• Title/Summary/Keyword: Melting properties

Search Result 1,103, Processing Time 0.039 seconds

Crystal structure and thermal properties of solution crystallized nylon 4,6 (용액 결정성장하의 Nylon 4,6 의 결정구조 및 열적성질)

  • 김연철;홍성권
    • Proceedings of the Materials Research Society of Korea Conference
    • /
    • 1993.05a
    • /
    • pp.99-100
    • /
    • 1993
  • Calorimetric (D.S.C) studies were carried out on the nylon 4,6 single crystals grown from 1,4-butanediol solution at various crystallisation temperatures, based on the assessment of the lamellar thickness by small angle x-ray scattering. Samples were annealed mainly ot get rid of residual solvents inside the crystals. The effect of annealing on the crystal perfection is inferred from the measured thermal properties of the crystals. Accordig to the scanning rates less than 80 K/min., D. S C. melting peaks indicate that changes in the internal morphology of nylon 4,6 crystals preapred at different crystallisation temeratures yield a thermodynamic melting temperature. Tm, of 319 $^{\circ}C$, for the infinitely extended crystal thickness (1/ι). The obtained heat of fusion value for the inginite crystal thickness, Ho, was 270 J/g from the plot of measured feat of fusion ($\Delta$Hm) vs. reciprocal crystal thickness (1/ι). based on these values, the fold surface energy, $\delta$e. of 65.4 erg/$\textrm{cm}^2$ was obtained from Hoffman-Waeeks equation. The thermodynamic melting temperature and heat of fusion of the infinite crystal thickness for the solution grow nylon 4,6 single crystals are found to be higher than of the reported corresponding solution grown nylon 6,6 single crystals. pbtained crystallinity from D. S. C measurements ranges from 40 to 50 %, which is close to the reported yalue for the nylon 6,6 single ctystals but lower than we expected.

  • PDF

Improvement of Thermoelectric Properties in Te-Doped Zintl Phase Magnesium-Antimonide

  • Rahman, Md. Mahmudur;Ur, Soon-Chul
    • Korean Journal of Materials Research
    • /
    • v.31 no.8
    • /
    • pp.445-449
    • /
    • 2021
  • Zintl compound Mg3Sb2 is a promising candidate for efficient thermoelectric material due to its small band gap energy and characteristic electron-crystal phonon-glass behavior. Furthermore, this compound enables fine tuning of carrier concentration via chemical doping for optimizing thermoelectric performance. In this study, nominal compositions of Mg3.8Sb2-xTex (0 ≤ x ≤ 0.03) are synthesized through controlled melting and subsequent vacuum hot pressing method. X-ray diffraction (XRD) and scanning electron microscopy (SEM) are carried out to investigate phase development and surface morphology during the process. It should be noted that 16 at. % of excessive Mg must be added to the system to compensate for the loss of Mg during melting process. Herein, thermoelectric properties such as Seebeck coefficient, electrical conductivity, and thermal conductivity are evaluated from low to high temperature regimes. The results show that Te substitution at Sb sites effectively tunes the majority carriers from holes to electrons, resulting in a transition from p to n-type. At 873 K, a peak ZT value of 0.27 is found for the specimen Mg3.8Sb1.99Te0.01, indicating an improved ZT value over the intrinsic value.

A Study on the Zone Melting Recrystallization of Sequentially Evaporated InSb Thin Films for Improvement of the Electron Mobility (순차 증착한 InSb 박막의 전자 이동도 향상을 위한 대용융 재결정에 관한 연구)

  • 김병윤;현규택;주승기
    • Journal of the Korean Institute of Telematics and Electronics A
    • /
    • v.30A no.6
    • /
    • pp.31-37
    • /
    • 1993
  • InSb thin films were fabricated by zone melting recrystallization of In/Sb multilayered thin films prepared by sequential evaporation. Unreacted metal phase or dispersed metal precipitates lowered the electron mobility and the electron mobility increased with development of (111) prefered orientation. Properties of the film could be controlled by changing mzximum temperature and scanning speed, and the electron mobility as high as 12, 000 cm $^2$/Vsec could be obtained under the optimized conditions.

