• Title/Summary/Keyword: LCD glass powder

Search Result 18, Processing Time 0.02 seconds

The Characteristics of P.H.C Pile using Admixture by Waste TFT-LCD Glass Powder (폐 TFT-LCD 유리분말을 혼입한 고강도 콘크리트 파일의 특성)

  • Jeon, Seong-Hwan;Min, Kyung-San;Soh, Yang-Seob
    • Journal of the Korean Ceramic Society
    • /
    • v.47 no.5
    • /
    • pp.419-425
    • /
    • 2010
  • In order to examine the P.H.C pile raw material using glass forming ceramic. The used materials is ordinary portland cement, waste TFT-LCD glass powder and reactive agent(Ca$(OH)_2$). The first experiment is characteristics analysis of the waste TFT-LCD glass powder, For the second experiment is mortar and concrete compressive strength for using of the concrete file raw material for waste TFT-LCD glass powder. The results of experiment showed that the substitution ratio of 10% waste TFT-LCD glass powder and 1% reactive agent(Ca$(OH)_2$) was excellent at a point of view for the physical characteristic. The study's most important finding is that the recycling of waste TFT-LCD glass powder.

Study on the engineering and electricity properties of cement mortar added with waste LCD glass and piezoelectric powders

  • Chang, Shu-Chuan;Wang, Chien-Chih;Wang, Her-Yung
    • Computers and Concrete
    • /
    • v.21 no.3
    • /
    • pp.311-319
    • /
    • 2018
  • This study used a volumetric method for design. The control group used waste Liquid Crystal Displayplay (LCD) glass powder to replace cement (0%, 10%, 20%, 30%), and the PZT group used Pd-Zr-Ti piezoelectric (PZT) powder to replace 5% of the fine aggregate to make cement mortar. The engineering and the mechanical and electricity properties were tested; flow, compressive strength, ultrasonic pulse velocity (UPV), water absorption and resistivity (SSD and OD electricity at 50 V and 100 V) were determined; and the correlations were determined by linear regression. The compressive strength of the control group (29.5-31.8 MPa) was higher than that of the PZT group (25.1-29 MPa) by 2.8-4.4 MPa at the curing age of 28 days. A 20% waste LCD glass powder replacement (31.8 MPa) can fill up finer pores and accelerate hydration. The control group had a higher 50 V-SSD resistivity ($1870-3244{\Omega}.cm$), and the PZT group had a lower resistivity ($1419-3013{\Omega}.cm$), meaning that the resistivity increases with the replacement of waste LCD glass powder. This is because the waste LCD glass powder contains 62% $SiO_2$, which is a low dielectric material that is an insulator. Therefore, the resistivity increases with the $SiO_2$ content.

Properties of PHC Piles Using TFT-LCD Waste Glass (TFT-LCD 폐유리 사용 고강도 콘크리트 파일의 특성)

  • Lee, Seung-Heun;Lee, Seung-Tae;Min, Kyung-San;Jeon, Sung-Hwan
    • Proceedings of the Korea Concrete Institute Conference
    • /
    • 2010.05a
    • /
    • pp.319-320
    • /
    • 2010
  • This Study aimed to investigate fundamental properties of PHC pile using waste TFT-LCD glass powder. Through the present study, waste TFT-LCD glass powder may be taken into consideration for the application of mineral admixture for PHC pile.

  • PDF

Assessment of compressive strength of cement mortar with glass powder from the early strength

  • Wang, Chien-Chih;Ho, Chun-Ling;Wang, Her-Yung;Tang, Chi
    • Computers and Concrete
    • /
    • v.24 no.2
    • /
    • pp.151-158
    • /
    • 2019
  • The sustainable development principle of replacing natural resources with renewable material is an important research topic. In this study, waste LCD (liquid crystal display) glass powder was used to replace cement (0%, 10%, 20% and 30%) through a volumetric method using three water-binder ratios (0.47, 0.59, and 0.71) to make cement mortar. The compressive strength was tested at the ages of 7, 28, 56 and 91 days. The test results show that the compressive strength increases with age but decreases as the water-binder ratio increases. The compressive strength slightly decreases with an increase in the replacement of LCD glass powder at a curing age of 7 days. However, at a curing age of 91 days, the compressive strength is slightly greater than that for the control group (glass powder is 0%). When the water-binder ratios are 0.47, 0.59 and 0.71, the compressive strength of the various replacements increases by 1.38-1.61 times, 1.56-1.80 times and 1.45-2.20 times, respectively, during the aging process from day 7 to day 91. Furthermore, a prediction model of the compressive strength of a cement mortar with waste LCD glass powder was deduced in this study. According to the comparison between the prediction analysis values and test results, the MAPE (mean absolute percentage error) values of the compressive strength are between 2.79% and 5.29%, and less than 10%. Thus, the analytical model established in this study has a good forecasting accuracy. Therefore, the proposed model can be used as a reliable tool for assessing the design strength of cement mortar from early age test results.

Durability Performance Evaluations on Resistance to Chloride Attack for Concrete Using LCD Waste Glass Powder (LCD 폐유리 미분말을 사용한 콘크리트의 염해내구성 평가)

  • Kim, Seong-Kyum;Lee, Kwang-Woon;Song, Jae-Ho;Jang, Il-Young
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.6 no.4
    • /
    • pp.289-296
    • /
    • 2018
  • In this study, we evaluated the feasibility and performance of LCD waste glass as a replacement for cement by using LCD waste glass powder which is generated from manufacturing process due to development of LCD industry. Experiments were carried out by replacing 10% and 20% cement of LCD waste glass with particle size of $12{\mu}m$ of LCD waste glass with OPC and particle size of $5{\mu}m$, respectively. Through experiments, basic properties, mechanical properties and durability of concrete were evaluated. Experimental results show that the compressive strength is high at 10% replacement ratio compared to 20%. The lower the particle size, the higher the strength. The durability test evaluated the chloride penetration performance through the chloride ion diffusion coefficient. The higher the substitution rate and the smaller the particle size, the lower the chloride ion diffusion coefficient and the better the OPC than the all substitution rate. As a result, LCD waste glass concrete with low granularity and proper replacement ratio is considered to be advantageous for durability under salt environment.

