Incoloy 825합금 및 탄소강의 이종강종간 용접특성 연구 (A Study of Dissimilar Weldability of Incoloy 825 with Mild Steel)

  • 김희봉;이창희
    • 한국재료학회지
    • /
    • 제7권2호
    • /
    • pp.162-170
    • /
    • 1997
  • This study has evaluated the dissimialr weldability of Incoloy 825 Ni base alloy with a mild steel(SS41). Further a compatibility study of wrveral Ni base filler metals with the dissimilar joint between the two alloys was also included. The dissimilar weldability of Incoloy 825 with mild steel is strongly dependent upon the type of the filler metal used. Among the filler metals, ENiCrFe which has a chemical comosition similar to that of Incoloy 825 was found to be most compatible to the joint. In addition, a filler metal which showed a good cracing resistance in one dissimiar alloy combination was not necessarily graranteed to other combination. Microstructural examination with SEM, TEM and Auger revealed that the solidification cracking resestance of the dissimilar joint. between Incoloy 835 and SS41 was closely with the Ti+Nb content and with the content of a low melting eutectic phase of Laves relatibve to that of MC type phase.

  • PDF

Heavy metals and VOCs contamination of urban Broundwaters in Seoul, Korea

  • Park, Seong-Sook;Yun, Seong-Taek;Park, Byoung-Young;Yu, Soon-Young
    • 한국지하수토양환경학회:학술대회논문집
    • /
    • 한국지하수토양환경학회 2002년도 추계학술발표회
    • /
    • pp.291-295
    • /
    • 2002
  • We measured the concentrations of heavy metals and VOCs in groundwaters (N=38) in Seoul. The comparison of our data with U.S. Environmental Protection Agency's Maximum Contaminant Levels for Drinking Water and with the Korean Drinking Water Standards shows that most of the metals except for Fe and Mn do not exceed the levels. However, the concentrations of most heavy metals (esp., Zn, Cu, Cr, Ni) tend to increase in residential and industrialized areas. The examination of the metal speciation using Anodic Stripping Voltammetry (ASV) and TOC analyzer Indicates that large amounts of Zn occur as labile metal fraction, whereas Cu occurs as non- labile forms at many sites, possibly due to its tendency to be adsorbed onto inorganic colloidal particles to form electroinactive species in groundwater. The most frequently existed VOCs in Seoul groundwaters are trichloroethylene and tetrachloroethylene, especially in agricultural, industrial, and high traffic areas.

  • PDF

Effect of Hydrodynamic Condition on the Electrochemical Behavior of Various Metals in 3.5 wt% NaCl Solution

  • Pan, Szu-Jung;Hadinata, Samuel-Sudibyo;Kao, Ruey-Chy;Tsai, Wen-Ta
    • Corrosion Science and Technology
    • /
    • 제14권5호
    • /
    • pp.218-225
    • /
    • 2015
  • The electrochemical behaviors of various metals with and without diamond-like-carbon (DLC) coating in 3.5 wt% NaCl solution were investigated. The effect of hydrodynamic conditions was focused by employing a rotating disc electrode (RDE). The experimental results showed that each bare metal had a more positive corrosion potential and a higher corrosion rate due to enhanced oxygen transport at the higher rotating speed of the RDE. DLC coating caused a substantial increase in the corrosion resistance of all metals studied. However, localized corrosion was still found in the DLC-coated metal at sites where deposition defects existed. Surface morphology examination was performed after the electrochemical test to confirm the roles of hydrodynamic conditions and DLC coating.

이산화타이타늄의 용융염 전기분해 반응기구 규명에 관한 연구 (A Study on the Examination of Reaction Mechanism for Molten Salt Electrolysis of Titanium Dioxide)

  • 조성구;정재영
    • 대한금속재료학회지
    • /
    • 제47권3호
    • /
    • pp.182-187
    • /
    • 2009
  • The molten salt electrolysis is applied to reduce titanium dioxide to titanium metal using calcium chloride as an electrolyte and the reaction mechanism of the reduction process is examined by analyzing the reaction products. The process conditions to obtain titanium metal for $900^{\circ}C$ correspond to 2.9~3.2 V and 24 hours. The reaction products for 2.9 V at $900^{\circ}C$ include irregular-shaped titanium oxides such as $Ti_4O_7$, $Ti_3O_5$ and $Ti_2O_3$ and polyhedral $CaTiO_3$. Using these microstructure analysis, the sequential reaction mechanism for the electrochemical reduction of titanium dioxide to titanium is proposed.

