The activities of Ni(20wt%)/$La_2O_3$, Ni(20wt%)/${\gamma}-Al_2O_3$, and Ni(20wt%)/$SiO_2$ catalyst for $CO_2$ reforming of $CH_4$ were investigated in a fixed bed flow reactor under atmospheric condition. Catalyst characterization using XRD, TEM, SEM, BET analysis were also conducted. The catalytic activity of Ni(20wt%)/$La_2O_3$ catalyst has relatively superior to that of Ni(20wt%)/${\gamma}-Al_2O_3$ and Ni(20wt%)/$SiO_2$ catalyst. The good activity of Ni(20wt%)/$La_2O_3$ catalyst seems to depend on reduced $Ni^{\circ}$ phases of NiO($\rightarrow$ Ni + O), $LaNiO_3$($\rightarrow$$Ni+La_2O_3$), Ni crystalline phases, and decoration of Ni phases by lanthanum species is also an important factor. Ni(20wt%)/${\gamma}-Al_2O_3$ and Ni(20wt%)/$SiO_2$ catalyst due to surface acidity resulted in the deposition of wisker type and encapsulate carbon on the surface of catalyst, but Ni(20wt%)/$La_2O_3$ catalyst did not show carbon on the surface of catalyst up to 8.5hr reaction.
고정층 상압 유통식 반응기를 사용하여 M(1)-Ni(5)/AlCeO3 (M = La, Ce, Y) 촉매상에서 메탄의 부분 산화 반응을 수행하여 수소의 수율을 조사하였다. XRD 분석으로 반응 전과 반응 후의 환원된 La(1)-Ni(5)/AlCeO3 촉매의 결정상 특성피크를 조사하였고 FESEM과 EDS 분석으로 La, Ni, Ce 금속 입자가 촉매 표면상에 균일하게 분포하고 있음을 조사하였다. XPS 분석으로 촉매 표면상에 O2-, O22-의 산소와 Ce3+, Ce4+, La3+, Ni2+ 등의 이온이 존재함을 알 수 있었고, Ni(5)/AlCeO3 촉매에 1 wt%의 La를 첨가하면 Ni2p3/2과 Ce3d5/2의 원자가 각각 52.7과 6.3%로 증가하였다. La(1)-Ni(5)/AlCeO3 촉매상에서 수소의 수율은 89.1%이었으며, M(1)-Ni(5)/AlCeO3 (M = Ce, Y)보다 매우 우수하였다. AlCeO3이 산소와 반응하여 만들어진 CeO2의 Ce4+ 이온이 La3+로 치환됨으로서 격자에 산소 빈자리를 만들고 strong metal-support interaction (SMSI) 효과로 Ni 원자의 분산을 증가시켜 수소 수율를 향상시켰다.
A series of catalysts, $NiO/La_2O_3-ZrO_2/WO_3$, for acid catalysis was prepared by the precipitation and impregnation methods. For the $NiO/La_2O_3-ZrO_2/WO_3$ samples, no diffraction lines of nickel oxide were observed, indicating good dispersion of nickel oxide on the catalyst surface. The catalyst was amorphous to X-ray diffraction up to 300 ${^{\circ}C}$ of calcination temperature, but the tetragonal phase of $ZrO_2$ and monoclinic phase of $WO_3$ by the calcination temperatures from 400 ${^{\circ}C}$ to 700 ${^{\circ}C}$ were observed. The role of $La_2O_3$ in the catalyst was to form a thermally stable solid solution with zirconia and consequently to give high surface area and acidity. The high acid strength and high acidity were responsible for the W=O bond nature of complex formed by the modification of $ZrO_2$ with $WO_3$. For 2-propanol dehydration the catalyst calcined at 400 ${^{\circ}C}$ exhibited the highest catalytic activity, while for cumene dealkylation the catalyst calcined at 600 ${^{\circ}C}$ showed the highest catalytic activity. 25-$NiO/5-La_2O_3-ZrO_2/15-WO_3$ exhibited maximum catalytic activities for two reactions due to the effects of $WO_3$ modifying and $La_2O_3$ doping.
