Features and Properties of $YBa_2$$Cu_3$$O_{7-x}$ Films Grown on SrTi$O_3$ by High Frequency PLD

  • Shi, D.Q.;Ko, R.K.;Song, K.J.;Chung, J.K.;Choi, S.J.;Park, Y.M.;Shin, K.C.;Yoo, S.I.;Park, C.
    • Progress in Superconductivity
    • /
    • v.5 no.1
    • /
    • pp.75-79
    • /
    • 2003
  • YBCO films were deposited with various thicknesses from 100nm to 1.6$\mu\textrm{m}$ on single crystal $SrTiO_3$ substrates by pulsed laser deposition (PLD). The effects of different deposition conditions, especially different deposition rates by means of changing the pulsed laser frequency up to 200Hz, on the J$_{c}$ value were studied. For YBCO film with the thickness of 200nm, the $J_{c}$ value of $2.1MA/\textrm{cm}^2$ has been achieved under the high deposition rate of 3.2nm/s (190nm/min). The $J_{c}$ can be maintained greater than $1M/\textrm{cm}^2$ with the thickness less than 1$\mu\textrm{m}$. The X-ray analysis was used to examine the texture, crystallization and surface quality. The SEM was employed to analyze the surface of YBCO, and it was shown the surface of YBCO film became rougher with increasing the thickness. There were many large singular outgrowths and networks of outgrowths on the surface of YBCO films which lowered the density of thick YBCO film. The outgrowth network was probably the a-axis YBCO corresponding to XRD $\theta$-2$\theta$scan and $\chi$-scan which were used to characterize a-axis orientation of YBCO film. The reason for J$_{c}$ declining with increasing the thickness was studied and discussed.sed.

  • PDF

Development of High Resolution Micro-CT System for In Vivo Small Animal Imaging (소형 동물의 생체 촬영을 위한 고해상도 Micro-CT 시스템의 개발)

  • Park, Jeong-Jin;Lee, Soo-Yeol;Cho, Min-Hyoung
    • Journal of Biomedical Engineering Research
    • /
    • v.28 no.1
    • /
    • pp.95-101
    • /
    • 2007
  • Recently, small-animal imaging technology has been rapidly developed for longitudinal screening of laboratory animals such as mice and rats. One of newly developed imaging modalities for small animals is an x-ray micro-CT (computed tomography). We have developed two types of x-ray micro-CT systems for small animal imaging. Both systems use flat-panel x-ray detectors and micro-focus x-ray sources to obtain high spatial resolution of $10{\mu}m$. In spite of the relatively large field-of-view (FOV) of flat-panel detectors, the spatial resolution in the whole-body imaging of rats should be sacrificed down to the order of $100{\mu}m$ due to the limited number of x-ray detector pixels. Though the spatial resolution of cone-beam CTs can be improved by moving an object toward an x-ray source, the FOV should be reduced and the object size is also limited. To overcome the limitation of the object size and resolution, we introduce zoom-in micro-tomography for high-resolution imaging of a local region-of-interest (ROI) inside a large object. For zoom-in imaging, we use two kinds of projection data in combination, one from a full FOV scan of the whole object and the other from a limited FOV scan of the ROI. Both of our micro-CT systems have zoom-in micro-tomography capability. One of both is a micro-CT system with a fixed gantry mounted with an x-ray source and a detector. An imaged object is laid on a rotating table between a source and a detector. The other micro-CT system has a rotating gantry with a fixed object table, which makes whole scans without rotating an object. In this paper, we report the results of in vivo small animal study using the developed micro-CTs.

Characteristics of nanolithograpy process on polymer thin-film using near-field scanning optical microscope with a He-Cd laser (He-Cd 레이저와 근접장현미경을 이용한 폴리머박막 나노리소그라피 공정의 특성분석)

  • Kwon S. J.;Kim P. K.;Chun C. M.;Kim D. Y.;Chang W. S.;Jeong S. H.
    • Laser Solutions
    • /
    • v.7 no.3
    • /
    • pp.37-46
    • /
    • 2004
  • The shape and size variations of the nanopatterns produced on a polymer film using a near-field scanning optical microscope(NSOM) are investigated with respect to the process variables. A cantilever type nanoprobe having a 100nm aperture at the apex of the pyramidal tip is used with the NSOM and a He-Cd laser at a wavelength of 442nm as the illumination source. Patterning characteristics are examined for different laser beam power at the entrance side of the aperture($P_{in}$), scan speed of the piezo stage(V), repeated scanning over the same pattern, and operation modes of the NSOM(DC and AC modes). The pattern size remained almost the same for equal linear energy density. Pattern size decreased for lower laser beam power and greater scan speed, leading to a minimum pattern width of around 50nm at $P_{in}=1.2{\mu}W\;and\;V=12{\mu}m/s$. Direct writing of an arbitrary pattern with a line width of about 150nm was demonstrated to verify the feasibility of this technique for nanomask fabrication. Application on high-density data storage is discussed.