Shear bond strength of veneering porcelain to zirconia and metal cores

  • Choi, Bu-Kyung;Han, Jung-Suk;Yang, Jae-Ho;Lee, Jai-Bong;Kim, Sung-Hun
    • The Journal of Advanced Prosthodontics
    • /
    • 제1권3호
    • /
    • pp.129-135
    • /
    • 2009
  • STATEMENT OF PROBLEM. Zirconia-based restorations have the common technical complication of delamination, or porcelain chipping, from the zirconia core. Thus the shear bond strength between the zirconia core and the veneering porcelain requires investigation in order to facilitate the material's clinical use. PURPOSE. The purpose of this study was to evaluate the bonding strength of the porcelain veneer to the zirconia core and to other various metal alloys (high noble metal alloy and base metal alloy). MATERIAL AND METHODS. 15 rectangular ($4\times4\times9mm$) specimens each of zirconia (Cercon), base metal alloy (Tillite), high noble metal alloy (Degudent H) were fabricated for the shear bond strength test. The veneering porcelain recommended by the manufacturer for each type of material was fired to the core in thickness of 3mm. After firing, the specimens were embedded in the PTFE mold, placed on a mounting jig, and subjected to shear force in a universal testing machine. Load was applied at a crosshead speed of 0.5mm/min until fracture. The average shear strength (MPa) was analyzed with the oneway ANOVA and the Tukey's test ($\alpha$= .05). The fractured specimens were examined using SEM and EDX to determine the failure pattern. RESULTS. The mean shear strength ($\pm\;SD$) in MPa was 25.43 ($\pm\;3.12$) in the zirconia group, 35.87 ($\pm\;4.23$) in the base metal group, 38.00 ($\pm\;5.23$) in the high noble metal group. The ANOVA showed a significant difference among groups, and the Tukey' s test presented a significant difference between the zirconia group and the metal group. Microscopic examination showed that the failure primarily occurred near the interface with the residual veneering porcelain remaining on the core. CONCLUSION. There was a significant difference between the metal ceramic and zirconia ceramic group in shear bond strength. There was no significant difference between the base metal alloy and the high noble metal alloy.

A Novel Method to Fabricate Tough Cylindrical Ti2AlC/Graphite Layered Composite with Improved Deformation Capacity

  • Li, Aijun;Chen, Lin;Zhou, Yanchun
    • 한국세라믹학회지
    • /
    • 제49권4호
    • /
    • pp.369-374
    • /
    • 2012
  • Based on the structure feature of a tree, a cylindrical $Ti_2AlC$/graphite layered composite has been fabricated through heat treating a graphite column and six close-matched thin wall $Ti_2AlC$ cylinders bonded with the $Ti_2AlC$ powders at $1300^{\circ}C$ and low oxygen partial pressure. SEM examination reveals that the bond interlayers between cylinders or that between cylinder and column are not fully dense without any crack formation. During the compressive test, the strain of the $Ti_2AlC$/graphite layered composite is about twice higher than that of the monolithic $Ti_2AlC$ ceramic, and the compressive strength of the layered composite is 348 MPa. The layered composite show the noncatastrophic fracture behaviors due to the debonding and shelling off of the layers, which are different from the monolithic $Ti_2AlC$ ceramic. The mechanism of the improved deformation capacity and noncatastrophic failure modes are attributed to the presence of the central soft graphite column and cracks deflection by the bond interlayers.