  • PDF

Variations of Mechanical Properties and Corrosion Rate with Melting Conditions and Alloying Elements in High Silicon Cast Irons (용해조건 및 합금원소 첨가에 따른 고규소 내산주철의 기계적 성질 및 부식속도의 변화)

  • Kim, Jung-Chul;Han, Dong-Woon;Baik, Jin-Hyun;Baik, Seung-Han;Moon, Byung-Moon;Shin, Je-Sik;Lee, Young-Kuk
    • Journal of Korea Foundry Society
    • /
    • v.24 no.4
    • /
    • pp.209-216
    • /
    • 2004
  • High silicon cast irons(HSCI) with the high acid resistance have been used for the prevention of acid corrosion occurring in various structures under acid conditions. However, the HSCI is only known as one of materials which have high acid resistance, but few work has dealt with this material in domestic. Therefore, in this study, the acid resistance of various cast irons with alloying elements and melting conditions have been examined, and studied the influences of the matrix structures, mechanical properties and morphologies of graphite. The results obtained in this study are as follows : In case of melting temperature, the mechanical properties of specimen manufactured with high temperature of $1650^{\circ}C$ showed higher value because the inclusion and impurity were removed. In case of pouring temperature, the mechanical properties of specimen fabricated below $1350^{\circ}C$ of pouring temperature showed higher value because the amount of gas absorption from atmosphere decreased during the solidification time. The corrosion rate decreased with increase in Si content. On the other hand, Mn addition appeared an opposite trend with Si.

Synthesis and Thermoelectric Properties of Skutterudite CoSb3 (Skutterudite CoSb3의 합성 및 열전특성)

  • Kim I. H.;You S. W.;Park J. B.;Lee J. I.;Ur S. C.;Jang K. W.;Choi G. S.;Kim J. S.;Kim H. J.
    • Korean Journal of Materials Research
    • /
    • v.15 no.10
    • /
    • pp.667-670
    • /
    • 2005
  • Binary skutterudite $CoSb_3$ compounds were prepared by the arc melting and hot pressing processes and their thermoelectric properties were investigated in the range from 300 to 600 K. Annealing effect was correlated to phase transformation and homogenization. Thermoelectric properties of the arc-melted and hot-pressed $CoSb_3$ were discussed and compared. Undoped intrinsic $CoSb_3$ prepared by the arc melting showed p-type conduction, while it showed metallic behavior with increasing measuring temperature. However, hot pressed specimens showed n-type conduction, possibly due to Sb evaporation. Thermoelectric properties were remarkably improved by annealing In vacuum and they were closely related to phase transformation.

Material Characteristics of Ti-6Al-4V Alloy Manufactured by Electron Beam Melting for Orthopedic Implants (전자빔 용해 방법으로 제조된 정형외과 임플란트용 Ti-6Al-4V 합금의 재료 특성 분석)

  • Gang, Gwan-Su;Jeong, Yong-Hun;Jang, Tae-Gon;Yang, Jae-Ung;Jeong, Jae-Yeong;Park, Gwang-Min;U, Su-Heon;Park, Tae-Hyeon
    • Proceedings of the Korean Institute of Surface Engineering Conference
    • /
    • 2018.06a
    • /
    • pp.25-25
    • /
    • 2018
  • Electron beam melting (EBM) is one of powder based additive manufacturing technology used to produce parts for high geometrical complexity and directly with three-dimensional computer aided design (CAD) model. It is kind of the most promising methods with additive manufacturing for a wide range of medical applications, such as orthopedic, dental implant, and etc. This research has been investigated the microstructure and mechanical properties of as fabricated and hot iso-static pressing (HIP) processed specimens, which are made by an Arcam A1 EBM system. The Ti-6Al-4V titanium alloy powder was used as a material for the 3 dimensional printing specimens. Mechanical properties were conducted with EBM manufacturing and computer numerical control (CNC) machining specimens, respectively. Surface morphological analysis was conducted by scanning electron microscopy (SEM) for their surface, dissected plan, and fractured surface after tensile test. The mechanical properties were included tensile stress-strain and nano-indentation test as a analysis level between nano and macro. As following highlighted results, the stress-strain curves on elastic region were almost similar between as fabricated and HIP processed while the ductile (plastic deformed region) properties were higher with HIP than that of as fabricated processed.

  • PDF

Properties of the White 5K Au-Ag-In Alloys with Indium Contents (백색 5K Au-Ag-In 합금재의 인듐 첨가량에 따른 물성 변화)

  • Song, Jeongho;Song, Ohsung
    • Korean Journal of Materials Research
    • /
    • v.27 no.7
    • /
    • pp.381-385
    • /
    • 2017
  • In order to replace 14K white gold alloys, the properties of 5K white gold alloys (Au20-Ag80) were investigated by changing the contents of In (0.0-10.0 wt%). Energy dispersive X-ray spectroscopy (EDS) was used to determine the precise content of alloys. Properties of the alloys such as hardness, melting point, color difference, and corrosion resistance were determined using Vickers Hardness test, TGA-DTA, UV-VIS-NIR-colorimetry, and salt-spray tests, respectively. Wetting angle analysis was performed to determine the wettability of the alloys on plaster. The results of the EDS analysis confirmed that the Au-Ag-In alloys had been fabricated with the intended composition. The results of the Vickers hardness test revealed that each Au-Ag-In alloy had higher mechanical hardness than that of 14K white gold. TGA-DTA analysis showed that the melting point decreased with an increase in the In content. In particular, the alloy containing 10.0 wt% In showed a lower melting temperature (> $70^{\circ}C$) than the other alloys, which implied that alloys containing 10.0 wt% In can be used as soldering materials for Au-Ag-In alloys. Color difference analysis also revealed that all the Au-Ag-In alloys showed a color difference of less than 6.51 with respect to 14K white gold, which implied a white metallic color. A 72-h salt-spray test confirmed that the Au-AgIn alloys showed better corrosion resistance than 14K white gold alloys. All Au-Ag-In alloys showed wetting angle similar to that of 14K white gold alloys. It was observed that the 10.0 wt% In alloy had a very small wetting angle, further confirming it as a good soldering material for white metals. Our results show that white 5K Au-Ag-In alloys with appropriate properties might be successful substitutes for 14K white gold alloys.

