오존산화 폐식용유와 pMDI접착제의 합판 접착력 (Bond Strength of Plywood Manufactured with Adhesive of pMDI-Ozonized Waste Cooking Oil)

  • 강찬영;이응수;서준원;박헌
    • Journal of the Korean Wood Science and Technology
    • /
    • 제39권6호
    • /
    • pp.498-504
    • /
    • 2011
  • The purpose of this study was to investigate and develop an eco-frendly wood adhesive based on vegetable oil (especially soybean oil), the renewable and sustainable natural resources, using ozonification technology for the chemical structure modification. The waste soybean oil (WSBO) was reacted with $O_3$ at the rate of $450m{\ell}$(acetone) : $50m{\ell}$ (WSBO) for different times, 1, 2, 3 hrs. The investigation of the modified chemical strecture of the ozonied WSBOs were conducted using FT-IR. As ozonification time increased, the peak of the unsaturated double bonds was disappeared especially ozonized-3hrs and aldehyde or carboxyl peak appeared because ozonification broke the oil into small molecules. The plywood were made at $150^{\circ}C$ with 4 minutes hot-press time using the different ozonized 3 hrs WSBO/pMDI adhesives and were tested for the dry, wet, cyclic boil test according to the Korea Industrial Standard F3101 Ordinary plywood. The bond strengths gradually increased until 1 : 0.5~1 : 3, but it decreased 1 : 4, as the contents of pMDI increased. The results of the dry, wet and cyclic bond strengths the equivalent ratio was formed approximately between 1 : 2~1 : 3. And the 1 : 1~1 : 4 strengths met constantly the standard requirement of 7.0kgf/$cm^2$ (KS F3101). From the comprehensive view on the results of above experiment, it could be confirmed that ozonized WSBO/pMDI has characteristics of effective reactivity and wet stability showed as an excellent candidate of wood adhesive applications.

고위험집단의 Bayley영아발달 검사 수행에 영향을 미치는 요인 탐색 (Exploratory Study on determinants of the Performance of Bayley Scales of Infant Development in Infants with High Risk)

  • 민동옥
    • 한국보육지원학회지
    • /
    • 제1권1호
    • /
    • pp.83-101
    • /
    • 2005
  • 조산 및 발달지연 등으로 발달장애의 가능성이 높은 고위험집단으로 진단된 132명의 영아를 대상으로 인구통계학적, 산전, 출산시 변인 및 산후 발달지표 등이 Bayley영아발달검사(BSID) 수행에 미치는 영향을 살펴보았다. 인구통계학적, 출생전후의 관련정보 및 영아기의 발달특성을 알기 위해 영아발달 질문지와 병원 의무기록지를 사용하였고, Bayley영아발달검사를 개별적으로 실시하였다. 인구통계학적 변인과 BSID의 인지발달지수(MDI), 동작발달지수(PDI)간의 상관 및 평균비교분석결과 산모의 학력이 높을수록 MDI 및 PDI가 높게 나타났다. 산전(prenatal) 관련변인과 발달간의 관계분석시 산전 산모의 질환과 임신중 약물복용여부는 각각 MDI 및 PDI와 부적 상관을 보였다. 출산시(perinatal) 관련변인에서는 저체중 출산, 인큐베이터, 산소호흡기의 사용 및 조산여부가 MDI 및 PDI와 정적 상관을 보였으며 출산시 질환은 PDI에 부적 영향을 미쳤다. 산후 발달지표 중 옹알이, 첫말의 발달은 BSID의 MDI 및 PDI와 정적 상관을 보였으며, 질환은 PDI와 부적 상관을 나타났다.

  • PDF

Relation between Multidimensional Linear Interpolation and Regularization Networks

  • 엄경식;민병구
    • 한국지능시스템학회논문지
    • /
    • 제7권3호
    • /
    • pp.89-95
    • /
    • 1997
  • This paper examines the relation between multidimensional linear interpolation (MDI) and regularization net-works, and shows that an MDI is a special form of regularization networks. For this purpose we propose a triangular basis function(TBF) network. Also we verified the condition when our proposed TBF becomes a well-known radial basis function (RBF).

  • PDF

Relation between Multidimensional Linear Interpolation and Fuzzy Reasoning

  • 엄경식;민병구
    • 한국지능시스템학회논문지
    • /
    • 제6권4호
    • /
    • pp.34-38
    • /
    • 1996
  • This paper examines the relation between multidimensional linear interpolation(MDI) and fuzzy reasoning, and shows that an MDI is a special form of Tsukamoto's fuzzy reasoning. From this result, we found new possibility of defuzzification strategy.

