Research Trends of the Mo-Si-B Alloys as Next Generation Ultra-high-temperature Alloys (차세대 초고온 합금인 Mo-Si-B 합금의 연구 동향)

  • Choi, Won June;Park, Chun Woong;Park, Jung Hyo;Kim, Young Do;Byun, Jong Min
    • Journal of Powder Materials
    • /
    • v.26 no.2
    • /
    • pp.156-165
    • /
    • 2019
  • Over the last decade, the next generation's ultra-high-temperature materials as an alternative to Nickel-based superalloys have been highlighted. Ultra-high-temperature materials based on refractory metals are one of several potential candidates. In particular, molybdenum alloys with small amounts of silicon and boron (Mo-Si-B alloys) have superior properties at high temperature. However, research related to Mo-Si-B alloys were mainly conducted by several developed countries but garnered little interest in Korea. Therefore, in this review paper, we introduce the development history of Mo-Si-B alloys briefly and discuss the properties, particularly the mechanical and oxidation properties of Mo-Si-B alloys. We also introduce the latest research trends of Mo-Si-B alloys based on the research paper. Finally, for domestic research related to this field, we explain why Mo-Si-B alloys should be developed and suggest the potential directions for Mo-Si-B alloys research.

Oxidation Behavior of $SiC/MoSi_2$ Composites Prepared by Reaction Sintering Method (반응소결에 의하여 제조된 $SiC/MoSi_2$ 복합체의 산화 거동)

  • 양준환;한인섭;우상국;서동수
    • Journal of the Korean Ceramic Society
    • /
    • v.31 no.12
    • /
    • pp.1588-1598
    • /
    • 1994
  • The SiC/MoSi2 composite materials were fabricated by infiltrating the mixture of molybdenum disilicide and metal silicon(MoSi2+Si=100) to a porous compact of silicon carbide and graphite under the vacuum atmosphere of 10-1 torr. The specimen were oxidized in dry air under 1 atm at 130$0^{\circ}C$~150$0^{\circ}C$ for 240 hours. The oxidation behavior was evaluated by the weight gain and loss per unit area of the oxidized samples. Also, SEM and XRD analysis of the oxidized surface of the samples were carried out. With increasing the MoSi2 content and oxidation temperature, the passive oxidation was found. The trend of weight gain of all samples was followed the parabolic rate law with the formation of a protective layer of cristobalite on the surface.

  • PDF

Synthesis and Properties of In-situ $MoSi_2$/W Composites ($MoSi_2$/W 복합재료의 합성과 성질에 관한 연구)

  • Jang, Dae-Kyu;Abbaschian, R.
    • Korean Journal of Materials Research
    • /
    • v.8 no.10
    • /
    • pp.938-944
    • /
    • 1998
  • $MoSi_2$/W composites were fabricated by vacuum hot press at $1600^{\circ}C$ under 30MPa for 3 hrs. The effects of the amount of tungsten in the composites was explained in terms of the microstructure and mechanical properties. Although tungsten was mainly substituted to Mo atoms forming a complete solid solution of (Mo.W).Si, (x= 1, 5, y=2, 3). the grain size of composites became smaller with the increase of tungsten added. Vickers hardness was increased with the increase of tungsten content due to the solid-solution hardening. On the other hand, toughness of composites decreased sharply by increasing the amount of tungsten. Optimum tungsten amount was determined to be a 10 vol% of composite. Indentation fracture toughness was calculated to be 4.5MPa\sqrt{m}$ in this composites, compared with $2.7MPa\sqrt{m}$ in pure $MoSi_2$.

  • PDF

Mechanical Properties and Fabrication of Nanostructured (Ti,Mo)Si2 by Pulsed Current Activated Combustion (펄스전류활성 연소합성에 의한 나노구조 (Ti,Mo)Si2 제조 및 기계적 특성)

  • Ko, In-Yong;Park, Na-Ra;Oh, Se-Hoon;Shon, In-Jin
    • Korean Journal of Metals and Materials
    • /
    • v.49 no.8
    • /
    • pp.608-613
    • /
    • 2011
  • Nanopowders of Mo, Ti and Si were made by high-energy ball milling. A dense nanostructured $(Ti,Mo)Si_2$ compound was sintered by the pulsed current activated combustion method within two minutes from mechanically activated powder of Mo, Ti and Si. A highly dense $(Ti,Mo)Si_2$ compound was produced under simultaneous application of 80 MPa pressure and a pulsed current. The mechanical properties and micorostructure were investigated. The hardness and fracture toughness of the $(Ti,Mo)Si_2$ were $1030kg/mm^2$ and $4.9MPa{\cdot}m^{1/2}$, respectively. The mechanical properties were higher than monolithic $TiSi_2$.

