Effect of WO3 or Ga2O3 Addition on the Phase Evolution and Properties of Y2O3-Doped AlN Ceramics (Y2O3-AlN 세라믹스의 생성상 및 물성에 미치는 WO3 및 Ga2O3의 첨가효과)

  • Shin, Hyunho;Yoon, Sang-Ok;Kim, Shin;Hwang, Injoon
    • Journal of the Korean Ceramic Society
    • /
    • v.50 no.3
    • /
    • pp.206-211
    • /
    • 2013
  • The effect of a $WO_3$ or $Ga_2O_3$ addition on the densification, phase evolution, optical reflectance, and elastic and dielectric properties of $Y_2O_3$-doped AlN ceramics sintered at $1800^{\circ}C$ for 3 h is investigated. The investigated compositions of the additives are 4.5 wt% $Y_2O_3$ (YA), 3.5 wt% $Y_2O_3$-1.0 wt% $Ga_2O_3$ (YGA), and 3.5 wt% $Y_2O_3$-1.0 wt% $WO_3$ (YWA). $YAlO_3$ and $Y_4Al_2O_9$ form as the secondary phases in all of the investigated compositions, whereas $W_2B$ appears additionally in the YWA. In the YGA, Ga is detected in the AlN grains, indicating that the dissolution of $Ga_2O_3$ into the AlN lattice occurs. The addition of $WO_3$ blackens the specimen more significantly than that of $Ga_2O_3$ does. In all of the investigated specimens, the linear shrinkage and the apparent density are above 20 percent and in the range of 3.34-3.37 $g/cm^3$, respectively. The elastic modulus, Poisson's ratio, the dielectric constant, and the dielectric loss are in the ranges of 335-368 GPa, 0.146-0.237, 8.60-8.63, $2.65-3.95{\times}10^{-3}$, respectively. The sinterability and the properties of $Y_2O_3$-doped AlN ceramics are not much altered by the addition of $WO_3$ or $Ga_2O_3$.

A Study on Properties of Domestic Fly Ash and Utilization as an Insulation material (국산 Fly Ash의 특성 및 단열재로의 이용에 관한 연구)

  • 박금철;임태영
    • Journal of the Korean Ceramic Society
    • /
    • v.20 no.2
    • /
    • pp.135-146
    • /
    • 1983
  • This study is to investigate the properties of domestic fly ash for utilization as data in regard to fly ash which is by-product of domestic coal powder plants and the possibility of utilization as insulation material of domestic fly ash. Composition refractoriness size distribution density contents of hollow particles and crystalline phase were examined as the properties of domestic fly ash. As to the fired test pieces of fly ash by itself that varied contents of hollow particles with four kinds and of the fly ash-clay-saw dust system linear shrinkage bulk density app. porosity compressive strength thermal conductivity and structures were investigated for the possibility of utilization as an insulation material. The results are as follows : 1. The properties of the fly ash I) The constituent particle of the fly ash is spherical and it contains not a few hollow particles (floats by water 0.30-0.50 floats by $ZnCl_2$ aq.(SpG=1.71) 6.97-16.72%). ii) The chemical compositions of fly ash are $SiO_243.9-54.1%$ , $Al_2O_321.0-30.7%$ Ig loss is 7.4-24.1% and the principal of Ig loss is unburned carbon. iii) Fly ash was not suitable to use for mortar and concrete mixture because Ig. loss value is higher than 5% 2. Utilization as insulation material I) The test pieces of original fly ash floats by water floats by ZnCl2 aq(SpG=1.71) p, p t by ZnCl2 aq.(SpG=1.71) that were fired at 110$0^{\circ}C$ represented 0.11-0.18 kcal/mh$^{\circ}$ C as thermal conductivity value. ii) The test pieces which (76.5-85.5) wt% fly ash-(8.5, 9.5) wt% clay-(5.0-15.0) wt% saw dust system(68.0-72.0) wt% fly ash -(17.0-18.0)wt% clay-(10.0-15.0) wt% saw dust system and 59.5 wt% fly ash-25.5 wt% clay-15.0wt% saw dust system were fired at 110$0^{\circ}C$ the thermal conductivity was less than 0.1Kcal/mh$^{\circ}$ C. iii) In view of thermal conductivity and economic aspect insulation materials which added saw dust as blowing agent and clay as inorganic binder are better than that of fly ash as it is or separated hollow fly ash particles. iv) When the saw dust contents increased in the (59.5-90.0) wt% saw dust system and when amount of clay de-creased and firing temperature decreased under the condition of equal addition of saw dust app. porosity increased but bulk density compressive strength and thermal conductivity decreased.

