• 제목/요약/키워드: Junction Strength

Search Result 96, Processing Time 0.028 seconds

Microstructure and Mechanical Properties of Gas Metal Arc Brazed Joint of DP Steel with Cu-Si Filler Metal (Cu-Si 삽입금속을 이용한 DP강의 MIG 아크 브레이징 접합부의 미세조직과 기계적 성질)

  • Cho, Wook-Je;Yoon, Tae-Jin;Kwak, Sung-Yun;Lee, Jae-Hyeong;Kang, Chung-Yun
    • Journal of Welding and Joining
    • /
    • v.34 no.5
    • /
    • pp.70-76
    • /
    • 2016
  • In this study, Microstructure and tensile properties in arc brazed joints of 1000MPa grade DP steel using Cu-Si insert metal were investigated. The fusion zone was composed of Cu phase which solidified a little Fe and Si. The former phase formed due to dilute the edge of base material by arc, although Fe was not solid solution in Cu at the room temperature. Cu3Si particles formed by crystallization at $1100^{\circ}C$ during faster cooling. After the tensile shear test, there are no differences between the brazed joint efficiencies. The maximum joint efficient was about 37% compared to strength of base metal. It is better than that of arc brazed joint of DP steel using Cu-Sn filler metal. Fracture position of all brazing conditions was in the fusion zone. Crack initiation occurred at three junction point which was a stress singularity point of upper sheet, lower sheet and the fusion zone. And then crack propagated across the fusion zone. The reason why the fracture occurred at fusion zone was that the hardness of fusion zone was lower than that of base material and heat affected zone. The correlation among maximum load and hardness of fusion zone and EST at fractured position was $R^2=0.9338$. Therefore, this means that hardness and EST can have great impact on maximum load.

MC3T3-E1 osteoblast adhesion to laser induced hydroxyapatite coating on Ti alloy

  • Huang, Lu;Goddard, Samuel C.;Soundarapandian, Santhanakrishnan;Cao, Yu;Dahotre, Narendra B.;He, Wei
    • Biomaterials and Biomechanics in Bioengineering
    • /
    • v.1 no.2
    • /
    • pp.81-93
    • /
    • 2014
  • An in vitro cell study evaluating cell adhesion to hydroxyapatite (HA) coated prosthetic Ti-6Al-4V alloy via laser treatment is presented in comparison with uncoated alloy. Based on our previous in vitro biocompatibility study, which demonstrated higher cell attachment and proliferation with MC3T3-E1 preosteoblast cells, the present investigation aims to reveal the effect of laser coating Ti alloy with HA on the adhesion strength of bone-forming cells against centrifugal forces. Remaining cells on different substrates after centrifugation were visualized using fluorescent staining. Semi-quantifications on the numbers of cells were conducted based on fluorescent images, which demonstrated higher numbers of cells retained on HA laser treated substrates post centrifugation. The results indicate potential increase in the normalized maximum force required to displace cells from HA coated surfaces versus uncoated control surface. The possible mechanisms that govern the enhancing effect were discussed, including surface roughness, chemistry, wettability, and protein adsorption. The improvement in cell adhesion through laser treatment with a biomimetic coating could be useful in reducing tissue damage at the prosthetic to bone junction and minimizing the loosening of prosthetics over time.

A Study on the Stability of the Single-Layer Latticed Dome during Erection Using the Step-Up Method (Step-Up 공법에 의한 단층래티스돔의 시공시 안정성 연구)