  • PDF

Trueness and precision of scanning abutment impressions and stone models according to dental CAD/CAM evaluation standards

  • Jeon, Jin-Hun;Hwang, Seong-Sig;Kim, Ji-Hwan;Kim, Woong-Chul
    • The Journal of Advanced Prosthodontics
    • /
    • v.10 no.5
    • /
    • pp.335-339
    • /
    • 2018
  • PURPOSE. The purpose of the present study was to compare scanning trueness and precision between an abutment impression and a stone model according to dental computer-aided design/computer-aided manufacturing (CAD/CAM) evaluation standards. MATERIALS AND METHODS. To evaluate trueness, the abutment impression and stone model were scanned to obtain the first 3-dimensional (3-D) stereolithography (STL) file. Next, the abutment impression or stone model was removed from the scanner and re-fixed on the table; scanning was then repeated so that 11 files were obtained for each scan type. To evaluate precision, the abutment impression or stone model was scanned to obtain the first 3-D STL file. Without moving it, scanning was performed 10 more times, so that 11 files were obtained for each scan type. By superimposing the first scanned STL file onto the other STL files one by one, 10 color-difference maps and reports were obtained; i.e., 10 experimental scans per type. The independent t-test was used to compare root mean square (RMS) data between the groups (${\alpha}=.05$). RESULTS. The $RMS{\pm}SD$ values of scanning trueness of the abutment impression and stone model were $22.4{\pm}4.4$ and $17.4{\pm}3.5{\mu}m$, respectively (P<.012). The $RMS{\pm}SD$ values of scanning precision of the abutment impression and stone model were $16.4{\pm}2.9$ and $14.6{\pm}1.6{\mu}m$, respectively (P=.108). CONCLUSION. There was a significant difference in scanning trueness between the abutment impression and stone model, as evaluated according to dental CAD/CAM standards. However, all scans showed high trueness and precision.

The evaluation of useful on the additional PET/CT Liver scan (PET/CT 검사에서 Gastrointestinal Cancer 환자의 Liver 추가촬영에 대한 유용성 평가)

  • Park, Se Youn;Lee, Hwa Jin;Lee, Mu Seok;Kim, Jung Uk;Ji, Hye In
    • The Korean Journal of Nuclear Medicine Technology
    • /
    • v.20 no.2
    • /
    • pp.46-48
    • /
    • 2016
  • Purpose The liver one of the most common site for distant metastasis for a variety of tumor, especially of gastrointestinal origin. the purpose of this study was to analyze image quality between standard scan and additional liver scan. Materials and Methods From September 2015 to February 2016. 152 patients were examined undergo gastrointestinal cancer. 32 patients confirmed liver metastasis analyzed same liver ROI level and check the SNR, SUV and T/N ratio Results The $SNR_{mean}$ of standard was $17.7{\pm}10.3$; addition was $22.3{\pm}9.7$ (p<0.05). In $SUV_{max}$ of standard was $6.7{\pm}2.8$; addition was $7.6{\pm}3.2$ (P<0.05). and the T/N ratio of standard was $2.1{\pm}0.6$; addition was $2.5{\pm}0.8$ (P<0.05). Conclusion The $SNR_{mean}$, $SUV_{max}$ and T/N ratio were higher than those on the first scan (P<0.05). The SNRmean showed the highest change rate among the parameters. A additional liver scan is more favorable for the detection of gastrointestinal cancer patients.

  • PDF

A Facile Electrochemical Fabrication of Reduced Graphene Oxide-Modified Glassy Carbon Electrode for Simultaneous Detection of Dopamine, Ascorbic Acid, and Uric Acid

  • Yu, Joonhee;Kim, Tae Hyun
    • Journal of Electrochemical Science and Technology
    • /
    • v.8 no.4
    • /
    • pp.274-281
    • /
    • 2017
  • This paper describes the simple fabrication of an electrode modified with electrochemically reduced graphene oxide (ERGO) for the simultaneous electrocatalytic detection of dopamine (DA), ascorbic acid (AA), and uric acid (UA). ERGO was formed on a glassy carbon (GC) electrode by the reduction of graphene oxide (GO) using linear sweep voltammetry. The ERGO/GC electrode was formed by subjecting a GO solution ($1mg\;mL^{-1}$ in 0.25 M NaCl) to a linear scan from 0 V to -1.4 V at a scan rate of $20mVs^{-1}$. The ERGO/GC electrode was characterized by Raman spectroscopy, Fourier transform infrared spectroscopy, contact angle measurements, electrochemical impedance spectroscopy, and cyclic voltammetry. The electrochemical performance of the ERGO/GC electrode with respect to the detection of DA, AA, and UA in 0.1 M PBS (pH 7.4) was investigated by differential pulse voltammetry (DPV) and amperometry. The ERGO/GC electrode exhibited three well-separated voltammetric peaks and increased oxidation currents during the DPV measurements, thus allowing for the simultaneous and individual detection of DA, AA, and UA. The detection limits for DA, AA, and UA were found to be 0.46, 77, and $0.31{\mu}M$ respectively, using the amperometric i-t curve technique, with the S/N ratio being 3.