  • PDF

Microwave Dielectric Properties of Ultra-Low Temperature Co-firable Ba3V4O13-BaV2O6 Ceramics (Ba3V4O13-BaV2O6계 초저온 동시소성 세라믹스의 마이크로파 유전 특성)

  • Yoon, Sang-Ok;Hong, Seoyoung;Cho, Hyung-Hwan;Kim, Shin
    • Journal of the Korean Institute of Electrical and Electronic Material Engineers
    • /
    • v.34 no.5
    • /
    • pp.342-347
    • /
    • 2021
  • Phase evolution, sintering behavior, microstructure, and microwave dielectric properties of (1-x) mol Ba3V4O13 - (x) mol BaV2O6 system were investigated. The sintered specimens of all compositions consisted of Ba3V4O13 and BaV2O6, and no secondary phase was observed. As x increased, the linear shrinkage decreased to the composition of x=0.5, and then increased again, implying that Ba3V4O13 and BaV2O6 phases interfered mutually with each other during sintering. All compositions showed a dense microstructure with a large grain growth. Cracks were observed in some compositions because of the relatively high sintering temperature of 620~640℃. As x increased, the dielectric constant increased, while the quality factor was maintained from about 50,000 GHz to about 70,000 GHz up to the composition of x=0.9, and then decreased to 20,987~27,180 GHz at the composition of x=1.0. As x increased, the temperature coefficient of the resonance frequency showed a (+) value from a (-) value. The dielectric constant, the quality factor, and the temperature coefficient of resonant frequency of x=0.7 composition sintered at 640℃ for 4 hours were 10.61, 71,126 GHz, and -4.9 ppm/℃, respectively. This composition showed a good chemical compatibility with Al powder, indicating that the Ba3V4O13-BaV2O6 ceramics are a candidate material for ULTCC (Ultra-Low Temperature Co-fired Ceramics) applications.

A Study on the Non-combustible Properties of High-density Fiber Cement Composites Mixed with Hemp Fibers (마 섬유 혼입에 따른 고밀도 섬유 시멘트 복합체의 불연 특성 연구)

  • Jang, Kyong-Pil;Song, Tae-Hyeob
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.10 no.3
    • /
    • pp.314-320
    • /
    • 2022
  • The function of reinforcing fibers used in building materials is to maintain resistance to bending loads and to function for cracking caused by drying shrinkage. High-density fiber-cement composites are mainly used for linear plates and are used to increase bending resistance. Therefore, tensile properties, bonding strength with cement hydrate, alkali resistance, and the like are required. Recently, as the non-combustible performance has been strengthened, a function to minimize the occurrence of sparks during high-temperature heating has been added. Therefore, the use of organic fibers is limited. In this study, a study was conducted to replace polypropylene used as reinforcing fiber with hemp fiber with excellent heat resistance. Hemp fibers have excellent heat resistance, good affinity with cement, and excellent alkali resistance. Based on the total volume of polypropylene fibers used in the existing formulation, the non-combustible performance was compared and evaluated by using hemp fibers instead of the polypropylene fibers, and basic physical properties such as flexural strength were tested. As a result of conducting a non-combustibility and physical property test using hemp fibers with a fiber length of 7 mm using 2 % and 3 % by weight, it was found that there is no remaining time of the flame, and the flexural strength can be secured at 95 % level of the existing polypropylene fiber.

