• 제목/요약/키워드: Output Characteristics of PV module

검색결과 83건 처리시간 0.034초

기계적 하중에 따른 스트레스로 인한 PV 모듈의 전기적 특성 (The Electrical Characteristics of PV Module by the Stress in accordance with Mechanical Weight Load)

  • 공지현;지양근;강기환;유권종;안형근;한득영
    • 한국태양에너지학회:학술대회논문집
    • /
    • 한국태양에너지학회 2009년도 추계학술발표대회 논문집
    • /
    • pp.104-109
    • /
    • 2009
  • If the Photovoltaic(PV) Module should get physical load, the PV module will be warped according to elongation of the front glass and then micro-crack will be occurred in the heat sealed Solar Cell. This micro-crack drops output of the short circuit current and the open circuit voltage of the PV Module. This is because of increase of resistance component by micro-crack. Micro-crack at specific Solar Cell in the module reduces the durability of PV Module such as less output, Hot-Spot in the PV module caused by Solar Cell output mismatch, heat generating as resistance component caused by micro-crack. In this study, among some factors which effect to the output of crystalline PV Module, we will see how the micro-crack caused by mechanical stress effects to the electrical output of PV Module.

  • PDF

단결정과 다결정 태양전지 모듈의 광학적 특성에 따른 전기적 출력 특성 분석 (Electrical Characteristics Analysis for single-crystalline and multi-crystalline PV module optical character.)

  • 이진섭;강기환;박지홍;유권종;안형근;한득영
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2008년도 제39회 하계학술대회
    • /
    • pp.1100-1101
    • /
    • 2008
  • After lamination process, Isc is increased by sheet reflection. This paper presents the electrical output characteristics by back sheet reflection. The experiments was conducted by using single crystalline and multi crystalline PV module. The reflection area of single crystalline PV module is larger than multi one due to the difference of solar cell manufacturing. The experiments show that the increased performance ratio of single crystalline PV module output power is 1.55% rather than that of multi crystalline PV module output power is 1.13%. In addition, it is expected that the output power of single one rather than multi-one is increased by the lower temperature when the PV module is installed outside. The results can be reconsidered by the test material and test process. Back sheet used for humidity prevention makes PV module output power increasing.

  • PDF

건물일체형 태양광발전시스템(BIPV)의 설치조건에 따른 발전특성 연구 (Power Performance Characteristics of Transparent Thin-film BIPV Module depending on an Installation Angle)

  • 안영섭;송종화;김석기;이성진;윤종호
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2008년도 춘계학술대회 논문집
    • /
    • pp.386-389
    • /
    • 2008
  • This study has analysed power output characteristics of transparent thin-film PV module depending on incidence angle and azimuth. The simulation results was evaluated power outputs of transparent thin-film PV module depending on incidence angle and azimuth after calibrating the experimental and computed data. As a result, the best power output performance of transparent thin-film PV module was obtained at slope of $30^{\circ}$ to the south, producing the annual power output of 977kWh/kWp. The annual power output data demonstrated that the PV module with a slope of $30^{\circ}$ could produce a 68 % higher power output than that with a slope of $90^{\circ}$, with respect to the inclined slope of the module. Furthermore, the PV module facing south showed a 22 % higher power output than that facing to the east in terms of the angle of the azimuth.

  • PDF

고출력 슁글드 태양광 모듈의 온도 저감에 따른 출력 특성 분석 (Analysis of Output Characteristics of High-Power Shingled Photovoltaic Module due to Temperature Reduction)

  • 배재성;유장원;지홍섭;이재형
    • 한국전기전자재료학회논문지
    • /
    • 제33권6호
    • /
    • pp.439-444
    • /
    • 2020
  • An increase in the temperature of photovoltaic (PV) modules causes reduced power output and shorter lifetime. Because of these characteristics, demands for the heat dissipation of PV modules are increasing. In this study, we attached a heat dissipation sheet to the back sheet of a shingled PV module and observed the temperature changes. The PV shingled module was tested under Standard Test Conditions (STCs; irradiance: 1,000 W/㎡, temperature: 25℃, air mass: 1.5) using a solar radiation tester, wherein the temperature of the PV module was measured by irradiating light for a certain duration. As a result, the temperature of the PV module with the heat dissipation sheet decreased by 3℃ compared to that without a heat dissipation sheet. This indicated that the power loss was caused by a temperature increase of the PV module. In addition, it was confirmed that the primary parameter contributing to the reduced PV module output power was the open circuit voltage (Voc).

건물일체형 투광성 PV모듈의 설치각도별 발전특성에 관한 연구 (Power Performance Characteristics of Transparent Thin-film BIPV Module depending on an installation angle)

  • 송종화;윤종호;안영섭;김석기;이성진;정연규
    • 한국태양에너지학회 논문집
    • /
    • 제28권2호
    • /
    • pp.58-63
    • /
    • 2008
  • This study has analysed power output characteristics of transparent thin-film PV module depending on incidence angle and azimuth. The experiment results showed power outputs of transparent thin-film PV module applied to full-scale mock up model on slope of $90^{\circ},\;30^{\circ},\;0^{\circ}$ to the south. The simulation results was evaluated power outputs of transparent thin-film PV module depending on incidence angle and azimuth after calibrating the experimental and computed data. As a result. the best power output performance of transparent thin-film PV module was obtained at slope of $30^{\circ}$ to the south, producing the annual power output of 977kWh/kWp. The annual power output data demonstrated that the PV module with a slope of $30^{\circ}$ could produce a 68 % higher power output than that with a slope of $90^{\circ}$ with respect to the inclined slope of the module, Furthermore, the PV module facing south showed a 22 % higher power output than that facing to the east in terms of the angle of the azimuth, Specipically. the varying power output with incidence angle of PV module can be resulted from the influence of incidence angle modifier of glass on PV module. That is, the solar energy transmission can be reduced as an increase of incidence angle of PV module. Therefore, when the inclined slope of the PV module was over $70^{\circ}$ there was a significant reduction of power output, and this was caused by the decrease of solar energy transmission in the transparent thin-film PV module.

