• Title/Summary/Keyword: Opening Load

Search Result 410, Processing Time 0.026 seconds

Fracture Toughness Comparison of Weld Metal and Heat-Affected Zone of Brittle Crack Arrest Steel Welding Joint (후물재 용접부의 용착금속과 열영향부의 파괴 인성 비교 연구)

  • Choi, Kyung-Shin;Kong, Seok-Hwan;Seol, Sang-Seok;Chung, Won-Jee
    • Journal of the Korean Society of Manufacturing Process Engineers
    • /
    • v.20 no.7
    • /
    • pp.8-14
    • /
    • 2021
  • Even welds that have passed non-destructive testing in the case of brittle crack arrest steel materials will actually have very fine weld defects. Based on studies showing that these defects adversely affect the structure if subjected to a certain period of load, the following conclusions were obtained by conducting CTOD tests on welding joints of high-strength BCA materials, structures comprising the upper decks of a large container vessel. First of all, the fatigue pre-cracking in the weld metal and heat affected areas was tested and the behavior was identified. Both parts of the welding joint are allowable range for the class regulations. In addition, CTOD results showed that the CTOD value in the heat affected area was more than 0.5 times higher than in the weld metal area.

Experimental research on vertical mechanical performance of embedded through-penetrating steel-concrete composite joint in high-temperature gas-cooled reactor pebble-bed module

  • Zhang, Peiyao;Guo, Quanquan;Pang, Sen;Sun, Yunlun;Chen, Yan
    • Nuclear Engineering and Technology
    • /
    • v.54 no.1
    • /
    • pp.357-373
    • /
    • 2022
  • The high-temperature gas-cooled reactor pebble-bed module project is the first commercial Generation-IV NPP(Nuclear Power Plant) in China. A new joint is used for the vertical support of RPV(Reactor Pressure Vessel). The steel corbel is integrally embedded into the reactor-cabin wall through eight asymmetrically arranged pre-stressed high-strength bolts, achieving the different path transmission of shear force and moment. The vertical monotonic loading test of two specimens is conducted. The results show that the failure mode of the joint is bolt fracture. There is no prominent yield stage in the whole loading process. The stress of bolts is linearly distributed along the height of corbel at initial loading. As the load increases, the height of neutral axis of bolts gradually decreases. The upper and lower edges of the wall opening contact the corbel plate to restrict the rotation of the corbel. During the loading, the pre-stress of some bolts decreases. The increase of the pre-stress strength ratio of bolts has no noticeable effect on the structure stiffness, but it reduces the ultimate bearing capacity of the joint. A simplified calculation model for the elastic stage of the joint is established, and the estimation results are in good agreement with the experimental results.

Seismic response of single-arch large-span fabricated subway station structure

  • He, Huafei;Li, Zhaoping
    • Earthquakes and Structures
    • /
    • v.23 no.1
    • /
    • pp.101-113
    • /
    • 2022
  • A new type of fabricated subway station construction technology can effectively solve these problems. For a new type of metro structure form, it is necessary to clarify its mechanical properties, especially the seismic performance. A soil-structure elastoplastic finite element model is established to perform three-dimensional nonlinear dynamic time-history analysis based on the first fabricated station structure-Yuanjiadian station of Changchun Metro Line 2, China. Firstly, the nonlinear seismic response characteristics of the fabricated and cast-in-place subway stations under different seismic wave excitations are compared and analyzed. Then, a comprehensive analysis of several important parameters that may affect the seismic response of fabricated subway stations is given. The results show that the maximum plastic strain, the interlayer deformation, and the internal force of fabricated station structures are smaller than that of cast-in-place structure, which indicates that the fabricated station structure has good deformation coordination capability and mechanical properties. The seismic responses of fabricated stations were mainly affected by the soil-structure stiffness ratio, the soil inertia effect, and earthquake load conditions rarely mentioned in cast-in-place stations. The critical parameters have little effect on the interlayer deformation but significantly affect the joints' opening distance and contact stress, which can be used as the evaluation index of the seismic performance of fabricated station structures. The presented results can better understand the seismic responses and guide the seismic design of the fabricated station.