An Experimental Study on High Strength Concrete Using the LCD Waste Glass Powder (LCD 폐유리 미분말을 사용한 고강도 콘크리트에 관한 실험적 연구)

  • Kim, Byung-Chul;Cha, Tae-Gweon;Jang, Pan-Ki;Kim, Chan-Woo;Jang, Il-Young
    • Journal of the Korean Recycled Construction Resources Institute
    • /
    • v.3 no.4
    • /
    • pp.335-341
    • /
    • 2015
  • Various display devices has been increasing also using waste LCD glass in accordance with the used developed, because circumstances that are most landfill or incineration, are needed research on recycling measure of the using waste LCD glass. Therefore, in this study, to try to assess the basic mechanical properties of concrete mixed with using waste LCD glass micropowder through the room mixed test. According to the study results, the more replacement rate increases, the characteristics of the concrete showed a tendency to decrease slightly. However, according to the small value, it is expected to improve the advanced experimental values by refining the grain size of the materials used to be processed into spheres.

Producing synthetic lightweight aggregates by treating waste TFT-LCD glass powder and reservoir sediments

  • Tang, Chao-Wei
    • Computers and Concrete
    • /
    • v.13 no.3
    • /
    • pp.325-342
    • /
    • 2014
  • The use of lightweight aggregate (LWA) instead of ordinary aggregate may make lightweight aggregate concrete, which possesses many advantages such as lightweight, lower thermal conductivity, and better fire and seismic resistance. Recently the developments of LWA have been focused on using industrial wastes as raw materials to reduce the use of limited natural resources. In view of this, the intent of this study was to apply Taguchi optimization technique in determining process condition for producing synthetic LWA by incorporating waste thin film transition liquid crystal displays (TFT-LCD) glass powder with reservoir sediments. In the study the waste TFT-LCD glass cullet was used as an additive. It was incorporated with reservoir sediments to produce LWA. Taguchi method with an orthogonal array L16(45) and five controllable 4-level factors (i.e., cullet content, preheat temperature, preheat time, sintering temperature, and sintering time) was adopted. Then, in order to optimize the selected parameters, the analysis of variance method was used to explore the effects of the experimental factors on the performances (particle density, water absorption, bloating ratio, and loss of ignition) of the produced LWA. The results showed that it is possible to produce high performance LWA by incorporating waste TFT-LCD glass cullet with reservoir sediments. Moreover, Taguchi method is a promising approach for optimizing process condition of synthetic LWA using recycled glass cullet and reservoir sediments and it significantly reduces the number of tests.

Properties of recycled green building materials applied in lightweight aggregate concrete

  • Wang, Her-Yung;Hsiao, Darn-Horng;Wang, Shi-Yang
    • Computers and Concrete
    • /
    • v.10 no.2
    • /
    • pp.95-104
    • /
    • 2012
  • This study uses recycled green building materials based on a Taiwan-made recycled mineral admixture (including fly ash, slag, glass sand and rubber powder) as replacements for fine aggregates in concrete and tests the properties of the resulting mixtures. Fine aggregate contents of 5% and 10% were replaced by waste LCD glass sand and waste tire rubber powder, respectively. According to ACI concrete-mixture design, the above materials were mixed into lightweight aggregate concrete at a constant water-to-binder ratio (W/B = 0.4). Hardening (mechanical), non-destructive and durability tests were then performed at curing ages of 7, 28, 56 and 91 days and the engineering properties were studied. The results of these experiments showed that, although they vary with the type of recycling green building material added, the slumps of these admixtures meet design requirements. Lightweight aggregate yields better hardened properties than normal-weight concrete, indicating that green building materials can be successfully applied in lightweight aggregate concrete, enabling an increase in the use of green building materials, the improved utilization of waste resources, and environmental protection. In addition to representing an important part of a "sustainable cycle of development", green building materials represent a beneficial reutilization of waste resources.

Resistance to Sulfate Attack of Concrete Containing LCD glass powder Using Industrial By-products (산업부산물을 활용한 LCD 유리 미분말 혼입 콘크리트의 황산염침식 저항성)

  • Kim, Seong-Kyum;Song, Jae-Ho
    • Journal of the Society of Disaster Information
    • /
    • v.15 no.2
    • /
    • pp.239-248
    • /
    • 2019
  • Purpose: This study aims to enhance the resistance against sulfate attack compared to ordinary Portland cement (OPC) concrete by using liquid crystal display (LCD) as binder. Method: The fundamental properties including compressive strength and porosity of concrete replaced by LCD up to 15% at increments of 5% and in turn, the weight, volume, and strength loss of LCD-mixed concrete was analyzed. Results: For the concrete substituted by 5% of LCD, it showed the highest compressive strength at 28 days of curing, and particular at immersion of $Na_2SO_4$ solution, it was achieved the lowest loss of weight, volume and strength due to an decreased porosity at capillaries. In contrast, there is no distinct difference of the sulfate attack resistance between LCD-mixed concretes under exposure of $MgSO_4$ solution, excepted for OPC concrete. Conclusion: In this study, comparison of resistance to sulfate attack between LCD-mixed concretes, and it would be proposed the possibility of LCD usage as binder through long-term verification with extended replacement ratio and identification of changes of hydrates in the cement matrix.