /
    • pp.745-748
    • /
    • 2006
  • This study investigates the fundamental properties and examines spalling appearances and residual compressive strength of high strength concrete containing hybrid organic fibers subjected to fire. Test showed that overall, an increase of fiber content decreased the fluidity of concrete, but specimens containing polyvinyl alcoho(PVA)+polypropylene(PP) fiber and nylon(NY)+PP fiber had improved flow. In addition, the air content of all specimens was properly ranged in target value, regardless of fiber content. As for the spalling properties when completed the fire test, control concrete exhibited spalling occurrence due to sudden elevated temperature. However, specimens containing more than 0.1 vol% of PP fiber prevented the spalling, while specimens containing PP+CL and PVA+PP fiber can protected from fire in more than 0.15vol% of the fiber content. Importantly, a specimen containing only 0.05vol% of NY+PP showed the favorable spalling resistance performance.

  • PDF