Seismic performance of precast assembled bridge piers with hybrid connection

  • Shuang, Zou;Heisha, Wenliuhan;Yanhui, Liu;Zhipeng, Zhai;Chongbin, Zhang
    • Structural Engineering and Mechanics
    • /
    • v.85 no.3
    • /
    • pp.407-417
    • /
    • 2023
  • Precast assembled bridge piers with hybrid connection (PASP) use both tendons and socket connections. To study the seismic performance of PASP, a full-scale in-situ test was performed based on an actual bridge project. The elastic-plastic fiber model of PASP was established using finite element software, and numerical analyses were performed to study the influence of prestress degree and socket depth on the PASP seismic performance. The results show that the typical failure mode of PASP under horizontal load is bending failure dominated by concrete cracking at the joint between the column and cushion cap. The cracking of the pier concrete and opening of joints depend on the prestress degree and socket depth. The prestressing tendons and socket connection can provide enough ductility, strength, restoration capability, and bending strength under small horizontal displacements. Although the bearing capacity and post yield stiffness of the pier can be improved to some extent by increasing the prestressing force, ductility is reduced, and residual deformation is increased. Overall, there are reasonable minimum socket depths to ensure the reliability of the socket connection.

Shear behaviour of Autoclaved Aerated Concrete (AAC) masonry walls with and without openings strengthened with welded wire mesh

  • Wanraplang Warlarpih;Comingstarful Marthong
    • Structural Engineering and Mechanics
    • /
    • v.87 no.5
    • /
    • pp.487-498
    • /
    • 2023
  • Unreinforced masonry (URM) buildings are extensively adopted in many of the growing nations, particularly in India. Window or door openings are required for architectural or functional reasons, which pose a threat to the building's safety. The past earthquakes have shown that the seismic capability of these structures was very weak. Strengthening these unreinforced masonry walls using welded wire mesh (WWM) is one of the most commonly and economical methods. The present experimental study investigates the impact of openings on the shear behaviour of URM walls and the effectiveness of WWM in enhancing the shear performance of masonry wall. In the experimental program 16 specimens were cast, 8 unstrengthen and 8 strengthened specimens, under 8 unstrengthen and strengthened specimens, every 2 specimens had 0%, 5%, 10%, and 15% openings and all these walls were tested under diagonal compression. The results show that the shear carrying capacity reduces as the opening percentage increases. However, strengthening the URM specimens using WWM significantly improves the peak load, shear strength, ductility, stiffness, and energy dissipation. Furthermore, the strengthening of the URM walls using WWM compensated the loss of wall capacity caused by the presence of the openings.

Finite Element Stress Analysis of Implant Prosthesis of Internal Connection System According to Position and Direction of Load (임플랜트-지대주의 내측연결 시스템에서 하중의 위치 및 경사에 따른 임플랜트 보철의 유한요소 응력분석)

  • Jang, Jong-Seok;Jeong, Yong-Tae;Chung, Chae-Heon
    • Journal of Dental Rehabilitation and Applied Science
    • /
    • v.21 no.1
    • /
    • pp.1-14
    • /
    • 2005
  • The purpose of this study was to assess the loading distributing characteristics of implant prosthesis of internal connection system(ITI system) according to position and direction of load, under vertical and inclined loading using finite element analysis (FEA). The finite element model of a synOcta implant and a solid abutment with $8^{\circ}$ internal conical joint used by the ITI implant was constructed. The gold crown for mandibular first molar was made on solid abutment. Each three-dimensional finite element model was created with the physical properties of the implant and surrounding bone. This study simulated loads of 200N at the central fossa in a vertical direction (loading condition A), 200N at the outside point of the central fossa with resin filling into screw hole in a vertical direction (loading condition B), 200N at the centric cusp in a $15^{\circ}$ inward oblique direction (loading condition C), 200N at the in a $30^{\circ}$ inward oblique direction (loading condition D) or 200N at the centric cusp in a $30^{\circ}$ outward oblique direction (loading condition E) individually. Von Mises stresses were recorded and compared in the supporting bone, fixture, and abutment. The following results have been made based on this study: 1. Stresses were concentrated mainly at the ridge crest around implant under both vertical and oblique loading but stresses in the cancellous bone were low under both vertical and oblique loading. 2. Bending moments resulting from non-axial loading of dental implants caused stress concentrations on cortical bone. The magnitude of the stress was greater with the oblique loading than with the vertical loading. 3. An offset of the vertical occlusal force in the buccolingual direction relative to the implant axis gave rise to increased bending of the implant. So, the relative positions of the resultant line of force from occlusal contact and the center of rotation seems to be more important. 4. In this internal conical joint, vertical and oblique loads were resisted mainly by the implant-abutment joint at the screw level and by the implant collar. Conclusively, It seems to be more important that how long the distance is from center of rotation of the implant itself to the resultant line of force from occlusal contact (leverage). In a morse taper implant, vertical and oblique loads are resisted mainly by the implant-abutment joint at the screw level and by the implant collar. This type of implant-abutment connection can also distribute forces deeper within the implant and shield the retention screw from excessive loading. Lateral forces are transmitted directly to the walls of the implant and the implant abutment mating bevels, providing greater resistance to interface opening.