For the $CO_2$ reforming of $CH_4$, Ni catalyst was supported on La-hexaaluminate or on $\gamma$-$Al_2O_3$. The catalytic activities of Ni/La-hexaaluminate catalysts were measured at $700^{\circ}C$ using gas chromatography (GC) for 72 h, and the reaction was maintained up to 72 hfor the investigation of catalyst deactivation. The surface of each catalyst after 72 h reaction was investigated using SEM and TEM, and the composition of the carbon deposits was investigated by using EA, TPO and TGA. Ni/La-hexaaluminate shows higher resistance to coke deposition than conventional Ni/$Al_2O_3$ which seems to be due to strong interaction between Ni and the support material. As a result of the reforming reaction, various types of carbon deposits were created on catalyst surface and the amounts of them were much smaller in the case of La-hexaaluminate than on $Al_2O_3$.
La을 기반으로 하는 다양한 페롭스카이트 촉매를 페치니(Pechini)법에 따라 제조하고, 이 촉매를 음식물 처리 과정에서 발생하는 악취 성분의 저온 산화 반응에 적용하여 효과적인 탈취가 이루어지도록 하였다. 배출 가스의 정량 및 정성 분석을 통하여 음식물 처리 시간에 따른 주요 악취 성분의 양을 조사하였다. 그리고 주요 악취 성분들로 구성된 표준 악취 시료는 산화 반응기의 반응물로 도입하였다. 먼저, 다양한 전이 금속 M이 치환된 La 기반 페롭스카이트 촉매($LaMO_{3}$: M=Cr, Mn, Fe, Co 및 Ni)를 제조하고 전이 금속 M의 영향을 알아보기 위해 악취 성분의 산화 반응에 적용한 결과, 테스트한 촉매 중에서 $LaNiO_3$ 촉매가 가장 우수한 촉매 활성을 보였다. 또한 촉매 활성을 증진시키기 위하여 Pt가 치환된 페롭스카이트 촉매($LaNi_{1-x}Pt_{x}O_{3}$: x=0, 0.03, 0.1 및 0.3)를 제조하였고, 이로부터 $LaNi_{0.9}Pt_{0.1}O_{3}$ 촉매가 가장 효율적인 촉매인 것을 알 수 있었다. 끝으로 저온 산화 반응에서의 페롭스카이트 촉매의 활성을 극대화하기 위하여 담지된 페롭스카이트 촉매($XLaNi_{0.9}Pt_{0.1}O_{3}/Al_{2}O_{3}$: X=페롭스카이트 함량(wt%), 0, 10, 20, 30, 40, 50 및 100)를 적용하였다. $XLaNi_{0.9}Pt_{0.1}O_{3}/Al_{2}O_{3}$ 촉매의 활성은 페롭스카이트 함량에 따라 화산형(Volcano-shaped) 곡선을 나타내었으며, 이 때 $20LaNi_{0.9}Pt_{0.1}O_{3}/Al_{2}O_{3}$ 촉매가 $180^{\circ}C$의 반응 온도에서 88.7%의 가장 높은 전환율을 보였다.
$Ni-La_2O_3-Ce_{0.8}Zr_{0.2}O_2$ catalysts with various $La_2O_3$ loading were investigated for hydrogen production from steam reforming of methane (SRM). The $La_2O_3$ loading influenced the physicochemical properties of $Ni-La_2O_3-Ce_{0.8}Zr_{0.2}O_2$ catalysts such as BET surface area, Ni dispersion, Ni size and reducibility. Among the prepared catalysts, $Ni-70La_2O_3-Ce_{0.8}Zr_{0.2}O_2$ catalyst showed the highest activity and stability at a very high gas hourly space velocity (GHSV) of $932,556h^{-1}$. This is mainly due to high Ni dispersion, small Ni size and high reducibility.
