• 제목/요약/키워드: Marginal adaptation

검색결과 106건 처리시간 0.021초

SLM 방식으로 제작한 도재관 금속하부구조물의 변연 및 내면 적합도 평가 (Evaluation of marginal and internal fit of metal copings fabricated by selective laser melting)

  • 배성령;이하빈;노미준;김지환
    • 대한치과기공학회지
    • /
    • 제45권1호
    • /
    • pp.1-7
    • /
    • 2023
  • Purpose: To evaluate the marginal and internal fit of metal coping fabricated by a metal three-dimensional (3D) printer that uses selective laser melting (SLM). Methods: An extraoral scanner was used to scan a die of the prepared maxillary right first molar, and the coping was designed using computer-aided design software and saved as an stereo lithography (STL) file. Ten specimens were printed with an SLM-type metal 3D printer (SLM group), and 10 more specimens were fabricated by casting the castable patterns output generated by a digital light processing-type resin 3D printer (casting the 3D printed resin patterns [CRP] group). The fit was measured using the silicon replica technique, and 8 points (A to H) were set per specimen to measure the marginal (points A, H) and internal (points B~G) gaps. The differences among the groups were compared using the Mann-Whitney U-test (α=0.05). Results: The mean of marginal fit in the SLM group was 69.67±18.04 ㎛, while in the CRP group was 117.10±41.95 ㎛. The internal fit of the SLM group was 95.18±41.20 ㎛, and that of the CRP group was 86.35±32 ㎛. As a result of statistical analysis, there was a significant difference in marginal fit between the SLM and CRP groups (p<0.05); however, there was no significant difference in internal fit between the SLM group and the CRP group (p>0.05). Conclusion: The marginal and internal fit of SLM is within the clinically acceptable range, and it seems to be applicable in terms of fit.

다른 스캐닝 방법으로 제작된 리튬 디실리케이트 단관의 변연 및 내면 적합도 평가 (Evaluation of the marginal and internal fit of lithium disilicate crowns fabricated by different scanning methods)

  • 김재홍;김웅철;김지환
    • 대한치과기공학회지
    • /
    • 제36권2호
    • /
    • pp.75-81
    • /
    • 2014
  • Purpose: This study was to compare adaptations of lithium disilicate CAD/CAM crowns fabricated with different scanning systems. Methods: This study selected the mandibular right first molar as an abutment for experiments and produced 10 working models. Lithium disilicate crowns appropriate for each abutment were produced by using a CEREC$^{(R)}$ CAD/CAM system. The independent t-test was then used to compare and analyze the data obtained from the two groups(${\alpha}$=0.05). Results: Mean(SD) adaptation were $86.93(22.82){\mu}m$ for the InS group, $88.42(26.77){\mu}m$ for the ExS group. They were no statistically significant differences between groups for adaptation(p>0.05). Conclusion: Within the limitations of this study, the results suggest that the accuracy of all investigated optical scanner were satisfactory for clinical use. Further assessment and improvement of the lithium disilicate ceramic for the fabrication of FPDs is evidently still required.

혈액투석 환자 가족의 적응 과정 (Adaptation Process of The Family with Hemodialysis)

  • 이영애
    • 재활간호학회지
    • /
    • 제2권2호
    • /
    • pp.184-192
    • /
    • 1999
  • Hemodialysis is a way of treatment for the patients with acute and chronic renal failure. "Marginal man" depicts the enormous amount of stress that hemodialytic patients suffer. It is known that family with chronic illness get stressed along with the patients and they need nursing care also. This qualitative study was conducted in order to identify the family adaptation process in patients with hemodialysis. 6 dyads of hemodialytic patients and caregivers were interviewed for this research. By way of grounded theoretical strategy the data was collected from October 20, 1999 to November 20, 1999. at a hemodialytic unit that was located in Iksan, Chonbuk by the researcher. The main research questions were "What's the adaptation experience of a patient since after being received with hemodialysis?" to the patients, and "What's the family adaptation experience of hemodialysis?" to the caregivers. The collected data was analyzed by grounded theoretical strategy built by Glaser & Strauss in 1967. Results were as follows; 7 grounded concepts were observed from the patients with hemodialysis and 4 grounded concepts were found from the caregivers. Two categories were derived ; 1) Holding hope that is related with treatment 2) Changing a value system.

