• 제목/요약/키워드: Metallic implants

검색결과 32건 처리시간 0.023초

저진공 분위기 전기방전소결에 의해 제조된 다공성 Ti-6Al-4V 임플란트의 표면특성 연구 (Surface Characteristics of Porous Ti-6Al-4V Implants Fabricated by Electro-Discharge-Sintering in a Low Vacuum Atmosphere)

  • 현창용;허재근;이원희
    • 한국재료학회지
    • /
    • 제16권3호
    • /
    • pp.178-182
    • /
    • 2006
  • A single electro-discharge-sintering (EDS) pulse (1.0 kJ/0.7 g), from a $300{\mu}F$ capacitor, was applied to atomized spherical Ti-6Al-4V powder in a low vacuum to produce porous-surfaced implant compacts. A solid core surrounded by a porous layer was formed by a discharge in the middle of the compact. XPS (X-ray photoelectron spectroscopy) was used to study the surface characteristics of the implant material. C, O, and Ti were the main constituents, with smaller amounts of Al, V, and N. The implant surface was lightly oxidized and was primarily in the form of $TiO_2$ with a small amount of metallic Ti. A lightly etched EDS implant sample showed the surface form of metallic Ti, indicating that EDS breaks down the oxide film of the as-received Ti-6Al-4V powder during the discharge process. The EDS Ti-6Al-4V implant surface also contained small amounts of aluminum oxide in addition to $TiO_2$. However, V detected in the EDS Ti-6Al-4V implant surface, did not contribute to the formation of the oxide film..

Dosimetric Impact of Ti Mesh on Proton Beam Therapy

  • Cho, Shinhaeng;Goh, Youngmoon;Kim, Chankyu;Kim, Haksoo;Jeong, Jong Hwi;Lim, Young Kyung;Lee, Se Byeong;Shin, Dongho
    • 한국의학물리학회지:의학물리
    • /
    • 제28권4호
    • /
    • pp.144-148
    • /
    • 2017
  • When a high density metallic implant is placed in the path of the proton beam, spatial heterogeneity can be caused due to artifacts in three dimensional (3D) computed tomography (CT) scans. These artifacts result in range uncertainty in dose calculation in treatment planning system (TPS). And this uncertainty may cause significant underdosing to the target volume or overdosing to normal tissue beyond the target. In clinical cases, metal implants must be placed in the beam path in order to preserve organ at risk (OARs) and increase target coverage for tumors. So we should introduce Ti-mesh. In this paper, we measured the lateral dose profile for proton beam using an EBT3 film to confirm dosimetric impact of Ti-mesh when the Ti-mesh plate was placed in the proton beam pathway. The effect of Ti-mesh on the proton beam was investigated by comparing the lateral dose profile calculated from TPS with the film-measured value under the same conditions.

Comparative evaluation of roughness of titanium surfaces treated by different hygiene instruments

  • Unursaikhan, Otgonbayar;Lee, Jung-Seok;Cha, Jae-Kook;Park, Jung-Chul;Jung, Ui-Won;Kim, Chang-Sung;Cho, Kyoo-Sung;Choi, Seong-Ho
    • Journal of Periodontal and Implant Science
    • /
    • 제42권3호
    • /
    • pp.88-94
    • /
    • 2012
  • Purpose: The use of appropriate instruments to clean surfaces with minimal change, is critical for the successful maintenance of a dental implant. However, there is no consensus about the type and methodology for such instruments. The aim of this study was to characterize changes in the roughness of titanium surfaces treated by various scaling instruments. Methods: Thirty-seven identical disks (5 mm in diameter) were investigated in this study. The specimens were divided into eight groups according to the types of instrumentation and the angle of application. Ultrasonic scaling systems were applied on a titanium disk to simulate standard clinical conditions. The equipment included a piezoelectric ultrasonic scaler with a newly developed metallic tip (NS group), a piezoelectric ultrasonic scaler with a conventional tip (CS group), a piezoelectric root planer ultrasonic scaler with a conventional tip (PR group), and a plastic hand curette (PH group). In addition, the sites treated using piezoelectric ultrasonic scaler systems were divided two sub-groups: 15 and 45 degrees. The treated titanium surfaces were observed by scanning electron microscopy (SEM), and the average surface roughness (Ra) and mean roughness profile depth (Rz) were measured with a profilometer. Results: SEM no significant changes in the titanium surfaces in the NS group, regardless of the angle of application. The PH group also showed no marked changes to the titanium surface, although some smoothening was observed. All CS and PR sites lost their original texture and showed irregular surfaces in SEM analysis. The profilometer analysis demonstrated that the roughness values (Ra and Rz) of the titanium surfaces increased in all, except the PH and NS groups, which showed roughness decreases relative to the untreated control group. The Ra value differed significantly between the NS and PR groups (P<0.05). Conclusions: The results of this study indicated that changes in or damage to titanium surfaces might be more affected by the hardness of the scaler tip than by the application method. Within the limitations of this study, the newly developed metallic scaler tip might be especially suitable for peri-implant surface decontamination, due to its limited effects on the titanium surface.