  • Koo, Choong-Mo;Jung, Hwan-Mok;Kim, Cheol-Hwan
    • Journal of Korean Association for Spatial Structures
    • /
    • v.12 no.4
    • /
    • pp.109-118
    • /
    • 2012
  • The large-space single-layer lattice dome is relatively simpler in terms of the arrangement of the various framework members and of the design of the junction than the multi-layered lattice dome, can reduce the numbers and quantity of the framework members, and has the merit of exposing the beauty of the framework as it stands. The single-layer lattice dome, however, requires a stability investigation of the whole structure itself, along with an analysis of the stress of the framework members, because an unstable phenomenon called "buckling" occurs when its weight reaches critical levels. Many researchers have systematically conducted researches on the stability evaluation of the single-layer lattice dome. No construction case of a single-layer lattice dome with a 300-m-long span, however, has yet been reported anywhere in the world. The large-space dome structure is difficult to erect due to the gigantic span and higher ceiling compared with other common buildings, and its construction cost is generally huge. The method of erecting a structure causes major differences in the construction cost and period. Therefore, many researchers have been conducting various researches on the method of erecting such structure. The step-up method developed by these authors can reduce the construction cost and period to a great extent compared with the other general methods, but the application of this method inevitably requires the development of system supports in the center section as well as pre-existing supports in the boundary sections. In this research, the safety during the construction of a single-layer lattice dome with 300-m-long span using pre-existing materials was examined in the aspect of structural strength, and the basic data required for manufacturing the supports in the application of the step-up method developed by these authors during the erection of the roof structure were obtained.

The Numerical Analysis of Extrusion Forming on the Manufactured Artificial Lightweight Aggregate Made of Incinerated Sewage Sludge Ash by a Finite Element Method (유한요소법을 이용한 하수슬러지 소각재의 인공경량골재 제조시 압출성형해석)

  • Jung, Byung-Gil;Bae, Jin-Woo;Sung, Nak-Chang
    • Journal of Environmental Science International
    • /
    • v.16 no.10
    • /
    • pp.1169-1177
    • /
    • 2007
  • The main objective of this research was to evaluate the effects of process variables which were forming ability, flow displacement, effective stress, effective strain, fluid vector and products defects on manufactured artificial lightweight aggregate made of both incinerated sewage sludge ash and clay by means of the numerical analysis of a rigid-plastic finite element method. CATIA (3D CAD program) was used for an extrusion metal mold design that was widely used in designing aircraft, automobile and metallic molds. A metal forming analysis program (ATES Co.) had a function of a rigid-plastic finite element method was used to analyze the program. The result of extrusion forming analysis indicated clearly that a shape retention of the manufactured artificial light-weight aggregate could be maintained by increasing the extrusion ratio (increasing compressive strength inside of extrusion die) and decreasing the die angle. The stress concentration of metal mold was increased by increasing an extrusion ratio, and it was higher in a junction of punch and materials, friction parts between a bottom of the punch and inside of a container, a place of die angle and a place of die of metal mold. Therefore, a heat treatment as well as a rounding treatment for stress distribution in the higher stress concentration regions were necessary to extend a lifetime of the metallic mold. A deformity of the products could have made from several factors which were a surface crack, a lack of the shape retention and a crack of inside of the products. Specially, the surface crack in the products was the most notably affected by the extrusion ratio.

Implant Anneal Process for Activating Ion Implanted Regions in SiC Epitaxial Layers

  • Saddow, S.E.;Kumer, V.;Isaacs-Smith, T.;Williams, J.;Hsieh, A.J.;Graves, M.;Wolan, J.T.
    • Transactions on Electrical and Electronic Materials
    • /
    • v.1 no.4
    • /
    • pp.1-6
    • /
    • 2000
  • The mechanical strength of silicon carbide dose nor permit the use of diffusion as a means to achieve selective doping as required by most electronic devices. While epitaxial layers may be doped during growth, ion implantation is needed to define such regions as drain and source wells, junction isolation regions, and so on. Ion activation without an annealing cap results in serious crystal damage as these activation processes must be carried out at temperatures on the order of 1600$^{\circ}C$. Ion implanted silicon carbide that is annealed in either a vacuum or argon environment usually results in a surface morphology that is highly irregular due to the out diffusion of Si atoms. We have developed and report a successful process of using silicon overpressure, provided by silane in a CAD reactor during the anneal, to prevent the destruction of the silicon carbide surface, This process has proved to be robust and has resulted in ion activation at a annealing temperature of 1600$^{\circ}C$ without degradation of the crystal surface as determined by AFM and RBS. In addition XPS was used to look at the surface and near surface chemical states for annealing temperatures of up to 1700$^{\circ}C$. The surface and near surface regions to approximately 6 nm in depth was observed to contain no free silicon or other impurities thus indicating that the process developed results in an atomically clean SiC surface and near surface region within the detection limits of the instrument(${\pm}$1 at %).