  • PDF

올인원 접착제의 미세누출에 관한 정량적 분석 (A QUANTITATIVE ANALYSIS ABOUT MICROLEAKAGE OF ALL-IN-ONE ADHESIVES)

  • 강용희;신수일;신동훈
    • Restorative Dentistry and Endodontics
    • /
    • 제29권1호
    • /
    • pp.66-72
    • /
    • 2004
  • All-in-one adhesives were recently developed for reducing the technique sensitivity and chair time, but lots of concerns were made on bondability, longevity, and microleakage. The object of this study was to evaluate microleakage and marginal quality of all-in-one adhesives using electrochemical method and SEM analysis quantitatively. After making Class V cavities, they were bulk filled with Heliomolar(#A1 after surface treatment with three adhesives: Adper Prompt (Group A), One up bond F (Group O), Xeno III (Group X) Electrical conductivity (microamphere, ${\mu}A$) was checked two times: before and after cavity filling. Percentage of leaky margin was estimated from SEM image (${\times}1,000$). The data were statistically analysed: ANOVA and Paired T test for electrical conductivity, Kruskal-Wallis and Mann-Whitney test for marginal quality, Spearman s rho test for checking of relationships between 2 methods. The result were as follows: 1. There was no difference in microleakage between adhesive systems and every specimen showed some of microleakage after filling. 2. Microleakage was reduced about 70% with composite resin filling. 3. Marginal quality was the best in group A. decreasing among groups in the following order: group O, followed by group X. There were significant differences between group A and group X (p=0.015), and between group 0 and group X (p=0.019). 4. There was no relationship between the microleakage measured by electrochemical method and marginal quality measured by SEM analysis. Within the results of this study, there was no difference in microleakage among groups by electrical conductivity. However, significant difference in marginal quality was seen among groups. It was believed that these dissimilar results might be induced because of their own characteristics. Analysis of microleakage needs various methods for accuracy.

Marginal and internal fit of 3D printed provisional crowns according to build directions

  • Ryu, Ji-Eun;Kim, Yu-Lee;Kong, Hyun-Jun;Chang, Hoon-Sang;Jung, Ji-Hye
    • The Journal of Advanced Prosthodontics
    • /
    • 제12권4호
    • /
    • pp.225-232
    • /
    • 2020
  • PURPOSE. This study aimed to fabricate provisional crowns at varying build directions using the digital light processing (DLP)-based 3D printing and evaluate the marginal and internal fit of the provisional crowns using the silicone replica technique (SRT). MATERIALS AND METHODS. The prepared resin tooth was scanned and a single crown was designed using computer-aided design (CAD) software. Provisional crowns were printed using a DLP-based 3D printer at 6 directions (120°, 135°, 150°, 180°, 210°, 225°) with 10 crowns in each direction. In total, sixty crowns were printed. To measure the marginal and internal fit, a silicone replica was fabricated and the thickness of the silicone impression material was measured using a digital microscope. Sixteen reference points were set and divided into the following 4 groups: marginal gap (MG), cervical gap (CG), axial gap (AG), and occlusal gap (OG). The measurements were statistically analyzed using one-way ANOVA and Dunnett T3. RESULTS. MG, CG, and OG were significantly different by build angle groups (P<.05). The MG and CG were significantly larger in the 120° group than in other groups. OG was the smallest in the 150° and 180° and the largest in the 120° and 135° groups. CONCLUSION. The marginal and internal fit of the 3D-printed provisional crowns can vary depending on the build angle and the best fit was achieved with build angles of 150° and 180°.