  • PDF

2-클로로벤질 알코올 및 2,4-디클로로벤질 알코올 유도체를 이용한 TDI, MDI 및 HDI의 가스크로마토그래피 분석 (Gas Chromatographic Analysis of TDI, MDI and HDI Using 2-Chlorobenzyl Alcohol and 2,4-Dichlorobenzyl Alcohol Derivatives)

  • 윤주송;박준호;이강명;최홍순;조영봉;고상백;차봉석
    • 한국산업보건학회지
    • /
    • 제16권3호
    • /
    • pp.222-232
    • /
    • 2006
  • Objectives: The objective of this study was to propose the total isocyanate analytical method which involves derivation of 2,4-toluene diisocyanate(2,4-TDI), 2,6-toluene diisocyanate(2,6-TDI), 4,4'-methylenediphenyl diisocyanate(4,4'-MDI) and 1,6-hexamethylene diisocyanate(1,6-HDI) using 2-chlorobenzyl alcohol(2-CBA) or 2,4-dichlorobenzyl alcohol(2,4-DCBA), and analyzing of hydrolysate of the synthesized urethane with the gas chromatography(GC)/flame ionization detector(FID), GC/pulsed discharge ionization detector-electron capture detector(PD-ECD) and GC/mass selective detector(MSD). Methods: Urethanes were synthesized by reacting 2,4-TDI, 2,6-TDI, 4,4'-MDI and 1,6-HDI to 2-CBA or 2,4-DCBA. Urethanes was verified by TLC, HPLC/UVD and GC/MSD. For field application, the most suitable condition that 2-CBA coated in glass fiber filter removed completely and urethanes were not removed was searched. 2-CBA generated from hydrolysis of urethanes according to hydrolysis conditions. Diisocyanates were collected on field air and analyzed. Results: Urethanes which were white and solid phase synthesized by reacting 2,4-TDI, 2,6-TDI, 4,4'-MDI, 1,6-HDI and 2-CBA or 2,4-DCBA. And urethanes were verified by TLC, HPLC/UVD and GC/MSD. The most suitable conditions to remove 2-CBA coated in glass fiber filter were $87^{\circ}C$ and 20 mmHg and urethanes were not removed under same condition. Hydrolysis yields of urethanes were 99 % to 111 %. 2-CBA, the hydrolysate of urethanes was analyzed by GC/FID, GC/PD-ECD and GC/MSD. Conclusions: Simultaneous analysis of 2,4-TDI, 2,6-TDI, 4,4'-MDI and 1,6-HDI deriving with 2-CBA and 2,4-DCBA, along with a total isocyanate analysis, was feasible with GC/FID, GC/PD-ECD and GC/MSD. This result will be a guide of further study on total isocyanate analysis.

Effect of Interface on the Properties of Polyamide 6/Carbon Nanotube Nanocomposites Prepared by In-situ Anionic Ring-opening Polymerization

  • Min, Jin Hong;Huh, Mongyoung;Yun, Seok Il
    • Composites Research
    • /
    • 제32권6호
    • /
    • pp.375-381
    • /
    • 2019
  • Multiwalled carbon nanotubes (MWCNTs) are covalently functionalized with isocyanates by directly reacting commercial hydroxyl functionalized MWCNTs with excess 4,4'-methylenebis (phenyl isocyanate) (MDI) and hexamethylene diiosocyanate (HDI). HDI-modified MWCNTs results in a higher surface isocyanate density than MDI-modified MWCNTs. Anionic ring-opening polymerization of ε-caprolactam is conducted using a sodium caprolactam initiator in combination with a di-functional hexamethylene-1,6-dicarbamoylcaprolactam activator in the presence of isocyanate functionalized MWCNTs. This polymerization proceeds in a highly efficient manner at relatively low reaction temperature (150℃) and short reaction times (10 min). During the polymerization, the isocyanate functionalized MWCNTs act not only as reinforcing fillers but also as second activators. Nanocomposites with HDI modified MWCNTs exhibit higher reinforcement and faster isothermal crystallization than MDI modified MWCNTs. The results show that PA6 chains grow more effectively from HDI modified MWCNT surface than from MDI modified MWCNT surface, resulting in stronger interaction between PA6 and MWCNTs.

Three-dimensional Capsular Volume Measurements in Multidirectional Shoulder Instability

  • Jun, Yong Cheol;Moon, Young Lae;Elsayed, Moustafa I.;Lim, Jae Hwan;Cha, Dong Hyuk
    • Clinics in Shoulder and Elbow
    • /
    • 제21권3호
    • /
    • pp.134-137
    • /
    • 2018
  • Background: In a previous study undertaken to quantify capsular volume in rotator cuff interval or axillary pouch, significant differences were found between controls and patients with instability. However, the results obtained were derived from two-dimensional cross sectional areas. In our study, we sought correlation between three-dimensional (3D) capsular volumes, as measured by magnetic resonance arthrography (MRA), and multidirectional instability (MDI) of the shoulder. Methods: The MRAs of 21 patients with MDI of the shoulder and 16 control cases with no instability were retrospectively reviewed. Capsular areas determined by MRA were translated into 3D volumes using 3D software Mimics ver. 16 (Materilise, Leuven, Belgium), and glenoid surface area was measured in axial and coronal MRA views. Then, the ratio between capsular volume and glenoid surface area was calculated, and evaluated with control group. Results: The ratio between 3D capsular volume and glenoid surface area was significantly increased in the MDI group ($3.59{\pm}0.83cm^3/cm^2$) compared to the control group ($2.53{\pm}0.62cm^3/cm^2$) (p<0.01). Conclusions: From these results, we could support that capsular volume enlargement play an important role in MDI of the shoulder using volume measurement.

