• Title/Summary/Keyword: Laser sheet

Search Result 428, Processing Time 0.029 seconds

Micro-LIF measurement of microchannel flow

  • Kim Kyung Chun;Yoon Sang Youl
    • 한국가시화정보학회:학술대회논문집
    • /
    • 2004.12a
    • /
    • pp.65-74
    • /
    • 2004
  • Measurement of concentration distributions of suspended particles in a micro-channel is out of the most crucial necessities in the area of Lab-on-a-chip to be used for various bio-chemical applications. One most feasible way to measure the concentration field in the micro-channel is using micro-LIF(Laser Induced Fluorescence) method. However, an accurate concentration field at a given cross plane in a micro-channel has not been successfully achieved so far due to various limitations in the light illumination and fluorescence signal detection. The present study demonstrates a novel method to provide an ultra thin laser sheet beam having five(5) microns thickness by use of a micro focus laser line generator. The laser sheet beam illuminates an exact plane of concentration measurement field to increase the signal to noise ratio and considerably reduce the depth uncertainty. Nile Blue A was used as fluorescent dye for the present LIF measurement. The enhancement of the fluorescent intensity signals was performed by a solvent mixture of water $(95\%)$ and ethanol (EtOH)/methanol (MeOH) $(5\%)$ mixture. To reduce the rms errors resulted from the CCD electronic noise and other sources, an expansion of grid size was attempted from $1\times1\;to\;3\times3\;or\;5\times5$ pixel data windows and the pertinent signal-to-noise level has been noticeably increased accordingly.

  • PDF

A study of Physically Implanted Surface Islands by direct Nd:YAG Laser Beam Irradiation

  • Oh, Chang-Heon;Cheon, Suyoung;Lim, Changjin;Lee, Jeongjun;Jeon, Jihyun;Kim, Kyoung-Kook;Chung, Chan-Moon;Cho, Soohaeng
    • Applied Science and Convergence Technology
    • /
    • v.26 no.4
    • /
    • pp.66-69
    • /
    • 2017
  • Physically implanted surface islands of Nano Carbon Tube (NCT) and ${\alpha}-F_2O_3$ particles have been produced on Al-doped ZnO (AZO)/glass surfaces by simple and direct ND:YAG laser beam irradiation. Sheet resistance of the reconstructed surface increased by about 3.6% of over AZO. Minimal surface damage can be repaired by ND:YAG laser beam irradiation in conjunction with proper impurities. Implanted islands of NCT, which are considered to be a good conductive impurity, on AZO increased the sheet resistance by about 1.8%, while implanted islands of ${\alpha}-F_2O_3$, an insulating impurity, on AZO increased sheet resistance by about 129% compared with a laser beam treated AZO. This study provides insight regarding surface implantations of nanowires and micro-circuits, doping effects for semiconductors and optical devices, surface area and impurity effects for catalysis.

Boron Doping Method Using Fiber Laser Annealing of Uniformly Deposited Amorphous Silicon Layer for IBC Solar Cells (IBC형 태양전지를 위한 균일하게 증착된 비정질 실리콘 층의 광섬유 레이저를 이용한 붕소 도핑 방법)

  • Kim, Sung-Chul;Yoon, Ki-Chan;Kyung, Do-Hyun;Lee, Young-Seok;Kwon, Tae-Young;Jung, Woo-Won;Yi, Jun-Sin
    • Proceedings of the Korean Institute of Electrical and Electronic Material Engineers Conference
    • /
    • 2009.06a
    • /
    • pp.456-456
    • /
    • 2009
  • Boron doping on an n-type Si wafer is requisite process for IBC (Interdigitated Back Contact) solar cells. Fiber laser annealing is one of boron doping methods. For the boron doping, uniformly coated or deposited film is highly required. Plasma enhanced chemical vapor deposition (PECVD) method provides a uniform dopant film or layer which can facilitate doping. Because amorphous silicon layer absorption range for the wavelength of fiber laser does not match well for the direct annealing. In this study, to enhance thermal affection on the existing p-a-Si:H layer, a ${\mu}c$-Si:H intrinsic layer was deposited on the p-a-Si:H layer additionally by PECVD. To improve heat transfer rate to the amorphous silicon layer, and as heating both sides and protecting boron eliminating from the amorphous silicon layer. For p-a-Si:H layer with the ratio of $SiH_4$ : $B_2H_6$ : $H_2$ = 30 : 30 : 120, at $200^{\circ}C$, 50 W, 0.2 Torr for 30 minutes, and for ${\mu}c$-Si:H intrinsic layer, $SiH_4$ : $H_2$ = 10 : 300, at $200^{\circ}C$, 30 W, 0.5 Torr for 60 minutes, 2 cm $\times$ 2 cm size wafers were used. In consequence of comparing the results of lifetime measurement and sheet resistance relation, the laser condition set of 20 ~ 27 % of power, 150 ~ 160 kHz, 20 ~ 50 mm/s of marking speed, and $10\;{\sim}\;50 {\mu}m$ spacing with continuous wave mode of scanner lens showed the correlation between lifetime and sheet resistance as $100\;{\Omega}/sq$ and $11.8\;{\mu}s$ vs. $17\;{\Omega}/sq$ and $8.2\;{\mu}s$. Comparing to the singly deposited p-a-Si:H layer case, the additional ${\mu}c$-Si:H layer for doping resulted in no trade-offs, but showed slight improvement of both lifetime and sheet resistance, however sheet resistance might be confined by the additional intrinsic layer. This might come from the ineffective crystallization of amorphous silicon layer. For the additional layer case, lifetime and sheet resistance were measured as $84.8\;{\Omega}/sq$ and $11.09\;{\mu}s$ vs. $79.8\;{\Omega}/sq$ and $11.93\;{\mu}s$. The co-existence of $n^+$layeronthesamesurfaceandeliminating the laser damage should be taken into account for an IBC solar cell structure. Heavily doped uniform boron layer by fiber laser brings not only basic and essential conditions for the beginning step of IBC solar cell fabrication processes, but also the controllable doping concentration and depth that can be established according to the deposition conditions of layers.

