$ZrO_2$$CeO_2$ 절연체를 이용한 BLT/절연체/Si 구조의 특성 (Characterization of BLT/insulator/Si structure using $ZrO_2$ and $CeO_2$ insulator)

  • 이정미;김경태;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 춘계학술대회 논문집 센서 박막재료 반도체 세라믹
    • /
    • pp.186-189
    • /
    • 2003
  • The MFIS capacitors were fabricated using a metalorganic decomposition method. Thin layers of $ZrO_2$ and $CeO_2$ were deposited as a buffer layer on Si substrate and BLT thin films were used as a ferroelectric layer. The electrical and structural properties of the MFIS structure were investigated. X -ray diffraction was used to determine the phase of the BLT thin films and the quality of the $ZrO_2$ and $CeO_2$ layer. AES show no interdiffusion and the formation of amorphous $SiO_2$ layer is suppressed by using the $ZrO_2$ and $CeO_2$ film as buffer layer between the BLT film and Si substrate. The width of the memory window in the C-V curves for the $BLT/ZrO_2/Si$ and $BLT/CeO_2/Si$ structure is 2.94 V and 1.3V, respectively. The experimental results show that the BLT-based MFIS structure is suitable for non-volatile memory FETs with large memory window.

  • PDF

FRAM 응용을 위한 BET 박막의 강유전 특성 (Ferroelectric properties of BET Thin Films for FRAM)

  • 김경태;김태형;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 춘계학술대회 논문집 센서 박막재료 반도체 세라믹
    • /
    • pp.200-203
    • /
    • 2003
  • Ferroelectric europium-substitution $Bi_4Ti_3O_{12}$ thin films were fabricated by spin-coating onto a Pt/Ti/$SiO_2$/Si substrate. The $Bi_{3.25}Eu_{0.75}Ti_3O_{12}$ (BET) films have polycrystalline structure annealed at 700 C. We investigated that the influence of $Bi_4Ti_3O_{12}$ thin films by substituting for Bi ions with Bi ions using X-ray diffraction (XRD), scanning electron microscopy (SEM), and X-ray photoelectron spectroscopy (XPS). From the XPS measurement, it was suggested that the stability of the metal-oxygen octahedral should be related to substitute for Bi ions with Eu ions at annealed $800^{\circ}C$. The BET thin films showed a large remanent polarization (2Pr) of $60.99C/cm^2$ at an applied voltage of 10 V. The BET thin films exhibited no significant degradation of switching charge at least up to $5{\times}10^9$ switching cycles at a frequency of 50 kHz.

  • PDF

$Pt/Bi_{3.25}La_{0.75}Ti_3O_{12}/CeO_2/Si$ 구조를 이용한 MFISFET의 구조 및 전기적 특성 (Structural and electrical properties of MFISFET using a $Pt/Bi_{3.25}La_{0.75}Ti_3O_{12}/CeO_2/Si$ structure)

  • 김경태;김창일;이철인;김태형
    • 대한전기학회:학술대회논문집
    • /
    • 대한전기학회 2004년도 추계학술대회 논문집 전기물성,응용부문
    • /
    • pp.183-186
    • /
    • 2004
  • The metal-ferroelectric-insulator-semiconductor(MFIS) capacitors were fabricated using a metalorganic decomposition (MOD)method. The $CeO_2$ thin films were deposited as a buffer layer on Si substrate and $Bi_{3.25}La_{0.75}Ti_3O_{12}$ (BLT) thin films were used as a ferroelectric layer. The electrical and structural properties of the MFIS structure were investigated by varying the $CeO_2$ layer thickness. The width of the memory window in the capacitance-voltage (C-V)curves for the MFIS structure decreased with increasing thickness of the $CeO_2$ layer. Auger electron spectroscopy (AES) and transmission electron microscopy (TEM) show no interdiffusion by using the $CeO_2$ film as buffer layer between the BLT film and Si substrate. The experimental results show that the BLT-based MFIS structure is suitable for non-volatile memory field-effect-transistors (FETs) with large memory window.

  • PDF

BLT 박막을 이용한 MFIS 구조에서 MgO buffer layer의 영향 (Effect of the MgO buffer layer for MFIS structure using the BLT thin film)

  • 이정미;김경태;김창일
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2003년도 추계학술대회 논문집 Vol.16
    • /
    • pp.23-26
    • /
    • 2003
  • The BLT thin film and MgO buffer layer were fabricated using a metalorganic decomposition method and the DC sputtering technique. The MgO thin film was deposited as a buffer layer on $SiO_2/Si$ and BLT thin films were used as a ferroelectric layer. The electrical of the MFIS structure were investigated by varying the MgO layer thickness. TEM showsno interdiffusion and reaction that suppressed by using the MgO film as abuffer layer. The width of the memory window in the C-Y curves for the MFIS structure decreased with increasing thickness of the MgO layer Leakage current density decreased by about three orders of magnitude after using MgO buffer layer. The results show that the BLT and MgO-based MFIS structure is suitable for non-volatile memory FETs with large memory window.

