• 제목/요약/키워드: J-R Curve

검색결과 229건 처리시간 0.022초

SG365강의 파괴저항곡선과 측면홈효과에 관한 연구 (A Study on the Fracture Resistance Curve and Effect of Side Grooves of SG365 Material)

  • 임만배
    • 한국안전학회지
    • /
    • 제16권4호
    • /
    • pp.14-21
    • /
    • 2001
  • SG-365 steel is an important material End used for manufacturing a pressure vessel and gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the unloading compliance method according to the ASTM E8l3-97 and E1152-97 method on the smooth and side groove In specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the $J_{IC}$. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides. it improves the accuracy of toughness values, decreases the scattering of them and crack tunneling effect and shear lip by the side groove.

  • PDF

역사이클하중이 원자력 배관재료의 파괴저항곡선에 미치는 영향 (Effect of Reverse Cyclic Loading on the Fracture Resistance Curve of Nuclear Piping Material)

  • 원종일;석창성
    • 대한기계학회논문집A
    • /
    • 제23권7호
    • /
    • pp.1112-1119
    • /
    • 1999
  • Fracture resistance(J-R) curves, which are used for the elastic-plastic fracture mechanics analyses, are known to be dependent on the cyclic loading history. The objective of this paper is to study the effect of reverse cyclic loading on J-R curves in CT specimens. The effect of two parameters was observed on the J-R curves during the reverse cyclic loading. One was the minimum-to-maximum load ratio(R) and the other was the incremental plastic displacement(${\delta}_{cycle}/{\delta}_i$), which is related to the amount of crack growth that occurs in a cycle. Fracture resistance test on CT specimens with varying load ratio and incremental plastic displacement were performed. For the SA 516 Gr. 70 steel, the results showed that the J-R curves were decreased with decreasing the load ratio and the incremental plastic displacement. When the load ratio was set to -1, the results of the J-R curves and the $J_i$ value were about $40{\sim}50$ percent of those for the monotonic loading condition. Also on condition that the incremental plastic displacement reached 1/40, the J-R curves and the $J_i$ value were about $50{\sim}60$ percent of those for the incremental plastic displacement of 1/10.

C(T) 시편 측면 홈 유무에 따른 파괴저항곡선 변화가 유한요소 손상모델 변수 결정에 미치는 영향 평가 (Evaluation of the Effect of Fracture Resistance Curve Change Owing to the Presence or Absence of Side Groove in C(T) Specimen on Finite Element Failure Model Parameter Determination)

  • 김훈태;류호완;김윤재;김종성;최명락;김진원
    • 대한기계학회논문집A
    • /
    • 제40권6호
    • /
    • pp.539-546
    • /
    • 2016
  • 본 연구에서는 C(T) 시편 측면 홈의 유무에 따른 J-R 곡선의 변화가 유한요소 손상해석의 모델변수 결정에 미치는 영향을 알아보았다. 손상해석은 수정 응력 파괴변형률 모델을 이용하였다. C(T) 시편은 SA508 Gr. 1a 배관재에서 채취하였고 일부에 측면 홈이 가공되었다. 시험은 상온과 원전 운전 온도인 $316^{\circ}C$에서 각각 수행되었으며, 시험 결과 얻은 J-R 곡선을 모사하여 손상모델 변수를 얻었다. 그 결과, 측면 홈의 유무에 따른 J-R 곡선의 변화는 손상모델 변수 결정에 영향을 주지 않음을 확인하였다.

압력용기강의 파괴저항곡선의 파괴변형률에 관한 연구 (A study on the Relations Between Fracture Strain and Fracture Resistance Curve of nuclear Pressure Vessel Steel)

  • 임만배
    • 한국해양공학회지
    • /
    • 제14권1호
    • /
    • pp.44-51
    • /
    • 2000
  • Safety and integrity are required for reactor pressure vessels because they are operated in high temperature. There are single specimen method multiple specimen method and load ratio analysis method which used as evaluation of safety and integrity for reactor pressure vessels. In this study the fracture resistance curve(J-R curve) elastic-plastic fracture toughness($J_{IC}$) and material tearing modulus ($T_{mat}$) of SA 508 class 3 alloy steel used as reactor pressure vessel steel are measured and evaluated at room temperature 20$0^{\circ}C$ and 30$0^{\circ}C$ according to unloading compliance method and load ration analysis method. And then the comparison with experimental $J_{IC}$ and theoretical$J_{IC}$ by local fracture strain is managed.

  • PDF

REVIEW OF DYNAMIC LOADING J-R TEST METHOD FOR LEAK BEFORE BREAK OF NUCLEAR PIPING

  • Oh, Young-Jin;Hwang, Il-Soon
    • Nuclear Engineering and Technology
    • /
    • 제38권7호
    • /
    • pp.639-656
    • /
    • 2006
  • In order to apply the leak before break (LBB) concept to nuclear piping systems, the dynamic strain aging effect of low carbon steel materials has to be taken into account, in compliance with the requirements of the Korean Standard Review Guide (KSRG) 3.6.3-1. For this goal, J-R tests are needed for a range of various temperatures and loading rates, including dynamic loading conditions. In the dynamic loading J-R test, the unloading compliance method can not be applied to measure the crack growth and direct current potential drop (DCPD) method; this method also has a problem defining the crack initiation point. The normalization method is known as a very useful method to determine the J-R curve under dynamic loading because it does not need additional equipment or complicated loading sequences such as electric current or unloading. This method was accepted by the American Society for Testing and Materials (ASTM) as a standard test method E1820 A15 in 2001. However, it has not yet been clearly verified yet if the normalization method is sufficiently reliable to be applied to LBB. In this study, the basic background of the J-integral, LBB and dynamic loading J-R test are explained, and the current status for dynamic loading J-R test methods are reviewed from the view point of LBB for nuclear piping. In particular, the theoretical and historical background of the normalization method which has received attention recently, is summarized. Recent studies for this method are introduced and future works are suggested that may improve the reliability of LBB for nuclear piping.

