Indentation Damage of Porous Alumina Ceramice

  • Ha, Jang-Hoon;Lee, Chul-Seung;Kim, Jong-Ho;Kim, Do-Kyung
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.1
    • /
    • pp.19-23
    • /
    • 2004
  • The Hertzian indentation contact damage behavior of porous alumina with controlled pore shape was investigated by experiments. Porous alumina ceramics containing well-defined pore shape, size and distribution were prepared by incorporation of fugitive spherical starch. Porous alumina with isolated pore structure was prepared with porosity range up to 30%. The indentation stress-strain curves of porous alumina were constructed. Elastic modulus and yield stress can be obtained from the stress-strain relationship. Impulse excitation method for the measurement of elastic modulus was also conducted as well as Hertzian indentation and was confirmed as a useful tool to evaluate the elasticity of highly porous ceramics. Elastic modulus of the inter-connected pore structure is more sensitive to porosity than that of the isolated pore structure. When the specimen had isolated pore structure, higher yield point was obtained than it had inter-connected pore structure. This study proposed that the elastic modiulus of porous ceramics is strongly related to not only porosity, but also the structure of pore.

Behavior of Isolated Pores during Liquid Phase Sintering of $MgO-CaMgSiO_4$ System ($MgO-CaMgSiO_4$ 계 액상소결중의 고립기공거동)

  • 송병무;김정주;김도연
    • Journal of the Korean Ceramic Society
    • /
    • v.22 no.3
    • /
    • pp.7-12
    • /
    • 1985
  • A theoretical model describing the behavior of isolated pores during liquid phase sintering was developed and the experimental results obtained by the $80MgO-CaMgSiO_4$ specimens were given. Most of isolated pores once formed in the interior of specimen were not eliminated because the pressure of trapped non-diffusable gas in the pore like $N_2$ increases very rapidly with pore volume contraction. As sint-ering time increase it was observed that the number of pores decreases whereas the average size of pore increases. This phenomenon was interpreted in terms of the MgO growth during sintering which results in the coalescence of isolated pores. The increase of pore size resulting from pore coalescence was attributed to the main cause of the overfiring phenomena ; the higher sintering temperature or a long time sintering leads to a decrease in density.

  • PDF

Isolated Pore Generation Mechanism and Mechanical Properties in MAS System with 3Y-TZP (MAS계에서 3Y-TZP 첨가에 따른 독립 기공 생성기구와 기계적 성질)

  • 최성철;박현철
    • Journal of the Korean Ceramic Society
    • /
    • v.30 no.11
    • /
    • pp.881-890
    • /
    • 1993
  • MAS system has narrow sintering temp. range due to the liquid phae sintering and thereby densify rapidly. And especially, its poor mechanical properties limitedthe industrial application. In this study, the improvement of mechanical properties and densification is suggested by the consideration of the toughening mechanisms and isolated pore generation mechanism which is derived by the liquid phase sintering theory in 3Y-TZP added composites. After Pressureless sintering up to 140$0^{\circ}C$ for 5hr, the dihedral angle and contact angle are analyzed by the observation of microstructure. As a result of microstructure analysis, the sintering stage of the specimen sintered for 5hr is analyzed as solid-skeleton stage. And the isolated pore generation mechanisms are considered as (1) The swelling of the liquid phase is predominent due to the facts that dihedral angle is larger than 60$^{\circ}$, contact angle is large and that liquid volume fraction is smaller than 10%. (2) The porous characteristics of the MAS system is also suggested as: the SiO2-rich liquid film is firstly formed at the srface and therefore this reduces the contiguity of the pore, which induces the isolated pore. The strength and fracture toughness increased with the addition of 3Y-TZP and the main fracture toughness improvement mechanisms are analyzed as the crack deflection.

  • PDF

Growth of silicon nitride whiskers using tailored pores (제어된 기공을 이용한 질화규소 휘스커의 성장)

  • Kim, Chang-Sam;Han, Kyong-Sop;Kim, Shin-Woo
    • Journal of the Korean Crystal Growth and Crystal Technology
    • /
    • v.15 no.2
    • /
    • pp.61-67
    • /
    • 2005
  • In this study a new growing method of silicon nitride whiskers in the inside of large pores made intentionally during the sintering was conducted. Pore size, pore vol%, and nitrogen pressure were used as experimental variables. Silicon nitride whiskers were well grown in the inside of pores with low pore vol% range from 14 to 27 but not grown with high pore vol% such as 39 and 50. On the other hand, pore size and nitrogen pressure did not have any influence on the whisker growth. Therefore the most important factor to grow silicon nitride whisker in the inside of large pores during sintering was to make pores isolated or closed.

Strength and Reliability of Porous Ceramics Measured by Sphere Indentation on Bilayer Structure

  • Ha, Jang-Hoon;Kim, Jong-Ho;Kim, Do-Kyung
    • Journal of the Korean Ceramic Society
    • /
    • v.41 no.7
    • /
    • pp.503-507
    • /
    • 2004
  • The importance of porous ceramics has been increasingly recognized and adequate strength of porous ceramics is now required for structural applications. Porosities of porous ceramics act as flaws in inner volume and outer surface which result in severe strength degradation. The effect of pore structure, however, on strength and reliability of porous ceramics has not been clearly understood. We investigate the relationship between pore structure and mechanical properties using a sphere indentation on bilayer structure, porous ceramic top layer with soft polymer substrate. Porous alumina and silica were prepared to characterize the isolated pore structure and interconnected pore structure, respectively. The porous ceramic with 1mm thickness were bonded to soft polycarbonate substrate and then fracture strengths were estimated from critical loads for radial cracking of porous ceramics during sphere indentation from top surface. This simple and reproducible technique provides Weibull modulus of strength of porous ceramics with different pore structure. It shows that the porous ceramics with isolated pore structure have higher strength and higher Weibull modulus as well, than those with interconnected pore structure even with the same porosity.