Loosening torque of Universal Abutment screws after cyclic loading: influence of tightening technique and screw coating

  • Bacchi, Atais;Regalin, Alexandre;Bhering, Claudia Lopes Brilhante;Alessandretti, Rodrigo;Spazzin, Aloisio Oro
    • The Journal of Advanced Prosthodontics
    • /
    • 제7권5호
    • /
    • pp.375-379
    • /
    • 2015
  • PURPOSE. The purpose of this study was to evaluate the influence of tightening technique and the screw coating on the loosening torque of screws used for Universal Abutment fixation after cyclic loading. MATERIALS AND METHODS. Forty implants (Titamax Ti Cortical, HE, Neodent) (n=10) were submerged in acrylic resin and four tightening techniques for Universal Abutment fixation were evaluated: A - torque with 32 Ncm (control); B - torque with 32 Ncm holding the torque meter for 20 seconds; C - torque with 32 Ncm and retorque after 10 minutes; D - torque (32 Ncm) holding the torque meter for 20 seconds and retorque after 10 minutes as initially. Samples were divided into subgroups according to the screw used: conventional titanium screw or diamond like carbon-coated (DLC) screw. Metallic crowns were fabricated for each abutment. Samples were submitted to cyclic loading at $10^6$ cycles and 130 N of force. Data were analyzed by two-way ANOVA and Tukey's test (5%). RESULTS. The tightening technique did not show significant influence on the loosening torque of screws (P=.509). Conventional titanium screws showed significant higher loosening torque values than DLC (P=.000). CONCLUSION. The use of conventional titanium screw is more important than the tightening techniques employed in this study to provide long-term stability to Universal Abutment screws.

Morphology of Bone-like Apatite Formation on Sr and Si-doped Hydroxyapatite Surface of Ti-6Al-4V Alloy after Plasma Electrolytic Oxidation

  • Yu, Ji-Min;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.79-79
    • /
    • 2017
  • Metallic biomaterials have been mainly used for the fabrication of medical devices for the replacement of hard tissue such as artificial hip joints, bone plates, and dental implants. Because they are very reliable on the viewpoint of mechanical performance. This trend is expected to continue. Especially, Ti and Ti alloys are bioinert. So, they do not chemically bond to the bone, whereas they physically bond with bone tissue. For their poor surface biocompatibility, the surface of Ti alloys has to be modified to improve the surface osteoinductivity. Recently, ceramic-like coatings on titanium, produced by plasma electrolytic oxidation (PEO), have been developed with calciumand phosphorus-enriched surfaces. A lso included the influences of coatings, which can accelerate healing and cell integration, as well as improve tribological properties. However, the adhesions of these coatings to the Ti surface need to be improved for clinical use. Particularly Silicon (Si) has been found to be essential for normal bone, cartilage growth and development. This hydroxyapatite, modified with the inclusion of small concentrations of silicon has been demonstrating to improve the osteoblast proliferation and the bone extracellular matrix production. Strontium-containing hydroxyapatite (Sr-HA) was designed as a filling material to improve the biocompatibility of bone cement. In vitro, the presence of strontium in the coating enhances osteoblast activity and differentiation, whereas it inhibits osteoclast production and proliferation. The objective of this work was to study Morphology of bone-like apatite formation on Sr and Si-doped hydroxyapatite surface of Ti-6Al-4V alloy after plasma electrolytic oxidation. Anodized alloys was prepared at 270V~300V voltages with various concentrations of Si and Sr ions. Bone-like apatite formation was carried out in SBF solution. The morphology of PEO, phase and composition of oxide surface of Ti-6Al-4V alloys were examined by FE-SEM, EDS, and XRD.

