• Title/Summary/Keyword: Magnesium potassium phosphate

Search Result 123, Processing Time 0.035 seconds

Feasibility of Phosphorus Recovery from Biological Livestock Wastewater Treatment Plant (생물학적 축산분뇨처리시설에서 인 회수의 가능성 평가)

  • Ahn, Johwan;Kim, Jangho;Min, Sungjae
    • Journal of Korean Society on Water Environment
    • /
    • v.32 no.4
    • /
    • pp.343-348
    • /
    • 2016
  • A chemical sequencing batch reactor was operated to test the feasibility of nutrient recovery from a biological livestock wastewater treatment plant. Both phosphate and ammonia could be successfully recovered as magnesium ammonium phosphate (MAP) crystals. The contents of TP and TN in the recovered MAP crystals were 26.2% and 4.0%, respectively. Zn, Cr and Ti were identified in the crystals, but the contents remained below the Korean standard for an organic fertilizer. Chemical analyses confirmed that the MAP crystals could be useful phosphate fertilizers. On the other hand, the results of physical analyses using an X-ray diffractometer and an energy dispersive X-ray spectrometer strongly suggested that crystalline materials like magnesium potassium phosphate (KMP) and hydroxyapatite (HAP) were also formed during the MAP crystallization, depending on the availability of K+ and Ca2+.

A Study on Early-Age bond strength of Magnesium Potassium Phosphate Mortar (마그네슘 인산칼륨 모르타르의 초기재령 부착성능에 관한 연구)

  • Kang, Hye-Ju;Lee, Yeong-Won;Kim, Jea-Hwan;Kang, Suk-Pyo
    • Proceedings of the Korean Institute of Building Construction Conference
    • /
    • 2015.05a
    • /
    • pp.98-99
    • /
    • 2015
  • In the study, based on analysing bond strength of MPC and existing rapid harding grout according to shape of cross section, early ages shape of cross section is investigated about effect on bond strength to use MPC as an emergency repair material for road defects such as the form of a pot-hole. The result, MPC is about 10% higher than the shear bond strength rapid harding grout, about 20% higher bending bond strength.

  • PDF

Magnesium potassium phosphate cements to immobilize radioactive concrete wastes generated by decommissioning of nuclear power plants

  • Pyo, Jae-Young;Um, Wooyong;Heo, Jong
    • Nuclear Engineering and Technology
    • /
    • v.53 no.7
    • /
    • pp.2261-2267
    • /
    • 2021
  • This paper evaluates the efficacy of magnesium potassium phosphate cements (MKPCs) as waste forms for the solidification of radioactive concrete powder wastes produced by the decommissioning of nuclear power plants. MKPC specimens that contained up to 50 wt% of simulated concrete powder wastes (SCPWs) were evaluated. We measured the porosity and compressive strength of the MKPC specimens, observing them using scanning electron microscopy and X-ray diffraction. The addition of SCPWs reduced the porosity and increased the compressive strength of the MKPC specimens. Struvite-K crystals were well-synthesized, and no additional crystal phase was formed. After thermal cycling and after immersion, MKPC specimens with 50 wt% SCPWs satisfied the waste-acceptance criteria (WAC) for compressive strength. Semi-dynamic leaching tests were performed using the ANS 16.1 method; the leachability indices of Cs, Co, and Sr were 11.45, 17.63, and 15.66, respectively, which also satisfy the WAC. Thus, MKPCs can provide stable matrices to immobilize radioactive concrete wastes generated by the decommissioning of nuclear power plants.

Long-term Variations of Chemical Properties in Controlled Horticultural Soils of Gyeongnam Province

  • Lee, Young-Han;Lee, Seong-Tae;Hong, Kang-Pyo;Lee, Sang-Dae;Kim, Je-Hong;Ok, Yong-Sik;Kim, Min-Keun;Kim, HyeRan
    • Korean Journal of Soil Science and Fertilizer
    • /
    • v.46 no.5
    • /
    • pp.308-312
    • /
    • 2013
  • The monitoring of chemical dynamic changes in controlled horticultural lands is very important for agricultural sustainability. Field monitoring was performed to evaluate the soil chemical properties of 200 controlled horticultural soil samples in Gyeongnam province every 4 years from 2000 to 2012. Soil chemical properties such as pH, amount of organic matter, available phosphate, nitrate nitrogen, and exchangeable potassium, calcium, magnesium, and sodium were analyzed. The amount of exchangeable calcium and soil pH were significantly higher in 2012 than in 2000. In 2012, the frequency distribution for values of pH, organic matter, available phosphate, and exchangeable potassium, calcium, and magnesium that were within the optimum range was 16.0%, 22.5%, 11.5%, 3.5%, 2.5%, and 5.0%, respectively. Especially, available phosphate and exchangeable calcium were excess level with portions of 76.0% and 96.5%, respectively. These results indicated that a balanced management of soil chemical properties can reduce the amount of fertilizer applied for sustainable agriculture in controlled horticultural lands.