Thermal Decomposition Behavior of Blocked Diisocyanates Derived from Mixture of Blocking Agents

  • Lee Jung Min;Subramani Sankaraiah;Lee Young Soo;Kim Jung Hyun
    • Macromolecular Research
    • /
    • 제13권5호
    • /
    • pp.427-434
    • /
    • 2005
  • To improve the performance and reduce raw material costs, blocked isocyanates were prepared with mixture of blocking agents in many industries. Three blocked isocyanates (adducts) namely $\varepsilon$-caprolactam/benzotriazole-blocked 4,4'-diphenylmethane diisocyanate (MDI), toluene-2,4-diisocyanate (TDI) and 4,4'-dicyclohexyl-methane diisocyanate ($H_{12}$MDI) were synthesized. Six reference adducts were also prepared by blocking MDI, TDI, and $H_{12}$MDI with $\varepsilon$-caprolactam ($\varepsilon$-CL) or benzotriazole. The reactions were carried out in acetone medium and dibutyltin dilaurate (DBTDL) was used as a catalyst. The progress of the blocking reaction was monitored by IR spectroscopy. De-blocking temperatures (dissociation temperatures) of these adducts were studied using DSC and TGA and the results were correlated. As expected, the thermal analysis data showed that de-blocking temperature of blocked aromatic isocyanates was lower than that of the blocked aliphatic isocyanates. The low de-blocking temperature of blocked aromatic isocyanate could be due to electron withdrawing benzene ring present in the blocked isocyanates. It was also found that benzotriazole-blocked adducts de-blocked at higher temperature compared with $\varepsilon$-CL-blocked adducts.

합성(合成)고무 보강제(補强劑) Silica의 화학처리(化學處理)에 관(關)한 연구(硏究)(I) -Silica의 MDI 처리(處理)- (Studies on the Chemical Treatment of Silica for Synthetic Rubber Reinforcement(I) - Silica Treatment by MDI-)

  • 진제용;김홍선;최세영
    • Elastomers and Composites
    • /
    • 제30권1호
    • /
    • pp.20-31
    • /
    • 1995
  • The purpose of this study is to investigate the reinforcement of inorganic filler silica, treated by MDI about SBR vulcanizate. The characteristics of vulcanization, physical properties, surface properties and dynamic properties were investigated after mixing those silica with SBR and unmodified silica with SBR. In this experiment only the quantity of silica was variable. In the vulcanization characteristics tested by rheometer, S-series showed the fastest scorch $time(t_{10})$ and optimum cure $time(t_{90})$. And in test or tensile characteristics hardness, tensile strength, 100%, 300% modulus and elongation were all appeared in the order of M>S-series. The characteristic bonding of urea between unmodified silica and MDI could be confirmed in IR spectrum. The shapes of silicas treated chemically were observed by SEM. And the dispersion of the filler in the SBR composite was uniform. In the dynamic characteristics by the RDS, the order of elastic modulus G' values was as follows : M>S-series, and also the order of damping values was as follows : M>S-series.

  • PDF

A Comparison of the Dielectric Behavior of Aromatic and Aliphatic Polyurethanes in Relation to Transitional Phenomena

  • Kim, Chy Hyung
    • Transactions on Electrical and Electronic Materials
    • /
    • 제18권4호
    • /
    • pp.211-216
    • /
    • 2017
  • The dielectric properties of two polyurethanes (PUs) with different hard segments, i.e., aromatic methylene di-p-phenyl diisocyanate (MDI) and aliphatic hexamethylene diisocyanate (HDI), were investigated in the temperature range of -100 to $100^{\circ}C$ and in the frequency range of 1 Hz to 3 kHz. The ${\alpha}$-relaxations induced by the glass transition of the equivalent soft segments in the two PUs occurred at relaxation times of ${\tau}=3.46{\times}10^{-3}s$ for MDI-PU and ${\tau}=3.39{\times}10^{-2}s$ for HDI-PU at $-20^{\circ}C$, in accord with the temperature-frequency superposition principle, resulting in similar shifting factors. However, different I-relaxations were observed for the two PUs. The I-relaxation of MDI-PU occurred due to the mobility of the chain extenders near $80^{\circ}C$ with a slower shifting rate than the ${\alpha}$-relaxation. On the other hand, I-relaxation arising from both the extender and the unconstrained hard segments of HDI-PU occurred at $70{\sim}100^{\circ}C$, indicating complicated dielectric behavior due to partial interaction with the ${\alpha}$-relaxation at high frequencies. Thus, the I-relaxation of HDI-PU did not follow the superposition principle. The dielectric behaviors of the PUs were mainly influenced by their phase transitions, which were affected by the structure and components of the materials.