  • PDF

솔 - 젤법을 이용한 Bismuth Layered Structure를 가진 강유진성 박막의 제조 및 특성평가에 관한 연구 (II. MOD법으로 제조한 강유전성 $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ 박막의 유전특성) (The Preparation and Characterization of Bismuth Layered Ferroelectric Thin Films by Sol-Gel Process (II. Dielectric Properties of Ferroelectric $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ Thin Films Prepared by MOD Process))

  • 최무용;송석표;정병직;김병호
    • 한국전기전자재료학회논문지
    • /
    • 제12권1호
    • /
    • pp.62-68
    • /
    • 1999
  • Ferroelectric $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$(x=0, 0.1, 0.2, 0.3) thin films were deposited on $Pt/SiO_2/Si$ substrate by MOD(Metalorganic Decomposition) process. Metal carboxylate and metal alkoxide were used as precursors, and 2-methoxyethanol, xylene as solvents. After spin coating, thin films were pre-annealed at $400^{\circ}C$, followed by RTA(Rapid Thermal Annealing) and final annealing at $800^{\circ}C$ in oxygen atmosphere. These procedures were repeated three times to obtain thin films with the thickness of $2000{\AA}$. To enhance the nucleation and growth of layered-perovskite phase, thin films were rapid-thermally annealed above $720^{\circ}C$ in oxygen atmosphere. As RTA temperature increased, fluorite phase was transformed to layered-perovskite phase. And the change of Nb contents affected dielectric / electrical properties and microstructure. The ferroelectric characteristics of $Sr_{0.7}/B_{2.3}(Ta_{1-x}Nb_x)_2O_9$ thin film were Pr=8.67 $\mu{C}/cm^2$, Ec=62.4kV/cm and $I_{L}=1.4\times10^{-7}A/cm^2$ at the applied voltage of 5V, respectively.

  • PDF

성장 온도에 따른 InP/GaP SPS 구조의 광학적 특성

  • 변혜령;류미이;송진동
    • 한국진공학회:학술대회논문집
    • /
    • 한국진공학회 2013년도 제45회 하계 정기학술대회 초록집
    • /
    • pp.229.1-229.1
    • /
    • 2013
  • 초격자는 동종의 III-V 삼원 합금층을 성장하는 동안 스피노달 분해(spinodal decomposition)로 인한 원자배열(atomic ordering)과 상분리phase separation)에 의해서 발생하는데 MBE (molecular beam epitaxy)과 MOVPE (metalorganic vapor phase epitaxy)를 이용하여 성장시킬 때 주로 발생한다. 본 논문에서는 성장온도에 따른 InP/GaP SPS (short-period superlattices) 구조의 광학적 특성 변화를 시료의 온도와 여기광의 세기를 이용하여 분석하였다. 시료는 MBE 장비를 이용하여 성장하였으며, SPS층은 659쌍의 GaP(2.9 ${\AA}$)과 InP(3.1 ${\AA}$)로 이루어져 있고, GaP 층을 처음에 증착한 뒤, InP 층을 증착 하였다. 성장시 온도를 $400^{\circ}C$, $425^{\circ}C$, $460^{\circ}C$ 그리고 $490^{\circ}C$로 변화를 주어 성장하였다. 이들 시료를 GT400, GT425, GT460 그리고 GT490이라 하였고 이에 대한 광학적 특성을 PL (photoluminescence)를 이용하여 분석하였다. 10 K에서 PL 피크는 GT400 시료는 634 nm, GT425 시료는 636 nm, GT460 시료는 680nm, 그리고 GT490 시료는 692 nm에서 나타났으며, GT425 시료의 PL 세기가 가장 강하게 나타나고 GT400 시료의 PL 세기가 가장 약하게 나타났다. 그러나 260 K에서 PL 세기는 GT460 시료가 가장 강하게 나타나고 GT425 시료가 가장 약하게 나타났다. 성장온도가 증가함에 따라 밴드갭이 감소하는 것은 특정 성장온도($460^{\circ}C$) 이상에서 LCM (lateral composition modulation)이 형성되는 것으로 설명할 수 있다. GT400 시료와 GT425 시료의 PL 피크가 1.94 eV와 1.95 eV로 비슷하고, GT460 시료와 GT490 시료의 PL 피크가 1.82 eV과 1.79 eV로 비슷하게 나타난 것은 $460^{\circ}C$이상에서 성장한 시료에서 LCM 구조 형성으로 설명할 수 있다.

  • PDF