  • PDF

Effect of Zn Content on the Corrosion Behavior of Ti-6Al-4V Alloy after Plasma Electrolytic Oxidation

  • Hwang, In-Jo;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2017년도 춘계학술대회 논문집
    • /
    • pp.159-159
    • /
    • 2017
  • Ti-6Al-4V alloy have been used for dental implant because of its excellent biocompatibility, corrosion resistance, and mechanical properties. However, the integration of such implant in bone was not in good condition to achieve improved osseointergraiton. For solving this problem, calcium phosphate (CaP) has been applied as coating materials on Ti alloy implants for hard tissue applications because its chemical similarity to the inorganic component of human bone, capability of conducting bone formation and strong affinity to the surrounding bone tissue. Various metallic elements are known to play an important role in the bone formation and also affect bone mineral characteristics. Especially, Zn is essential for the growth of the human and Zn coating has a major impact on the improvement of corrosion resistance. Plasma electrolytic oxidation (PEO) is a promising technology to produce porous and firmly adherent inorganic Zn containing TiO2(Zn-TiO2)coatings on Ti surface, and the a mount of Zn introduced in to the coatings can be optimized by altering the electrolyte composition. In this study, effect of Zn content on the corrosion behavior of Ti-6Al-4V alloy after plasma electrolytic oxidation were studied by SEM, EDS, XRD, AC impedance, and potentiodynamic polarization test. The potentiodynamic polarization and AC impedance tests for corrosion behaviors were carried out in 0.9% NaCl solution at similar body temperature using a potentiostat with a scan rate of 1.67 mV/s and potential range from -1500 mV to +2000 mV. Also, AC impedance was performed at frequencies ranging from 10 MHz to 100 kHz for corrosion resistance.

  • PDF

Corrosion Behavior of Ti-6Al-4V Alloy after Plasma Electrolytic Oxidation in Solutions Containing Ca, P and Zn

  • Hwang, In-Jo;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2016년도 추계학술대회 논문집
    • /
    • pp.120-120
    • /
    • 2016
  • Ti-6Al-4V alloy have been used for dental implant because of its excellent biocompatibility, corrosion resistance, and mechanical properties. However, the integration of such implant in bone was not in good condition to achieve improved osseointergraiton. For solving this problem, calcium phosphate (CaP) has been applied as coating materials on Ti alloy implants for hard tissue applications because its chemical similarity to the inorganic component of human bone, capability of conducting bone formation and strong affinity to the surrounding bone tissue. Various metallic elements, such as strontium (Sr), magnesium (Mg), zinc (Zn), sodium (Na), silicon (Si), silver (Ag), and yttrium (Y) are known to play an important role in the bone formation and also affect bone mineral characteristics, such as crystallinity, degradation behavior, and mechanical properties. Especially, Zn is essential for the growth of the human and Zn coating has a major impact on the improvement of corrosion resistance. Plasma electrolytic oxidation (PEO) is a promising technology to produce porous and firmly adherent inorganic Zn containing $TiO_2(Zn-TiO_2)$coatings on Ti surface, and the a mount of Zn introduced in to the coatings can be optimized by altering the electrolyte composition. In this study, corrosion behavior of Ti-6Al-4V alloy after plasma electrolytic oxidation in solutions containing Ca, P and Zn were studied by scanning electron microscopy (SEM), AC impedance, and potentiodynamic polarization test. A series of $Zn-TiO_2$ coatings are produced on Ti dental implant using PEO, with the substitution degree, respectively, at 0, 5, 10 and 20%. The potentiodynamic polarization and AC impedance tests for corrosion behaviors were carried out in 0.9% NaCl solution at similar body temperature using a potentiostat with a scan rate of 1.67mV/s and potential range from -1500mV to +2000mV. Also, AC impedance was performed at frequencies ranging from 10MHz to 100kHz for corrosion resistance.