  • PDF

A TEM STUDY OF THE RESIN-DENTIN INTERDIFFUSION ZONE FORMED BY ONE-BOTTLE DENTIN ADHESIVE SYSTEMS (단일용기 상아질 접착제 처리 후 레진-상아질 경계면에 대한 투과전자현미경적 연구)

  • Yang, Dong-Woon;Park, Seong-Ho;Lee, Chan-Young
    • Restorative Dentistry and Endodontics
    • /
    • v.25 no.2
    • /
    • pp.180-192
    • /
    • 2000
  • One bottle system was recently developed in order to simplify the clinical skills and save chair time after continuous improvements on dentin bonding agents. There has been many studies to measure the bond strength of one bottle systems but no actual work has been done on micromorphologic study of resin-dentin interdiffusion zone after one bottle system application. To evaluate the bonding patterns of various commercially available one bottle systems to dentin, observation of resin-dentin interdiffusion zone under TEM was performed. Caries-free human third molars within one month of extractions were chosen for the experiments. The molars were sectioned 1mm above the cementoenamel junction and got rid of the root portions. Crown portions of the teeth were sectioned parallel to occlusal surface so that dentin discs of 1mm in thickness were remained. 7 one bottle systems and 1 two bottle system were applied according to manufacturer's instructions and followings were the results. 1. In every experimental groups, cross bandings of collagen fiber were distinguishable and tight bon dings between the bonding agents and dentin were observed. 2. Hybrid layer was clearly observed in ONE-STEP$^{(R)}$, Prime & Bond$^{(R)}$ 2.1, Syntac$^{(R)}$ SC, MAC-BOND II groups but it was not clear in Single Bond, D-Liner Dual PLUS, ONE COAT BOND groups. 3. Electron-density of hybrid layer was uniform in pattern in MAC-BOND II, Prime & Bond$^{(R)}$ 2.1 groups but not so uniform in ONE-STEP$^{(R)}$ group. 4. Electron-dense amorphous phase in most superior layer of the resin-dentin interdiffusion zone was characteristically observed in Single Bond, Syntac$^{(R)}$ SC, ONE COAT BOND groups. It can be concluded that bondings between the dentin bonding agents and dentin can be various in pattern according to their chemical compositions and the condition during applications.

  • PDF

Bilateral foot drop caused by T12 infectious spondylitis after vertebroplasty: a case report

  • Kim, Dong Hwan;Shin, Yong Beom;Ha, Mahnjeong;Kim, Byung Chul;Han, In Ho;Nam, Kyoung Hyup
    • Journal of Trauma and Injury
    • /
    • v.35 no.1
    • /
    • pp.56-60
    • /
    • 2022
  • The most common cause of foot drop is lumbar degenerative disc herniation, particularly at L4/5. We present a rare case of spinal cord injury accompanied by a thoracolumbar lesion that presented with bilateral foot drop. A 69-year-old male patient presented with sudden-onset severe bilateral leg pain and bilateral foot drop. Radiologic findings revealed T12 spondylitis compressing the conus medullaris. He had undergone vertebroplasty for a T12 compression fracture after a fall 6 months before. A physical examination showed bilateral foot drop, paresthesia of both L5 dermatomes, increased deep tendon reflex, and a positive Babinski sign. An acute bilateral L5 root lesion and a conus medullaris lesion were suspected based on electromyography. A surgical procedure was done for decompression and reconstruction. After the operation, bilateral lower extremity muscle strength recovered to a good grade from the trace grade, and the patient could walk without a cane. The current case is a very rare report of bilateral foot drop associated with T12 infectious spondylitis after vertebroplasty. It is essential to keep in mind that lesions of the thoracolumbar junction can cause atypical neurological symptoms. Furthermore, understanding the conus medullaris and nerve root anatomy at the T12-L1 level will be helpful for treating patients with atypical neurological symptoms.