Bond Performance of Magnesium Potassium Phosphate Cement Mortar according to Moisture Condition of Substrate (바탕면 함수조건에 따른 마그네시아 인산칼륨 시멘트 모르타르의 부착성능)

  • Kang, Suk-Pyo;Kim, Jae-Hwan
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.21 no.1
    • /
    • pp.15-22
    • /
    • 2017
  • This study focuses on the investigation of bond strength of magnesium potassium phosphate cement mortar(MKPC) according to moisture condition of substrate. Tensile bond test, shear bond test and interfacial bond test are adopted for evaluating the adhesion characteristics of MKPC to conventional cement mortar substrate. The main experimental variables are test methods and moisture levels of substrate. Because the moisture condition of the substrate may be critical to achieving bond, optimum moisture condition for a conventional concrete substrate has evaluated in this study. The results are as follows ; The effects of moisture condition at substrate into the bonding of MKPC are less different than polymer cement mortar and epoxy mortar. But the saturated and surface dry condition is the most appropriate moisture level among the considered, followed by saturated condition and wet condition. Thus, an adequate moisture level of substrate for MKPC is essential for good bond strength.

Solidification/stabilization of simulated cadmium-contaminated wastes with magnesium potassium phosphate cement

  • Su, Ying;Yang, Jianming;Liu, Debin;Zhen, Shucong;Lin, Naixi;Zhou, Yongxin
    • Environmental Engineering Research
    • /
    • v.21 no.1
    • /
    • pp.15-21
    • /
    • 2016
  • Magnesium potassium phosphate cement (MKPC) is an effective agent for solidification/stabilization (S/S) technology. To further explore the mechanism of the S/S by MKPC, two kinds of Cd including $Cd(NO_3)_2$ solution (L-Cd) and municipal solid waste incineration fly ash (MSWI FA) adsorbed Cd (S-Cd), were used to compare the effects of the form of heavy metal on S/S. The results showed that all the MKPC pastes had a high unconfined compressive strength (UCS) above 11 MPa. For L-Cd pastes, Cd leaching concentration increased with the increase of Cd content, and decreased with the increase of curing time. With the percentage of MSWI FA below 20%, S-Cd pastes exhibited similar Cd leaching concentrations as those of L-Cd pastes, while when the content of MSWI FA come up to 30%, the Cd leaching concentration increased significantly. To meet the standard GB5085.3-2007, the highest addition of S-Cd was 30% MSWI FA (6% Cd contained), with the Cd leaching concentration of 0.817 mg/L. The S/S of L-Cd is mainly due to chemical fixation, and the hydration compound of Cd was $NaCdPO_4$, while the S/S of S-Cd is due to physical encapsulation, which is dependent on the pore/crack size and porosity of the MKPC pastes.

Solidification of high level waste using magnesium potassium phosphate compound

  • Vinokurov, Sergey E.;Kulikova, Svetlana A.;Myasoedov, Boris F.
    • Nuclear Engineering and Technology
    • /
    • v.51 no.3
    • /
    • pp.755-760
    • /
    • 2019
  • Compound samples based on the mineral-like magnesium potassium phosphate matrix $MgKPO_4{\times}6H_2O$ were synthesized by solidification of high level waste surrogate. Phase composition and structure of synthesized samples were studied by XRD and SEM methods. Compressive strength of the compounds is $12{\pm}3MPa$. Coefficient of thermal expansion of the samples in the range $250-550^{\circ}C$ is $(11.6{\pm}0.3){\times}10^{-6}1/^{\circ}C$, and coefficient of thermal conductivity in the range $20-500^{\circ}C$ is $0.5W/(m{\times}K)$. Differential leaching rate of elements from the compound, $g/(cm^2{\times}day)$: $Mg-6.7{\times}10^{-6}$, $K-3.0{\times}10^{-4}$, $P-1.2{\times}10^{-4}$, $^{137}Cs-4.6{\times}10^{-7}$; $^{90}Sr-9.6{\times}10^{-7}$; $^{239}Pu-3.7{\times}10^{-9}$, $^{241}Am-9.6{\times}10^{-10}$. Leaching mechanism of radionuclides from the samples at the first 1-2 weeks of the leaching test is determined by dissolution ($^{137}Cs$), wash off ($^{90}Sr$) or diffusion ($^{239}Pu$ and $^{241}Am$) from the compound surface, and when the tests continue to 90-91 days - by surface layer depletion of compound. Since the composition and physico-chemical properties of the compound after irradiation with an electron beam (absorbed dose of 1 MGy) are constant the radiation resistance of compound was established.