Analysis of a micro-processed sample surface using SCM and AFM (공초점현미경과 원자현미경을 이용한 초정밀 가공된 시료 표면의 영상측정)

  • Kim Jong-Bae;Bae Han-Sung;Kim Kyeong-Ho;Nam Gi-Jung;Kwon Nam-Ic
    • Proceedings of the Korean Society of Precision Engineering Conference
    • /
    • 2005.06a
    • /
    • pp.577-580
    • /
    • 2005
  • Surface quality of a micro-processed sample with laser has been investigated by using of scanning confocal microscope(SCM) and atomic force microscope(AFM). Samples are bump electrodes and ITO glass of LCD module used in a mobile phone and a wafer surface scribed by UV laser. A image of $140\times120{\mu}m^2$ is obtained within 1 second by SCM because scan speed of a x-axis and y-axis are 1kHz and 1Hz, respectively. AFM is able to measure correctly hight and width of ITO and scribing depth and width of a wafer with a resolution less than 300 . However, the scan speed is slow and it is difficult to distinguish a surface composed of different nm kinds of materials. Results show that SCM is preferable to obtain a image of a sample composed of different kinds of material than AFM because the intensity of a reflected light from surface is different from each material.

  • PDF

Dislocation Density Estimation and mosaic Model for GaN/SiC(0001) by High Resolution x-ray Diffraction

  • Yang, Quankui;Li, Aizhen
    • Journal of the Korean Vacuum Society
    • /
    • v.6 no.S1
    • /
    • pp.43-46
    • /
    • 1997
  • High resolution x-ray diffraction and two dimensional triple axis mapping were used to characterize a group of GaN layers of about 1.1$\mu$m grown by direct current plasma molecular beam epitaxy technique on 6H-SiC(0001). A FWHM of 11.9 arcmins for an $\omega$ scan and 1.2 arcmins for an $\omega$/2$\theta$ scan were observed. A careful study of the rocking curves showed there were some large mosaics in the GaN layer and a tilt of $0.029^{\circ}$ between the GaN layer and the SIC substrate was detected. The two dimensional triple axis mapping showed that the GaN mosaica were disoriented in the (0001) plane but rather uniformed in direction perpendicular to the plane. A mosaics were disoriented in the (0001) plane but rather uniformed in direction perpendicular to the plane. A mosaic model was deduced to explain the phenomenon and the dislocation density was estimated to be about~$10^9\;\textrm{cm}^{-2}$ acc ding to the model.

  • PDF

Effect of the Laser Beam Size on the Cure Properties of a Photopolymer in Stereolithography

  • Sim, Jae-Hyung;Lee, Eun-Dok;Kweon, Hyeog-Jun
    • International Journal of Precision Engineering and Manufacturing
    • /
    • v.8 no.4
    • /
    • pp.50-55
    • /
    • 2007
  • Stereolithography (SLA) is a technique using a laser beam to cure a photopolymer liquid resin with three-dimensional computer-aided design (CAD) data, The accuracy of the prototype, the build time, and the cured properties of the resins are controlled by the SLA process parameters such as the size of the laser beam, scan velocity, hatch spacing, and layer thickness, In particular, the size of the laser beam is the most important parameter in SLA, This study investigated the curing properties of photopolymers as a function of the laser beam size, The cure width and depth were measured either on a single cure line or at a single cure layer for various hatch spacings and laser beam sizes, The cure depth ranged from 0.23 to 0.34 mm and was directly proportional to the beam radius, whereas the cure width ranged from 0.42 to 1.07 mm and was inversely proportional to the beam radius, The resulting surface roughness ranged from 1.12 to $2.23{\mu}m$ for a ratio of hatch spacing to beam radius in the range 0.5-2.0 at a beam radius of 0.17 mm and a scan velocity of 125 mm/sec.

Development of Defect Inspection System for PDP ITO Patterned Glass

  • Song Jun-Yeob;Park Hwa-Young;Kim Hyun-Jong;Jung Yeon-Wook
    • International Journal of Precision Engineering and Manufacturing
    • /
    • v.7 no.3
    • /
    • pp.18-23
    • /
    • 2006
  • The formation degree of sustain (ITO pattern) determines the quality of a PDP (Plasma Display Panel). Thus, in the present study, we attempt to detect 100% of the defects that are larger than $30{\mu}m$. Currently, the inspection method in the PDP manufacturing process is dependent upon the naked eye or a microscope in off-line mode. In this study, a prototype inspection system for PDP ITO patterned glass is developed. The developed system, which is based on a line-scan mechanism, obtains information on the defects and sorts the defects by type automatically. The developed inspection system adopts a multi-vision method using slit-beam formation for minimum inspection time and the detection algorithm is embodied in the detection ability. Characteristic defects such as pin holes, substances, and protrusions are extracted using the blob analysis method. Defects such as open, short, spots and others are distinguished by the line type inspection algorithm. It was experimentally verified that the developed inspection system can detect defects with reliability of up to 95% in about 60 seconds for the 42-inch PDP panel.