3차원 프린팅 기술에 의해 제작된 3본 금속 코어의 변연 간격 평가 (Evaluation of Marginal Gap of Three Unit Metal Cores Fabricated by 3-Dimensional Printing Technique)

  • 김재홍;김원수;김기백
    • 치위생과학회지
    • /
    • 제15권2호
    • /
    • pp.196-201
    • /
    • 2015
  • 본 연구에서는 최근 창조경제의 일환으로서 3차원 프린팅 기술의 개발이 눈에 띄게 발전함에 따라 치의학계 보철물 제작 기술에도 영향을 주고 있는 이 기술에 의해 제작된 3본 고정성 보철물의 임상적 허용 가능성을 변연 간격을 기준으로 가늠하여보고자 하였다. 3차원 프린팅 기술에 의해 제작된 보철물 평가와 관련한 연구가 부족함에 따라 본 연구 결과를 통해 해당 종사자들(치과의사, 치과위생과, 치과기공사)에게 참고자료를 제시하고자 하였다. 연구 결과들을 종합하여 보면 3차원 프린팅 기술에 의해 제작된 3본 고정성 보철물은 같은 증례를 대상으로 전통적인 제작방식에 의해 제작된 것보다 변연 간격이 우수하지 못하였다. 비록 몇몇 임상가들이 제시한 임상적 허용 수치 내에는 존재하였으나 기존의 제작 기술을 대신하기 위해서는 앞으로 많은 연구들을 통하여 기술의 발전이 이루어져야 할 것으로 생각된다.

Correlation between different methodologies used to evaluate the marginal adaptation of proximal dentin gingival margins elevated using a glass hybrid

  • Hoda S. Ismail;Brian R. Morrow;Ashraf I. Ali;Rabab El. Mehesen;Franklin Garcia-Godoy;Salah H. Mahmoud
    • Restorative Dentistry and Endodontics
    • /
    • 제47권4호
    • /
    • pp.36.1-36.17
    • /
    • 2022
  • Objectives: This study aimed to evaluate the effect of aging on the marginal quality of glass hybrid (GH) material used to elevate dentin gingival margins, and to analyze the consistency of the results obtained by 3 in vitro methods. Materials and Methods: Ten teeth received compound class II cavities with subgingival margins. The dentin gingival margins were elevated with GH, followed by resin composite. The GH/gingival dentin interfaces were examined through digital microscopy, scanning electron microscopy (SEM) using resin replicas, and according to the World Dental Federation (FDI) criteria. After initial evaluations, all teeth were subjected to 10,000 thermal cycles, followed by repeating the same marginal evaluations and energy dispersive spectroscopy (EDS) analysis for the interfacial zone of 2 specimens. Marginal quality was expressed as the percentage of continuous margin at ×200 for microscopic techniques and as the frequency of each score for FDI ranking. Data were analyzed using the paired sample t-test, Wilcoxon signed-rank test, and Pearson and Spearmen correlation coefficients. Results: None of the testing techniques proved the significance of the aging factor. Moderate and strong significant correlations were found between the testing techniques. The EDS results suggested the presence of an ion-exchange layer along the GH/gingival dentin interface of aged specimens. Conclusions: The marginal quality of the GH/dentin gingival interface defied aging by thermocycling. The replica SEM and FDI ranking results had stronger correlations with each other than either showed with the digital microscopy results.

지르코니아 세라믹 소결조건이 치과보철물의 적합도에 미치는 영향 (Effect of zirconia ceramic sintering condition on the precision of fit in dental restorations)

  • 김재홍;김기백
    • 대한치과기공학회지
    • /
    • 제42권2호
    • /
    • pp.121-128
    • /
    • 2020
  • Purpose: This study aimed to investigate the effects of the sintering conditions of zirconia core on the adaptability. Methods: Ten specimens of each of commercial brand of zirconia(Razor 1100, U&C international, Seoul, Korea) were made and sintered under three different conditions. Specimens were divided into three subgroup(n=10) and sintered with various total time(1hr, 3hr, 9hr) at the maximum temperature(1500℃). The digitized data was superimposed with 3D inspection software to quantitatively obtain the adaptation of a zirconia core, and visual differences were confirmed with a color map. The root mean square(RMS) values of group were statistically analyzed with one-way ANOVA(α=0.05). Results: The overall adaptation of the zirconia cores were as follows; ss-1hr: 36.18±5.2㎛, ss-3hr: 39.55±3.9㎛, cs-9hr: 46.62±4.3㎛. They were statistically significant differences between groups for adaptation(p<0.05). Conclusion: Based on the results of this study, it could be considered that sintering condition of 1500℃ and 1~3 hour is recommended for the better marginal and internal fit. Speed sintering can be widely utilized to fabricate zirconia prothesis as the properties of those almost are to dentistry uses.