철제용기의 보존처리 (Conservation of the Iron Vessel)

  • 박학수;최희윤;김우현;권혁남
    • 박물관보존과학
    • /
    • 제5권
    • /
    • pp.17-22
    • /
    • 2004
  • 일제시대에 발굴되어 여러 편으로 분리되어 있던 철제용기를 보존처리하였다. 보존처리를 통하여 유물을 안정화시키고, 본래의 형상을 복원하였다. 보존처리 결과 철제용기는 굽이 있으며 구연부에 턱이 있고 안으로 오므라드는 유선형이었다. X-선 투과검사 결과 주조과정에서 기공이 많이 발생한 것이 관찰되었으며, 금속조직을 통해 재질이 초정흑연을 가진 과공정 백주철임을 알 수 있었다.

Relationships of Lead, Mercury and Cadmium Levels with the Timing of Menarche among Korean Girls

  • Choi, Hye Seon
    • Child Health Nursing Research
    • /
    • 제26권1호
    • /
    • pp.98-106
    • /
    • 2020
  • Purpose: This study utilized data from the Korean National Health and Nutrition Examination Survey (KNHANES) to explore differences in the timing of menarche in Korean girls according to blood heavy metal concentrations. Methods: This study performed a secondary analysis of cross-sectional data from the sixth KNHANES. Data from 179 female children and adolescents aged 10~18 were included in this study. The relationships of blood heavy metal concentrations (lead, mercury, and cadmium) with age of menarche were analyzed using complex sample multiple logistic regression. Results: In the participants of this study, the geometric mean values of blood lead, mercury, and cadmium concentrations were 1.15±0.04 ㎍/dL, 1.80±0.08 ㎍/L, and 0.30±0.03 ㎍/L, respectively. Mercury poisoning (>5 ㎍/L) was found in 1.5% of participants. Furthermore, significant relationships were found between blood lead and mercury concentrations and age at menarche (p for trend: p<.001 and p=.015, respectively). Conclusion: Through an analysis of national big data, this study found evidence that Korean girls showed a younger age at menarche in response to higher blood lead and mercury concentrations. To prevent and manage precocious puberty in Korean children and adolescents, a systematic policy that monitors both exposure to environmental hazards and blood heavy metal concentrations is needed.

3 차원 프린팅 기술의 열간 체적 성형 공정 적용에 관한 기초 연구 - 예비형상 설계 예 및 열간 금형강으로 적층된 표면 특성 분석 (A Preliminary Study on the Application of Three-Dimensional (3D) Printing Technologies to Hot Bulk Forming Processes - Example of Preform Design and Investigation of Hot-working Tool Steel Deposited Surface)

  • 안동규;김세훈;이호진
    • 한국정밀공학회지
    • /
    • 제31권12호
    • /
    • pp.1093-1100
    • /
    • 2014
  • The goal of this paper is to investigate preliminary the applicability of 3D printing technologies for the development of the hot bulk forming process and die. 3D printing technology based on the plastic material was applied to the preform design of the hot forging process. Plastic hot forging dies were fabricated by Polyjet process for the physical simulation of the workpiece deformation. The feasibility of application of Laser-aided Direct Metal Rapid Tooling (DMT) process to the fabrication of the hot bulk metal forming die was investigated. The SKD61 hot-working tool steel was deposited on the heat treated SKD61 using the DMT process. Fundamental characteristics of SKD 61 hot-working tool steel deposited specimen were examined via hardness and wear experiments as well as the observation of the morphology. Using the results of the examination of fundamental characteristics, the applicability of the DMT process to manufacture hot bulk forming die was discussed.

Ultrasonic Examination of Thick Austenitic Stainless Steel Welds and Factors Influence the Sensitivity

  • Palaniappan, M.;Subbaratnam, R.
    • 비파괴검사학회지
    • /
    • 제23권4호
    • /
    • pp.372-379
    • /
    • 2003
  • The problems encountered by ultrasonic testing of austenitic stainless steel weld joints are discussed in the paper. Due to low thermal conductivity and the occurrence of single phase between the melting point and the room temperature, coarse and oriented grains are formed in such weld metals more in thick sections. This leads to higher scattering at the grain boundaries and low signal to noise ratio, and extensive beam skewing. Experimental results to understand these problem are explained.