Preparation and Electrochemical Performance of CNT Electrode with Deposited Titanium Dioxide for Electrochemical Capacitor

  • Kim, Hong-Il;Kim, Han-Joo;Morita, Masayuki;Park, Soo-Gil
    • Bulletin of the Korean Chemical Society
    • /
    • 제31권2호
    • /
    • pp.423-428
    • /
    • 2010
  • To reduce polarization of electrochemical capacitor based on carbon nanotube, titanium oxide nanoparticles were deposited by ultrasound. The pore distribution of $TiO_2$/CNT nanoparticle exhibited surface area of $341\;m^2g^{-1}$ when $TiO_2$ content was 4 wt %, which was better than that of pristine CNT with surface area of $188\;m^2g^{-1}$. The analyses indicated that titanium oxide (particle diameter < 20 nm) was deposited on the CNT surface. The electrochemical performance was evaluated by using cyclic voltammetry (CV), impedance measurement, and constant-current charge/discharge cycling techniques. The $TiO_2$/CNT composite electrode showed relatively better electrochemical behaviors than CNT electrode by increasing the specific capacitance from $22\;Fg^{-1}$ to $37\;Fg^{-1}$ in 1 M $H_2SO_4$ solution. A symmetric cell assembled with the composite electrodes showed the specific capacitance value of $11\;Fg^{-1}$ at a current loading of $0.5\;mAcm^{-2}$ during initial cycling.

아말감의 표면연마에 관한 전기화학적 연구 (AN ELECTROCHEMICAL STUDY ON SURFACE FINISH OF DENTAL AMALGAM)

  • 석창인;엄정문
    • Restorative Dentistry and Endodontics
    • /
    • 제16권2호
    • /
    • pp.18-32
    • /
    • 1991
  • The purpose of this study was to observe characteristic properties of amalgam through the polarization curves and SEM images from 4 type amalgams (Amalcap, Shofu spherical. Dispersalloy and Tytin) with 3 different surface finish procedures (polishing, burnishing and carving) by using the potentiostats (EG & GPARC) and SEM (Jeol JSM-35). After each amalgam alloy and Hg was triturated as the direction of the manufacturer by means of mechanical amalgamator (Samki), the triturated mass was inserted into the cylndrical metal mold which was 12 mm in diameter and 10 mm in height and was pressed with $100kg/cm^2$. 4 specimens of each type amalgam were burnished with egg burnisher and another 4 specimens of each type amalgam were carved with Hollenback carver. Above 8 specimens and remaining untreated 4 specimens were stored at room temperature for about 7 days. Untreated 4 specimens of each type amalgam were polished with abrasive papers (Deer) from #400 to #1200 and finally on the polishing cloth with $0.5{\mu}m$ and $0.06{\mu}m$ $Al_2O_3 $ powder suspended water. Anodic polarization measurements was employed to compare the corrosion behaviours of the amalgams in 0.9% saline solution at $37^{\circ}C$. The open circuit potential was determined after 30 minutes immersion of specimen in electrolyte. The scan rate was 1 mV/sec and the surface area of amalgam exposed to the solution was $0.64cm^2$ for each specimen. All the potentials reported are with respect to a saturated calomel electrode (SCE). SEM images of each specimen were taken after + 800 mV (SCE) polarization. The results were as follows: 1. The corrosion potential of high copper amalgam was more anodic than that of low copper amalgam. 2. The polished amalgam were more resistant to corrosion than any other burnished and carved amalgam. 3. In the case of polishing, current density of high copper amalgam was lower than that of low copper amalgam.

  • PDF

정전압 분극곡선법에 의한 아말감의 부식 거동에 관한 연구 (A STUDY ON THE CORROSION BEHAVIOUR OF AMALGAMS BY USING OF POTENTIOSTATIC POLARIZATION METHOD)

  • 신동훈;엄정문
    • Restorative Dentistry and Endodontics
    • /
    • 제12권1호
    • /
    • pp.39-49
    • /
    • 1986
  • The purpose of this study was to observe characteristic properties through the polarization curves and SEM images from 4 different types of amalgam obtained by using the potentiostats (Princeton EG & G) & SEM (Jeol/35), and to investigate the degree of corrosion on the oxidation peak of the each phase of amalgam. After each amalgam alloy and Hg was triturated as the direction of the manufacturer by means of the mechanical amalgamator (Shofu Co.), the triturated mass was inserted into the cylindrical metal mold which was 12mm in diameter and 10.0mm in height and was condensed by using routine manner. The specimen was removed from the mold and stored at room temperature for about 24 hours. The standard surface preparation was routinely carried out. Anodic polarization measurement was employed to confirm the corrosion behaviour of the amalgams in a 0.9% saline solution (P.H: 6.8-7.0) at $37^{\circ}C$. The initial rest potential (corrosion potential) was determined after 30 minutes of immersion of specimen in electrolyte, and the potential scan was begun at the point of 100mV cathodic from the corrosion potential. The scan rate was 0.17mV/sec. in the study to observe the degree of corrosion of each phase. SEI and EPMA images on the determined oxidation peaks of each amalgam were observed. The results were as follows: 1. In the four anodic polarization curves, low copper amalgams have three oxidation peaks and high copper amalgams have two oxidation peaks, -270mV, +26mV and +179mV(SEC) in the low copper lathe cut, and -300mV, +39mV and +163mV(SEC) in the low copper spherical. -4mV and +154mV(SEC) in the Dispersalloy, and +17mV and +180mV(SEC) in the Tytin as high copper amalgams. 2. ${\gamma}_2$ phase in the low copper amalgam and ${\eta}$ phase in the high copper amalgam were the most corrodible phases and Ag-Cu eutectic in high copper amalgam was the most slowly corroded phase. 3. Low copper amalgam was more susceptible in corrosion than high copper amalgam.

