• Title/Summary/Keyword: Opening mode stress intensity factor

Search Result 42, Processing Time 0.026 seconds

Fatigue Crack Propagation Behavior in STS304 Under Mixed-Mode Loading

  • Lee, Jeong-Moo;Song, Sam-Hong
    • Journal of Mechanical Science and Technology
    • /
    • v.17 no.6
    • /
    • pp.796-804
    • /
    • 2003
  • The use of fracture mechanics has traditionally concentrated on crack growth under an opening mechanism. However, many service failures occur from cracks subjected to mixed-mode loading. Hence, it is necessary to evaluate the fatigue behavior under mixed-mode loading. Under mixed-mode loading, not only the fatigue crack propagation rate is of importance, but also the crack propagation direction. In modified range 0.3$\leq$a/W$\leq$0.5, the stress intensity factors (SIFs) of mode I and mode II for the compact tension shear (CTS) specimen were calculated by using elastic finite element analysis. The propagation behavior of the fatigue cracks of cold rolled stainless steels (STS304) under mixed-mode conditions was evaluated by using K$\_$I/ and $_{4}$ (SIFs of mode I and mode II). The maximum tangential stress (MTS) criterion and stress intensity factor were applied to predict the crack propagation direction and the propagation behavior of fatigue cracks.

KI Criteria of Surface Check under Stepwise Loadings of Drying Stresses

  • Park, Jung-Hwan
    • Journal of the Korean Wood Science and Technology
    • /
    • v.27 no.4
    • /
    • pp.51-56
    • /
    • 1999
  • Finite element method was utilized to analyze crack tip stress and displacement field under drying stress case as stepwise loading. Opening mode of single-edge-notched model was employed and analyzed by linear elastic fracture mechanics of plane stress case. The drying stresses were applied as stepwise loads at the boundary elements of the model with 10 steps of time serial. The stress intensity factor($K_I$) for opening mode reached to its maximum just prior to the stress reversal. The $K_I$ from the displacement fields revealed 1.7 times higher than those from stress fields. By comparing the two sets of $K_I$ from displacement and stress fields, single parameter $K_I$ showed its validity to characterize displacement fields around the crack tip front while stress field could not be characterized due to large variations between two sets of data.

  • PDF

Determination of Stress Intensity Factor $K_I$ from Two Fringe Orders by Fringe Multiplication and Sharpening

  • Chen, Lei;Baek, Tae-Hyun
    • Journal of the Korean Society for Nondestructive Testing
    • /
    • v.27 no.6
    • /
    • pp.550-555
    • /
    • 2007
  • Stress intensity factor is one of the most important parameters in fracture mechanics. Both the stress field distribution and the crack propagation are closely related to these parameters. Due to the complexity of actual engineering problems, it is difficult to calculate the stress intensity factor by theoretical formulation, so photoelasticity method is a good choice. In this paper, modified two parameter method is employed to calculate stress intensity factor for opening mode by using data from more than one photoelastic fringe loop. For getting accurate experiment results, the initial fringes are doubled and sharpened by digital image programs from the fringe patterns obtained by a CCD camera. Photoelastic results are compared with those obtained by the use of empirical equation and FEM. Good agreement shows that the methods utilized in experiments are considerably reliable. The photoelastic experiment can be used for bench mark in theoretical study and other experiments.

Behaviour of Fatigue Crack Propagation under Mixed Mode(I+II) with variation of Angle and Crack Length (혼합모드(I+II)하에서 각도와 균열길이 변화를 갖는 피로균열 전파 거동)

  • 정의효
    • Journal of the Korean Society of Manufacturing Technology Engineers
    • /
    • v.9 no.5
    • /
    • pp.73-79
    • /
    • 2000
  • The applications of fracture mechanics have traditionally concentrated on cracks loaded by tensile stresses, and growing under an opening or mode I mechanism. However, many cases of failures occur from growth of cracks subjected to mixed mode loading. Several criteria have been proposed regarding the crack growth direction under mixed mode loadings. This paper is aimed at investigation of fatigue crack growth behaviour under mixed mode(I+II) with variation of angle and pre-crack length in two dimensional branched type precrack. Especially the direction of fatigue crack propagation was predicted and effective stress intensity factor was calculated by finite element analysis(FEA. In this paper, the maximum tangential stress(MTS) criterion was used to predict crack growth direction. Not only experiment but also finite element analysis was carried out and the theoretical predictions were compared with experimental results.

  • PDF

Fatigue Crack Propagation Behavior in STS304 under Mixed Mode Loading (혼합모드 하중에서의 STS304의 피로균열 전과거동)

  • Song, Sam-Hong;Lee, Jeong-Moo
    • Journal of the Korean Society for Precision Engineering
    • /
    • v.18 no.9
    • /
    • pp.131-139
    • /
    • 2001
  • The use of fracture mechanics has traditionally concentrated on crack growth under an opening mechanism. However, many service failure occur from cracks subjected to mixed mode loadings. Hence, it is necessary to evaluate the fatigue behavior under mixed mode loading. Under mixed mode loading conditions, not only the fatigue crack propagation rate is of importance, but also the crack propagation direction. The mode I and II stress intensity factors of CTS specimen were calculated using elastic finite element method. The propagation behavior of the fatigue crack of the STS304 steeds under mixed mode loading condition was evacuated by using stress intensity factors $K_I$ and $K_II. The MTS criterion and effective stress intensity factor were applied to predict the crack propagation direction and the fatigue crack propagation rate.