Particle Agglomerate Effect on Intermediate/Final Microstructure (입자 응집이 중기/말기 미구조에 미치는 영향)

  • 손영돈;전병세
    • Journal of the Korean Ceramic Society
    • /
    • v.29 no.11
    • /
    • pp.843-850
    • /
    • 1992
  • The purpose of this study was to describe the heterogeneity effects on Intermediate/Final microstructure in isothermal liquid phase sintering. Several kinds of pore shapes were made by the different in the heterogeneity stress level during Intermediate/Final stage. Specimen with 48% green density especially showed that the local regions of a sintered compact were subject to more rapid shrinkage than the surroundings. This densification limiting factors generally inhibited sintering and made the large isolated crack-like pore in heterogeneous microstructures.

  • PDF

Effect of Green Microstructure on the Sintering and Properties of Aluminum Nitride (성형미세구조가 질화알루미늄의 소결 및 물성에 미치는 영향)

  • 이해원;전형우;송휴섭
    • Journal of the Korean Ceramic Society
    • /
    • v.32 no.2
    • /
    • pp.209-216
    • /
    • 1995
  • In order to investigate the effect o green microstructure on the sintering behavior and properties of AlN ceramics, samples were prepared by slip casting and dry pressing. The slip cast samples had high green density, fine pore size and narrow pore size distribution. They showed much higher sinterability and more homogeneous sintered microstructure compared to the dry pressed samples. Both increased thermal conductivity and flexural strength for samples prepared by slip casting could be attributed to the improved microstructural homogeneity with isolated second phase(s).

  • PDF

Effect of Porous Membrane on Culture Properties of Blood-Brain Barrier Endothelial Cell (다공성막이 혈액뇌관문 내피세포의 배양에 끼치는 영향)

  • Lee, Keum-Jeong;Cho, Hye-Jin;Choi, Hyung-Taek;Na, O-Soon;Kim, Kyung-Yong
    • Applied Microscopy
    • /
    • v.33 no.4
    • /
    • pp.261-266
    • /
    • 2003
  • The growth patterns of primary culture of bovine brain microvessel endothelial cells (BBMECs) were studied using electron microscopy when grown on $3.0{\mu}m$ and $0.4{\mu}m$ pore Transwell. The capillary fragments and isolated endothelial cells grew on collagen coated culture plate and Transwell membrane. The BBMECs grew only on the upper surface of membrane of $0.4{\mu}m$. But BBMECs on $3.0{\mu}m$ pore membrane migrated through the pore and grew on the opposite side of the membrane. In summary, BBMECs isolated by enzyme digestion could migrate through $3.0{\mu}m$ pore membrane but not through $0.4{\mu}m$ pore membrane. So $0.4{\mu}m$ pore membrane instead of $3{\mu}m$ pore membrane should be used for drug transport experiment or transendothelial electrical resistance measurement.

Processing of Porous Ceramics with a Cellular Structure Using Polymer Beads

  • Ha, Jung-Soo;Kim, Chang-Sam
    • Journal of the Korean Ceramic Society
    • /
    • v.40 no.12
    • /
    • pp.1159-1164
    • /
    • 2003
  • Two processing routes (i.e., the gel casting and polymer preform routes) using polymer beads were studied to fabricate porous ceramics with a cellular structure. The gel casting route, comprising the gel casting of a ceramic slurry mixed with polymer beads, was found to be inadequate to produce porous ceramic bodies with a interconnected pore structure, due to complete coating of the slurry on the polymer beads, which left just isolated pores in the final sintered bodies. The polymer preform route, involving the infiltration of a polymer beads preform with the ceramic slurry, successfully produced porous ceramics with a highly interconnected network of spherical pores. The pore size of 250-300 $\mu\textrm{m}$ was demonstrated and the porosity ranged from 82 to 86%. This process is advantageous to control the pore size because it is determined by the sizes of polymer beads used. Another feature is the avoidance of hollow skeleton, giving a high strength.

Antimicrobial Peptides (AMPs): Peptide Structure and Mode of Action

  • Park, Yoon-Kyung;Hahm, Kyung-Soo
    • BMB Reports
    • /
    • v.38 no.5
    • /
    • pp.507-516
    • /
    • 2005
  • Antimicrobial peptides (AMPs) have been isolated and characterized from tissues and organisms representing virtually every kingdom and phylum. Their amino acid composition, amphipathicity, cationic charge, and size allow them to attach to and insert into membrane bilayers to form pores by 'barrel-stave', 'carpet' or 'toroidal-pore' mechanisms. Although these models are helpful for defining mechanisms of AMP activity, their relevance to resolving how peptides damage and kill microorganisms still needs to be clarified. Moreover, many AMPs employ sophisticated and dynamic mechanisms of action to carry out their likely roles in antimicrobial host defense. Recently, it has been speculated that transmembrane pore formation is not the only mechanism of microbial killing by AMPs. In fact, several observations suggest that translocated AMPs can alter cytoplasmic membrane septum formation, reduce cell-wall, nucleic acid, and protein synthesis, and inhibit enzymatic activity. In this review, we present the structures of several AMPs as well as models of how AMPs induce pore formation. AMPs have received special attention as a possible alternative way to combat antibiotic-resistant bacterial strains. It may be possible to design synthetic AMPs with enhanced activity for microbial cells, especially those with antibiotic resistance, as well as synergistic effects with conventional antibiotic agents that lack cytotoxic or hemolytic activity.