A STUDY ON THE ELASTIC DEFORMATION AND STRESS DISTRIBUTION OF THE MANDIBLE WITH OSSEOINTEGRATED IMPLANT PROSTHESES USING THREE DIMENSIONAL FINITE ELEMENT ANALYSIS METHOD (골유착성 임플랜트 보철물 장착시 하악골의 탄성변형 및 응력분포에 관한 삼차원 유한요소법적 연구)

  • Kim, Yong-Ho;Kim, Yung-Soo;Kim, Chang-Whe
    • The Journal of Korean Academy of Prosthodontics
    • /
    • v.36 no.2
    • /
    • pp.203-244
    • /
    • 1998
  • The human mandible is always under the condition of loading by the various forces extorted by the attached muscles. The loading is an important condition of the stomatognathic system. This condition is composed of the direction and amount of forces of the masticatory muscles, which are controlled by the neuromuscular system, and always influenced by the movement of both opening and closing. Mandible is a strong foundation for the teeth or various prostheses, nevetheless it is a elastic body which accompanies deformation by the external forces on it. The elastic properties of the mandible is influenced by the various procedures such as conventional restorative treatments, osseointegrated implant treatments, reconstructive surgical procedures and so forth. Among the treatments the osseointegrated implant has no periodontal ligaments, which exist around the natural teeth to allow physiologic mobility in the alveolar socket. And so around the osseointegrated implant, there is almost no damping effect during the transmission of occlusal stress and displacements. If the osseointegrated implants are connected by the superstructure for the stabilization and effective distribution of occlusal stresses, the elastic properties of mandible is restricted according to the extent of 'splinting' by the superstructure and implants. To investigate the change of elastic behaviour of the mandible which has osseointegrated implant prosthesis of various numbers of implant installment and span of superstructre, a three dimensional finite element model was developed and analyzed with conditions mentioned above. The conclusions are as follows : 1. The displacements are primarily developed at the area of muscle attachment and distributed all around the mandible according to the various properties of bone. 2. The segmentation in the superstructure has few influence on the distribution of stress and displacement. 3. In the load case of ICP, the concentration of tensional stress was observed at the anterior portion of the ramus($9.22E+6N/m^2$) and at the lingual portion of the symphysis menti($8.36E+6N/m^2$). 4. In the load case of INC, the concentration of tensional stress was observed at the anterior portion of the ramus($9.90E+6N/m^2$) and the concentration of tensional stress was observed at the lingual portion of the symphysis menti($2.38E+6N/m^2$)). 5. In the load case of UTCP, the relatively high concentration of tensional stress($3.66E+7N/m^2$) was observed at the internal surface of the condylar neck.