  • PDF

금속 임플란트 소재의 내마모성 향상을 위하여 적용되는 질소 이온주입 및 이온도금법의 한계 (Limitation of Nitrogen ion Implantation and Ionplating Techniques Applied for Improvement of Wear Resistance of Metallic Implant Materials)

  • 김철생
    • 대한의용생체공학회:의공학회지
    • /
    • 제25권2호
    • /
    • pp.157-163
    • /
    • 2004
  • 금속 임플란트 재료들의 마모저항을 향상시키기 위하여 질소 이온주입 및 이온도금 기술을 적용하였다. 질소 이온주입 된 초내식성 스테인리스강(S.S.S)의 마모이온용출 특성을 S.S.S, 316L SS, TiN코팅된 316S SS와 비교 평가하기 위하여 탄소로 원자흡수분광분석기를 이용하여 시편들로부터 마모용출된 Cr과 Ni 이온량을 측정하였다. 또한, 저온아크증착법을 이용하여 TiN, ZrN, TiCN코팅된 Ti(Grade 2)원반의 마모저항을 비교하였고, 질소이온주입 및 질화물 코팅된 표면충의 화학적 조성은 SAES(scanning Auger electron spectroscopy)를 이용하여 분석하였다. 질소 이온주입된 S.S.S 표면으로부터 마모에 의하여 용출된 Cr과 Ni 이온량은 표면처리하지 않은 스테인리스강들에 비하여 크게 감소하였다 그러나 인공고관절에 걸리는 하중조건 하에서 실행된 마모이온용출실험에서 이온에너지 100 KeV로 질소이온 주입된 표면층은 20만회 내에서 쉽게 제거되었다. 질화물 코팅된 Ti 시편들의 마모저항도 크게 향상되었고, 그 마모특성은 코팅층의 화학적 조성에 따라 크게 차이가 났다. 코팅두께 3Um의 코팅시편들 중 TiCN 코팅된 티타늄이 가장 높은 내마모 특성을 보였으나 같은 하중조건 하에서 disk(Ti)-on-disk 마모실험에서 그 질화물 코팅면들의 마모 무게감 소비는 1만회 아래에서 모두 Ti의 마모비와 유사하게 전환되었다. 본 실험으로부터 얻어진 연구결과에 의하면, 100 KeV 질소이온주입 및 두께 3$\mu\textrm{m}$의 길화코팅된 표면층의 경우 표면 경화충의 깊이가 충분치 않아 높은 하중을 받는 임플란트의 마찰부위에 사용하기에는 한계가 있음을 보였다.

Si and Mg doped Hydroxyapatite Film Formation by Plasma Electrolytic Oxidation

  • Park, Seon-Yeong;Choe, Han-Cheol
    • 한국표면공학회:학술대회논문집
    • /
    • 한국표면공학회 2016년도 추계학술대회 논문집
    • /
    • pp.195-195
    • /
    • 2016
  • Titanium and its alloys are widely used as implants in orthopedics, dentistry and cardiology due to their outstanding properties, such as high strength, high level of hemocompatibility and enhanced biocompatibility. Hence, recent works showed that the synthesis of new Ti-based alloys for implant application involves more biocompatible metallic alloying element, such as, Nb, Hf, Zr and Mo. In particular, Nb and Hf are one of the most effective Ti ${\beta}-stabilizer$ and reducing the elastic modulus. Plasma electrolyte oxidation (PEO) is known as excellent method in the biocompatibility of biomaterial due to quickly coating time and controlled coating condition. The anodized oxide layer and diameter modulation of Ti alloys can be obtained function of improvement of cell adhesion. Silicon (Si) and magnesium (Mg) has a beneficial effect on bone. Si in particular has been found to be essential for normal bone and cartilage growth and development. In vitro studies have shown that Mg plays very important roles in essential for normal growth and metabolism of skeletal tissue in vertebrates and can be detected as minor constituents in teeth and bone. The aim of this study is to research Si and Mg doped hydroxyapatite film formation by plasma electrolytic oxidation. Ti-29Nb-xHf (x= 0, 3, 7 and 15wt%, mass fraction) alloys were prepared Ti-29Nb-xHf alloys of containing Hf up from 0 wt% to 15 wt% were melted by using a vacuum furnace. Ti-29Nb-xHf alloys were homogenized for 2 hr at $1050^{\circ}C$. Each alloy was anodized in solution containing typically 0.15 M calcium acetate monohydrate + 0.02 M calcium glycerophosphate at room temperature. A direct current power source was used for the process of anodization. Anodized alloys was prepared using 270V~300V anodization voltage at room. A Si and Mg coating was produced by RF-magnetron sputtering system. RF power of 100W was applied to the target for 1h at room temperature. The microstructure, phase and composition of Si and Mg coated oxide surface of Ti-29Nb-xHf alloys were examined by FE-SEM, EDS, and XRD.