Effect of Gelation Condition on Physical Properties of Yellowfin Sole Gelatin Prepared by Ethanol Fractional Precipitation (에탄올처리 각시가자미껍질 젤라틴의 물리적 특성에 대한 겔화조건의 영향)

  • Kim, Jin-Soo;Cho, Soon-Yeong;Ha, Jin-Hwan;Lee, Eung-Ho
    • Korean Journal of Food Science and Technology
    • /
    • v.27 no.4
    • /
    • pp.483-486
    • /
    • 1995
  • With a view to increase utility of ethanol fractionated fish skin gelatin as a food source, the effect of gelation condition on physical properties of the gelatin was investigated. The physical properties of gelatins treated with or without ethanol were improved with a concentration of gelatin increased. The properties such as gel strength, melting point and gelling point of 10% gelatin sol or gel were reached to maximum at pH 6.0 in ethanol treated gelatin and pH 5.0 in non treated one, respectively. Gel strength and melting point of both gelatin gels chilled for long time at low temperature were superior to those of both gelatin gels chilled for short time at high temperature. Gel strength, melting point and gelling point of ethanol treated gelatin gel or sol prepared under optimized gelation conditioning were superior to those of non treated one.

  • PDF

Effect of Sn Doping on the Thermoelectric Properties of P-Type Mg3Sb2 Synthesized by Controlled Melting, Pulverizing Followed by Vacuum Hot Pressing

  • Rahman, Md. Mahmudur;Kim, Il-Ho;Ur, Soon-Chul
    • Korean Journal of Materials Research
    • /
    • v.32 no.3
    • /
    • pp.132-138
    • /
    • 2022
  • Zintl phase Mg3Sb2 is a promising thermoelectric material in medium to high temperature range due to its low band gap energy and characteristic electron-crystal phonon-glass behavior. P-type Mg3Sb2 has conventionally exhibited lower thermoelectric properties compared to its n-type counterparts, which have poor electrical conductivity. To address these problems, a small amount of Sn doping was considered in this alloy system. P-type Mg3Sb2 was synthesized by controlled melting, pulverizing, and subsequent vacuum hot pressing (VHP) method. X-ray diffraction (XRD) and scanning electron microscopy (SEM) were used to investigate phases and microstructure development during the process. Single phase Mg3Sb2 was successfully formed when 16 at.% of Mg was excessively added to the system. Nominal compositions of Mg3.8Sb2-xSnx (0 ≤ x ≤ 0.008) were considered in this study. Thermoelectric properties were evaluated in terms of Seebeck coefficient, electrical conductivity, and thermal conductivity. A peak ZT value ≈ 0.32 was found for the specimen Mg3.8Sb1.994Sn0.006 at 873 K, showing an improved ZT value compared to intrinsic one. Transport properties were also evaluated and discussed.

Dyeing of Thermal Bonded Polyester Fabric by using Low-melting-point Bicomponent Filament Yarn - Head tie - (저융점 복합사에 의해 열융착된 폴리에스테르 직물의 염색 - 헤드타이를 중심으로 -)

  • Ji, Myeong-Gyo;Lee, Shin-Hee
    • Fashion & Textile Research Journal
    • /
    • v.11 no.4
    • /
    • pp.661-666
    • /
    • 2009
  • The purpose of this study is to analyze the dyeability of polyester(PET) fabric by thermal bonding with low melting component of bicomponent fiber and to describe the change of physical properties of thermal bonded PET fabrics. The PET fabrics were prepared with regular PET fiber as warp and bicomponent fiber as weft. The bicomponent fiber of sheath-core type was composed with a regular PET core and low melting PET sheath. The thermal bonding of PET fabric was carried out in pin tenter($195^{\circ}C$) for 60 seconds. In this study, we investigated the dye ability and fastness of the dyed PET fabric. Dye ability of E-type dyestuff is higher than S-type dyestuff. In the case of E- type dyestuff, the saturated dyeing time was 10minutes at $130^{\circ}C$. The washing fastness and light fastness were excellent as 4-5grade.