  • PDF

Geometrical Analysis on Parts of Load Limit Valve for Static Structural Test of Aerospace Flight Vehicles (항공우주 비행체 정적구조시험용 하중제한밸브 부품 형상 분석)

  • Shim, Jae-Yeul
    • Journal of the Korean Society for Aeronautical & Space Sciences
    • /
    • v.47 no.9
    • /
    • pp.607-616
    • /
    • 2019
  • Free body diagram analysis is done for key parts of pilot stage of LLV (Load Limit Valve) which is used to protect overload for static structural test of aerospace flight vehicle. It is shown through the analysis that diameter ratio($D_2)^{ten}/D_2)^{comp}$) of two poppets in a pilot stage must be equal to piston area ratio($A_{comp}/A_{ten}$) of a hydraulic actuator for making a poppet open consistently at constant force applied by an actuator. The result of the analysis is verified by measuring geometries of the poppets in the four different LLVs which are corresponding to four actuators with different capacity and have been used after being imported in this laboratory. Results of "Adjuster resolution tests" with two different pilot stages show the max. deviation of Fi(actuator force in instant of opening poppet) from average Fi obtained for each turn of adjuster is 0.3KN and max. deviation of the Fi normalized by average Fi of each turn of adjuster is 3.7%. From the results, it is verified that the two pilot stages with same poppet diameter ratio make a poppet consistently open at Fis within ${\pm}3.7%$ deviation from the average Fi. The deviation is shown to be caused from frictional force of O-ring in the poppet. Additionally, design factors for poppet spring and adjuster, which are also key parts of the pilot stage, are distinguished and procedure for deciding the factors are also shown in this study.

Nonlinear Lateral Behavior and Cross-Sectional Stress Distribution of Concrete Rocking Columns (콘크리트 회전형 기둥의 비선형 횡방향 거동 및 단면응력 분포 분석)

  • Roh, Hwa-Sung;Hwang, Woong-Ik;Lee, Hu-Seok;Lee, Jong-Seh
    • Journal of the Korea Concrete Institute
    • /
    • v.24 no.3
    • /
    • pp.285-292
    • /
    • 2012
  • Fixed connection is generally used for beam and column connections of concrete structures, but significant damages at the connection due to severe earthquakes have been reported. In order to reduce damages of the connection and improve seismic performance of the connection, several innovative connections have been suggested. One newly proposed connection type allows a rotation of the connection for applications in rotating or rocking beams, columns, and shear walls. Such structural elements would provide a nonlinear lateral force-displacement response since their contact depth developed during rotation is gradually reduced and the stress across the sections of the elements is non-linearly distributed around a contact area, which is called an elastic hinge region in the present study. The purpose of the present study is to define the elastic hinge region or length for the rocking columns, through investigating the cross-sectional stress distribution during their lateral behavior. Performing a finite element analysis (FEA), several parameters are considered including axial load levels (5% and 10% of nominal strength), different boundary conditions (confined-ends and cantilever types), and slenderness ratios (length/depth = 5, 7, 10). The FEA results showed that the elastic hinge length does not directly depend on the parameters considered, but it is governed by a contact depth only. The elastic hinge length started to develop after an opening state and increased non-linearly until a rocking point(pre-rocking). However, the length did not increase any more after the rocking point (post-rocking) and remained as a constant value. Half space model predicting the elastic hinge length is adapted and the results are compared with the numerical results.

Experiments of Water Mist System Application for Rack Storage (랙크식 창고에 대한 미분무 시스템 적용성 실험)

  • Myoung, Sang-Yup;Kim, Jong-Hoon
    • Journal of the Society of Disaster Information
    • /
    • v.16 no.4
    • /
    • pp.627-637
    • /
    • 2020
  • Purpose: This experimental study was conducted to find out whether a water-mist fire suppression system can be applied to C.E.P., a representative combustible material of a rack storage. Method: First, it was confirmed whether the water-mist fire-extinguishing system used in this experiment was capable of extinguishing oil fires. After that, the C.E.P. boxes were loaded in the same small space as used in the oil fire experiment, and then the experiment was conducted on three scenarios; door opening, door closing, and door closing and increasing the internal load. The scenario was set considering the opening and space size conditions, which are important factors for the water-mist fire suppression. Result: Oil fire suppression tests have shown that fires are well extinguished in both the door open and closed conditions. In case of a fire of C.E.P. boxes in the same space condition as an oil fire, the fire was not extinguished in the door open condition. Fires were extinguished in the case with the door closed condition, but the afterglow was confirmed. Conclusion: In the oil fire suppression test, a water-mist fire suppression system extinguished a fire in both the door open and closed conditions. However, for the C.E.P fire, it was possible to extinguish only under the door closed condition, and there was a possibility of re-ignition.