  • PDF

Fracture Characteristics of Concrete at Early Ages

  • Lee, Yun;Kim, Jin-Keun
    • International Journal of Concrete Structures and Materials
    • /
    • v.18 no.3E
    • /
    • pp.191-198
    • /
    • 2006
  • The objective of this study is to examine fracture characteristics of concrete at early ages, i.g. critical stress intensity factor, critical crack-tip opening displacement, fracture energy, and bilinear softening curve based on the concepts of effective-elastic crack model and cohesive crack model. A wedge splitting test for Mode I was performed on cubic wedge specimens with a notch at the edge. By experimenting with various strengths and ages, load-crack mouth opening curves were obtained, and the results were analyzed by linear elastic fracture mechanics and FEM(finite element method). The results from the test and analysis showed that critical stress intensity factor and facture energy increased while critical crack-tip opening displacement decreased with concrete aging from 1 day to 28 days. Four parameters of bilinear softening curve from 1 day to 28 days were obtained from a numerical analysis. The obtained fracture parameters and bilinear softening curves at early ages from this study are to be used as a fracture criterion and an input data for the finite element analysis of concrete at early ages.

Study on fracture mechanics of granite specimens with different precast notch depths based on DIC method

  • Shuwen Cao;Hao Shu
    • Geomechanics and Engineering
    • /
    • v.33 no.4
    • /
    • pp.393-400
    • /
    • 2023
  • Displacements near crack and stress intensity factor (SIF) are key parameters to solve rock failure issue when using fracture mechanics. In order to study the horizontal displacement and stress intensity factor of the mode I fracture, a series of three-point bending tests of granite specimens with central notch were carried out. The evolution of horizontal displacements of precast notch and crack tip opening displacements (CTOD) were analyzed based on the digital image correlation (DIC) method. Stress intensity factors for three-point bending beams with arbitrary span-to-width ratios(S/W) were calculated by using the WU-Carlsson analytical weight function for edge-crack finite width plate and the analytical solution of un-cracked stress by Filon. The present study provides a high efficient and accurate method for fracture mechanics analysis of the three-point bending granite beams.

Fracture Characteristics of Concrete at Early Ages (초기재령 콘크리트의 파괴특성)

  • Lee, Yun;Kim, Jin-Keun
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2001.05a
    • /
    • pp.215-220
    • /
    • 2001
  • The objective of this study is to examine the fracture characteristics of concrete at early ages such as critical stress intensity factor, critical crack-tip opening displacement, fracture energy based on the concepts of the effective-elastic crack model and the cohesive crack model. A wedge splitting test for Mode I was performed on cubic wedge specimens with a notch at the edge. By varying strength and age, load-crack mouth opening displacement curves were obtained and the results were analyzed by linear elastic fracture mechanics. The results from the test and analysis showed that critical stress intensity factor and fracture energy increased, and critical crack-tip opening displacement decreased with concrete age from 1 day to 28 days. The obtained fracture parameters at early ages may be used as a fracture criterion and an input data for finite element analysis of concrete at early ages.

  • PDF

Variations of the stress intensity factors for a planar crack parallel to a bimaterial interface

  • Xu, Chunhui;Qin, Taiyan;Yuan, Li;Noda, Nao-Aki
    • Structural Engineering and Mechanics
    • /
    • v.30 no.3
    • /
    • pp.317-330
    • /
    • 2008
  • Stress intensity factors for a planar crack parallel to a bimaterial interface are considered. The formulation leads to a system of hypersingular integral equations whose unknowns are three modes of crack opening displacements. In the numerical analysis, the unknown displacement discontinuities are approximated by the products of the fundamental density functions and polynomials. The numerical results show that the present method yields smooth variations of stress intensity factors along the crack front accurately. The mixed mode stress intensity factors are indicated in tables and figures with varying the shape of crack, distance from the interface, and elastic constants. It is found that the maximum stress intensity factors normalized by root area are always insensitive to the crack aspect ratio. They are given in a form of formula useful for engineering applications.

Fracture Characteristics of Concrete at Early Ages (초기재령 콘크리트의 파괴 특성)

  • Lee, Yun;Kim, Jin-Keun
    • Journal of the Korea Concrete Institute
    • /
    • v.14 no.1
    • /
    • pp.58-66
    • /
    • 2002
  • The objective of this study is to examine the fracture characteristics of concrete at early ages such as critical stress intensity factor, critical crack-tip opening displacement, fracture energy, and bilinear softening curve based on the concepts of the effective-elastic crack model and the cohesive crack model. A wedge splitting test for Mode I was performed on cubic wedge specimens with a notch at the edge. By taking various strengths and ages, load-crack mouth opening displacement curves were obtained, and the results were analyzed by linear elastic fracture mechanics and the finite element method. The results from the test and analysis showed that critical stress intensity factor and fracture energy increased, and critical crack-tip opening displacement decreased with concrete ages from 1 day to 28 days. By numerical analysis four parameters of bilinear softening curve from 1 day to 28 days were obtained. The obtained fracture parameters and bilinear softening curves at early ages may be used as a fracture criterion and an input data for finite element analysis of concrete at early ages.