  • PDF

Corrosion Behavior and Inhibition Studies of AZ31B Magnesium Alloy With and Without Cl- in the Alkaline Electrolytes in Addition with Various Inhibitor Additives

  • Shin, Yoonji;Cho, Kyehyun
    • Corrosion Science and Technology
    • /
    • 제18권6호
    • /
    • pp.243-252
    • /
    • 2019
  • The pitting corrosion and inhibition studies of AZ31B magnesium alloy were investigated in the alkaline solution (pH12) with chloride and inhibitors. The corrosion behavior of passive film with/without Cl- in the alkaline electrolyte were conducted by polarization curve and immersion tests in the presence of various additives (inhibitors) to clarify the inhibition efficiency of pitting corrosion at higher potential region. Critical concentration of pitting corrosion for Mg alloy was evaluated with 0.005 M NaCl in 0.01 M NaOH on the anodic polarization behavior. Critical pitting of AZ31B Mg alloy in 0.01 M NaOH is a function of chlorides; Epit = - 1.36 - 0.2 log [Cl-]. When the Sodium Benzoate (SB) was only used as an inhibitor, a few metastable pits developed on the Mg surface by an immersion test despite no pitting corrosion on the polarization curve meaning that adsorption of SB on the surface is insufficient protection from pitting corrosion in the presence of chloride. The role of SB and Sodium Dodecylbenzenesulfonate (SDBS) inhibitors for the Mg alloy surface in the presence of chloride was suppressed from pitting corrosion to co-adsorb on the Mg alloy surface with strong formation of passive film preventing pitting corrosion.

Diffusion Coefficients of CdSe/CdS Quantum Rods in Water Measured Using Polarized Fluorescence Correlation Spectroscopy

  • Lee, Jaeran;Pack, Chan-Gi;Kim, Soo Yong;Kim, Sok Won
    • Journal of the Optical Society of Korea
    • /
    • 제18권5호
    • /
    • pp.598-604
    • /
    • 2014
  • A polarization fluorescence correlation spectroscopy system based on a confocal microscope was built to study the rotational and translational diffusion of CdSe/CdS quantum rods (Q-rods), with the same and different polarization states between the polarizer and the analyzer (i.e. the XXX and XYY states). The rotational diffusion amplitude showed the dependences on polarization of $0.75{\pm}0.05$ in the XXX state and $0.26{\pm}0.03$ in the XYY state, when the translational diffusion amplitude was 1. The diffusion coefficients of the Q-rods were found based on their translational and rotational diffusion times in the two polarization states, in solutions with viscosity ranging from 0.9 to 6.9 cP. The translational and rotational diffusion coefficients ranged from $1.5{\times}10^{-11}$ to $2.6{\times}10^{-12}m^2s^{-1}$ and from $2.9{\times}10^5$ to $5.6{\times}10^4s^{-1}$, respectively.

All-optical Flip-flop Operation Based on Polarization Bistability of Conventional-type 1.55-㎛ Wavelength Single-mode VCSELs

  • Lee, Seoung-Hun;Jung, Hae-Won;Kim, Kyong-Hon;Lee, Min-Hee
    • Journal of the Optical Society of Korea
    • /
    • 제14권2호
    • /
    • pp.137-141
    • /
    • 2010
  • We report, for the first time to our knowledge, observation of polarization bistability from 1.55-${\mu}m$ wavelength single-mode VCSELs of a conventional cylinder-shape under control of their driving current, and demonstration of all-optical flip-flop (AOFF) operations based on the bistability with optical set and reset pulse injection at a 50 MHz switching frequency. The injection pulse energy was less than 14 fJ. The average on-off contrast ratio of the flip-flopped signals was about 7 dB. These properties of the VCSELs will be potentially useful for future high-speed all-optical signal processing applications.