태양전지 모듈의 설치방향에 따른 오염특성 분석 (Analysis of Soiling for the Installation Direction of PV Module)

  • 이충근;신우균;임종록;주영철;황혜미;고석환;장효식;강기환
    • 신재생에너지
    • /
    • 제16권4호
    • /
    • pp.76-82
    • /
    • 2020
  • Soiling on the surface of a PV module reduces the amount of light reaching the solar cells, decreasing power performance. The performance of the PV module is generally restored after contaminants on the module surface are washed away by rain, but it accumulates at the bottom of the module owing to the thickness of the module frame, causing an output mismatch on the PV module. Since PV modules are usually installed horizontally or vertically outdoors, soiling can occur at the bottom of the PV module, depending on the installation direction due to external environmental factors. This paper is analyzed the output characteristics of a PV module considering its installation direction and the soiling area. The soiling was simulated to use transparent films with 5% transmittance, and the transmission film was attached to the bottom part of the PV module horizontally and vertically. When the soiling area was 33% of the string at the bottom of the PV module, the power output decreased similarly regardless of installation direction. However, when the soiling area was 66% of the string at the bottom of the PV module, it was confirmed that the output performance decreased sharply when installed vertically rather than horizontally.

비정질 박막 투과형 태양전지모듈의 온도특성에 따른 발전성능 평가 연구 (A Study on the Evaluation of Power Performance according to Temperature Characteristics of Amorphous Transparent Thin-Film)

  • 안영섭;송종화;이성진;윤종호
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2009년도 춘계학술대회 논문집
    • /
    • pp.45-48
    • /
    • 2009
  • This study evaluated the influence of temperature on the PV module surface on power output characteristics, especially for an amorphous transparent thin-film PV module which was applied to a full-scale mock-up model as building integrated photovoltaic system. The tested mock-up consisted of various slopes of PV module, facing to the south. The annual average temperature of the module installed with the slope of $30^{\circ}$ revealed $43.1^{\circ}C$, resulting in $7^{\circ}C$ higher than that measured in PV modules with the slope of $0^{\circ}$and $90^{\circ}$ did. This $30^{\circ}$ inclined PV module also showed the highest power output of 28.5W (measured at 2 PM) than other two modules having the power output of 20.4W and 14.9W in the same time for $0^{\circ}$ and $90^{\circ}$ in the slope, respectively. In case of the $30^{\circ}$ inclined PV module, it exhibited very uniform distribution of power output generation even under the higher temperature on the module surface. Consequently, the surface temperature of the PV module analyzed in this study resulted in 0.22% reduction in power output in every $1^{\circ}C$ increase of the module surface temperature.

  • PDF

기계적 스트레스에 의한 태양전지모듈의 전기적 특성변화 (The Variation of Electrical Characteristics of PV Module due to Mechanical Stress)

  • 공지현;지양근;강기환;김경수;유권종;안형근;한득영
    • 신재생에너지
    • /
    • 제6권1호
    • /
    • pp.38-45
    • /
    • 2010
  • Abstract Under the physical stress on photovoltaic (PV) module, it will be warped according to elongation of the front glass and then micro-crack will be occurred in the thermally sealed solar cell. This micro-crack leads to drop of short circuit current of the PV module. This is because of increase of resistance component by micro-crack. Micro-crack at specific solar cell in the module lessens the durability of PV module with reduced output, hot-spot caused by solar cell output mismatch and increased resistance component. This study shows the relation between electrical characteristics and micro- cracks due to mechanical stress on PV module.

태양전지 셀의 고온에 의한 전기적 특성 변화 연구 (A study of the electrical characteristics changes of PV cell at high temperature)

  • 정태희;신준오;김태범;강기환;안형근;한득영
    • 한국신재생에너지학회:학술대회논문집
    • /
    • 한국신재생에너지학회 2009년도 추계학술대회 논문집
    • /
    • pp.387-389
    • /
    • 2009
  • PV module is manufactured by several steps such as cell sort, tabbing & string, lay-up, lamination processes. In oder to manufacture PV module, solar cell must be placed in high temperature. Soldering Process in high temperature is important because it directly influences electric output performance changes of solar cell in solar cell module. We consider applying momentary high temperature, while soldering solar cell, and expect change electric characteristics of PV module. In this paper, we measure electric output characteristics of solar cells after those are applied with high temperature changes for two seconds. From these results, we confirm with application of high temperature, $I_{sc}$ increase and $V_{oc}$ slightly decreases.

  • PDF

PV모듈 제조공정에서 Interconnection에 따른 전기적 손실 특성 분석 (The Analysis of electrical loss characteristics by interconnection during PV module fabrication process)

  • 이진섭;강기환;박지홍;유권종;안형근;한득영
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2007년도 제38회 하계학술대회
    • /
    • pp.216-217
    • /
    • 2007
  • In this study, we analyzed the electrical loss characteristics between ribbon and output terminal of constituent material according to electrical resistance during interconnection process of PV module. From this result, the electrical output power reduction rate caused by interaction between ribbon and cell's interconnection was 2.88%. There was 1W electrical output power reduction through the 16 solar cells. So it is expected that the wider size of PV module gives the higher loss in electricity production. Also, the average output power of PV module passed lamination process was increased by 0.081W per one solar cell and the increase rate was 3.7%.PV module's electrical loss before and after lamination process according to constituent material's terminal was 0.49W and 0.50W, respectively.

  • PDF