The oxidation of carbon monoxide on a catalyst, $LaSrNiCoO_3$ was investigatigated with a plug flow system. Kinetic quantities such as reaction-rate, reaction order and Arhenius-parameters at various reactor temperature from 200$^\circ$C to 300$^\circ$C were determined. Also, the optimum condition for the oxidation of carbon monoxide with this catalyst was determined and are as follows. Partial pressure of oxigen ; 428mmHg Partial pressure of carbon monoxide ; 332mmHg Mixed moral ratio of oxigen and Carbon monoxide ; 1.3 : 1 Total gas flow ; 224ml/min Reaction temperature ; 340$^\circ$C The reaction kinetic equation at the optimum condition, temperature range from 200$^\circ$C to 340$^\circ$C, are as follow. $$ $v = Ae^{6.5Kcal/RT} [CO]^{0.93 \sim 0.98} [O_2]^{0.42 \sim 0.50}$ $$ In addition to this, numerical calculation were performed to evaluate the mass and heat transfer effect on this system.
NiO and Co3O4-doped porous La(CoNi)O3 perovskite oxides were prepared from excess Ni addition by a hydrothermal method using porous silica template, and characterized as bifunctional catalysts for oxygen reduction reaction (ORR) and oxygen evolution reaction (OER) for Zn-air rechargeable batteries in alkaline solution. Excess Ni induced to form NiO and Co3O4 in La(CoNi)O3 particles. The NiO and Co3O4-doped porous La(CoNi)O3 showed high specific surface area, up to nine times of conventionally synthesized perovskite oxide, and abundant pore volume with similar structure. Extra added Ni was partially substituted for Co as B site of ABO3 perovskite structure and formed to NiO and Co3O4 which was highly dispersed in particles. Excess Ni in La(CoNi)O3 catalysts increased OER performance (259 mA/㎠ at 2.4 V) in alkaline solution, although the activities (211 mA/㎠ at 0.5 V) for ORR were not changed with the content of excess Ni. La(CoNi)O3 with excess Ni showed very stable cyclability and low capacity fading rate (0.38 & 0.07 ㎶/hour for ORR & OER) until 300 hours (~70 cycles) but more excess content of Ni in La(CoNi)O3 gave negative effect to cyclability.
Performance tests on $Ni/Ce-ZrO_2/Al_2O_3$ catalysts with additives (MgO, $La_2O_3$) were investigated in the combined reforming processes (SCR, ATR, TRM) in order to produce hydrogen and carbon monoxide (it is called "syngas".). The catalyst characterization was conducted using the BET surface analyzer, X-ray diffraction (XRD), SEM, TPR and TGA. The combined reforming process was developed to adjust the syngas ratio depending on the synthetic fuel (methanol, DME and GTL) manufacturing processes. Ni-based catalysts supported on alumina has been generally recommended as a combined reforming reaction catalyst. It was found that both free NiO and complexed NiO species were responsible for the catalytic activity in the combined reforming of methane conversion, and the $Ce-ZrO_2$ binary support employed had improved the oxygen storage capacity and thermal stability. The additives, MgO and $La_2O_3$, also seemed to play an important role to prevent the formation of the carbon deposition over the catalysts. The experimental results were compared with the equilibrium data using a commercial simulation tool (PRO/II).
본 웹사이트에 게시된 이메일 주소가 전자우편 수집 프로그램이나
그 밖의 기술적 장치를 이용하여 무단으로 수집되는 것을 거부하며,
이를 위반시 정보통신망법에 의해 형사 처벌됨을 유념하시기 바랍니다.
[게시일 2004년 10월 1일]
이용약관
제 1 장 총칙
제 1 조 (목적)
이 이용약관은 KoreaScience 홈페이지(이하 “당 사이트”)에서 제공하는 인터넷 서비스(이하 '서비스')의 가입조건 및 이용에 관한 제반 사항과 기타 필요한 사항을 구체적으로 규정함을 목적으로 합니다.
제 2 조 (용어의 정의)
① "이용자"라 함은 당 사이트에 접속하여 이 약관에 따라 당 사이트가 제공하는 서비스를 받는 회원 및 비회원을
말합니다.
② "회원"이라 함은 서비스를 이용하기 위하여 당 사이트에 개인정보를 제공하여 아이디(ID)와 비밀번호를 부여
받은 자를 말합니다.
③ "회원 아이디(ID)"라 함은 회원의 식별 및 서비스 이용을 위하여 자신이 선정한 문자 및 숫자의 조합을
말합니다.