A Hardening and Strength Properties of Magnesium Phosphate Mortars for Rapid Repair Materials (급속 보수용 마그네슘 인산염 모르타르의 경화 및 강도특성)

  • Oh, Hongseob;Lee, Inhee
    • Journal of the Korea institute for structural maintenance and inspection
    • /
    • v.23 no.3
    • /
    • pp.103-110
    • /
    • 2019
  • Damage to the pavement system due to various causes will be required rapid repair work for reopening the vehicle traffic. The magnesium oxide phosphate composite(MPC) has a short curing time and is capable of early compressive strength development, is suitable for rapid repair materials. The aim of this study was to evaluate the hardening and compressive strength characteristics of MPC according to the water-binder (W / B) ratio and magnesium-phosphate(M / P) ratio in order to develop repair materials consisted with light burned magnesia and potassium dihydrogen phosphate. In order to ensure the workability in the field application, the difference of mechanical properties according to standard sand and ordinary sand and performance of retards were evaluated. The mix proportion with W/B ratio was about 35% and the M/P ratio was about 1.0 ~ 1.2 has a superior perfomance with strength and hardening condition. Especially, the strength of composite at only 1 day curing with W/B ratio of 0.35 and the M/P ratio of 1.2 was shown the higher than 25.0 MPa. Boric acid as a retarder was found to be suitable for ensuring the working time, and the purity of magnesium oxide was about 90 ~ 95%, which is effective for ensuring curing time and strength.

Soil and Leaf Chemical Properties and Fruit Quality in Kiwifruit Orchard (국내 키위 주산지 토양 및 엽 화학성과 과실 특성)

  • Kim, Hong Lim;Lee, Mock-hee;Chung, Kyeong-Ho
    • Korean Journal of Environmental Agriculture
    • /
    • v.41 no.3
    • /
    • pp.158-166
    • /
    • 2022
  • BACKGROUND: Kiwifruit is a fruit tree with relatively small cultivation area in Korea and researches on its soil and physiology are very limited compared to those on cultivar development. Therefore, there are limited information for farmers to cope with the reduction in productivity due to various physiological disorders and premature aging. This study was conducted to investigate the soil and leaf chemical properties, and fruit characteristics, which will be used as basic data for stable kiwifruit orchard soil management. METHODS AND RESULTS: The soil and leaf chemical properties, and fruit characteristics were investigated for two years in 16 kiwifruit orchards growing 'Hayward' (Actinidia deliciosa) in Jeollanam-do and Gyeongsangnam-do. Soil and leaf samples were collected in July and fruit quality was investigated by harvesting fruits about 170 days after full bloom. The average soil chemical properties of kiwi orchards were generally higher than the recommended level, except for pH, and especially, the exchangeable potassium reached about 300% of the recommended level. The proportions of orchards that exceeded the recommended level of soil chemical properties were 63, 31, 100, 69, 94, 88 and 69% for pH, EC, organic content, available phosphate, and exchangeable potassium, calcium and magnesium, respectively. Thirty-three percent of orchards had more than 100 mg/kg of nitrate nitrogen in soil. Available phosphate in soil showed a significantly positive correlation with leaf nitrogen, phosphoric acid and calcium content, but showed a significantly negative correlation with leaf potassium content. The magnesium content in the leaves was significantly correlated with soil pH. The highest fruit weight was observed in about 25 g/kg of leaf nitrogen content which could be attained when plants were grown on the soil containing about 100 mg/kg of nitrate nitrogen content. The average soluble solids content among 16 orchards was 9.58 °Brix at harvest and 13.9 °Brix after ripening, which increased about 45%, and the average fruit weight was about 110 g. CONCLUSION(S): For fruit quality, fruit soluble solids (sugar compounds) content was significantly correlated with leaf potassium content, fruit hardiness with leaf total nitrate, calcium and magnesium, and fruit titratable acidity with leaf magnesium; however, leaf calcium and magnesium negatively affect the soluble solids contents in fruits.

Effect of Phosphate-to-binder and Water-to-binder Ratio on Magnesia-potassium Phosphate Cement (마그네시아-인산칼륨 시멘트에 대한 인산염 비 및 물-결합재비의 영향)

  • Lee, Kyung-Ho;Yoon, Hyun-Sub;Yang, Keun-Hyeok
    • Journal of the Korea Concrete Institute
    • /
    • v.29 no.3
    • /
    • pp.275-281
    • /
    • 2017
  • This study examined the effect of water-to-binder ratio (W/B) and phosphate-to-binder ratio (P/B) on the flow, setting time, compressive strength development, and pH variation of magnesium-potassium phosphate composites, MKPC mortars. Ten mortars mixtures were prepared with the W/B varying from 20% to 40% at each P/B of 0.3 or 0.5. The hydration products and microstructural pore distribution of the MKPC pastes were investigated using X-ray diffraction (XRD), scanning electron microscope (SEM) and mercury intrusion porosimetry (MIP). The initial flow and setting time of MKPC mortars tended to decrease with an increase of P/B, indicating that the final setting time was shortened by approximately 24% when P/B increased from 0.3 to 0.5. The slope of the early-strength development measured in the MKPC mortars was considerably higher than that of cement concrete specified in code provisions. For obtaining a relatively good 28-day strength (above 30 MPa) and a near neutral pH (below 9.0) in MKPC mortars, the P/B and W/B need to be selected as 0.5 and 30%, respectively. The strubite-K crystal increased with the increases of P/B and W/B, which leads to the decrease of the macro-capillary pores.