CURVES WITH MAXIMAL RANK, BUT NOT ACM, WITH VERY HIGH GENERA IN PROJECTIVE SPACES

  • Ballico, Edoardo
    • 대한수학회지
    • /
    • 제56권5호
    • /
    • pp.1355-1370
    • /
    • 2019
  • A curve $X{\subset}\mathbb{P}^r$ has maximal rank if for each $t{\in}\mathbb{N}$ the restriction map $H^0(\mathcal{O}_{\mathbb{P}r}(t)){\rightarrow}H^0(\mathcal{O}_X(t))$ is either injective or surjective. We show that for all integers $d{\geq}r+1$ there are maximal rank, but not arithmetically Cohen-Macaulay, smooth curves $X{\subset}\mathbb{P}^r$ with degree d and genus roughly $d^2/2r$, contrary to the case r = 3, where it was proved that their genus growths at most like $d^{3/2}$ (A. Dolcetti). Nevertheless there is a sector of large genera g, roughly between $d^2/(2r+2)$ and $d^2/2r$, where we prove the existence of smooth curves (even aCM ones) with degree d and genus g, but the only integral and non-degenerate maximal rank curves with degree d and arithmetic genus g are the aCM ones. For some (d, g, r) with high g we prove the existence of reducible non-degenerate maximal rank and non aCM curves $X{\subset}\mathbb{P}^r$ with degree d and arithmetic genus g, while (d, g, r) is not realized by non-degenerate maximal rank and non aCM integral curves.

흰 광폭평판 시험을 이용한 원자력 배관의 파괴거동예측 (Prediction of Failure Behavior for Nuclear Piping Using Curved Wide-Plate Test)

  • 허남수;김윤재;최재붕;김영진;임혁순;정대율
    • 대한기계학회논문집A
    • /
    • 제28권4호
    • /
    • pp.352-361
    • /
    • 2004
  • One important element of the Leak-Before-Break analysis of nuclear piping is how to determine relevant fracture toughness (or the J-resistance curve) for nonlinear fracture mechanics analysis. The practice to use fracture toughness from a standard C(T) specimen is known to often give conservative estimates of toughness. To improve the accuracy, this paper proposes a new method to determine fracture toughness using a nonstandard testing specimen, curved wide-plate in tension. To show validity of the proposed curved wide-plate test, the J-resistance curve from the full-scale pipe test is compared with that from the curved wide-plate test and that from the C(T) specimen. It is shown that the J-resistance curve form the curved wide-plate tension test is similar to, but that from the C(T) specimen is lower than, the J-resistance curve from the full-scale pipe test. Further validation is performed by investigating crack-tip constraint conditions via detailed 3-D FE analyses, which shows that the crack-tip constraint condition in the curved wide-plate tension specimen is indeed similar to that in the full-scale pipe under bending.

가스배관재의 탄소성파괴인성에 미치는 측면홈 영향 (Effect of Side Groove on the Elastic Plastic Fracture Toughness of Gas Piping Material)

  • 임만배;차귀준;윤한기;공유식;김정호
    • 한국해양공학회지
    • /
    • 제15권3호
    • /
    • pp.63-68
    • /
    • 2001
  • SG-365 steel is an important material and used for manufacturing a pressure vessel which the gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the an unloading compliance method according to the ATM E813-97 method on the smooth and side groove 1CT specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the $J_IC. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides, it improves the accuracy of toughness values, decreases the scattering of them and tunneling and shear lip by the side groove.

  • PDF

가스배관재의 탄소성파괴인성에 미치는 측면홈영향 (Effect of Side Grooved on the Elastic Plastic Fracture Toughness of Gas Piping Meterial)

  • 임만배;차귀준;윤한기;김정호
    • 한국해양공학회:학술대회논문집
    • /
    • 한국해양공학회 2001년도 춘계학술대회 논문집
    • /
    • pp.350-356
    • /
    • 2001
  • SG-50 steel is an important material and used for manufacturing a pressure vessel which the gas piping. In this investigation, the elastic plastic fracture toughness of this material is evaluated by the an unloading compliance method according to the ASTM E813-97 and E1152-97 method on the smooth and side groove 1CT specimens. The effect of smooth and side groove is studied on the elastic plastic fracture toughness. The side grooved specimen is very useful in estimation of the J$_{IC}$. Because it is much easier than the smooth specimen to the onset of the ductile tearing by the R curve method. Besides, it improves the accuracy of toughness values, decreases the scattering of them and tunneling and shear lip by the side groove.e.

  • PDF

Cr-Mo 강과 Cr 강의 J-R곡선의 측정 및 응용 (Measurement and Application of J-R Curves of Cr-Mo Steel and Cr Steel)

  • 안승균;허용학;박재학
    • 대한기계학회:학술대회논문집
    • /
    • 대한기계학회 2000년도 추계학술대회논문집A
    • /
    • pp.328-332
    • /
    • 2000
  • Following the method described in ASTM E1737, J resistance curves are measured for Cr-Mo steel SA387, and Cr steel A240 which are used as piping materials in nuclear industry. Crack driving force diagrams are generated in order to find out instability points in crack growth. The $J_{appl}$ curves, which are used in the crack driving force diagram, are obtained from EPRI J estimation method and the finite element analysis. Crack growth instability points are plotted in load-crack length plane and the results are discussed.

  • PDF