Evaluation of Mechanical Performance Considering Prolonged Length of Glass Fiber-Reinforced Composite on Structure Weakness by Thermal Stress at Secondary Barrier in Cryogenic Liquified Gas Storage (극저온 액화가스 화물창 2차방벽 구조 열 응력 취약 부 Prolonged 길이 고려 유리섬유 강화 복합재 기계적 물성 평가)

  • Yeon-Jae Jeong;Hee-Tae Kim;Jeong-Dae Kim;Jeong-Hyun Kim;Seul-Kee Kim;Jae-Myung Lee
    • Composites Research
    • /
    • v.36 no.4
    • /
    • pp.246-252
    • /
    • 2023
  • A secondary barrier made of glass fiber reinforced composites has been installed infinitely using automatic bonding machine(ABM) in membrane type LNG cargo containment system (CCS). At the same time, significant thermal stress due to cryogenic heat shrinkage has occurred in the composite on the non-bonding area between the adhesive fixation at both ends. There have been studies from the perspective of structural safety evaluation taking this into account, but none that have analyzed mechanical property taking an prolonged length into account. In this study, 2-parameter Weibull distribution statistical analysis was used to standardize reliable mechanical property for actual length, taking into account the composite's brittle fracture of ceramic material with wide fracture strength dispersion. Related experimental data were obtained by performing uniaxial tensile tests at specific temperatures below cryogenic condition considering LNG environment. As a result, the mechanical strength increased about 1.5 times compared to -20℃ at -70℃ and initial non-linear behavior of fiber stretched was suppressed. As the temperature decreased until the cryogenic, the mechanical strength continued to increase due to cold brittleness. The suggested mechanical property in this study would be employed to secure reliable analysis support material property when assessing the safety of secondary barrier's structures.

Treatment Margin Assessment using Mega-Voltage Computed Tomography of a Tomotherapy Unit in the Radiotherapy of a Liver Tumor (간종양 방사선치료 시 토모테라피 메가볼트 CT를 이용한 치료 여백 평가)

  • You, Sei-Hwan;Seong, Jin-Sil;Lee, Ik-Jae;Koom, Woong-Sub;Jeon, Byeong-Chul
    • Radiation Oncology Journal
    • /
    • v.26 no.4
    • /
    • pp.280-288
    • /
    • 2008
  • Purpose: To identify the inter-fractional shift pattern and to assess an adequate treatment margin in the radiotherapy of a liver tumor using mega-voltage computed tomography (MVCT) of a tomotherapy unit. Materials and Methods: Twenty-six patients were treated for liver tumors by tomotherapy from April 2006 to August 2007. The MVCT images of each patient were analyzed from the $1^{st}$ to the $10^{th}$ fraction for the assessment of the daily liver shift by four groups based on Couinard's proposal. Daily setup errors were corrected by bony landmarks as a prerequisite. Subsequently, the anterior-, posterior-, right-, and left shifts of the liver edges were measured by maximum linear discrepancies between the kilo-voltage computed tomography (KVCT) image and MVCT image. All data were set in the 2-dimensional right angle coordinate system of the transverse section of each patient's body. Results: The liver boundary shift had different patterns for each group. In group II (segment 2, 3, and 4), the anterior mean shift was $2.80{\pm}1.73\;mm$ outwards, while the left mean shift was $2.23{\pm}1.37\;mm$ inwards. In group IV (segment 7 and 8), the anterior-, posterior-, right-, and left mean shifts were $0.15{\pm}3.93\;mm$ inwards, $3.15{\pm}6.58\;mm$ inwards, $0.60{\pm}3.58\;mm$ inwards, and $4.50{\pm}5.35\;mm$ inwards, respectively. The reduced volume in group II after MVCT reassessment might be a consequence of stomach toxicity. Conclusion: Inter-fractional liver shifts of each group based on Couinard's proposal were somewhat systematic despite certain variations observed in each patient. The geometrical deformation of the liver by respiratory movement can cause shrinkage in the left margins of liver. We recommend a more sophisticated approach in free-breathing mode when irradiating the left lobe of liver in order to avoid stomach toxicity.