Fabrication and Impact Properties of $Nb/MoSi_2-ZrO_2$ Laminate Composites ($Nb/MoSi_2-ZrO_2$ 적층복합재료의 제조 및 충격특성)

  • Lee, Sang-Pill;Yoon, Han-Ki;Kong, Yoo-Sik
    • Proceedings of the Korea Committee for Ocean Resources and Engineering Conference
    • /
    • 2002.05a
    • /
    • pp.29-34
    • /
    • 2002
  • [ $Nb/MoSi_2-ZrO_2$ ] laminate composites have been successfully fabricated by alternately stacking $MoSi_2-ZrO_2$ powder layer and Nb sheet, followed by hot pressing in a graphite mould. The fabricating parameters were selected as hot press temperatures. The instrumented Charpy impact test was carried out at the room temperature in order to investigate the relationship between impact properties and fabricating temperatures. The interfacial shear strength between $MoSi_2-ZrO_2$ and Nb, which is associated with the fabricating temperature and the growth of interfacial reaction layer, is also discussed. The plastic deformation of Nb sheet and the interfacial delamination were macroscopically observed. The $Nb/MoSi_2-ZrO_2$ laminate composites had the maximum impact value when fabricated at 1623K, accompanying the increase of fracture displacement and crack propagation energy. The interfacial shear strength of $Nb/MoSi_2-ZrO_2$ laminate composites increased with the growth of interfacial reaction layer, which resulted from the increase of fabricating temperature. there is an appropriate interfacial shear strength for the enhancement of impact value of $Nb/MoSi_2-ZrO_2$ laminate composites. A large increase of interfacial shear strength restrains the plastic deformation of Nb sheet.

  • PDF

Impact Fracture Characteristics on Fabricating Process of $Nb/MoSi_2$ Laminate Composite (I)

  • Lee, Sang-Pill;Yoon, Han-Ki
    • Journal of Mechanical Science and Technology
    • /
    • v.14 no.8
    • /
    • pp.823-829
    • /
    • 2000
  • [ $Nb/MoSi_2$ ]laminate composites have been successfully fabricated by hot pressing in a graphite mould. Lamination of Nb foil and $MoSi_2$ layer showed a sufficient improvement in the absorbed impact energy compared to that of monolithic $MoSi_2$ material. The impact value of $Nb/MoSi_2$ laminate composites obviously is reduced when sintered at temperatures higher than 1523K, even if the composite density contributing to impact load increased along with fabricating temperatures. Impact value of laminate composites was also drastically decreased with the growth of reaction layer after the heat treatment. However, it was effective to increase the pressure at the same sintering temperature for the improvement of the impact value.

  • PDF

MoS2-Embedded Schottky Photoelectric Devices (MoS2 기반의 쇼트키 반도체 광전소자)

  • Ban, Dong-Kyun;Park, Wang-Hee;Jong, Bok-Mahn;Kim, Joondong
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.30 no.7
    • /
    • pp.417-422
    • /
    • 2017
  • A high-performing photoelectric device was realized for the $MoS_2$-embedded Si device. $MoS_2$-coating was performed by an available large-scale sputtering method. The $MoS_2$-layer coating on the p-Si spontaneously provides the rectifying current flow with a significant rectifying ratio of 617. Moreover, the highly optical transmittance of the $MoS_2$-layer provides over 80% transmittance for broad wavelengths. The $MoS_2$-embedded Si photodetector shows the sensitive photo-response for middle and long-wavelength photons due to the functional $MoS_2$-layer, which resolves the conventional limit of Si for long wavelength detection. The functional design of $MoS_2$-layer would provide a promising route for enhanced photoelectric devices, including photovoltaic cells and photodetectors.

Mechanical Properties and Fabrication of Nanostructured 2MoSi2-SiC by Pulsed Current Activated Combustion Synthesis (펄스 전류 활성 연소합성에 의한 나노구조의 2MoSi2-SIC제조 및 기계적 성질)

  • Shon, In-Jin;Kim, Dong-Ki;Jeong, In-Kyoon;Doh, Jung-Mann;Yoon, Jin-Kook;Ko, In-Yong
    • Journal of Powder Materials
    • /
    • v.14 no.4
    • /
    • pp.245-250
    • /
    • 2007
  • Dense nanostructured $2MoSi_{2}-SiC$ composites were synthesized by the pulsed current activated combustion synthesis (PCACS) method within 3 minutes in one step from mechanically activated powders of $Mo_{2}C$ and 5Si. Simultaneous combustion synthesis and densification were accomplished under the combined effects of a pulsed current and mechanical pressure. Highly dense $2MoSi_{2}-SiC$ with relative density of up to 96% was produced under simultaneous application of a 60 MPa pressure and the pulsed current. The average grain size of $MoSi_{2}$ and SiC were about 120 nm and 90 nm, respectively. The hardness and fracture toughness values obtained were 1350 $kg/mm^{2}$ and 4 $MPa{\cdot}m^{1/2}$, respectively.

Influence of Oxidation Inhibitor on Carbon-Carbon Composites: 9. Studies on Impact Properties of the Composites (산화억제제 첨가에 의한 탄소/탄소 복합재료의 물성에 관한 연구: 9. 복합재료의 충격특성에 관한 연구)

  • 박수진;서민강;이재락
    • Composites Research
    • /
    • v.16 no.3
    • /
    • pp.41-48
    • /
    • 2003
  • In this work, the effect of molybdenum disilicide(MoSi$_2$) content on the impact properties of carbon-carbon composites(C/C composites) was investigated in the presence of MoSi$_2$. The content of MoSi$_2$ was varied in 0, 4, 12 and 20 wt% on the basis of resin matrix for anti-oxidation properties of the composites under high temperature. As a result, the composites made with MoSi$_2$ resulted in an increase of interfacial adhesion between fibers and matrix, which could improve the impact properties of the composites. Especially, 12 wt% Mosi$_2$ composites showed the highest impact properties in the present system. This was probably due to the existence of brittle-to-ductile transition(BDT) properties of MoSi$_2$ in the vicinity of 90$0^{\circ}C$, resulting from increasing the interfacial adhesion force among fibers, filler, and matrix in the composites.