  • PDF

듀얼에너지 CT(kvp switching)의 임상 적용: MAR(Metal Artifact Reduction) 알고리즘의 적용 (Clinical Apply of Dual Energy CT (kVp switching) : A Novel Approach for MAR(Metal Artifact Reduction) Method)

  • 김명성;정종성;김명구
    • Journal of Radiation Protection and Research
    • /
    • 제36권2호
    • /
    • pp.79-85
    • /
    • 2011
  • 본 논고의 목적은 듀얼 에너지 시스템의 금속 인공물 감약 (MAR) 기법을 팬텀과 환자를 대상으로 적용하여보고 그 유용성에 대해서 알아보고자 한다. 사용한 장비는 GE사(社)의 750HD CT이고 AW 4.5 볼륨 share 4 워크스테이션에서 영상 분석을 하였다. 팬텀으로는 victoreen사(社)의 사람 모형 흉부팬텀을 사용하였고 사람 대상은 2010년 12월 20일부터 2011년 2월 10일까지 금속물질이 삽입된 환자 25명을 대상으로 목 부위와 복부 부위에 MAR 알고리즘을 적용하였다. 사용한 파라미터는 복부검사의 경우 GSI-4Body-Large 0.9 sec 40 mm이고 목 부위에서는 GSI-3Body-Medium 0.5 sec 40 mm를 선택하여 시행하였다. 영상시험은 국립암센터 CT영상실에서 기본적으로 시행하고 있는 프로토콜에 MAR 옵션을 적용하여 동일하게 시행하였다. 영상분석은 MAR기법을 적용한 영상과 적용하지 않은 영상에서 검은색 인공물과 줄무늬 인공물이 있는 부위에 관심부위 (ROI)를 설정한 후 hounsfield unit(HU)과 노이즈를 이용한 정량적 평가를 하였고 임상 경험이 풍부한 의사와 방사선사가 CT영상에 대한 평가를 하여 MAR 알고리즘에 대한 유용성을 비교하였다. 환자 대상 시험 결과 MAR 알고리즘을 적용함으로서 금속 인공물이 있는 부위에서의 검은색 인공물(금속이 있는 부위) 과 줄무늬 인공물이 있는 영상에서 HU의 p값이 각각 p=0.01과 p=0.04를 보였지만 금속 인공물의 영향에서 벗어난 부위에서의 노이즈는 오히려 증가하는 모습을 보였다(p=0.05). 그리고 그 외의 영상(금속이 있는 부위에서 1 cm 떨어진 단면 영상) 에서 검은색 인공물과 줄무늬 인공물 부위의 HU와 노이즈의 p값에 대해서는 통계적 유의성은 만족하지 못하였지만 대체적으로 MAR알고리즘을 적용함으로서 금속인공물 발생이 감약 되는 결과를 보였다. 결론적으로 금속 물질이 삽입된 환자의 경우에 MAR 알고리즘을 적용함으로서 조직의 선예도가 적용하지 안했을 때보다 증가하였고 검은색 인공물 발생 또한 개선되는 모습을 보였다.