  • PDF

Forming Characteristics of Laser Welded Tailored Blanks III : Stretch Forming Characteristics (레이저 용접 테일러드 블랭크의 기본 성형특성 III : 신장성형 특성)

  • Park, Gi-Cheol;Han, Su-Sik;Jin, Jo-Gwan;Gwon, O-Jun
    • Transactions of Materials Processing
    • /
    • v.7 no.4
    • /
    • pp.354-363
    • /
    • 1998
  • In order to analyze the stretch forming characteristics of tailored blanks, laser welded blanks of different thickness and strength combinations were prepared and stretching tests were done. The stretching formability of laser welded blanks was reduced as increasing the deformation restraining force ($strength{\times}thickness$) ratio between two welded sheets. Weld line movement was attributed to strain concentration at weaker sheets and resulted in fracture at weaker sid, so that fracture could be predicted by the forming limit of the weak sheet. In the case of a welded blank with the similar deformation restraining force rations between two welded sheets, crack occurred at weld and its forming limit was about 15% less than the base sheet. The effects of lubrication and weld line position on stretch-ing formability were also investigated by experiments. Lower friction did not always give better formability for tailored blanks. Stretching formability was observed to be improved as increasing the area of weak sheet.

  • PDF

Forming Characteristics of Laser Welded Tailored Blanks (레이저 용접 테일러드 블랭크의 성형특성)

  • 박기철;한수식;김광선;권오준
    • Proceedings of the Korean Society for Technology of Plasticity Conference
    • /
    • 1998.06a
    • /
    • pp.121-130
    • /
    • 1998
  • In order to analyze the forming characteristics of laser welded tailored blanks, laser welded blanks of different thickness and strength combinations were prepared and tensile, stretching, stretch flanging and deep drawing tests were done. The tensile elongation perpendicular to the weld line, stretching and stretch flanging formability decreased with increasing the deformation restraining force (strength ${\times}$ thickness) ratio between two welded sheets. The tensile elongation along weld line reached a value above 90% of the single sheet's elongation. Stretch flanging formability was reduced to approximately 10% of the single sheet value when the deformation restraining force ratio between two welded sheets was increased to two. Weld line movement of deep drawing test specimens was also affected by the strength ratio of the combined sheets, the weld line location and forming conditions. In all forming modes of tailored blanks, excessive weld line movement resulted from strain concentrations at the weaker sheet and resulted in fracture of the weaker side.

A study on the characterization of open-type swirl injector (오픈형 압력 스월 분무의 특성 측정에 관한 연구)

  • Song, Da Hun;Lee, Hyunchang
    • Journal of the Korean Society of Visualization
    • /
    • v.19 no.1
    • /
    • pp.43-49
    • /
    • 2021
  • In this experimental study, measurement techniques such as backlight imaging, optical patternator, and laser sheet drop sizing were applied to characterize open-type swirl injector used in Russian liquid rocket engine, RD 107. The typical development of swirl spray was observed in backlight images. The breakup length was measured by using the ratio between Mie scattering and fluorescence signal. Relative Sauter Mean Diameter was measured by using laser sheet drop sizing and the possible source of errors were discussed.

Parameter Characterization for Underwater Laser forming of SUS430/Cu/SUS430 Laminated Composite Layer (수중 레이저 굽힘시 SUS430/Cu/SUS430 복합판재 성형 특성 분석)

  • Park, S.H.;Oh, I.Y.;Han, S.W.;Woo, Y.Y.;Hwang, T.W.;Seyedkashi, S.M.H.;Moon, Y.H.
    • Transactions of Materials Processing
    • /
    • v.26 no.1
    • /
    • pp.35-40
    • /
    • 2017
  • Laser forming is an advanced process in sheet metal forming in which thermal stress originated from the laser heat source is used to shape the metal sheet. However, substantial waiting time is normally necessary for the workpiece to cool down between consecutive scans so that a steep temperature gradient can be reestablished in the next scan. In order to solve this drawback, laser bending characteristics are experimentally implemented in underwater condition. Laser forming effects under various conditions, including different laser power, scanning velocity, beam diameter, number of passes and material, are investigated. The results show that the underwater laser forming facilitates deliberate forming. The bending angle per respective laser scan is decreased with increasing the number of passes and scanning velocity.