Differential expression and localization of tight junction proteins in the goat epididymis

  • Sung Woo, Kim;Yu-Da, Jeong;Ga-Yeong, Lee;Jinwook, Lee;Jae-Yeung, Lee;Chan-Lan, Kim;Yeoung-Gyu, Ko;Sung-Soo, Lee;Bongki, Kim
    • Journal of Animal Science and Technology
    • /
    • v.64 no.3
    • /
    • pp.500-514
    • /
    • 2022
  • The blood-epididymis barrier (BEB) forms a unique microenvironment that is crucial for the maturation, protection, transport, and storage of spermatozoa in the epididymis. To characterize the function of tight junctions (TJs), which are constitutive components of the BEB, we determined the expression and localization of TJ proteins such as zonula occludens (ZO)-1, 2, and 3, occludin, and claudin3 (Cldn3) during postnatal development in the goat epididymis. To assess the expression patterns of TJ proteins in immature (3 months of age) and mature (14 months of age) goat epididymides, two different experimental methods were used including immunofluorescence labeling and western blotting. We show that, ZO-1, 2, and 3, and occludin, were strictly expressed and localized to the TJs of the goat epididymis, whereas Cldn3 was present in basolateral membranes as well as TJs. All TJ proteins examined were more highly expressed in the immature epididymis compared to levels in mature tissue. In conclusion, our study indicates that at least five TJ proteins, namely ZO-1, ZO-2, ZO-3, occludin, and Cldn3, are present in TJs, and the expression strength and pattern of TJ proteins tend to be age dependent in the goat epididymis. Together, these data suggest that the distinct expression patterns of TJ proteins are essential for regulating components of the luminal contents in the epididymal epithelium and for forming adequate luminal conditions that are necessary for the maturation, protection, transport, and storage of spermatozoa in the goat epididymis.

A COMPARATIVE STUDY ON THE STRENGTH AND THE BONE FORMATION AT THE RATS CALVARIAL DEFECTS OF DFDB GRAFT AND THOSE OF THE COMPOSITE GRAFT WITH DFDB AND RESORBABLE HYDROXYAPATITE (백서 두개골 결손부에 동결 건조 동종 탈회골을 단일매식한 경우와 동결 건조 동종 탈회골과 흡수성 수산화인회석을 복합매식한 경우의 강도 및 골형성에 관한 비교 연구)

  • Seo, Young-Ho;Yim, Chang-Joon;Lee, Jae-Il
    • Journal of the Korean Association of Oral and Maxillofacial Surgeons
    • /
    • v.26 no.6
    • /
    • pp.557-564
    • /
    • 2000
  • The bone graft materials can be grossly divided into autogenous bone, allogenic bone, xenogenic bone, and alloplastic material. Much care was given to other bone graft materials away from autogenous bone due to its additional operation for harvesting, delayed resorption and limitation of quantity. Demineralized freeze-dried bone(DFDB) and hydroxyapatite are the representatives of bone graft materials. As resorbable hydroxyapatite is developed in these days, the disadvantage of nonresorbability can be overcome. So we planned to study on the strength and the bone formation at the rats calvarial defects of DFDB graft and those of the composite graft with DFDB and resorbable hydroxyapatite. We used the 16 male rats weighting range from 250 to 300 gram bred under the same environment during same period. After we made the 6mm diameter calvarial defect, we filled the DFDB in 8 rats and DFDB and resorbable hydroxyapatite in another 8 rats. We sacrificed them at the postoperative 1 month and 2 months with the periostium observed. As soon as the specimens were delivered, we measured the compressive forces to break the normal calvarial area and the newly formed bone in calvarial defect area using Instron(Model Autograph $S-2000^{(R)}$, Shimadzu, Japan). The rest of the specimens were stained with H&E(Hematoxylin & Eosin) and evaluated with the light microscope. So we got the following results. 1. In every rats, there was no significant difference between the measured forces of normal bone area and those of the bone graft area. 2. In 1 month, the measured forces at DFDB graft group were higher than those of the DFDB and resorbable hydroxyapatite composite graft group(P<0.05). 3. In 2 months, there was no significant differences between the measured forces of DFDB graft group and those of the DFDB and resorbable hydroxyapatite composite graft group. 4. In lightmicroscopic examination, most of the grafted DFDB were transformed into bone in 1 month and a large numbers of hydroxyapatite crystal were observed in DFDB and resorbable hydroxyapatite composite graft group in 1 month. 5. Both group showed no inflammatory reaction in 1 month. And hydroxyapatite crystals had a tight junction without soft tissue invagination when consolidated with newly formed bone. 6. In both groups, newly formed bone showed the partial bone remodeling and the lamellar bone structures and some of reversal lines were observed in 2 months. From the above results, it is suggested that DFDB and resorbable hydroxyapatite composite graft group had a better resistance to compressive force in early stage than DFDB graft group, but there would be no significant difference between two groups after some period. And it is suggested that the early stage of bone formation procedure of DFDB and resorbable hydroxyapatite composite graft group was slight slower than that of DFDB graft group, but there would be no significant difference between two groups after some period.