Heat and mass transfer analysis in air gap membrane distillation process for desalination

  • Pangarkar, Bhausaheb L.;Sane, Mukund G.
    • Membrane and Water Treatment
    • /
    • 제2권3호
    • /
    • pp.159-173
    • /
    • 2011
  • The air gap membrane distillation (AGMD) process was applied for water desalination. The main objective of the present work was to study the heat and mass transfer mechanism of the process. The experiments were performed on a flat sheet module using aqueous NaCl solutions as a feed. The membrane employed was hydrophobic PTFE of pore size 0.22 ${\mu}m$. A mathematical model is proposed to evaluate the membrane mass transfer coefficient, thermal boundary layers' heat transfer coefficients, membrane / liquid interface temperatures and the temperature polarization coefficients. The mass transfer model was validated by the experimentally and fitted well with the combined Knudsen and molecular diffusion mechanism. The mass transfer coefficient increased with an increase in feed bulk temperature. The experimental parameters such as, feed temperature, 313 to 333 K, feed velocity, 0.8 to 1.8 m/s (turbulent flow region) were analyzed. The permeation fluxes increased with feed temperature and velocity. The effect of feed bulk temperature on the boundary layers' heat transfer coefficients was shown and fairly discussed. The temperature polarization coefficient increased with feed velocity and decreased with temperature. The values obtained were 0.56 to 0.82, indicating the effective heat transfer of the system. The fouling was observed during the 90 h experimental run in the application of natural ground water and seawater. The time dependent fouling resistance can be added in the total transport resistance.

임피던스를 이용한 흑연재료의 전극특성에 관한 연구 (A study on the characterization of electrode at graphite materials by impedance spectroscopy)

  • 오한준;김인기;이종호;이영훈
    • 한국결정성장학회지
    • /
    • 제6권4호
    • /
    • pp.571-583
    • /
    • 1996
  • 1 mM의 $[Fe(CN)_{6}]^{3-}/[Fe(CN)_{6}]^{4-}$ 이온이 첨가된 0.5 M $K_{2}SO_{4}$용액에서 Impedance spectroscopy를 통하여 비교적 porous한 표면조직을 갖는 흑연재료인 electrographite와 graphite foil의 계면의 전기화학적 거동을 조사하였다. 이들 두 흑연재료의 변전위 전류 전압곡선의 경우 전극표면의 구조로 인하여 비교적 높은 전류가 나타났으며, graphite foil의 경우 높은 이중층 용량이 나타났다. 또한 두 재료 모두 field transport의 작용에 의해 분극증가에 따른 임피던스 스펙트럼의 변화와 Faraday-임피던스의 변화가 크게 나타나지 않았다. 특히 electrographite의 경우 전극계면에서 흡착현상이 나타났으며, 양극분극의 증가에 의해 흡착현상은 현저하게 증가하였다.

  • PDF

Corrosion Inhibitors For Zinc in 2 M HCI Solution

  • A. S. Fouda;L. H. Madkour;A. A. El-Shafel;S. A. Abd ElMaksoud
    • Bulletin of the Korean Chemical Society
    • /
    • 제16권5호
    • /
    • pp.454-458
    • /
    • 1995
  • Inhibiting action of semicarbazide, thiosemicarbazide, sym. diphenylcarbazide towards corrosion of zinc in hydrochloric acid has been investigated. The rate of corrosion depends on the nature of the inhibitor and its concentration. The values of inhibition efficiency from, weight loss, thermometric measurements are in good agreement with those obtained from polarization studies. From the polarization studies, the inhibitors used act as mixed absorption type inhibitors, increased adsorption resulting from an increase in the electron density at the reactive C=S and C=O groups and N-atoms. The thermodynamic parameters of adsorption obtained using Bockris-Swinkels adsorption isotherm reveal a strong interaction of these carbazides on zinc surface.

적층형 세라믹 액츄에이터의 유전 및 압전특성 (Dielectric and Piezoelectric Properties in Multilayer Ceramic Actuator)

  • 최형봉;정순종;하문수;고중혁;이대수;송재성
    • 한국전기전자재료학회:학술대회논문집
    • /
    • 한국전기전자재료학회 2004년도 하계학술대회 논문집 Vol.5 No.2
    • /
    • pp.615-618
    • /
    • 2004
  • The piezoelectricity and polarization of multilayer ceramic actuators, being designed to stack ceramic layer and electrode layer alternately, were investigated under a consideration of geometry, the thickness ratio of the ceramic layer to electrode layer The actuators were fabricated by tape-casting of $0.42PbTiO_3-0.38PbZrO_3-0.2Pb(Mn_{1/3}Nb_{2/3})O_3$ followed by laminating, burn-out and co-firing process. The actuators of $5\times5mm^2$ in area were formed in a way that $60{\sim}200{\mu}m$ thick ceramics were stacked 10 times alternately with $5{\mu}m$ thick electrode. Increase in polarization and electric field-displacement with increasing thickness ratio of the ceramic/electrode layer and thickness/cross section ratio were attributed to the change of $non-180^{\circ}/180^{\circ}$ domain ratio which was affected by the interlayer internal stress and Poisson ratio of ceramic layer. The piezoelectricity and actuation behaviors were found to be dependent upon the volume ratio (or thickness ratio) of ceramic layer relative to ceramic layer. Concerning with the existence of internal stress, the field-induced polarization and deformation were described in the multilayer actuator.

  • PDF