④ "비밀번호(패스워드)"라 함은 회원이 자신의 비밀보호를 위하여 선정한 문자 및 숫자의 조합을 말합니다.
제 3 조 (이용약관의 효력 및 변경)
① 이 약관은 당 사이트에 게시하거나 기타의 방법으로 회원에게 공지함으로써 효력이 발생합니다.
② 당 사이트는 이 약관을 개정할 경우에 적용일자 및 개정사유를 명시하여 현행 약관과 함께 당 사이트의
초기화면에 그 적용일자 7일 이전부터 적용일자 전일까지 공지합니다. 다만, 회원에게 불리하게 약관내용을
변경하는 경우에는 최소한 30일 이상의 사전 유예기간을 두고 공지합니다. 이 경우 당 사이트는 개정 전
내용과 개정 후 내용을 명확하게 비교하여 이용자가 알기 쉽도록 표시합니다.
제 4 조(약관 외 준칙)
① 이 약관은 당 사이트가 제공하는 서비스에 관한 이용안내와 함께 적용됩니다.
② 이 약관에 명시되지 아니한 사항은 관계법령의 규정이 적용됩니다.
제 2 장 이용계약의 체결
제 5 조 (이용계약의 성립 등)
① 이용계약은 이용고객이 당 사이트가 정한 약관에 「동의합니다」를 선택하고, 당 사이트가 정한
온라인신청양식을 작성하여 서비스 이용을 신청한 후, 당 사이트가 이를 승낙함으로써 성립합니다.
② 제1항의 승낙은 당 사이트가 제공하는 과학기술정보검색, 맞춤정보, 서지정보 등 다른 서비스의 이용승낙을
포함합니다.
제 6 조 (회원가입)
서비스를 이용하고자 하는 고객은 당 사이트에서 정한 회원가입양식에 개인정보를 기재하여 가입을 하여야 합니다.
제 7 조 (개인정보의 보호 및 사용)
당 사이트는 관계법령이 정하는 바에 따라 회원 등록정보를 포함한 회원의 개인정보를 보호하기 위해 노력합니다. 회원 개인정보의 보호 및 사용에 대해서는 관련법령 및 당 사이트의 개인정보 보호정책이 적용됩니다.
제 8 조 (이용 신청의 승낙과 제한)
① 당 사이트는 제6조의 규정에 의한 이용신청고객에 대하여 서비스 이용을 승낙합니다.
② 당 사이트는 아래사항에 해당하는 경우에 대해서 승낙하지 아니 합니다.
- 이용계약 신청서의 내용을 허위로 기재한 경우
- 기타 규정한 제반사항을 위반하며 신청하는 경우
제 9 조 (회원 ID 부여 및 변경 등)
① 당 사이트는 이용고객에 대하여 약관에 정하는 바에 따라 자신이 선정한 회원 ID를 부여합니다.
② 회원 ID는 원칙적으로 변경이 불가하며 부득이한 사유로 인하여 변경 하고자 하는 경우에는 해당 ID를
해지하고 재가입해야 합니다.
③ 기타 회원 개인정보 관리 및 변경 등에 관한 사항은 서비스별 안내에 정하는 바에 의합니다.
제 3 장 계약 당사자의 의무
제 10 조 (KISTI의 의무)
① 당 사이트는 이용고객이 희망한 서비스 제공 개시일에 특별한 사정이 없는 한 서비스를 이용할 수 있도록
하여야 합니다.
② 당 사이트는 개인정보 보호를 위해 보안시스템을 구축하며 개인정보 보호정책을 공시하고 준수합니다.
③ 당 사이트는 회원으로부터 제기되는 의견이나 불만이 정당하다고 객관적으로 인정될 경우에는 적절한 절차를
거쳐 즉시 처리하여야 합니다. 다만, 즉시 처리가 곤란한 경우는 회원에게 그 사유와 처리일정을 통보하여야
합니다.
제 11 조 (회원의 의무)
① 이용자는 회원가입 신청 또는 회원정보 변경 시 실명으로 모든 사항을 사실에 근거하여 작성하여야 하며,
허위 또는 타인의 정보를 등록할 경우 일체의 권리를 주장할 수 없습니다.