  • PDF

THE EFFECT OF SMEAR LAYER REMOVAL AND POSITION OF DENTIN ON SHEAR BOND PROPERTIES OF DENTIN BONDING SYSTEMS TO INTERNAL CERVICAL DENTIN (도말층 제거와 상아질의 부위가 치수강 내부 상아질에 대한 수종 상아질 결합제의 전단결합성질에 미치는 영향)

  • Lim, Yoen-Ah;You, Young-Dae;Lee, Yong-Keun;Lee, Su-Jong;Im, Mi-Kyung
    • Restorative Dentistry and Endodontics
    • /
    • v.24 no.3
    • /
    • pp.465-472
    • /
    • 1999
  • The aim of this study was to determine the shear bond properties of four dentin bonding systems to internal cervical dentin, and to investigate the effect of the pretreatment for removing smear layer and position of dentin on shear bond strength of dentin bonding agents. The materials tested in this study were consisted of four commercially available dentin bonding systems[Allbond 2(AB), Clearfil Linerbond 2(CL), Optibond FL(OP), Scotchbond Multi-purpose(SB)], a restorative light-cured composite resin[Z100]J and a chelating agent[RC-prep(RC)]. Fifty-six freshly extracted human molars were used in this study. Dentin specimens were prepared by first cutting the root of the tooth 1mm below the cementoenamel junction with a diamond bur in a high speed handpiece under air-water coolant, and then removing occlusal part at pulp horn level by means of a second parallel section, The root canal areas were exposed by means of cutting the dent in specimens perpendicular to the root axis. Dentin specimens were randomly assigned to two groups(pretreated group, not-pretreated group) based on the pretreatment method of dentin surface. In pretreated group, RC was applied to dentin surface for 1minute and then rinsed with NaOCl. In not-pretreated group, dentin surface was rinsed with saline Each groups were subdevided into four groups according to dentin bonding systems. Four dentin bonding systems and a restorative resin were applied according to the directions of manufacturer. The dentin-resin specimens were embedded in a cold cure acrylic resin, and were cut with a low speed diamond saw to the dimension of $1{\times}1mm$. The cut specimens were divided into three groups according to the position of internal cervical dentin. The shear bond properties of dentin-resin specimens were measured with Universal testing machine (Zwick, 020, Germany) with the cross head speed of 0.5mm/min. From this experiment. the following results were obtained : 1. In case of shear bond strength, there was no significant difference among dentin bonding systems in not-pretreated groups, whereas in pretreated groups, the shear bond strengths of AB and of SB were statistically significantly higher than those of CL and of OP. 2. The shear bond strengths of AB and of SB in pretreated groups were significantly higher than those in not-pretreated groups. 3. The shear bond strengths of radicular layer of OP were higher than those of occlusal layer of OP in not-pretreated groups, and of AB in pretreated groups. The shear bond strengths of radicular layer of AB and of CL in not-pretreated groups were higher than those in pretreated group.

  • PDF