② 당 사이트가 관계법령 및 개인정보 보호정책에 의거하여 그 책임을 지는 경우를 제외하고 회원에게 부여된
ID의 비밀번호 관리소홀, 부정사용에 의하여 발생하는 모든 결과에 대한 책임은 회원에게 있습니다.
③ 회원은 당 사이트 및 제 3자의 지적 재산권을 침해해서는 안 됩니다.
제 4 장 서비스의 이용
제 12 조 (서비스 이용 시간)
① 서비스 이용은 당 사이트의 업무상 또는 기술상 특별한 지장이 없는 한 연중무휴, 1일 24시간 운영을
원칙으로 합니다. 단, 당 사이트는 시스템 정기점검, 증설 및 교체를 위해 당 사이트가 정한 날이나 시간에
서비스를 일시 중단할 수 있으며, 예정되어 있는 작업으로 인한 서비스 일시중단은 당 사이트 홈페이지를
통해 사전에 공지합니다.
② 당 사이트는 서비스를 특정범위로 분할하여 각 범위별로 이용가능시간을 별도로 지정할 수 있습니다. 다만
이 경우 그 내용을 공지합니다.
제 13 조 (홈페이지 저작권)
① NDSL에서 제공하는 모든 저작물의 저작권은 원저작자에게 있으며, KISTI는 복제/배포/전송권을 확보하고
있습니다.
② NDSL에서 제공하는 콘텐츠를 상업적 및 기타 영리목적으로 복제/배포/전송할 경우 사전에 KISTI의 허락을
받아야 합니다.
③ NDSL에서 제공하는 콘텐츠를 보도, 비평, 교육, 연구 등을 위하여 정당한 범위 안에서 공정한 관행에
합치되게 인용할 수 있습니다.
④ NDSL에서 제공하는 콘텐츠를 무단 복제, 전송, 배포 기타 저작권법에 위반되는 방법으로 이용할 경우
저작권법 제136조에 따라 5년 이하의 징역 또는 5천만 원 이하의 벌금에 처해질 수 있습니다.
제 14 조 (유료서비스)
① 당 사이트 및 협력기관이 정한 유료서비스(원문복사 등)는 별도로 정해진 바에 따르며, 변경사항은 시행 전에
당 사이트 홈페이지를 통하여 회원에게 공지합니다.
② 유료서비스를 이용하려는 회원은 정해진 요금체계에 따라 요금을 납부해야 합니다.
제 5 장 계약 해지 및 이용 제한
제 15 조 (계약 해지)
회원이 이용계약을 해지하고자 하는 때에는 [가입해지] 메뉴를 이용해 직접 해지해야 합니다.
제 16 조 (서비스 이용제한)
① 당 사이트는 회원이 서비스 이용내용에 있어서 본 약관 제 11조 내용을 위반하거나, 다음 각 호에 해당하는
경우 서비스 이용을 제한할 수 있습니다.
- 2년 이상 서비스를 이용한 적이 없는 경우
- 기타 정상적인 서비스 운영에 방해가 될 경우
② 상기 이용제한 규정에 따라 서비스를 이용하는 회원에게 서비스 이용에 대하여 별도 공지 없이 서비스 이용의
일시정지, 이용계약 해지 할 수 있습니다.
제 17 조 (전자우편주소 수집 금지)
회원은 전자우편주소 추출기 등을 이용하여 전자우편주소를 수집 또는 제3자에게 제공할 수 없습니다.
제 6 장 손해배상 및 기타사항
제 18 조 (손해배상)
당 사이트는 무료로 제공되는 서비스와 관련하여 회원에게 어떠한 손해가 발생하더라도 당 사이트가 고의 또는 과실로 인한 손해발생을 제외하고는 이에 대하여 책임을 부담하지 아니합니다.
제 19 조 (관할 법원)
서비스 이용으로 발생한 분쟁에 대해 소송이 제기되는 경우 민사 소송법상의 관할 법원에 제기합니다.
[부 칙]
1. (시행일) 이 약관은 2016년 9월 5일부터 적용되며, 종전 약관은 본 약관으로 대체되며, 개정된 약관의 적용일 이전 가입자도 개정된 약관의 적용을 받습니다.